CN202741706U - 一种连铸机浇注用水口 - Google Patents
一种连铸机浇注用水口 Download PDFInfo
- Publication number
- CN202741706U CN202741706U CN 201220270210 CN201220270210U CN202741706U CN 202741706 U CN202741706 U CN 202741706U CN 201220270210 CN201220270210 CN 201220270210 CN 201220270210 U CN201220270210 U CN 201220270210U CN 202741706 U CN202741706 U CN 202741706U
- Authority
- CN
- China
- Prior art keywords
- arc side
- tapping hole
- inner arc
- outer arc
- casting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
一种连铸机浇注用水口,在水口的左侧、右侧、内弧侧、外弧侧均设有出钢口,本实用新型根据浇注断面的宽度和厚度,左侧、右侧的出钢口与内弧侧、外弧侧的出钢口大小、出钢角度单独设定;并且,根据需要,左侧、右侧、内弧侧、外弧侧的出钢口相对结晶器中心偏置分布,在浇注超厚断面的铸坯时,使得结晶器内的钢水注流状态更合理,更有利于主流热量的分散,更有利于坯壳的均匀生长。
Description
技术领域
本实用新型涉及冶金技术领域,特别涉及超厚断面即板坯或方坯厚度大于450mm,圆坯直径大于600mm)的连铸机浇注用的一种连铸机浇注用水口。
背景技术
浸入式水口位于中间包和结晶器之间。浸入式水口的作用是防止钢水二次氧化、飞溅、控制进入结晶器内钢流在结晶器内的分布,避免热流集中,消除铸坯表面纵裂,有利于夹杂物的上浮及防止保护渣卷入。
浸入式水口参数是影响结晶器内的钢流流动、钢渣界面稳定程度和铸坯传热的重要影响因素。
传统的浸入式水口结构是只在水口的左侧、右侧设出钢口;传统的浸入式水口左侧、右侧出钢口中心线与结晶器横向中心线平行。当浇注超厚断面的铸坯时,传统的浸入式水口不利于钢水注流的流动状态,不利于分散注流热量,不利于坯壳的均匀生长等。
发明内容
为了克服上述现有技术的缺陷,本实用新型的目的在于提供一种连铸机浇注用水口,在浇注超厚断面的铸坯时,使得结晶器内的钢水注流状态更合理,更有利于主流热量的分散,更有利于坯壳的均匀生长。
为了达到上述目的,本实用新型采用的技术解决方案是:
一种连铸机浇注用水口,其特征在于,在水口的左侧、右侧、内弧侧、外弧侧均设有出钢口2、3、4、5。
左侧、右侧的出钢口2、3大小均为:宽*高为:25mm~100mm*25mm~120mm或直径为:φ30mm~φ120mm。
左侧、右侧的出钢口2、3向上倾角角度均为:0°-15°。
左侧、右侧的出钢口2、3向下倾角角度均为:0°-40°。
内弧侧、外弧侧的出钢口4、5向上倾角均为:0°-15°
内弧侧、外弧侧的出钢口4、5向下倾角均为:0°-40°。
内弧侧、外弧侧的出钢口4、5大小均为:宽*高为:25mm~100mm*25mm~120mm或直径为:φ30mm~φ120mm
左侧、右侧、内弧侧、外弧侧出钢口2、3、4、5相对结晶器中心的偏置分布角度均:0°-45°。
本实用新型根据浇注断面的宽度和厚度,左侧、右侧的出钢口与内弧侧、外弧侧的出钢口大小、出钢角度单独设定;并且,根据需要,左侧、右侧、内弧侧、外弧侧的出钢口相对结晶器中心偏置分布,在浇注超厚断面的铸坯时,使得结晶器内的钢水注流状态更合理,更有利于主流热量的分散,更有利于坯壳的均匀生长。
附图说明
图1是浸入式水口示意图,其中图1a为内弧侧、外弧侧的出钢口示意图,图1b为左侧、右侧出钢口示意图,图1c为截面图。
图2是左侧、右侧出钢口向上倾角示意图。
图3是左侧、右侧出钢口向下倾角示意图。
图4是内弧侧、外弧侧出钢口向上倾角示意图。
图5是内弧侧、外弧侧出钢口向下倾角示意图。
图6是左侧、右侧、内弧侧、外弧侧的出钢口相对结晶器中心的偏置分布示意图。
具体实施方式
下面结合附图对本实用新型的结构和主要参数作详细叙述。
参照附图1,一种连铸机浇注用水口本体1在其左侧、右侧、内弧侧、外弧侧均设有出钢口2、3、4、5;左侧、右侧的出钢口2,3大小均为:宽*高为:25mm~100mm*25mm~120mm或直径为:φ30mm~φ120mm;内弧侧、外弧侧的出钢口4、5宽*高均:25mm~100mm*25mm~120mm或直径均为:φ30mm~φ120mm。
参照附图2,左侧、右侧出钢口2,3向上倾角。左侧、右侧的出钢口2,3向上倾角角度均为:0°-15°。
参照附图3,左侧、右侧出钢口2,3向下倾角。左侧、右侧的出钢口2,3向下倾角角度均为:0°-40°。
参照附图4,内弧侧、外弧侧出钢口4,5向上倾角。内弧侧、外弧侧的出钢口4,5向上倾角角度均:0°-15°。
参照附图5,内弧侧、外弧侧出钢口4,5向下倾角。内弧侧、外弧侧的出钢口4,5向下倾角角度均为:0°-40°。
参照附图6,左侧、右侧、内弧侧、外弧侧的出钢口2、3、4、5相对结晶器中心偏置分布。左侧、右侧、内弧侧、外弧侧出钢口2、3、4、5相对结晶器中心偏置分布角度均为:0°-45°。
本实用新型的目的在于提供一种连铸机浇注用水口,在水口的左侧、右侧、内弧侧、外弧侧均设有出钢口。根据浇注断面的宽度和厚度,左侧、右侧的出钢口与内弧侧、外弧侧的出钢口大小、出钢角度单独设定;左侧、右侧、内弧侧、外弧侧的出钢口相对结晶器中心偏置分布。在浇注超厚断面的铸坯时,使得结晶器内的钢水注流状态更合理,更有利于主流热量的分散,更有利于坯壳的均匀生长。此方法具有一定的推广价值。
Claims (1)
1.一种连铸机浇注用水口,其特征在于,在水口的左侧、右侧、内弧侧、外弧侧均设有出钢口(2、3、4、5);
左侧、右侧的出钢口(2、3)大小均为:宽*高为:25mm~100mm*25mm~120mm或直径为:φ30mm~φ120mm;
左侧、右侧的出钢口(2、3)向上倾角角度均为:0°-15°;
左侧、右侧的出钢口(2、3)向下倾角角度均为:0°-40°;
内弧侧、外弧侧的出钢口(4、5)向上倾角角度均为:0°-15°;
内弧侧、外弧侧的出钢口(4、5)向下倾角角度均为:0°-40°;
内弧侧、外弧侧的出钢口(4、5)大小均为:宽*高为:25mm~100mm*25mm~120mm或直径为:φ30mm~φ120mm;
左侧、右侧、内弧侧、外弧侧出钢口(2、3、4、5)相对结晶器中心的偏置分布角度均为:0°-45°。