CN202521132U - 耐腐蚀纤维膨胀节 - Google Patents
耐腐蚀纤维膨胀节 Download PDFInfo
- Publication number
- CN202521132U CN202521132U CN 201220135773 CN201220135773U CN202521132U CN 202521132 U CN202521132 U CN 202521132U CN 201220135773 CN201220135773 CN 201220135773 CN 201220135773 U CN201220135773 U CN 201220135773U CN 202521132 U CN202521132 U CN 202521132U
- Authority
- CN
- China
- Prior art keywords
- pipe
- joint pipe
- corrosion resistant
- joint
- expansion joint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种耐腐蚀纤维膨胀节,包括左接管、右接管和拉杆,拉杆通过支架分别与左接管、右接管固定连接;左接管的右端伸入右接管内;还包括设置在左接管和右接管外面的保温层,所述保温层至少覆盖住左接管和右接管相重合的部位;所述左接管和右接管都为复合钢板,所述复合钢板由外管和位于外管内的内管组成,外管和内管紧密接触;内管内表面镀有一层耐腐蚀合金。本实用新型的耐腐蚀纤维膨胀节将膨胀节与管道内介质接触的部分分为内接管和外接管两层,在直接与管道内介质接触的内接管表面涂上一层耐腐蚀合金,可以大大减低腐蚀性介质对外接管的腐蚀,延长膨胀节的使用寿命。
Description
技术领域
本实用新型涉及一种膨胀节,特别是一种纤维膨胀节。
背景技术
纤维膨胀节可以在较小轴向安装距离上提供较大的多方向的补偿量,同时能有效消除整个系统的安装累计误差,故而被广泛采用,纤维膨胀节圈带覆盖在保温层外面,主要作用是承受管道系统压力以及来自烟气和外界的化学腐蚀,保护保温层。纤维膨胀节往往在环境恶劣的管道中使用,介质中含有各种酸性物质,如二氧化硫、三氧化硫、氯化钠等,对膨胀节的腐蚀性极强,故而膨胀节的使用寿命往往不长。
实用新型内容
本实用新型所要解决的技术问题是针对上述现有技术的不足,提供一种使用寿命较长的耐腐蚀纤维膨胀节。
为解决上述技术问题,本实用新型所采用的技术方案为:一种耐腐蚀纤维膨胀节,包括左接管、右接管和拉杆,拉杆通过支架分别与左接管、右接管固定连接;左接管的右端伸入右接管内;还包括设置在左接管和右接管外面的保温层,所述保温层至少覆盖住左接管和右接管相重合的部位;所述左接管和右接管都为复合钢板,所述复合钢板由外管和位于外管内的内管组成,外管和内管紧密接触;内管内表面镀有一层耐腐蚀合金。
作为本实用新型进一步改进的技术方案,所述所述耐腐蚀合金为奥氏体不锈钢。
本实用新型的耐腐蚀纤维膨胀节将膨胀节与管道内介质接触的部分分为内接管和外接管两层,在直接与管道内介质接触的内接管表面涂上一层耐腐蚀合金,可以大大减低腐蚀性介质对外接管的腐蚀,延长膨胀节的使用寿命。
附图说明
图1为本实用新型的结构示意图。
下面结合附图对本实用新型的具体实施方式做进一步说明。
具体实施方式
实施例1
参见图1,本耐腐蚀纤维膨胀节,包括左接管1、右接管2和拉杆7,拉杆通过支架分别与左接管1、右接管2固定连接;左接管1的右端伸入右接管2内;还包括设置在左接管1和右接管2外面的保温层3,所述保温层3至少覆盖住左接管1和右接管2相重合的部位;其特征在于:所述左接管1和右接管2都为复合钢板,所述复合钢板由外管4和位于外管4内的内管5组成,外管4和内管5紧密接触;内管内表面6镀有一层奥氏体不锈钢。本耐腐蚀纤维膨胀节在直接与管道内介质接触的内接管表面涂上一层耐腐蚀合金,可以大大减低腐蚀性介质对外接管的腐蚀,延长膨胀节的使用寿命。
Claims (2)
1.一种耐腐蚀纤维膨胀节,包括左接管(1)、右接管(2)和拉杆(7),拉杆通过支架分别与左接管(1)、右接管(2)固定连接;左接管(1)的右端伸入右接管(2)内;还包括设置在左接管(1)和右接管(2)外面的保温层(3),所述保温层(3)至少覆盖住左接管(1)和右接管(2)相重合的部位;其特征在于:所述左接管(1)和右接管(2)都为复合钢板,所述复合钢板由外管(4)和位于外管(4)内的内管(5)组成,外管(4)和内管(5)紧密接触;内管内表面(6)镀有一层耐腐蚀合金。
2.根据权利要求1所述的耐腐蚀纤维膨胀节,其特征在于:所述耐腐蚀合金为奥氏体不锈钢。