CN202356772U - Welding tool for copper tip of oxygen lance and short section of steel tube - Google Patents

Welding tool for copper tip of oxygen lance and short section of steel tube Download PDF

Info

Publication number
CN202356772U
CN202356772U CN201120479349XU CN201120479349U CN202356772U CN 202356772 U CN202356772 U CN 202356772U CN 201120479349X U CN201120479349X U CN 201120479349XU CN 201120479349 U CN201120479349 U CN 201120479349U CN 202356772 U CN202356772 U CN 202356772U
Authority
CN
China
Prior art keywords
welding
steel tube
induction heating
heating coils
welding tool
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201120479349XU
Other languages
Chinese (zh)
Inventor
刘西斌
朱惠红
马连春
方明宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shijiazhuang Juli Technology Co ltd
Original Assignee
Shijiazhuang Juli Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shijiazhuang Juli Technology Co ltd filed Critical Shijiazhuang Juli Technology Co ltd
Priority to CN201120479349XU priority Critical patent/CN202356772U/en
Application granted granted Critical
Publication of CN202356772U publication Critical patent/CN202356772U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model relates to a welding tool for a copper tip of a oxygen lance and a short section of a steel tube, comprising a frame, a work piece clamping assembly, two induction heating coils, a welding gun holder, and two non-contact temperature sensors, wherein the two induction heating coils are configured in parallel and suspended; the welding gun holder is located between the two induction heating coils; a welding gun is provided on the welding gun holder; and the two non-contact temperature sensors are configured in the positions corresponding to the induction heating coils. By using two induction heating coils to quickly heat the copper tip and the short section of the steel tube, the welding tool provided by the utility model enables two work pieces to reach different optimum preheating temperatures within a short period for further welding process. With the welding tool provided by the utility model, the operator can accurately control the preheating temperatures of the cooper tip and the short sections of the internal and external steel tubes according to the process requirements, and the welding tool can realize quick heating, reduce oxide layers and increase the weld strength, so as to improve the production efficiency while ensuring the welding quality of the oxygen lance tip.

Description

Oxygen rifle copper termination and steel tube pipe nipple welding tooling
Technical field
The utility model relates to a kind of welding tooling, specifically pipe pipe nipple or outer tube pipe nipple welding tooling in steel making oxygen lance copper termination and the steel.
Background technology
The copper termination of steel making oxygen gun sprayer and steel inner and outer pipe pipe nipple adopt argon arc welding to be welded as a whole.For reducing welding stress and the width that strengthens weld bond alloying component transition region; To guarantee welding quality; The method that adopts at present is with copper termination after the machined and steel tube pipe nipple, in electric furnace, is preheating to about 600 ℃, from electric furnace, takes out then; Be installed to special-purpose argon arc welding and meet sb. at the airport and go up welding, welding finishes and promptly accomplishes the manufacturing of product through cooling.The following drawback that this processing method exists: the one, warm is heating in electric furnace, insulation, the time needs one hour approximately, because of heat time heating time long, the oxidation bed thickness of workpiece outer surface generation, the weld seam slag inclusion is serious, influences the weld seam mechanical performance; The 2nd, copper termination and steel inner and outer pipes pipe nipple are in the hot installation down of high temperature, and the workman is not easy to operate, has the danger of being scalded; The 3rd, differ greatly because copper material and steel fusing point differ about 400 ℃, the coefficient of heat conduction, and identical preheat temperature makes workpiece welding back be prone to generation cold shut defective.
The utility model content
The utility model is used to overcome the defective of prior art and a kind of oxygen rifle copper termination and steel tube pipe nipple welding tooling of enhancing productivity with welding quality is provided
The said problem of the utility model is solved by following technical scheme:
A kind of oxygen rifle copper termination and steel tube pipe nipple welding tooling; Its special feature is that it comprises frame, workpiece mounting board assembly, two load coils, gun rack and two non-contact temperature sensors, wherein; Two load coils suspend setting side by side in midair; Gun rack is between two load coils, and gun rack is provided with welding gun, and the position of said two non-contact temperature sensors is corresponding load coil respectively.
Above-mentioned oxygen rifle copper termination and steel tube pipe nipple welding tooling, said mounting board assembly toply is made up of power chuck and rotation, and said power chuck, rotation is top and two load coil conllinear are provided with.
Above-mentioned oxygen rifle copper termination and steel tube pipe nipple welding tooling, said gun rack frame relatively moves forward and backward.
The problem that the utility model is to existing oxygen rifle copper termination and steel tube pipe nipple welding method weld strength is low, welding quality is difficult for assurance is improved; Designed a kind of special tooling that adopts Frequency Induction Heating and weld; This frock is carried out Fast Heating through two load coils to pipe nipple inside and outside copper termination and the steel tube; Make two workpiece reach different optimum Preheating Temperature at short notice respectively, and then carry out the argon arc welding.Adopt the utility model to carry out accuracy controlling by technological requirement to the preheat temperature of copper termination, steel inner and outer pipes pipe nipple, Fast Heating reduces oxide layer, improves weld strength, when having guaranteed oxygen rifle head welding quality, has improved production efficiency.
Description of drawings
Fig. 1 is the utility model structural representation.
The label of each parts is represented as follows in the accompanying drawing: 1. frame; 2. power chuck; 3-1. the first heat induced coil; 3-2. the second heat induced coil; 4. gun rack; 5. welding gun; 6. rotate top; 7. copper termination; 8. steel tube pipe nipple; 9-1. the first temperature sensor temperature probe; 9-2. the second temperature sensor temperature probe.
The specific embodiment
Referring to Fig. 1; The utility model comprises frame 1, workpiece mounting board assembly, two Frequency Induction Heating coil 3-1,3-2, gun rack 4 and two non-contact temperature sensor temperature probe 9-1,9-2 that suspend setting side by side in midair; Gun rack 4 is seated on the frame; Between two load coils, gun rack is provided with welding gun 5, and gun rack can move front and back on frame.Two non-contact temperature sensors are arranged on the frame 1, respectively corresponding two load coils in its position.Said mounting board assembly is made up of with rotation top 6 power chuck 2 that is positioned on the frame, and said power chuck, rotation is top and two load coil conllinear are provided with.
Still referring to Fig. 1, the solder side joggle of copper termination 7 and steel tube pipe nipple 8 during the utility model work, an end of copper termination are by power chuck 2 clampings, and an end of steel tube pipe nipple holds out against by rotating top 6.Be inserted in the first heat induced coil 3-1, the second heat induced coil 3-2 respectively on the pipe pipe nipple in copper termination and the steel; Two heat induced coil electricities; The workpiece temperature of measuring according to two temperatures sensor temperature probe 9-1,9-2 is the current strength of adjustment two heat induced coils in good time; The temperature of copper termination and steel pipe nipple is at the uniform velocity risen, reach the welding temperature synchronously; Start power chuck then, power chuck drives two workpiece and slowly rotates, and moves gun rack, makes welding gun alignment pieces weld seam, can weld.

Claims (3)

1. oxygen rifle copper termination and steel tube pipe nipple welding tooling; It is characterized in that it comprises frame (1), workpiece mounting board assembly, two load coils (3-1,3-2), gun rack (4) and two non-contact temperature sensors (9-1,9-2), wherein; Two load coils suspend setting side by side in midair; Gun rack is between two load coils, and gun rack is provided with welding gun (5), and the position of said two non-contact temperature sensors is corresponding load coil respectively.
2. oxygen rifle according to claim 1 copper termination and steel tube pipe nipple welding tooling is characterized in that: said mounting board assembly is made up of power chuck (2) and rotation top (6), and said power chuck, rotation is top and two load coil conllinear are provided with.
3. oxygen rifle according to claim 2 copper termination and steel tube pipe nipple welding tooling is characterized in that: said gun rack (4) frame (1) relatively moves forward and backward.
CN201120479349XU 2011-11-28 2011-11-28 Welding tool for copper tip of oxygen lance and short section of steel tube Expired - Fee Related CN202356772U (en)