CN202259466U - 一种防漏液锌镍电池盖帽 - Google Patents
一种防漏液锌镍电池盖帽 Download PDFInfo
- Publication number
- CN202259466U CN202259466U CN2011200103974U CN201120010397U CN202259466U CN 202259466 U CN202259466 U CN 202259466U CN 2011200103974 U CN2011200103974 U CN 2011200103974U CN 201120010397 U CN201120010397 U CN 201120010397U CN 202259466 U CN202259466 U CN 202259466U
- Authority
- CN
- China
- Prior art keywords
- nickel
- battery
- plated
- zinc
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供了一种防漏液锌镍电池盖帽,属于电池用具技术领域。本实用新型的技术方案是;包括:上层镀镍箔、上层排气孔、丁腈橡胶阀芯、下层镀镍铜箔、下层排气孔、下层镀镍钢箔而构成,它由上层镀镍上组件,(下层镀镍)钢(下层镀锡)铜覆合材质下组件,两组件中间放一圆柱体材质为丁腈橡胶的阀芯用于调节电池防爆压力,且在下组件覆铜镀锡排气孔表面涂覆一层自制的耐碱、憎水、透气特殊涂层。本锌镍电池盖帽结构简单,使用安装方便,能有效防止锌镍电池中的锌极与盖帽间发生的腐蚀析H2。从而使电池内压处于正常安全范围,电液不会外泄,促使电池性能进一步稳定,循环寿命大大延长,容量衰减速度减小。
Description
技术领域
本实用新型涉及的是一种专用于锌镍电池的盖帽材料、结构、电镀材料、憎水耐碱涂层,属于电池技术领域。
背景技术
在锌镍电池中,人们为了避免钢壳与锌极直接接触而将结构改成反极结构,即盖帽端与锌极接触,虽然这一结构有助于降低锌极的析H2,但不能完全杜绝这一现象的发生,因此在电池使用与贮存期间,现有材质、结构的盖帽将不可避免与锌电极进行腐蚀反应从而析出大量的H2气,不间断地使锌极和电液自行消耗,即Fe(Ni)/KOH水溶液/Zn,这样会导致电池内部压力急骤上升直至盖帽安全阀开启。电液会随着使用次数递增又或者贮存时间延长大量流失。从而使电池使用寿命缩短、自放电大、容量衰减又不可逆。达不到实际使用要求,在各类的文献中已采用了各种方法与措施来延缓或抑制H2气的产生或者加强盖帽的结构、表面防腐涂层改进,但最终效果并不理想。
发明内容
本实用新型的目的在于克服现有技术存在的不足,而提供一种结构简单,使用安装方便,能有效防止锌镍电池中的锌极与盖帽间发生的腐蚀析H2。从而使电池内压处于正常安全范围,电液不会外泄,促使电池性能进一步稳定,循环寿命大大延长,容量衰减速度减小。
本实用新型的目的是通过如下技术方案来完成的,它主要由上组件上层镀镍钢箔(2)和上层排气孔(3),下组件底层镀镍铜箔(7)和底层镀镍钢箔(5),上下组件中间放一圆柱体材质丁腈橡胶阀芯(4)用于调节电池防爆压力,且在底层排气孔(6)表面涂覆一层自制的自制防水、透气、憎水、耐碱涂层(1)。
所述上组件为0.2mm钢带,按尺寸成型后其表面镀镍层厚度为3-5μm。部件上有2-5个直径为ф1-2mm排气孔,均分于组件之上。
所述下组件材质由0.4mm镀镍钢箔与材质为0.4mm镀锡铜箔(T2)通过加热,加压碾压覆合而成。钢箔镀镍厚度为3-5μm,铜箔镀锡厚度为1-2μm。按要求的尺寸冲压成型。位于中间部位有一个直径为ф2-8mm排气孔。
所述两个组件之间有一个材质为丁腈橡胶的阀芯,其形状为圆柱体,主要作用调节电池内部的防爆压力。
所述盖帽是将三个主要部件即上组件、下组件、圆柱体丁腈橡胶的阀芯先通过组装 (圆柱体丁腈橡胶的阀芯位于组件中间部位),再通过贮能焊机将上、下组件进行牢固焊接。
所述下组件排气孔位于铜层镀锡表面涂覆一层自制耐碱、憎水、透气涂层。
本实用新型与现有技术相比,具有结构简单,使用安装方便,能有效防止电池因长期贮存、循环使用过程中锌极与盖帽间腐蚀析H2反应发生,从而有效降低了电池内压、降低电池自放电、提高电池循环寿命与容量可恢复性。
附图说明
图1是本实用新型的整体示意图
具体实施方式
下面将结合附图对本实用新型做详细的介绍:附图1所示,本实用新型采用0.2mm钢质带箔通过冲压成型后在其表层镀镍3-5μm的上组件。且在其部件上均匀分布有2-4个直径为ф1-2mm排气孔,用于电池内压过高时对外排泄气体。
本实用新型所述下组件由一层厚0.4mm钢质带箔表面镀镍厚3-5μm与一层厚0.4mm铜质(T2)带箔表面镀锡厚度1-2μm通过加热,加压形成覆合带材,以后根据要求尺寸冲压成下组件.且部件中间部位有一直径为ф2-8mm排气孔。
所述圆柱体丁腈橡胶阀芯根据电池防爆压力泄气要求做成一定的高度,主要作用于调节电池内压,当压力达到一定值,阀芯受内压作用而变形,释放出气体,当内压趋于稳定时阀芯恢复原状阻止气体外泄。
所述的覆合材质铜箔镀锡下组件与镀镍钢箔的下组件,在两组件之间放置已经按要求制成的圆柱体丁腈橡胶阀芯,再将两组件用贮能焊机进行牢固焊接,制成的盖帽由于与锌极联部位采用了铜层表面镀锡,又于下组件的排气孔上及四周用自制憎水,透气,耐碱的特殊涂层进行处理,因Zn在KOH溶液中其平衡电极电位,
φ平=φ°+0.059/2.1g.az-o.aH2O/a2oH- φ°=-1.245V
另又因为铜电位略高于Zn,即使ZnO初期会在Cu箔表面发生阴极还原,一旦铜表面全部被锌覆盖这种反应就会停止.考虑到延缓,抑制这种情况的发生在其表层镀Sn,这一措施对抑制锌极腐蚀将起到非常好的作用.通过以上的步骤锌镍电池的析氢问题得到很好解决,电池内压处于较低的范围漏液问题得以控制,自放电减小贮存性能得以提高,锌极自耗得到控制,电池循环寿命更长,容量衰减更小,电池性能更稳定。
Claims (1)
1.一种防漏液锌镍电池盖帽,包括有上层镀镍箔(2)、上层排气孔(3)、丁腈橡胶阀芯(4)、下层镀镍铜箔(5)、下层排气孔(6)、下层镀镍钢箔(7)、自制防水、透气、憎水、耐碱涂层(1);其特征在于:上组件上层镀镍箔(2),下组件下层镀镍铜箔(5)和下层镀镍钢箔(7),上下组件中间放一圆柱体材质丁腈橡胶阀芯(4)用于调节电池防爆压力,且在下层覆铜镀锡排气孔表面涂覆一层自制的自制防水、透气、憎水、耐碱涂层(1)。