CN202108145U - Ardealite wall brick - Google Patents
Ardealite wall brick Download PDFInfo
- Publication number
- CN202108145U CN202108145U CN2011201942596U CN201120194259U CN202108145U CN 202108145 U CN202108145 U CN 202108145U CN 2011201942596 U CN2011201942596 U CN 2011201942596U CN 201120194259 U CN201120194259 U CN 201120194259U CN 202108145 U CN202108145 U CN 202108145U
- Authority
- CN
- China
- Prior art keywords
- ardealite
- wall body
- wall brick
- body brick
- tenon
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model discloses an ardealite wall brick, which comprises a rectangular ardealite wall brick body. Two top surfaces of the wall brick body are respectively provided with a groove and/ or a tenon. The main raw material of the ardealite wall brick is ardealite. The ardealite wall brick is used for a non-bearing wall and has the advantages of being firm in bonding, low in cost, beneficial for straight-line laying and the like. Compared with traditional wall bricks, bonding between bricks is firm, and walls are more stable due to the groove and/ or the tenon arranged on the top faces of the wall brick body. Meanwhile, a large amount of ardealite is utilized so that an effective way is provided for comprehensive utilization of the industrial waste residue of ardealite in recycling manner.
Description
Technical field
The utility model belongs to building material technical field, is specifically related to a kind of ardealite wall body brick.
Background technology
Ardealite is the industrial by-products that discharges in the production process of phosphoric acid, and 1 ton of phosphoric acid of every production will be discharged 5 tons of ardealites, and along with the development of China's chemical industry, the discharge value of ardealite constantly increases.The main thing phase constituent of its of ardealite is calcium sulphate dihydrate (CaSO
42H
2O), wherein also contain small amount of impurities, like solvable phosphorus, eutectic phosphorus, organic matter, solvable fluorine etc.Impurity is to gypsum time of setting and intensity all causing adverse effect, and is difficult to remove, therefore; China's comprehensive utilization of phosphogypsum rate is very low at present; Many mode simple process with air storage or landfill, not only the appropriation of land resource also can cause the pollution of atmosphere and water environment through wind and weather.
Traditional wall body brick is complete cuboid, and the big face of brick, bar face, end face are flat surface, and brick and brick only depend on mortar bonding in the masonry panel, and resistance to overturning is bad.
Summary of the invention
The purpose of the utility model is to provide a kind of ardealite wall body brick, have agree with firmly, cost of production straight line low, that help body of wall builds by laying bricks or stones.
The above-mentioned purpose of the utility model realizes through following technical scheme: a kind of ardealite wall body brick, comprise rectangle ardealite wall body brick, and on two end faces of wall body brick, be respectively equipped with groove and/or tenon.
Groove on each end face of the utility model or tenon are two, and the size of said groove and tenon is identical with shape of cross section.
The cross section of described groove of the utility model and tenon promptly is preferably equilateral triangle in the projection of shape perpendicular to big face direction, and the length of side of each groove and tenon is identical.
The length of side of the described equilateral triangle of the utility model is preferably 5-15mm.
The utility model ardealite wall body brick is being cementitious materials through the ardealite of 150 ℃ of calcinings, carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Rubble, stone flour are respectively slightly, fines; Adding Admixture glauber salt, water glass, calcium formate, calcium lignosulfonate etc. mix with water and process slip; Inject mould vibration extrusion forming, treat to make after the cementitious materials sclerosis.
The utility model has the advantages that:
(1) the ardealite wall body brick that provides of the utility model has and advantage such as agrees with firmly, cost of production straight line low, that help wall body brick is built by laying bricks or stones;
(2) wall body brick that adopts this programme wall body brick to make is compared with traditional body of wall, because the end face of wall body brick is provided with groove and/or tenon, makes agreeing with firmly between brick and the brick, and body of wall is more firm;
(3) the utility model utilizes ardealite in a large number, for the comprehensive utilization of resources of industrial residue-ardealite provides effective way.
Description of drawings
Fig. 1 is provided with groove is provided with the walltile of tenon on another end face structural representation on one of them end face of wall body brick in the utility model specific embodiment 1;
Fig. 2 is the vertical view of Fig. 1;
Fig. 3 is the structural representation that on two end faces of wall body brick, is equipped with the walltile of groove in the utility model specific embodiment 2;
Fig. 4 is the structural representation that on two end faces of wall body brick, is equipped with the walltile of tenon in the utility model specific embodiment 3.
The specific embodiment
Shown in accompanying drawing 1-2, a kind of ardealite wall body brick comprises rectangle ardealite wall body brick 1; This ardealite wall body brick 1 is a primary raw material with ardealite, carbide slag, hydraulic admix ture; Rubble and stone flour are respectively slightly, fines, are equipped with Admixtures such as glauber salt, water glass, calcium formate, calcium lignosulfonate and process, and size is preferably built conventional with being of a size of 240 * 115 * 53mm; Other size also can; It has big face 2, end face 3 and bar face 4, on one of them end face of wall body brick, is provided with two grooves 5 and on another end face, is provided with two tenons 6, and two grooves 5 on each end face and the cross section of tenon 6 are equilateral triangle in the projection of shape perpendicular to big face direction promptly; The length of side of each tenon 6 is all identical, and its length of side a is 8mm.
Wherein this ardealite wall body brick is being cementitious materials through the ardealite of 150 ℃ of calcinings, carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Rubble, stone flour are respectively slightly, fines; Adding Admixture glauber salt, water glass, calcium formate, calcium lignosulfonate etc. mix with water and process slip; Inject mould vibration extrusion forming, treat to make after the cementitious materials sclerosis.
Ardealite is through 150 ℃ of calcination processing; Can make it make the semi-hydrated gypsum with gelling by the dihydrate gypsum dehydration, the ardealite in the preparation process after the calcining is a powder, mixes with carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Add water and mix and stir, in product, make cementitious materials.
Shown in accompanying drawing 3, a kind of ardealite wall body brick comprises rectangle ardealite wall body brick 1; This ardealite wall body brick 1 is a primary raw material with ardealite, carbide slag, hydraulic admix ture; Rubble and stone flour are respectively slightly, fines, are equipped with Admixtures such as glauber salt, water glass, calcium formate, calcium lignosulfonate and process, and size is preferably built conventional with being of a size of 240 * 115 * 115mm; Other size also can; It has big face 2, end face 3 and bar face 4, and this ardealite wall body brick is to be equilateral triangle in the projection of shape perpendicular to big face direction promptly at the cross section that is equipped with four grooves 5 on 5, two end faces 3 of two grooves on each end face 3 of wall body brick; The length of side of each groove 5 is all identical, and its length of side a is 15mm.
Wherein this ardealite wall body brick is being cementitious materials through the ardealite of 150 ℃ of calcinings, carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Rubble, stone flour are respectively slightly, fines; Adding Admixture glauber salt, water glass, calcium formate, calcium lignosulfonate etc. mix with water and process slip; Inject mould vibration extrusion forming, treat to make after the cementitious materials sclerosis.
Ardealite is through 150 ℃ of calcination processing; Can make it make the semi-hydrated gypsum with gelling by the dihydrate gypsum dehydration, the ardealite in the preparation process after the calcining is a powder, mixes with carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Add water and mix and stir, in product, make cementitious materials.
Shown in accompanying drawing 4, a kind of ardealite wall body brick comprises rectangle ardealite wall body brick 1; This ardealite wall body brick 1 is a primary raw material with ardealite, carbide slag, hydraulic admix ture, and rubble and stone flour are respectively slightly, fines, are equipped with Admixtures such as glauber salt, water glass, calcium formate, calcium lignosulfonate and process; Be of a size of 240 * 115 * 115mm; It has big face 2, end face 3 and bar face 4, and this ardealite wall body brick is to be equilateral triangle in the projection of shape perpendicular to big face direction promptly at the cross section that is equipped with four tenons 6 on 6, two end faces 3 of two tenons on each end face of wall body brick; The length of side of each tenon 6 is all identical, and its length of side a is 10mm.
Wherein this ardealite wall body brick is being cementitious materials through the ardealite of 150 ℃ of calcinings, carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Rubble, stone flour are respectively slightly, fines; Adding Admixture glauber salt, water glass, calcium formate, calcium lignosulfonate etc. mix with water and process slip; Inject mould vibration extrusion forming, treat to make after the cementitious materials sclerosis.
Ardealite is through 150 ℃ of calcination processing; Can make it make the semi-hydrated gypsum with gelling by the dihydrate gypsum dehydration, the ardealite in the preparation process after the calcining is a powder, mixes with carbide slag, hydraulic admix ture quick hardening sulphoaluminate cement etc.; Add water and mix and stir, in product, make cementitious materials.
The utility model is not limited in the above-mentioned specific embodiment scope, and those skilled in the art are according to the description of preamble, just can find different adjustment schemes according to needs separately, and these adjustment all should be in the scope of the claims by the appended claims herein.
Claims (4)
1. an ardealite wall body brick comprises rectangle ardealite wall body brick, it is characterized in that: on two end faces of wall body brick, be respectively equipped with groove and/or tenon.
2. ardealite wall body brick according to claim 1 is characterized in that: groove on each end face or tenon are two, and the cross section of said groove and tenon is identical.
3. ardealite wall body brick according to claim 1 and 2 is characterized in that: the cross section of described groove and tenon be shaped as equilateral triangle.
4. ardealite wall body brick according to claim 3 is characterized in that: the length of side of described equilateral triangle is 5-15mm.