CN202030838U - 铝电解阳极装置 - Google Patents

铝电解阳极装置 Download PDF

Info

Publication number
CN202030838U
CN202030838U CN2011201118642U CN201120111864U CN202030838U CN 202030838 U CN202030838 U CN 202030838U CN 2011201118642 U CN2011201118642 U CN 2011201118642U CN 201120111864 U CN201120111864 U CN 201120111864U CN 202030838 U CN202030838 U CN 202030838U
Authority
CN
China
Prior art keywords
anode
aluminum electrolysis
charcoal
carbon
bowl
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011201118642U
Other languages
English (en)
Inventor
朱振国
谭春耕
谭春雷
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zibo Chungeng Industry & Trade Co Ltd
Original Assignee
Zibo Chungeng Industry & Trade Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zibo Chungeng Industry & Trade Co Ltd filed Critical Zibo Chungeng Industry & Trade Co Ltd
Priority to CN2011201118642U priority Critical patent/CN202030838U/zh
Application granted granted Critical
Publication of CN202030838U publication Critical patent/CN202030838U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供了一种铝电解阳极装置,包括阳极炭块,阳极炭块上设置炭碗,阳极钢爪置入炭碗内,阳极钢爪与炭碗间的空腔内安装炭素料,炭素料包覆阳极钢爪下部。本实用新型采用炭素料替代磷生铁,从而彻底改变了铝电解阳极装置的生产环境,本实用新型的生产过程无任何污染,耗能极低,对操作人员的身体无任何损害,并且,由于炭素料与阳极钢爪的接触面积增大,从而增加了导电面积,保护了铝电解时电解质易冲刷腐蚀钢爪,从而延长了铝电解阳极装置的使用寿命等。

Description

铝电解阳极装置
技术领域
[0001] 本实用新型涉及铝电解生产设备,是一种铝电解阳极装置。
背景技术
现有的铝电解阳极设置是由阳极炭块、阳极导杆和阳极钢爪构成,采用磷生铁水浇铸冷却后使阳极钢爪与阳极炭块连接在一起。这种结构的铝电解阳极装置存在较多不足:溶化磷生铁时需要在频炉或冲天炉中加热至130℃以上,耗电量极大,并且在溶化过程中产生大量的氧化碳等有害气体,严重污泥环境,并对操作人员的身体健康造成较大的损害;铝电解阳极装置在铝电解的生产过程中,当阳极氧化及电解质水平上涨时,易造成磷生铁被冲刷熔化掉,导致原铝质量下降,并使铝电解阳极装置的使用寿命缩短等。
实用新型内容
本实用新型的目的是提供一种铝电解阳极装置,它改变阳极炭块与阳极钢爪的连接,从而解决现有技术的不足。
本实用新型为实现上述目的,通过以下技术方案实现:铝电解阳极装置,包括阳极炭块,阳极炭块上设置炭碗,阳极钢爪置入炭碗内,阳极钢爪与炭碗间的空腔内安装炭素料,炭素料包覆阳极钢爪下部。炭素料的顶面高于阳极炭块的顶面。炭素料的顶面高于阳极炭块的顶面距离为20-40毫米。炭素料位于阳极钢爪底面与炭碗间的高度为10-20毫米。
本实用新型采用炭素料替代磷生铁,从而彻底改变了铝电解阳极装置的生产环境,本实用新型的生产过程无任何污染,耗能极低,对操作人员的身体无任何损害,并且,由于炭素料与阳极钢爪的接触面积增大,从而增加了导电面积,保护了铝电解时电解质易冲刷腐蚀钢爪,从而延长了铝电解阳极装置的使用寿命等。
附图说明
附图1是本实用新型结构示意图。
具体实施方式
对照附图及实施例对本实用新型做进一步说明。
本实用新型为了完成发明目的,达到本实用新型所述的优点,提供的技术方案中的实施例是:如图1所示,图中4是阳极炭块,阳极炭块4上设置炭碗5,阳极钢爪3置入炭碗5内,阳极钢爪3与炭碗5间的空腔内安装炭素料6,炭素料6包覆阳极钢爪3下部。
本实用新型为了增加导电面积,可以使炭素料6的顶面高于阳极炭块4的顶面。
本实用新型为了增加导电面积,并达到较好效果的设计方案为:将炭素料6的顶面高于阳极炭块4的顶面距离H设计为20-40毫米。
本实用新型的进一步方案是为了增加炭碗5与阳极钢爪3的粘接牢固性,将炭素料6位于阳极钢爪3底面与炭碗5间的高度H1设计为10-20毫米。
本实用新型所述的炭素料6是由人造石墨60%、金属屑30%和树脂结合剂10%混合后采用压力压实制成。
图中,1是阳极导杆,2是阳极钢爪连接筋。

Claims (4)

1.铝电解阳极装置,包括阳极炭块(4),阳极炭块(4)上设置炭碗(5),阳极钢爪(3)置入炭碗(5)内,其特征在于:阳极钢爪(3)与炭碗(5)间的空腔内安装炭素料(6),炭素料(6)包覆阳极钢爪(3)下部。
2.根据权利要求1所述的铝电解阳极装置,其特征在于:炭素料(6)的顶面高于阳极炭块(4)的顶面。
3.根据权利要求1所述的铝电解阳极装置,其特征在于:炭素料(6)的顶面高于阳极炭块(4)的顶面距离(H)为20-40毫米。
4.根据权利要求1或2所述的铝电解阳极装置,其特征在于:炭素料(6)位于阳极钢爪(3)底面与炭碗(5)间的高度(H1)为10-20毫米。
CN2011201118642U 2011-04-15 2011-04-15 铝电解阳极装置 Expired - Fee Related CN202030838U (zh)