CN201955152U - 敲击法测试混凝土抗冻试件自振频率的系统 - Google Patents
敲击法测试混凝土抗冻试件自振频率的系统 Download PDFInfo
- Publication number
- CN201955152U CN201955152U CN2011200573931U CN201120057393U CN201955152U CN 201955152 U CN201955152 U CN 201955152U CN 2011200573931 U CN2011200573931 U CN 2011200573931U CN 201120057393 U CN201120057393 U CN 201120057393U CN 201955152 U CN201955152 U CN 201955152U
- Authority
- CN
- China
- Prior art keywords
- vibration
- test piece
- concrete
- transducer
- hammering method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种敲击法测试混凝土抗冻试件自振频率的系统,它包括与混凝土试件相配合的微型击振锤、粘接于混凝土试件上的振动传感器和振动测试分析仪,振动传感器与振动测试分析仪连接;振动传感器为加速度传感器;振动传感器通过耦合剂粘接在混凝土试件上。本实用新型提供的敲击法测试混凝土抗冻试件自振频率的系统,可以克服现有测试方法的不足,结构简单、操作快捷、测值准确;振动传感器通过耦合剂粘接在混凝土试件上,不易松动,接收振动稳定;振动传感器采用加速度传感器,适用频率范围包含所测混凝土试件的自振频率。
Description
技术领域
本实用新型涉及一种自振频率测试系统,尤其是一种敲击法测试混凝土抗冻试件自振频率的系统。
背景技术
在测试混凝土的抗冻性能试验中,需要测出混凝土试件在经受不同次数冻融循环时的自振频率,用以计算试件的相对动弹性模量。目前,常用的测试自振频率方法是扫频方法,在混凝土试件的一端用击振器有规律产生一系列单一频率的振动,同时在混凝土试件的另一端用接收器接收试件传播过来的这些振动。当击振频率和试件的自振频率相等时引起试件共振,此时振幅和相位都有明显的变化,观察到这些变化时即认为此时击振器产生的振动频率就是试件的自振频率。该方法需要能够有规律产生多个单一频率振动的击振装置,结构复杂;测试过程中,击振装置、接收装置和试件的接触紧密程度会发生变化,从而引起测值不准确。
发明内容
本实用新型所要解决的技术问题是提供一种敲击法测试混凝土抗冻试件自振频率的系统,可以克服现有测试方法的不足,结构简单、操作快捷、测值准确。
为解决上述技术问题,本实用新型所采用的技术方案是:一种敲击法测试混凝土抗冻试件自振频率的系统,它包括与混凝土试件相配合的微型击振锤、粘接于混凝土试件上的振动传感器和振动测试分析仪,振动传感器与振动测试分析仪连接。
振动传感器为加速度传感器。
振动传感器通过耦合剂粘接在混凝土试件上。
本实用新型提供的敲击法测试混凝土抗冻试件自振频率的系统,由于微型击振锤可在操作者的手动操作下使混凝土试件产生振动,并且其自重较小,不会破坏混凝土试件的结构,振动测试分析仪可将振动传感器采集到的振动时域波形通过傅立叶变换转换为频率—幅值波形,显示频率范围宽、测值准确,可以克服现有测试方法的不足,结构简单、操作快捷;振动传感器通过耦合剂粘接在混凝土试件上,不易松动,接收振动稳定;振动传感器采用加速度传感器,适用频率范围包含所测混凝土试件的自振频率。
附图说明
下面结合附图和实施例对本实用新型作进一步说明:
图1为本实用新型的结构示意图。
具体实施方式
如图1所示,一种敲击法测试混凝土抗冻试件自振频率的系统,它包括与混凝土试件4相配合的微型击振锤1、粘接于混凝土试件4上的振动传感器3和振动测试分析仪2,振动传感器3与振动测试分析仪2连接。
振动传感器3为加速度传感器。
振动传感器3通过耦合剂粘接在混凝土试件4上。
本实用新型的使用过程如下:
测试时,先清理棱柱体混凝土试件4的表面,然后将混凝土试件4侧面向上,平稳放在柔软的衬垫上;再将振动传感器3置于混凝土试件4一端的上表面,振动传感器3与混凝土试件4表面通过耦合剂(如凡士林或黄油)粘接在一起。
将振动传感器3与振动测试分析仪2连接,并打开振动测试分析仪2;再用微型击振锤1轻敲混凝土试件4的另一端上表面。
振动测试分析仪2接收到振动时域波形后,将波形进行傅立叶分析,得到频率—幅值波形,在混凝土试件4通常的自振频率范围内,找出最大幅值对应的频率即为试件的自振频率。
Claims (3)
1. 一种敲击法测试混凝土抗冻试件自振频率的系统,其特征在于:它包括与混凝土试件(4)相配合的微型击振锤(1)、粘接于混凝土试件(4)上的振动传感器(3)和振动测试分析仪(2),振动传感器(3)与振动测试分析仪(2)连接。
2.根据权利要求1所述的敲击法测试混凝土抗冻试件自振频率的系统,其特征在于:振动传感器(3)为加速度传感器。
3.根据权利要求1或2所述的敲击法测试混凝土抗冻试件自振频率的系统,其特征在于:振动传感器(3)通过耦合剂粘接在混凝土试件(4)上。