CN201842998U - Regenerated protein fiber fabric - Google Patents

Regenerated protein fiber fabric Download PDF

Info

Publication number
CN201842998U
CN201842998U CN2010205580405U CN201020558040U CN201842998U CN 201842998 U CN201842998 U CN 201842998U CN 2010205580405 U CN2010205580405 U CN 2010205580405U CN 201020558040 U CN201020558040 U CN 201020558040U CN 201842998 U CN201842998 U CN 201842998U
Authority
CN
China
Prior art keywords
lining
azlon
enhancement layer
protein fiber
basic unit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010205580405U
Other languages
Chinese (zh)
Inventor
朱根兴
施恩
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Textile Technology Co., Ltd. Zhejiang Europe and America
Original Assignee
TONGXIANG AUMERRY TEXTILE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGXIANG AUMERRY TEXTILE CO Ltd filed Critical TONGXIANG AUMERRY TEXTILE CO Ltd
Priority to CN2010205580405U priority Critical patent/CN201842998U/en
Application granted granted Critical
Publication of CN201842998U publication Critical patent/CN201842998U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model discloses a regenerated protein fiber fabric which can be widely used on exterior decorations of all kinds of materials such as dresses, shoes, caps and sofas and other products. The regenerated protein fiber fabric is characterized in that the fabric comprises three layers, i.e. a substrate, a reinforcing layer and a surface coating layer, wherein the substrate and the reinforcing layer are compositely formed through hydro-entanglement, the substrate is coated with the surface coating layer and is made from protein fiber, the reinforcing layer is made of polyester fibers, cotton fibers or polyester-cotton blended fibers, the surface coating layer is made of polyurethane resin, and the weight ratio of the polyester fibers of the reinforcing layer is 10 percent to 20 percent. The regenerated protein fiber fabric has the advantages that the range of raw materials is wide, the production cost is low, the environment is protected and the sustainable development is realized.

Description

The azlon lining
Technical field
The utility model relates to a kind of regenerated protein lining, is widely used in clothes, and shoes and hats on the extraneous adornment of various materials such as sofa, also can use on other products.
Background technology
Product originally is the heat molten type nonwoven fabric, press combination by the glue hot melt between each aspect material, its shortcoming is the recovery of can not degrading fully, because the cause of glue exists certain pollution to environment, and the ABRASION RESISTANCE and the mechanical strength of hot melt nonwoven lining are not enough, therefore also can influence service life.
The utility model content
Technical problem to be solved in the utility model is to overcome deficiency of the prior art and provide a kind of raw material extensive, and production cost is lower, the azlon lining of environmental protection, sustainable development.
The technical scheme in the invention for solving the above technical problem is: this azlon lining, its characteristics are: described lining comprises three layers, be respectively basic unit, enhancement Layer and face coat, basic unit and enhancement Layer sting composite molding by water, be coated with face coat in the basic unit, basic unit is an azelon, and enhancement Layer adopts polyster fibre, cotton fiber or polyester cotton blending fiber, face coat is a polyurethane resin, and the polyster fibre weight ratio of enhancement Layer is 10% ~ 20%.
Azelon fineness described in the utility model is 1.44dtex ~ 2.15dtex, and length range is 10mm-20mm.
Lining Gram Mass described in the utility model is 300 grams ~ 500 grams.
Groundwork thickness described in the utility model is 1.0cm ~ 1.2cm.
Enhancement Layer thickness described in the utility model is 0.1cm ~ 0.5cm.
Face coat thickness described in the utility model is 0.01cm ~ 0.2cm.
The utility model compared with prior art has the following advantages: 1, be to form with discarded various animals and plants materials processings, as ox-hide, sheepskin, cotton etc., it is extensive to have raw material sources, environmental protection, advantages such as sustainable development.2, the various physical properties that have general lining, cutting flexibly, graceful magnificent, reduce environmental pollution, the field of development is extensive.3, by the composite molding of water thorn, environment friendly and pollution-free, the lining long service life, and can degrade fully.
Figure of description
Fig. 1 is the utility model lining schematic cross-section.
The specific embodiment
Referring to Fig. 1, the utility model comprises three layers, be respectively basic unit 1, enhancement Layer 2 and face coat 3, basic unit 1 and enhancement Layer 2 are by the composite molding of water thorn, be coated with face coat 3 in the basic unit 1, basic unit 1 is an azelon, as the leftover bits and pieces of ox-hide, the azelon fineness is 1.44dtex ~ 2.15dtex, and length range is 10mm-20mm.Basic unit's 1 thickness is 1.0cm ~ 1.2cm.
Enhancement Layer 2 adopts polyster fibre or cotton fiber or polyester cotton blending fiber, and the polyster fibre fineness is 0.8dtex ~ 1.23 dtex, and enhancement Layer 2 thickness are 0.1cm ~ 0.5cm.The polyster fibre weight of enhancement Layer accounts for about 10% ~ 20% of whole fabric.
Face coat 3 is a polyurethane resin, and the thickness of face coat 3 is 0.01cm ~ 0.2cm.
The whole Gram Mass of lining is 300 grams ~ 500 grams, is generally about 436 grams.
In addition, need to prove, allly conceive equivalence or the simple change that described structure, feature and principle are done, be included in the protection domain of the utility model patent according to the utility model patent.The utility model person of ordinary skill in the field can make various modifications or replenishes or adopt similar mode to substitute described specific embodiment; only otherwise depart from structure of the present utility model or surmount the defined scope of these claims, all should belong to protection domain of the present utility model.

Claims (6)

1. azlon lining, it is characterized in that: described lining comprises three layers, be respectively basic unit, enhancement Layer and face coat, basic unit and enhancement Layer sting composite molding by water, be coated with face coat in the basic unit, basic unit is an azelon, and enhancement Layer adopts polyster fibre, cotton fiber or polyester cotton blending fiber, face coat is a polyurethane resin, and the polyster fibre weight ratio of enhancement Layer is 10% ~ 20%.
2. azlon lining according to claim 1 is characterized in that: described azelon fineness is 1.44dtex ~ 2.15dtex, and length range is 10mm-20mm.
3. azlon lining according to claim 1 is characterized in that: described lining Gram Mass is 300 grams ~ 500 grams.
4. azlon lining according to claim 1 is characterized in that: described groundwork thickness is 1.0cm ~ 1.2cm.
5. azlon lining according to claim 1 is characterized in that: described enhancement Layer thickness is 0.1cm ~ 0.5cm.
6. azlon lining according to claim 1 is characterized in that: described face coat thickness is 0.01cm ~ 0.2cm.
CN2010205580405U 2010-10-13 2010-10-13 Regenerated protein fiber fabric Expired - Fee Related CN201842998U (en)