CN201825990U - Continuous annealing cooling device for bright band steel - Google Patents

Continuous annealing cooling device for bright band steel Download PDF

Info

Publication number
CN201825990U
CN201825990U CN2010205458545U CN201020545854U CN201825990U CN 201825990 U CN201825990 U CN 201825990U CN 2010205458545 U CN2010205458545 U CN 2010205458545U CN 201020545854 U CN201020545854 U CN 201020545854U CN 201825990 U CN201825990 U CN 201825990U
Authority
CN
China
Prior art keywords
band steel
continuous annealing
cooling device
cooling
gas
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010205458545U
Other languages
Chinese (zh)
Inventor
沈贤法
施良
赵文扬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Jiulong Kitchenware Group Co., Ltd
Original Assignee
HANGZHOU JIULONG KITCHEN TOOLS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HANGZHOU JIULONG KITCHEN TOOLS CO Ltd filed Critical HANGZHOU JIULONG KITCHEN TOOLS CO Ltd
Priority to CN2010205458545U priority Critical patent/CN201825990U/en
Application granted granted Critical
Publication of CN201825990U publication Critical patent/CN201825990U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model relates to a cooling device, in particular to a continuous annealing cooling device for bright band steel, which belongs to the technical field of metallurgy rolling. The continuous annealing cooling device comprises the band steel which passes through the continuous annealing cooling device as well as at least two cooling chambers, sealing rollers, conveying rollers, gas pipeline systems, gas nozzles and heat exchangers, wherein each cooling chamber comprises an upper cavity and a lower cavity; the band steel is arranged between the upper cavity and the lower cavity; the sealing rollers are arranged at the end parts of the upper cavity and the lower cavity; the conveying rollers are arranged between the sealing rollers; the sealing rollers and the conveying rollers are contacted with the band steel; the gas pipeline systems pass through the cooling chambers and are provided with the gas nozzles; the gas nozzles correspond to the band steel; and the heat exchangers are arranged among the gap pipeline systems. The continuous annealing cooling device is simple in structure, and is capable of improving the product quality, reducing the production cost, obviously reducing energy consumption, and enhancing the utilization rate of the energy consumption.

Description

A kind of euphotic zone steel continuous annealing refrigerating unit
Technical field
The utility model is a kind of refrigerating unit, and particularly a kind of euphotic zone steel continuous annealing refrigerating unit belongs to the metallurgy rolling technical field.
Background technology
Cold rolled strip of the prior art can cause the inner defectives such as bigger internal stress and internal fissure that exist of band steel after the rate that presses down the greatly processing of cold-rolling process.By recrystallization annealing, can eliminate cold rolling work hardening, improve moulding and toughness, remove unrelieved stress, and eliminate the partial interior defective.
The tradition annealing process be because need heat and be incubated to the band steel, usually causes the band steel secondary oxidation at high temperature behind the pickling descaling, and the surface luster of steel is with in forfeiture, even produces oxide skin again.
For addressing the above problem, produced technology such as annealing furnace by the reducing gas protection, guarantee with steel not oxidized under the high temperature of annealing process with anaerobic or reducing atmosphere.Even if but in reducing atmosphere, the high temperature of annealing process still can cause the emulsion of steel strip surface when cold rolling and ROLLING OIL carbonization to decompose, and produces " black-tape " defective of belt steel surface.
Be to remove the emulsion and the ROLLING OIL of steel strip surface, often need before annealing, increase off-line or online degreasing system, or the emitted dose of increasing shielding gas causes the serious waste of the energy and shielding gas to blow emulsion and ROLLING OIL off.
Summary of the invention
The utility model mainly is to solve the deficiencies in the prior art; provide a kind of and be difficult to avoid " black-tape " defective in order to overcome traditional technology; and waste energy and the problem of shielding gas; a kind of euphotic zone steel continuous annealing refrigerating unit; separate a plurality of independently cooling rooms by sealed roller; and in each cooling room, adopt different process for cooling, with the cooling and the heat insulation effect of raising continuous annealing, and realize the effect energy-conservation and loss of minimizing shielding gas.
Above-mentioned technical problem of the present utility model is mainly solved by following technical proposals:
A kind of euphotic zone steel continuous annealing refrigerating unit, comprise the band steel, the band steel is by the continuous annealing refrigerating unit, the continuous annealing refrigerating unit comprises at least two cooling rooms, sealed roller, conveying roller, gas pipeline system, gas jet and interchanger, described cooling room comprises upper plenum and following cavity, be provided with the band steel between upper plenum and following cavity, the end of upper plenum and following cavity is provided with sealed roller, be provided with conveying roller between described sealed roller, sealed roller and conveying roller contact with the band steel, and gas pipeline system is provided with gas jet by cooling room in the gas pipeline system, gas jet is corresponding with the band steel, is provided with interchanger between described gas pipeline system.The band steel through pickling, cold rolling, annealing, the heating, the insulation after, enter refrigerating work procedure.Cool furnace of the present utility model is by high-speed gas injection cooling down high-temperature band steel; and cool furnace is divided into a plurality of independently cooling rooms by interior partition wall and sealed roller; be equipped with independently cooling gas nozzle and gas pipeline system in each cooling room; make the cold rolled strip steel production merchant can adjust composition, flow and the flow velocity of each cooling room internal cooling gas respectively at the cold rolled strip of different size and unlike material; to optimize the annealing process for cooling as far as possible; improve the quality of products; and reduce cost, reduce the loss of the energy and shielding gas.Because the band steel is in temperature-fall period, temperature reduces gradually, so the in the past shielding gas that extracts in the road cooling room can be used for the cooling gas of road cooling room after the preheating.Effectively utilize refrigerative used heat, significantly cut down the consumption of energy, before cool furnace, add the degreasing system, to improve the effect of removing emulsion and ROLLING OIL.
As preferably, have three cooling rooms in the continuous annealing refrigerating unit at least, pass through inwall separately between described cooling room.
As preferably, described conveying roller is evenly distributed in the back side of band steel, and described gas pipeline system is located in the upper plenum.
Therefore, a kind of euphotic zone steel continuous annealing refrigerating unit that the utility model provides, simple in structure, improve the quality of products, reduce production costs, significantly cut down the consumption of energy, improve energy utilization rate.
Description of drawings
Fig. 1 is a structural representation of the present utility model.
Embodiment
Below by embodiment, and in conjunction with the accompanying drawings, the technical solution of the utility model is described in further detail.
Embodiment: as shown in Figure 1, a kind of euphotic zone steel continuous annealing refrigerating unit, comprise band steel 1, band steel 1 is by the continuous annealing refrigerating unit, the continuous annealing refrigerating unit comprises at least two cooling rooms 2, sealed roller 3, conveying roller 4, gas pipeline system 5, gas jet 6 and interchanger 7, described cooling room 2 comprises upper plenum 8 and following cavity 9, upper plenum 8 and 9 of following cavitys are provided with band steel 1, the end of upper plenum 8 and following cavity 9 is provided with sealed roller 3,3 of described sealed rollers are provided with conveying roller 4, sealed roller 3 and conveying roller 4 contact with band steel 1, gas pipeline system 5 is by cooling room 2, be provided with gas jet 6 in the gas pipeline system 5, gas jet 6 is corresponding with band steel 1, and 5 of described gas pipeline systems are provided with interchanger 7, have three cooling rooms 2 in the continuous annealing refrigerating unit at least, described conveying roller 4 is evenly distributed in the back side of band steel 1 to 2 of described cooling rooms by inwall 10 separately, and described gas pipeline system 5 is located in the upper plenum 8.
Cool furnace is separated into a plurality of independently cooling rooms, and each cooling room can independently be formulated process for cooling, has obviously improved the controllability of refrigerating work procedure; Be convenient to optimize process for cooling, improve the performance and the quality of product; Different cooling rooms effectively seal with sealed roller, can use the cooling gas of heterogeneity proportioning, can significantly reduce production costs; Each road, back cooling room all can effectively utilize preceding road refrigerative used heat, significantly cuts down the consumption of energy; Because of being with steel reducing by road cooling afterreaction activity with temperature, can use the waste gas of preceding road cooling generation in the back road cooling room, obviously improve the utilization ratio of shielding gas.

Claims (3)

1. euphotic zone steel continuous annealing refrigerating unit, comprise band steel (1), it is characterized in that: band steel (1) is by the continuous annealing refrigerating unit, the continuous annealing refrigerating unit comprises at least two cooling rooms (2), sealed roller (3), conveying roller (4), gas pipeline system (5), gas jet (6) and interchanger (7), described cooling room (2) comprises upper plenum (8) and following cavity (9), be provided with band steel (1) between upper plenum (8) and following cavity (9), the end of upper plenum (8) and following cavity (9) is provided with sealed roller (3), be provided with conveying roller (4) between described sealed roller (3), sealed roller (3) and conveying roller (4) contact with band steel (1), gas pipeline system (5) is by cooling room (2), be provided with gas jet (6) in the gas pipeline system (5), gas jet (6) is corresponding with band steel (1), is provided with interchanger (7) between described gas pipeline system (5).
2. a kind of euphotic zone steel continuous annealing refrigerating unit according to claim 1 is characterized in that: have three cooling rooms (2) in the continuous annealing refrigerating unit at least, pass through inwall (10) separately between described cooling room (2).
3. a kind of euphotic zone steel continuous annealing refrigerating unit according to claim 1 and 2 is characterized in that: described conveying roller (4) is evenly distributed in the back side of band steel (1), and described gas pipeline system (5) is located in the upper plenum (8).
CN2010205458545U 2010-09-28 2010-09-28 Continuous annealing cooling device for bright band steel Expired - Fee Related CN201825990U (en)