Prior art keywords
continuous annealing
annealing furnace
burner hearth
band
heater
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2010202931698U
Other languages
Chinese (zh)
Inventor
宋生权
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHEJIANG HAODA INDUSTRIAL FURNACE CO LTD
Original Assignee
ZHEJIANG HAODA INDUSTRIAL FURNACE CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG HAODA INDUSTRIAL FURNACE CO LTD filed Critical ZHEJIANG HAODA INDUSTRIAL FURNACE CO LTD
Priority to CN2010202931698U priority Critical patent/CN201785465U/en
Application granted granted Critical
Publication of CN201785465U publication Critical patent/CN201785465U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Landscapes

  • Heat Treatment Of Strip Materials And Filament Materials (AREA)

Abstract

The utility model discloses a continuous annealing furnace, which comprises a furnace body. The front end of the furnace body is provided with a material feeding port, the rear end of the furnace body is provided with a material discharging port, a hearth heating belt materials is arranged in the furnace body, the hearth is filled with protective atmosphere during operation, the front end of the hearth is provided with a tension roller I, the rear end of the hearth is provided with a tension roller II, the furnace body is provided with a circulation fan assembly, and the belt materials are blown to float by high-speed gas flow sprayed through the circulation fan assembly under tension of the tension roller I and the tension roller II. The continuous annealing furnace is simple and practical, has the advantages of high heating speed, high efficiency, uniform heating temperature, fine grain, easy performance control, no surface scratch, high degree of equipment automation and the like, is suitable for domestic market demands, and can realize localization of the continuous annealing furnace equipment.

Description

A kind of continuous annealing furnace
Technical field
The utility model relates to the Aluminum Plate and Strip Equipment for Heating Processing, particularly a kind of continuous annealing furnace.
Background technology
China's Aluminum strip, foil are underproduce, thereby a large amount of year after year import, and the import Aluminum Plate and Strip mainly is the domestic high-precision strip goods of can not producing or seldom produce, and import high precision Aluminum Plate and Strip is that China YouSe metal industry first is used the foreign exchange rich and influential family.High-precision at home strip goods demand gap is very big, and this is not enough relevant with the high-precision strip equipment assembling of production.Continuous annealing is as one of key equipment of production high precision plates alternate product, equipment such as continuous annealing production line machine row comprise uncoiling, stitching, tension control roll, annealing furnace, cooling room and aligning, curl are formed, wherein peripherals is mature equipment, the Selection and Design of stove and tensile process control are the key elements of comparison key on this production line, so far still grasp gordian technique by external producer, the price of overseas equipment costliness causes a lot of enterprises can't equip the continuous annealing furnace production line.
Domestic anneal for Aluminum Plate and Strip much all adopts common box-annealing furnace at present, and its shortcoming is a lot, is difficult to guarantee to produce high-quality Aluminum Plate and Strip, and its reason is as follows:
1) aluminium and aluminum alloy sheets and strips are in annealing, intensity is very low under the quenching temperature, and viscosity is bigger, easily bonding or with other contactant bonding and cause scuffing mutually;
2) Aluminum Plate and Strip is to heat in roll coil of strip mode in common box heat treatment furnace, heat passes in the volume outside rolling up by conduction gradually, increase along with roll coil of strip diameter, also will increase heat-up time, reaches tens hours sometimes, in long like this heat-processed, because the volume skin is under the high temperature for a long time, the grain growth especially severe, the result causes the inside and outside crystal grain of volume seriously uneven, causes the physicals of Aluminum Plate and Strip and mechanical property inconsistent;
3), needed 3-5 days just can reach the cooling requirement with roll coil of strip mode naturally cooling; Box-annealing furnace roll coil of strip cooling problem can solve on air cushion furnace at present, and band launches cooling on the air cushion furnace, so accelerated cooling time greatly;
, not volatile in heat-processed when 4) rolling attached to lip-deep oil stain of strip material or greasy dirt, thereby stain appears, influence surface quality;
5) owing to heat-treat in batches, so efficient is low, the cost height.
Shortcoming such as just be to use in addition that the air-cushion type annealing furnace can solve effectively that the annealing time of box-annealing furnace is long, the surface easily scratches, strip surface greasy dirt, efficient are lower, but air-cushion type annealing furnace equipment investment cost is bigger, complex structure is not suitable for the demand of domestic market.Also do not have home-made aluminium strip continuous annealing furnace in the market, have vast market prospect so develop the continuous annealing furnace of suitable domestic market, moderate cost.
The utility model content
Problem to be solved in the utility model just provides a kind of simple and practical continuous annealing furnace, have that rate of heating is fast, efficient is high, Heating temperature is even, crystal grain is thin, performance is easily controlled, the surface does not have scuffing, equipment automatization advantages of higher, be fit to domestic market demand, realize the continuous annealing furnace home-made equipment.
In order to solve the problems of the technologies described above; the utility model adopts following technical scheme: a kind of continuous annealing furnace; it is characterized in that: comprise body of heater; front end at body of heater is provided with opening for feed; the rear end of body of heater is provided with discharge port; in body of heater, be provided with the burner hearth of heating band; charge into protective atmosphere during work in the burner hearth; the front end of burner hearth is provided with tensioning roller I; the rear end of burner hearth is provided with tensioning roller II; be provided with the recirculation blower assembly on body of heater, the high velocity air by the ejection of recirculation blower assembly under the tensioning of tensioning roller I and tensioning roller II blows floating band.
Further, described recirculation blower assembly comprises that the blower fan and that is fixed on the body of heater terminates at the air outlet tube on the blower fan, an and aspiration channel that terminates on the blower fan, the other end of air outlet tube is provided with blowing mouth I and blowing mouth II side by side, the other end of aspiration channel is provided with the air suction inlet, and blowing mouth I is located at the burner hearth top, and blowing mouth II is located at the burner hearth below, band is blowed floating by the high velocity air of blowing mouth I and blowing mouth II ejection under the tensioning of tensioning roller I and tensioning roller II, and the air suction inlet is located on the burner hearth sidewall.
Further, described aspiration channel is along the hearth wall setting.The air suction inlet with the burner hearth central gas suck when aspiration channel is delivered to blower fan by hearth wall to aspiration channel in gas heat.
Further, described burner hearth is divided into preheating section, heating zone and cooling section successively from the opening for feed to the discharge port, cooling section is provided with induction pipe and is communicated with the aspiration channel of preheating section fan, and the hot gas that the band after blower fan will be annealed by induction pipe distributes sucks and delivers in the preheating section unannealed band is carried out preheating.Increase heat utilization efficiency, energy-conserving and environment-protective reduce cost.
Further, be connected to the inlet seal section on the described opening for feed, be connected to the exit seal section on the discharge port.Make the unlikely loss of protective atmosphere too much by inlet seal section and exit seal section.
Further, also be provided with between described discharge port and the exit seal section band is carried out quick refrigerative spray cooling system.
After adopting technique scheme, the utlity model has following advantage: band rate of heating under levitated state is fast, do not have and scratch, annealing temperature is even, heating rapidly and evenly can access tiny and the even metal crystal structure has guaranteed that band has higher mechanical properties, lower anisotropy, and the tangerine peel defective that occurs when having eliminated punching press.
Description of drawings
The utility model is described in further detail below in conjunction with accompanying drawing:
Fig. 1 is the structural representation of a kind of embodiment of the utility model;
Fig. 2 is the structural representation of recirculation blower assembly.
Embodiment
The structural representation of a kind of embodiment of the utility model as illustrated in fig. 1 and 2; a kind of continuous annealing furnace; comprise body of heater 1; front end at body of heater is provided with opening for feed 11; the rear end of body of heater is provided with discharge port 12; in body of heater, be provided with the burner hearth 2 of heating band; charge into protective atmosphere during work in the burner hearth; the front end of burner hearth is provided with tensioning roller I13; the rear end of burner hearth is provided with tensioning roller II14; burner hearth is divided into preheating section 21 successively from the opening for feed to the discharge port; heating zone 22 and cooling section 23; cooling section is provided with induction pipe and is communicated with the aspiration channel of preheating section fan, and the hot gas that the band after blower fan will be annealed by induction pipe distributes sucks and delivers in the preheating section unannealed band is carried out preheating.On body of heater, be provided with the recirculation blower assembly, described recirculation blower assembly comprises that the blower fan 3 and that is fixed on the body of heater terminates at the air outlet tube 31 on the blower fan, an and aspiration channel 32 that terminates on the blower fan, the other end of air outlet tube is provided with blowing mouth I311 and blowing mouth II312 side by side, the other end of aspiration channel is provided with air suction inlet 321, blowing mouth I is located at the burner hearth top, blowing mouth II is located at the burner hearth below, band is blowed floating by the high velocity air of blowing mouth I and blowing mouth II ejection under the tensioning of tensioning roller I and tensioning roller II, and the air suction inlet is located on the burner hearth sidewall.Be connected to inlet seal section 4 on the opening for feed, be connected to exit seal section 5 on the discharge port, make the unlikely loss of protective atmosphere too much by inlet seal section and exit seal section.
In the foregoing description, aspiration channel is along the hearth wall setting, the air suction inlet of blower fan with the burner hearth central gas suck when aspiration channel is delivered to blower fan by hearth wall to aspiration channel in gas heat, from the blowing mouth I of blower fan and blowing mouth II, spray then, realize circulation.Between discharge port and exit seal section, also be provided with the spray cooling system 6 of accelerating the band speed of cooling.
The utility model is simple and practical, and band is not contacted with member by the effect of upper and lower hot gas flow in stove, has avoided any scratch on surface, thereby has guaranteed quality.In addition, because band is unfolded heating, the high speed hot gas flow directly blows on the band plate surface, makes attached to the rolling oil stain of strip surface to remove rapidly, prevents the strip surface filth, and is same, because band launches cooling, greatly reduces cooling time.In continuous annealing furnace, hot gas flow sprays to the unfolded strip surface from upper and lower both direction with the speed of 30~50 meter per seconds, and band is heated under the effect of hot gas flow, and its convective heat-transfer coefficient can reach 90~120 kilocalories/meter 2Hour ℃, bigger 2.5~3 times than box-type furnace, so band heats in air cushion furnace rapidly and evenly, can access tiny and the even metal crystal structure, guaranteed that band has higher mechanical properties, lower anisotropy, and the tangerine peel defective that occurs when having eliminated punching press also can reduce and form the metal loss that " ear " caused simultaneously when punching press.Adopt continuous annealing furnace just can organically get in touch with the finishing unit according to demand in addition and be one, directly anneal continuously, operation such as aligning, smooth, oiling, inspection, lining paper, cutting plate and buttress plate, a lot of unnecessary loading and unloading material process have been removed from, not only guarantee the Aluminum Plate and Strip surface quality, can enhance productivity greatly again simultaneously.
Except that above preferred embodiment, the utility model also has other embodiment, those skilled in the art can make various changes and distortion according to the utility model, only otherwise break away from spirit of the present utility model, all should belong to the defined scope of the utility model claims.

Claims (6)

1. continuous annealing furnace; it is characterized in that: comprise body of heater (1); front end at body of heater is provided with opening for feed (11); the rear end of body of heater is provided with discharge port (12); in body of heater, be provided with the burner hearth (2) of heating band; charge into protective atmosphere during work in the burner hearth; the front end of burner hearth is provided with tensioning roller I (13); the rear end of burner hearth is provided with tensioning roller II (14); be provided with recirculation blower assembly (3) on body of heater, the high velocity air by the ejection of recirculation blower assembly under the tensioning of tensioning roller I and tensioning roller II blows floating band.
2. a kind of continuous annealing furnace according to claim 1, it is characterized in that: described recirculation blower assembly comprises that the blower fan (30) and that is fixed on the body of heater terminates at the air outlet tube (31) on the blower fan, an and aspiration channel (32) that terminates on the blower fan, the other end of air outlet tube is provided with blowing mouth I (311) and blowing mouth II (312) side by side, the other end of aspiration channel is provided with air suction inlet (321), blowing mouth I is located at the burner hearth top, blowing mouth II is located at the burner hearth below, band is blowed floating by the high velocity air of blowing mouth I and blowing mouth II ejection under the tensioning of tensioning roller I and tensioning roller II, and the air suction inlet is located on the burner hearth sidewall.
3. a kind of continuous annealing furnace according to claim 2 is characterized in that: described aspiration channel is along the hearth wall setting.
4. a kind of continuous annealing furnace according to claim 1, it is characterized in that: described burner hearth is divided into preheating section (21), heating zone (22) and cooling section (23) successively from the opening for feed to the discharge port, cooling section is provided with induction pipe and is communicated with the aspiration channel of preheating section fan, and the hot gas that the band after blower fan will be annealed by induction pipe distributes sucks and delivers in the preheating section unannealed band is carried out preheating.
5. a kind of continuous annealing furnace according to claim 1 is characterized in that: be connected to inlet seal section (4) on the described opening for feed, be connected to exit seal section (5) on the discharge port.
6. a kind of continuous annealing furnace according to claim 5 is characterized in that: also be provided with between described discharge port and the exit seal section band is carried out quick refrigerative spray cooling system (6).
CN2010202931698U 2010-08-12 2010-08-12 Continuous annealing furnace Expired - Lifetime CN201785465U (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010202931698U CN201785465U (en) 2010-08-12 2010-08-12 Continuous annealing furnace

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010202931698U CN201785465U (en) 2010-08-12 2010-08-12 Continuous annealing furnace

Publications (1)

Publication Number Publication Date
CN201785465U true CN201785465U (en) 2011-04-06

Family

ID=43817439

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010202931698U Expired - Lifetime CN201785465U (en) 2010-08-12 2010-08-12 Continuous annealing furnace

Country Status (1)

Country Link
CN (1) CN201785465U (en)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101914736A (en) * 2010-08-12 2010-12-15 浙江浩大工业炉有限公司 Continuous annealing furnace
CN103266206A (en) * 2013-05-24 2013-08-28 樊永君 Novel continuous spheroidizing annealing furnace
CN103551392A (en) * 2013-11-22 2014-02-05 宝钢工程技术集团有限公司 Transmission device for cold-rolled strip steel production line and transmission method of transmission device
CN105420483A (en) * 2014-09-12 2016-03-23 阿莱利斯铝业迪弗尔私人有限公司 Continuous annealing furnace for processing aluminium alloy sheet
EP3006579A1 (en) * 2014-12-11 2016-04-13 Aleris Aluminum Duffel BVBA Method of continuously heat-treating 7000-series aluminium alloy sheet material
WO2017132476A1 (en) * 2016-01-29 2017-08-03 Corning Incorporated Thermally treated metallic materials and related methods
CN109628709A (en) * 2018-12-29 2019-04-16 佛山市诚德新材料有限公司 A kind of method for annealing of stainless steel band
CN110760767A (en) * 2019-10-31 2020-02-07 重庆中铝华西铝业有限公司 Annealing and oil removing method for large-width double-sided polished aluminum foil

Cited By (16)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101914736A (en) * 2010-08-12 2010-12-15 浙江浩大工业炉有限公司 Continuous annealing furnace
CN103266206A (en) * 2013-05-24 2013-08-28 樊永君 Novel continuous spheroidizing annealing furnace
CN103551392A (en) * 2013-11-22 2014-02-05 宝钢工程技术集团有限公司 Transmission device for cold-rolled strip steel production line and transmission method of transmission device
CN103551392B (en) * 2013-11-22 2015-10-07 宝钢工程技术集团有限公司 For transmission device and the drive method thereof of cold rolled strip steel production line
US10294553B2 (en) 2014-09-12 2019-05-21 Aleris Aluminum Duffel Bvba Method of annealing aluminium alloy sheet material
CN105420483A (en) * 2014-09-12 2016-03-23 阿莱利斯铝业迪弗尔私人有限公司 Continuous annealing furnace for processing aluminium alloy sheet
CN106687609B (en) * 2014-09-12 2020-01-07 阿莱利斯铝业迪弗尔私人有限公司 Method for annealing aluminum alloy sheet material
CN106687609A (en) * 2014-09-12 2017-05-17 阿莱利斯铝业迪弗尔私人有限公司 Method of annealing aluminium alloy sheet material
CN105420483B (en) * 2014-09-12 2019-12-24 阿莱利斯铝业迪弗尔私人有限公司 Continuous annealing furnace for processing aluminum alloy sheet material
US10513767B2 (en) 2014-12-11 2019-12-24 Aleris Aluminum Duffel Bvba Method of continuously heat-treating 7000-series aluminium alloy sheet material
WO2016091550A1 (en) * 2014-12-11 2016-06-16 Aleris Aluminum Duffel Bvba Method of continuously heat-treating 7000-series aluminium alloy sheet material
EP3006579A1 (en) * 2014-12-11 2016-04-13 Aleris Aluminum Duffel BVBA Method of continuously heat-treating 7000-series aluminium alloy sheet material
WO2017132476A1 (en) * 2016-01-29 2017-08-03 Corning Incorporated Thermally treated metallic materials and related methods
CN109628709A (en) * 2018-12-29 2019-04-16 佛山市诚德新材料有限公司 A kind of method for annealing of stainless steel band
CN110760767A (en) * 2019-10-31 2020-02-07 重庆中铝华西铝业有限公司 Annealing and oil removing method for large-width double-sided polished aluminum foil
CN110760767B (en) * 2019-10-31 2020-08-14 重庆中铝华西铝业有限公司 Annealing and oil removing method for large-width double-sided polished aluminum foil

Similar Documents

Publication Publication Date Title
CN201785465U (en) Continuous annealing furnace
CN106865964B (en) Isothermal and isobaric multipurpose ultrathin glass physical tempering equipment
CN101914736B (en) Continuous annealing furnace
CN104060202B (en) A kind of magnesium alloy extrusion online temperature correction device
CN113998877B (en) Toughened glass shaping auxiliary device
CN205188115U (en) Curved stove of glass heat of tunnel type
CN106066627A (en) A kind of safety glass production control system
CN210754952U (en) Roller forging cooling device
CN110002732A (en) A method of control glass heating
CN101892360A (en) Novel heated-air circulation tempering furnace
CN105198197B (en) A kind of toughened glass production line
CN102140574B (en) Annealing process for improving deep drawability of 430 ferrite stainless steel
CN211170466U (en) Microcrystalline glass cooling and annealing production line
CN202626022U (en) Physical glass tempering furnace for glass substrate
CN106219957B (en) High-temperature air clamping vertical type transmission glass toughening furnace
CN206486427U (en) Isothermal, isobaric Multi-use ultra-thin glass toughening equipment equipment
CN110079647A (en) A kind of zincincation of thin gauge household electrical appliances DX51D galvanized sheet
CN216377923U (en) Forced convection device for producing vacuum LOW-E glass by toughening furnace
CN203112868U (en) After-heat-usable roller-type quick cooling furnace
CN202157002U (en) Structure of precise annealing furnace
CN207313658U (en) A kind of automatic annealing device of cold-strip steel
CN206157044U (en) Vertical transmission glass tempering furnace of high temperature wind centre gripping
CN209797757U (en) glass annealing kiln updraft ventilator
CN202007263U (en) Silicon steel annealing furnace
CN210140529U (en) Gas heating glass product annealing furnace

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
AV01 Patent right actively abandoned

Granted publication date: 20110406

Effective date of abandoning: 20120509