CN201648535U - 一种铝电解槽用炉底测温仪 - Google Patents

一种铝电解槽用炉底测温仪 Download PDF

Info

Publication number
CN201648535U
CN201648535U CN2010202993285U CN201020299328U CN201648535U CN 201648535 U CN201648535 U CN 201648535U CN 2010202993285 U CN2010202993285 U CN 2010202993285U CN 201020299328 U CN201020299328 U CN 201020299328U CN 201648535 U CN201648535 U CN 201648535U
Authority
CN
China
Prior art keywords
corrosion
thermoelectric couple
heat insulation
hearth
aluminum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010202993285U
Other languages
English (en)
Inventor
覃海棠
张松江
岳世豹
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Henan Zhongfu Industry Co Ltd
Original Assignee
Henan Zhongfu Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Henan Zhongfu Industry Co Ltd filed Critical Henan Zhongfu Industry Co Ltd
Priority to CN2010202993285U priority Critical patent/CN201648535U/zh
Application granted granted Critical
Publication of CN201648535U publication Critical patent/CN201648535U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型旨在提供一种耐高温电解质和铝水的浸蚀、可反复使用、测量成本低的一种铝电解槽用炉底测温仪。本实用新型包括热电偶,其中,在热电偶外套装有隔热防腐套管,隔热防腐套管内设置有隔热层。本实用新型在热电偶外套装的隔热防腐套管,它既可隔热以保证测量的准确度,又可防止高温电解质和铝水对热电偶的腐蚀,延长了仪器的使用寿命,降低了测量成本;测温时,热电偶探头伸入到电解槽的沉淀物中,若隔热防腐套管与热电偶探头的距离小于1cm,则热电偶探头不直接与铝水接触,防止其被腐蚀,进一步延长了仪器的使用寿命,使仪器可反复使用,从而降低了成本。

Description

一种铝电解槽用炉底测温仪
技术领域
本实用新型属于铝电解槽的自动控制或调节领域,具体涉及一种铝电解槽用炉底测温仪。
背景技术
铝电解槽的炉膛内底部,常称炉底。炉底温度是电解槽正常生产的重要参数之一,测试炉膛底部的温度,可以为电解槽的技术条件管理提供重要的数据信息,使电解槽长期处于规整的炉膛状态下,提高对电解槽炉膛的管理水平,从而提高电解槽的稳定性;如果炉底温度过低,炉底会形成厚厚一层沉淀,甚至结壳,造成炉底压降升高,增加电解铝的电能单耗,从而增加电解铝的成本。炉底温度的测量常采用热电偶直接插入炉底,热电偶必须先穿过950℃高温的电解质,然后再穿过高于900℃的铝水到达炉膛内底部并保持30秒左右以测得稳定的温度值。但是在这30秒的时间里,热电偶的探头以上部分会一直浸在高温电解质与铝水中,很快会熔化损坏,有时一根热电偶只能测一次就会损坏,以致测量成本很高,也造成了正常生产过程中不能经常获得此项参数。
实用新型内容
本实用新型克服了现有技术的不足,提供了一种耐高温电解质和铝水的浸蚀、可反复使用、测量成本低的一种铝电解槽用炉底测温仪。
为达到上述目的,本实用新型采用的技术方案为:
一种铝电解槽用炉底测温仪,包括热电偶,其中,在热电偶外套装有隔热防腐套管,隔热防腐套管内设置有隔热层。
进一步,所述的隔热防腐套管的内径比热电偶的外径大至少1cm。
进一步,所述的隔热防腐套管与热电偶探头的距离小于1cm。
进一步,所述的隔热层为氧化铝。
本实用新型的积极效果为:
1、本实用新型的测温仪可以方便、快速地测试炉膛底部的温度,为电解槽的技术条件管理提供重要的数据信息,使电解槽长期处于规整的炉膛状态下,提高了对电解槽炉膛的管理水平,从而提高了电解槽的稳定性,提高了经济指标;
2、本实用新型是在普通的热电偶外加一个隔热防腐套管,它不仅可以隔热以保证测量的准确度,又可以防止高温电解质和铝水对热电偶的腐蚀,延长了仪器的使用寿命,降低了测量成本;测温时,探头伸入到电解槽的沉淀物中,若隔热防腐套管与热电偶探头的距离小于1cm,则探头不直接与铝水接触,防止其被腐蚀。
附图说明:
图1为本实用新型的结构示意图。
具体实施方式
下面结合附图来对本实用新型作进一步的详细描述。
如图1所示,在热电偶1外套装有隔热防腐套管2, 隔热防腐套管2的内径比热电偶1的外径大2cm,隔热防腐套管2内设置有隔热层3;隔热层3为氧化铝材料;隔热防腐套管2与热电偶探头4之间的距离为0.5 cm。测温时,热电偶1先穿过950℃高温的电解质,然后再穿过高于900℃的铝水到达炉膛内底部并保持30秒左右以测得稳定的温度值。在热电偶1外加装有一个隔热防腐套管2,它不仅可以隔热以保证测量的准确度,又可以防止高温电解质和铝水对热电偶1的腐蚀,延长了仪器的使用寿命,降低了测量成本;由于隔热防腐套管2与热电偶探头4的距离小于1cm,热电偶探头4可以完全伸入到电解槽的沉淀物中,不直接与铝水接触,防止其被腐蚀,进一步延长了仪器的使用寿命,使仪器可反复使用,从而降低了成本。
要说明的是,以上所述实施例是对本实用新型技术方案的说明而非限制,所属技术领域普通技术人员的等同替换或者根据现有技术而做的其它修改,只要没超出本实用新型技术方案的思路和范围,均应包含在本实用新型所要求的权利范围之内。

Claims (4)

1.一种铝电解槽用炉底测温仪,包括热电偶(1),其特征在于:在热电偶(1)外套装有隔热防腐套管(2),隔热防腐管(2)内设置有隔热层(3)。
2.根据权利要求1所述的一种铝电解槽用炉底测温仪,其特征在于:所述的隔热防腐套管(2)的内径比热电偶(1)的外径大至少1cm。
3.根据权利要求1所述的一种铝电解槽用炉底测温仪,其特征在于:所述的隔热防腐套管(2)与热电偶探头(4)的距离小于1cm。
4.根据权利要求1所述的一种铝电解槽用炉底测温仪,其特征在于:所述的隔热层(3)为氧化铝。
CN2010202993285U 2010-08-20 2010-08-20 一种铝电解槽用炉底测温仪 Expired - Fee Related CN201648535U (zh)