CN201626150U - 317l奥氏体不锈钢复合钢板 - Google Patents
317l奥氏体不锈钢复合钢板 Download PDFInfo
- Publication number
- CN201626150U CN201626150U CN2009202943531U CN200920294353U CN201626150U CN 201626150 U CN201626150 U CN 201626150U CN 2009202943531 U CN2009202943531 U CN 2009202943531U CN 200920294353 U CN200920294353 U CN 200920294353U CN 201626150 U CN201626150 U CN 201626150U
- Authority
- CN
- China
- Prior art keywords
- steel plate
- stainless steel
- austenitic stainless
- composite
- plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及的是317L奥氏体不锈钢复合钢板,其特征是:设置有双层复合板,其中一层为317L奥氏体不锈钢板,另外一层为普通钢板。本实用新型提供的产品,能够有效的将317L奥氏体不锈钢板与普通钢板复合,从而在保证复合钢板具有317L奥氏体不锈钢所有的优点的前提下,拥有了需要的强度,从而节约了昂贵金属的使用量。同时本产品具有很高的焊接质量,保证长期稳定使用不会脱落。
Description
所属技术领域
本实用新型涉及的是金属爆炸复合板。
背景技术
317L(00Cr17Ni14Mo3)奥氏体不锈钢是含钼的奥氏体不锈钢。它与常规的铬-镍奥氏体不锈钢如304合金相比,具有更强的抗化学腐蚀能力。另外,317L合金具有更高的延展性、抗应力腐蚀性能、耐压强度及耐高温性能。所以广泛的作为各种腐蚀性原料的容器或者管道的直接接触面,但是由于317L的市场价格较高,又要满足强度的需要,所以需要将317L和普通的金属复合使用。
爆炸焊接技术是通过炸药爆轰产生的高压脉冲载荷,推动一种材料(复材)高速倾斜碰撞另一种材料(基材),其加载应力远远高于金属材料的屈服强度,加载过程的瞬间性(一般以毫秒计),材料受载的局部性,交织发生在作用点的微小的邻近区域并且高速地移动等方式,实现两种金属的冶金结合,结合区呈现为波状的冶金结合。爆炸焊接又是用炸药作能源进行金属间焊接和生产金属复合材料的一种很有实用价值的高新技术。其最大特点是在瞬间能将金属组合,简单、迅速和强固地焊接在一起。与轧制、堆焊等焊接技术相比爆炸焊接技术的优点在于:
广泛的材料适应性的可焊性,适用于大多可塑性金属或合金;尤其是对于大面积金属的焊接,可以说是唯一的连接方法;不仅适用于相溶性金属的组合,而且适用于非相溶性金属的组合,也适用于易产生脆性金属间化合物的金属及合金;具有良好的导热性,低的界面电阻,结合区无热影响区构成良好的接头性能,瞬间的热过程使界面没有或仅有少量的溶化。
发明内容
本实用新型的目的是提供一种317L奥氏体不锈钢复合钢板以弥补现有技术之不足。
本实用新型的目的是这样实现的:317L奥氏体不锈钢复合钢板,其特征是:设置有双层复合板,其中一层为317L奥氏体不锈钢板,另外一层为普通钢板。
有益效果
本实用新型提供的产品,能够有效的将317L奥氏体不锈钢板与普通钢板复合,从而在保证复合钢板具有317L奥氏体不锈钢所有的优点的前提下,拥有了需要的强度,从而节约了昂贵金属的使用量。同时本产品具有很高的焊接质量,保证长期稳定使用不会脱落。
下面结合附图通过实施例对本实用新型作进一步描述:
附图说明
图1为本实用新型实施例的结构示意图。
317L奥氏体不锈钢复合钢板,其特征是:设置有双层复合板,其中一层为317L奥氏体不锈钢板1,另外一层为普通钢板2。
具体实施方式
实施例:
将普通钢板2水平放置,317L奥氏体不锈钢板1在其上平行放置,在317L奥氏体不锈钢板1外表面均匀放置炸药,炸药的爆速为1.8×103-2.2×103m/s、猛度为6-10mm、密度为0.6g/cm-3-0.85g/cm-3,通过雷管引爆,在高制动压力下,317L奥氏体不锈钢板1和普通钢板2的表面就牢牢的粘结在一起。再经过补焊、热处理工艺、校平工艺、切边工艺、机械抛光工艺或酸洗工艺即可得到成品。
Claims (1)
1.317L奥氏体不锈钢复合钢板,其特征是:设置有双层复合板,其中一层为317L奥氏体不锈钢板,另外一层为普通钢板。