CN201464415U - 带钢表面氧化膜电位差曲线测定的电极装置 - Google Patents
带钢表面氧化膜电位差曲线测定的电极装置 Download PDFInfo
- Publication number
- CN201464415U CN201464415U CN2009200777414U CN200920077741U CN201464415U CN 201464415 U CN201464415 U CN 201464415U CN 2009200777414 U CN2009200777414 U CN 2009200777414U CN 200920077741 U CN200920077741 U CN 200920077741U CN 201464415 U CN201464415 U CN 201464415U
- Authority
- CN
- China
- Prior art keywords
- potential difference
- division board
- electrode assembly
- film potential
- oxide film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及带钢表面氧化膜电位差曲线的测定,尤其涉及带钢表面氧化膜电位差曲线测定的试样和电极。一种带钢表面氧化膜电位差曲线测定的电极装置,它包括作为电极的一对金属夹板,该夹板上端设连有导线的接线柱,它包括:一把手,它包括下部的凸起的长条部分,所述金属夹板分列于长条部分的两侧;一个隔离板,它设于所述把手长条部分中段,所述金属夹板固定于隔离板上,且以一端穿过隔离板。
Description
技术领域
本实用新型涉及带钢表面氧化膜电位差曲线的测定,尤其涉及带钢表面氧化膜电位差曲线测定的试样和电极。本实用新型适用于快速评价带钢表面氧化膜的组成和质量。
背景技术
带钢表面氧化膜电位差曲线(Potential Differential Curve)是快速评价带钢脱碳板表面氧化膜质量及组成,其原理是在以试样为正极,同批次无膜基板为负极;放在一定温度和浓度的电解液中形成原电池,测定其电位变化随时间的关系曲线(即Potential Differential Curve,简称P-D曲线)。通过电位峰值的变化评价、检测膜的质量。
原方法采用将导线焊接在正负两极上并用胶带按一定的尺寸进行封闭,用两个锲型板大小端配合将正负两极固定,放入电解槽中进行测定。此方法操作麻烦,样品腐蚀面积和正负两极距离难以保证,并且不能满足不同厚度样品测定要求,在实际工作中有一定的局限性。
发明内容
本实用新型旨在解决现有技术的缺陷,提供一种续监测的采样及前处理装置,有效提高烟气采集样品的代表性,减少维护工作量。
本实用新型是这样实现的:一种带钢表面氧化膜电位差曲线测定的电极装置,它包括作为电极的一对金属夹板,该夹板上端设连有导线的接线柱,它包括:
一把手,它包括下部的凸起的长条部分,所述金属夹板分列于长条部分的两侧;
一个隔离板,它设于所述把手长条部分中段,所述金属夹板固定于隔离板上,且以一端穿过隔离板。
所述的带钢表面氧化膜电位差曲线测定的电极装置,它还包括一对安装在隔离板下部的防偏架,所述金属夹板穿过隔离板的部分被防偏架夹持。
所述带钢表面氧化膜电位差曲线测定的电极装置,它还包括一对支架,它们分别固定于把手下部长条部分的两侧。
所述的带钢表面氧化膜电位差曲线测定的电极装置,所述把手、隔离板、防偏架及支架均为有机玻璃制作而成。
本实用新型采用两片不锈钢作为试验片夹,分别作为样品的正、负极,并作为电信号输出接线柱,分别引出两根导线与X-Y图形记录仪的正负两极连接,由于不锈钢的韧性可以将不同厚度的样品夹住.为了防止试样夹被酸雾腐蚀,其下方设计了一个有机玻璃防护板,将电信号输出部分和试验腐蚀部分分为上下两个部分.在其下方设计四个有机玻璃防偏架,以防止试验片插偏,当试验片插偏时将不能插入不锈钢支架中,以确保基板和试验片二者之间的距离满足试验要求;此外防偏架还能增强装置的耐腐蚀性,能确保试样夹和导线接线柱不被酸雾腐蚀,增加电极装置的耐用性.为了方便取放电极装置,本实用新型设计了一个有机玻璃手柄,并将导线从其中引入,避免在拿取电极装置时导线接头容易脱离现象发生.在电极装置中设计了两个有机玻璃支架,可以使电极装置容易地架在电解槽上.
附图说明
下面,结合附图进一步说明本实用新型的具体实施方式:
图1为本实用新型的正视图;
图2为本实用新型的俯视图。
具体实施方式
一种带钢表面氧化膜电位差曲线测定的电极装置,它包括作为电极的一对金属夹板4,该夹板4上端设连有导线1的接线柱3,它包括:
一把手2,它包括下部的凸起的长条部分,所述金属夹板4分列于长条部分的两侧;
一个隔离板5,它设于所述把手2长条部分中段,所述金属夹板4固定于隔离板5上,且以一端穿过隔离板5。
所述的带钢表面氧化膜电位差曲线测定的电极装置,它还包括一对安装在隔离板5下部的防偏架6,所述金属夹板4穿过隔离板5的部分被防偏架6夹持。
所述带钢表面氧化膜电位差曲线测定的电极装置,它还包括一对支架7,它们分别固定于把手2下部长条部分的两侧。
所述把手2、隔离板5、防偏架6及支架7均为有机玻璃制作而成。。
测试时,样品作为正极、同批次无膜基板为负极,将其插入试样尺寸定位器,用胶带沿试样尺寸定位器上将试样封闭,分别插入电极装置中对应极的试样夹中,将两根导线分别与X-Y记录仪正负极连接,打开记录仪,将电极装置放入电解液槽中进行带钢表面氧化膜电位差曲线测量。
Claims (4)
1.一种带钢表面氧化膜电位差曲线测定的电极装置,它包括作为电极的一对金属夹板,该夹板上端设连有导线的接线柱,其特征在于,它包括:
一把手,它包括下部的凸起的长条部分,所述金属夹板分列于长条部分的两侧;
一个隔离板,它设于所述把手长条部分中段,所述金属夹板固定于隔离板上,且以一端穿过隔离板。
2.根据权利要求1所述的带钢表面氧化膜电位差曲线测定的电极装置,其特征在于,它还包括一对安装在隔离板下部的防偏架,所述金属夹板穿过隔离板的部分被防偏架夹持。
3.根据权利要求1所述带钢表面氧化膜电位差曲线测定的电极装置,其特征在于,它还包括一对支架,它们分别固定于把手下部长条部分的两侧。
4.根据权利要求1、2或3所述的带钢表面氧化膜电位差曲线测定的电极装置,其特征在于,所述把手、隔离板、防偏架及支架均为有机玻璃制作而成。