CN201367473Y - 铝电解槽阴极结构 - Google Patents
铝电解槽阴极结构 Download PDFInfo
- Publication number
- CN201367473Y CN201367473Y CNU2009203003720U CN200920300372U CN201367473Y CN 201367473 Y CN201367473 Y CN 201367473Y CN U2009203003720 U CNU2009203003720 U CN U2009203003720U CN 200920300372 U CN200920300372 U CN 200920300372U CN 201367473 Y CN201367473 Y CN 201367473Y
- Authority
- CN
- China
- Prior art keywords
- cathode
- cathode carbon
- carbon blocks
- aluminum
- electrolysis bath
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种预焙阳极铝电解槽阴极结构,它包括阴极炭块和阴极钢棒,每间隔一组或几组低阴极炭块(1)设置一组高阴极炭块(2)。在高阴极炭块(2)中部开设豁口(4)。豁口(4)的底面等高于或高于低阴极炭块(1)的顶面。高阴极炭块(2)中的阴极钢棒(3)的断面尺寸可以大于或等于低阴极炭块(1)中的阴极钢棒的断面尺寸。高阴极炭块开设的豁口使电解槽内的铝液能通过豁口流至出铝端。本实用新型通过高低阴极的交错布置对铝电解槽规整的炉膛进行适当的分割,以减小铝液界面的波动对铝电解槽稳定性的影响,同时减少铝液的二次反应以提高铝电解的电流效率。
Description
技术领域
本实用新型涉及一种铝电解槽,特别是涉及一种铝电解槽阴极结构。
背景技术
在铝电解槽中,由阴极炭块、内衬、侧部炭块、人造伸腿构成了规整的、底部水平的铝冶炼槽。随着铝电解技术不断发展和完善以及对铝电解理论的深入研究,铝电解槽槽型出现了越来越大型化的趋势,同时根据国内外的生产实践来看槽型越大,其稳定性越不好掌握,而电解槽的稳定性又与电解槽内铝液界面的波动密切相关,而一个稳定性不好的电解槽,是无法正常生产的。
同时,由于阴极炭块高度及宽度的限制,阴极钢棒的截面改变范围不大,很难最大限度地改善铝液内及阴极炭块内的电流分配。
实用新型内容
本实用新型的目的是:提供一种铝电解槽阴极结构,该结构能够减小铝液界面的波动对铝电解槽稳定性的影响,同时减少铝液的二次反应以提高铝电解的电流效率,以克服现有技术存在的铝电解槽稳定性差等不足。
本实用新型是这样构成的:它包括两个或多个不同高度的阴极炭块,每间隔一组或几组低阴极炭块设置一组高阴极炭块,高阴极炭块中部开设豁口,使电解槽内的铝液能通过豁口流至出铝端,豁口的高度最低可低至阴极炭块的顶面。
为降低阴极电压降及为减少电解槽铝液内的水平电流,可根据高阴极炭块的高度适当调节其阴极钢棒断面尺寸及高度,阴极钢棒的截面大小在钢棒长度方向上可以保持一致,也可以按比例逐步变化(增大或减小),还可以阶梯形突变其截面大小。
本实用新型的有益效果是:通过高低阴极的交错布置对铝电解槽规整的炉膛进行适当的分割,以减小铝液界面的波动对铝电解槽稳定性的影响,同时减少铝液的二次反应以提高铝电解的电流效率。
附图说明
图1为本实用新型的示意图,图中示意出高低阴极及豁口。
图2为本实用新型断面图;
具体实施方式
本实用新型的实施例:如附图1与附图2所示,在一个电解槽内由不同高度的阴极炭块构成电解槽炉膛阴极,阴极炭块高度可以有两种或多种规格。低阴极炭块1与高阴极炭块2在电解槽内交错排列布置,每间隔一组或几组低阴极炭块1设置一组高阴极炭块2;高阴极炭块2上开设豁口4,使电解槽内的铝液能通过豁口4流至出铝端,豁口4的高度最低可低至阴极炭块1的顶面。
高阴极炭块2中的阴极钢棒3的断面尺寸可以大于或等于低阴极炭块1中的阴极钢棒的断面尺寸。可以根据高阴极炭块2的高度适当调节其阴极钢棒3断面尺寸及高度,阴极钢棒3的截面大小在钢棒长度方向上可以保持一致,也可以按比例逐步变化(增大或减小),还可以阶梯形突变其截面大小。
Claims (4)
1.一种铝电解槽阴极结构,它包括阴极炭块和阴极钢棒,其特征在于:每间隔一组或几组低阴极炭块(1)设置一组高阴极炭块(2)。
2.根据权利要求1所述的铝电解槽阴极结构,其特征在于:在高阴极炭块(2)中部开设豁口(4)。
3.根据权利要求2所述的铝电解槽阴极结构,其特征在于:豁口(4)的底面等高于或高于低阴极炭块(1)的顶面。
4.根据权利要求1所述的铝电解槽阴极结构,其特征在于:高阴极炭块(2)中的阴极钢棒(3)的断面尺寸大于低阴极炭块(1)中的阴极钢棒的断面尺寸。