CN201011092Y - 木塑复合地板 - Google Patents

木塑复合地板 Download PDF

Info

Publication number
CN201011092Y
CN201011092Y CNU2007200190073U CN200720019007U CN201011092Y CN 201011092 Y CN201011092 Y CN 201011092Y CN U2007200190073 U CNU2007200190073 U CN U2007200190073U CN 200720019007 U CN200720019007 U CN 200720019007U CN 201011092 Y CN201011092 Y CN 201011092Y
Authority
CN
China
Prior art keywords
wood
surface layer
timber
base material
composite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2007200190073U
Other languages
English (en)
Inventor
于淑聪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
QINGDAO LIANYI WOOD CO Ltd
Original Assignee
QINGDAO LIANYI WOOD CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO LIANYI WOOD CO Ltd filed Critical QINGDAO LIANYI WOOD CO Ltd
Priority to CNU2007200190073U priority Critical patent/CN201011092Y/zh
Application granted granted Critical
Publication of CN201011092Y publication Critical patent/CN201011092Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

木塑复合地板是一种可供家庭、公共场所使用的新型复合地板,属于装修、装饰技术领域。包括有木塑复合基材2,在木塑复合基材的两侧设置有互相配合的安装用的槽口21和榫舌22,木塑复合基材内部有纵向排列的空心孔23,其特征在于在木塑复合基材上面粘接一层木材上表面层1,木塑复合基材的下面粘接一层木材平衡底面层3。优点是节约大量的木材,减少胶粘剂对环境的污染,甲醛释放量为0,对人体健康没有危害,解除使用过程中变形开裂等后顾之忧;可以将使用范围扩大到实木复合地板无法使用的区域,如厨房、户外、广场等;能防震、隔音、防变形,减少建筑重量负荷。

Description

木塑复合地板
(一)技术领域
本实用新型涉及一种可供家庭、公共场所使用的新型复合地板,属于装修、装饰技术领域,具体说是一种木塑复合地板。
(二)背景技术
目前现有的复合地板是由木材经胶粘剂粘合而成,地板制作消耗木材多,不符合国家“保护森林资源”政策,胶粘剂中的甲醛在室内释放时间可长达10年之久,严重危害人们的健康。纯木质地板因受潮或吸收水分膨胀率达到8%以上,纯木地板会反复出现吸水膨胀、干燥收缩的现象,导致地板容易产生变形、开裂,严重影响使用效果。
(三)发明内容
本实用新型目的在于要解决上述技术问题,提出一种木塑复合地板,使得受潮吸水膨胀率<1%,不会因为受潮吸水膨胀引起地板变形开裂,使地板甲醛释放量为0,不会对人体健康造成危害。
本实用新型目的由以下技术方案实现:该木塑复合地板,包括有木塑复合基材2,在木塑复合基材的两侧设置有互相配合的安装用的槽口21和榫舌22,木塑复合基材内部有纵向排列的空心孔23,其特征在于在木塑复合基材上面粘接一层木材上表面层1,木塑复合基材的下面粘接一层木材平衡底面层3。
木塑复合基材2是120-200目的塑料粉末40-60份与120-200目的木材纤维60-40份混合加热到140-150℃,经螺杆挤出的中间空心木塑板材。
木材上表面层1和木材平衡底面层3是厚度0.3-6.0mm的硬质木材。
木塑复合基材2与木材上表面层1、木材平衡底面层3之间粘接的胶粘剂是pvc-8808胶粘剂,是塑料复合材料与木材粘合的专用产品,涂胶量为200-300克/平方米。木塑复合基材2经过两面砂光定厚后辊涂胶粘剂,两面覆盖木质单板:木材上表面层1、木材平衡底面层3,进入压力机加压40-50分钟,养生72小时以上使胶液完全固化。
木材上表面层1的上表面辊涂紫外光固化树脂耐磨树脂油漆,木材平衡底面层3的底面辊涂紫外光固化树脂油漆。
两端有插销孔24,使用槽口插肖件锁扣25插入插销孔24中连接两块木塑复合地板。
采用四面刨、双端铣对地板进行四周企口加工,两侧的槽口21和榫舌22槽榫接合,两端槽口插肖接合,两面单板进行砂光抛光后,木材上表面层1的上表面辊涂一层紫外光固化树脂耐磨油漆,木材平衡底面层3的底面辊涂紫外光固化树脂油漆。
本实用新型优点是木塑复合基材2是塑料与木纤维合成的复合材料,可以利用废弃木材、木屑,节约大量的木材,符合我国森林保护政策;挤出时一次成型,不用胶粘剂合成,减少胶粘剂制造、使用过程中造成的环境污染;胶粘剂中不含甲醛、苯等有害物质,甲醛释放量为0,对人体健康没有危害,是新型的环保产品;木塑复合基材是塑料和木纤维均匀混合挤出的复合材料,受潮或吸水膨胀率明显低于木材,为用户解除地板使用过程中变形开裂等后顾之忧;可以将复合地板的使用范围扩大到实木复合地板无法使用的区域,如厨房、户外、广场等;地板表面采用木材与人体亲合力好,辊涂紫外光固化树脂油漆采用光固化没有气味、甲醛、苯等有害物质挥发,硬度高耐磨;中间空心结构抗压、防震、隔音、防变形,减少建筑重量负荷。
(四)附图说明
图1是一种木塑复合地板结构示意图,
图2是木塑复合地板端部连接示意图。
(五)具体实施方式
结合附图说明一个实施例。图1表示一种木塑复合地板结构。包括有木塑复合基材2,在木塑复合基材的两侧设置有互相配合的安装用的槽口21和榫舌22,木塑复合基材内部有纵向排列的空心孔23,在木塑复合基材上面粘接一层木材上表面层1,木塑复合基材的下面粘接一层木材平衡底面层3,均为厚度0.3-6.0mm的硬质木材。木塑复合基材2与木材上表面层1、木材平衡底面层3之间由pvc-8808胶粘剂粘接。木材上表面层1的上表面辊涂紫外光固化树脂耐磨树脂油漆,木材平衡底面层3的底面辊涂紫外光固化树脂油漆。两端有插销孔(24),使用槽口插肖件锁扣(25)插入插销孔(24)中连接两块木塑复合地板。

Claims (5)

1.一种木塑复合地板,包括有木塑复合基材(2),在木塑复合基材的两侧设置有互相配合的安装用的槽口(21)和榫舌(22),木塑复合基材内部有纵向排列的空心孔(23),其特征在于在木塑复合基材上面粘接一层木材上表面层(1),木塑复合基材的下面粘接一层木材平衡底面层(3)。
2.按照权利要求1所述的木塑复合地板,其特征在于木材上表面层(1)和木材平衡底面层(3)是厚度0.3-6.0mm的硬质阔叶木材。
3.按照权利要求1所述的木塑复合地板,其特征在于木塑复合基材(2)与木材上表面层(1)、木材平衡底面层(3)之间粘接的胶粘剂是pvc-8808胶粘剂,涂胶量为200-300克/平方米。
4.按照权利要求1所述的木塑复合地板,其特征在于木材上表面层(1)的上表面辊涂紫外光固化树脂耐磨树脂油漆,木材平衡底面层(3)的底面辊涂紫外光固化树脂油漆。
5.按照权利要求1所述的木塑复合地板,其特征在于两端有插销孔,(24)使用槽口插肖件锁扣(25)插入插销孔(24)中连接。
CNU2007200190073U 2007-02-15 2007-02-15 木塑复合地板 Expired - Fee Related CN201011092Y (zh)