CN200988090Y - Large cross section round blank crystallizer for continuous casting - Google Patents

Large cross section round blank crystallizer for continuous casting Download PDF

Info

Publication number
CN200988090Y
CN200988090Y CN 200620152010 CN200620152010U CN200988090Y CN 200988090 Y CN200988090 Y CN 200988090Y CN 200620152010 CN200620152010 CN 200620152010 CN 200620152010 U CN200620152010 U CN 200620152010U CN 200988090 Y CN200988090 Y CN 200988090Y
Authority
CN
China
Prior art keywords
water tank
water
section round
crystallizer
continuous casting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200620152010
Other languages
Chinese (zh)
Inventor
耿福轩
池海波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin Seri Machinery Equipment Corp Ltd
Original Assignee
Tianjin Seri Machinery Equipment Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin Seri Machinery Equipment Corp Ltd filed Critical Tianjin Seri Machinery Equipment Corp Ltd
Priority to CN 200620152010 priority Critical patent/CN200988090Y/en
Application granted granted Critical
Publication of CN200988090Y publication Critical patent/CN200988090Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model provides a large section round billet crystallizer for continuous casting, comprising a water tank, the inner side of which is lined with a copper tube, a radiation source box and a foot roll support connected with the water tank. The radiation source box is arranged on the lateral side upper the water tank, the inner side of the water tank is provided with a spray water supply component surrounding the bottom, the lateral side of the water tank bottom is provided with a plurality of grooves which are connected with the foot roll support by a T-shaped bolt, one end of the T-shaped bolt is inlayed in the grooves of the water tank bottom, the other end is crossed the upper connecting plate of the foot roll support; the copper tube lined within the water tank is 700 to 1000 mm in length and 0.05 to 0.07 mm in taper; the water pipe of the foot roll support is provided with multi layers spray tube with nozzle. The effects of the utility model are that: the crystallizer of the structure can produce out large section round casting billet of PHI 35.6 mm to PHI 408 mm on the production platform of 10.5 m, the surface quality and the internal quality of the large section round casting billet are improved. The structure can be combined with the platform space, the maintenance is convenient, the sealing and safety performance of the whole equipment is improved.

Description

Continuous casting is with big section round mold
Technical field
The utility model relates to a kind of continuous casting round mold, particularly a kind of 10.5m production platform that uses, and the continuous casting of producing φ 353.6mm ~ φ 408mm circle base is with big section round mold.
Background technology
The domestic round strand that on the production platform of 10.5m, can produce φ 310mm, and the crystallizer of producing the drawn special steel of φ 353.6mm ~ φ 408mm still belongs to not having and has.Development and needs along with market, the production of big section circle base is necessary, but can not go up new continuous casting line again, original space constraints the external form and the structure of φ 353.6mm ~ φ 408mm crystallizer, only on the production line (Germany is by producing the production line that φ 310mm circle base designs) of former design production φ 310mm, carry out structural improvement, produce the round base of φ 353.6mm ~ φ 408mm, to solve the needs of market and development.
Summary of the invention
For solving the problem that exists in the above-mentioned technology, the purpose of this utility model provides a kind of continuous casting with big section round mold, for the production platform that keeps the original production line is constant, makes new crystallizer and original crystallizer that interchangeability be arranged.
For achieving the above object, the technical solution adopted in the utility model provides a kind of continuous casting with big section round mold, include the water tank that the inboard is lined with copper pipe, the sufficient roller support of penetrating source capsule and being connected with water tank, wherein: penetrate source capsule in the water tank upper arranged outside, be provided with shower water water supply component around its bottom in the water tank inboard, be provided with a plurality of grooves in the outside of water tank bottom, be connected with sufficient roller support by T type bolt, one end of T type bolt is set in the groove of water tank bottom, and its other end passes the upper junction plate of sufficient roller support; The copper pipe length of described water tank liner is 700-1000mm, and tapering is 0.05-.0.76mm; The water pipe of sufficient roller support is provided with the shower that multilayer has water nozzle.
The copper pipe tapering of described water tank liner is a kind of of single tapering, many taperings or the continuous tapering of parabola.
Four layers of shower preferably are set on the water pipe of described sufficient roller support, and the angle of per two shower water nozzles is 60 ° of angles.
The beneficial effects of the utility model are that the crystallizer of this structure has been realized on the production platform of 10.5m, can produce the big section circle of φ 353.6mm ~ 408mm strand.Owing to enlarged and drawn the steel pricker degree, increased the contact area of molten steel, satisfied the needs of molten steel in copper pipe, improved the surface and the inherent quality of big section circle strand.The outer water supply that has changed crystallizer be built-in after, can cooperate with platform space, reduced dismounting and maintenance on ordinary days.The crystallizer of this structure has also improved the sealing and the security of integral device.
Description of drawings
Fig. 1 is the utility model overall structure schematic diagram;
Fig. 2 is a sufficient roller supporting structure schematic diagram of the present utility model.
Among the figure:
1, water tank 2, penetrate source capsule 3, shower water water supply component
4, T type bolt 5, copper pipe 6, water pipe
7, sufficient pipe holder
The specific embodiment
Reaching embodiment in conjunction with the accompanying drawings is illustrated with big section round mold continuous casting of the present utility model.
As shown in Figure 1, continuous casting of the present utility model includes the water tank 1 that the inboard is lined with copper pipe, the sufficient roller support 7 of penetrating source capsule 2 and being connected with water tank with big section round mold structure, be provided with in water tank 1 upper outside and penetrate source capsule 2, utilize the end face of flange and the set bolt of water tank 1 and penetrate the end face of flange and the hole of source capsule 2, two end face of flange are close to, and meanwhile the set bolt cap also plays positioning action.Be provided with shower water water supply component 3 in water tank 1 inboard, make water tank 1 bottom intact, do not leak outside and to say around its bottom.Be provided with a plurality of rectangular grooves in the outside of water tank 1 bottom, be connected with sufficient roller support 7 by T type bolt 4, one end of T type bolt 4 is set in the groove of water tank 1 bottom, it can't be rotated, its other end passes the upper junction plate of sufficient roller support 7, this connected mode was both firmly simple and direct, had avoided the sealing problem of water tank 1 again.
The copper pipe 5 of described water tank 1 liner is the core component of this crystallizer, draws the success or not of steel billet, and cc billet surface quality and crystallizer life-span, copper pipe 5 is most important.Therefore, copper pipe 5 is designed to length 700-1000mm, and tapering is 0.05-.0.76mm, and copper pipe 5 taperings are according to the difference of drawing steel billet, and it is multi-form to can be single tapering, many taperings or the continuous tapering of parabola.
The water pipe 6 of sufficient roller support 7 is provided with the shower that multilayer has water nozzle.Be set to four layers of shower on the water pipe 6 of the sufficient roller support 7 of present embodiment, the angle of per two shower water nozzles is 60 ° of angles.Such structure strengthens injection flow rate, has guaranteed the supply of cooling water, with contact area and the uniformity to steel billet, has realized needs and rigidity when steel billet passes through to greatest extent.
Continuous casting of the present utility model is to realize like this with big section round mold.
As shown in Figure 1, 2, at first shorten water tank and enlarge the copper pipe tapering, the crystallizer of making because of the Circular measure that draws copper radius crystallizer self of 10.5m can't be put in the former vibration solenoid, dwindles external form so reduce water tank length, the box sizes up and down of water tank differs, and mutual dislocation, up-small and down-big, flange diameter is reduced, so resistance to compression strengthens, sealing improves, and effectively utilizes the space, has guaranteed output.
Enlarging the copper pipe tapering is the contact area that increases molten steel, also is to draw the needs of steel pricker degree to satisfy the needs of molten steel in copper pipe as far as possible.Because of copper pipe shortens, reduced the cooling of molten steel, steel billet has just gone out copper pipe so promptly increases output, and to guarantee the intensity and the thickness of steel billet shell, last lower box dislocation is to make it to put into solenoid in order to reduce external form, adapts with former design space.
Change into the external supply channel built-in.Be provided with shower water water supply component 3 around its bottom in water tank 1 inboard, because of the outer water supply of crystallizer has increased external form, change into built-in after, can cooperate with platform space, and reduce dismounting and maintenance from now on.
The built-in source capsule 2 of penetrating is changed into external, be arranged at water tank 1 upper outside, in water tank 1, cause the crystallizer external form too big, and the gland diameter causes the pressure testing distortion to leak too greatly because of penetrating source capsule 2.So consider to change external into, effectively utilized space outerpace, solved key problem in technology.
Former crystallizer is following sufficient roller support 7 to be connected by top flange by four pull bars, both takes up room, makes trouble, easily leaks again, maintenance difficulty is big.The utility model changes in the outside of water tank 1 bottom and is provided with a plurality of rectangular grooves after above-mentioned pull bar is removed, and is connected with sufficient roller support 7 by T type bolt 4, has avoided the appearance of the problems referred to above.
Adopt copper pipe 5 manufacturing process of round mold, silver-bearing copper or phosphorized copper Huo Chrome zirconium copper are extruded into pipe, carry out annealing in process, after the annealing pipe is pressed the crystallizer copper pipe that becomes greater than φ 350mm, after machined and coating processing, just finished product, copper pipe 5 cross dimensions are more than or equal to φ 350mm, crystallizer cooling water seam is formed by stainless steel water jacket and crystallizer copper pipe, the taper design of crystallizer copper pipe 5 is the continuous tapering of parabola, surface of internal cavity adopts Cr coating or composite deposite, adopts the crystallizer of this spline structure, and its steel transportation amount and disposable service life can significantly improve.
Continuous casting is as follows with the concrete parameter of big section round mold:
Crystallizer copper pipe section: φ 408mm
Crystallizer copper length of tube: 780mm
Crystallizer copper thickness of pipe wall: 17.93mm
Crystallizer copper pipe tapering: 4.68mm
Strand radius: 10.5m
Strand pulling rate: 0.6-0.8m/min.

Claims (3)

1, a kind of continuous casting is with big section round mold, include the water tank that the inboard is lined with copper pipe, the sufficient roller support of penetrating source capsule and being connected with water tank, it is characterized in that: be provided with in water tank (1) upper outside and penetrate source capsule (2), be provided with shower water water supply component (3) around its bottom in water tank (1) inboard, the outside in water tank (1) bottom is provided with a plurality of grooves, be connected with sufficient roller support (7) by T type bolt (4), one end of T type bolt (4) is set in the groove of water tank (1) bottom, and its other end passes the upper junction plate of sufficient roller support (7); Copper pipe (5) length of described water tank (1) liner is 700-1000mm, and tapering is 0.05-.0.76mm; The water pipe (6) of sufficient roller support (7) is provided with the shower that multilayer has water nozzle.
2, continuous casting according to claim 1 is with big section round mold, and it is characterized in that: copper pipe (5) tapering of described water tank (1) liner is a kind of of single tapering, many taperings or the continuous tapering of parabola.
3, continuous casting according to claim 1 is with big section round mold, and it is characterized in that: on the water pipe (6) of described sufficient roller support (7) four layers of shower are set preferably, the angle of per two shower water nozzles is 60 ° of angles.
CN 200620152010 2006-12-22 2006-12-22 Large cross section round blank crystallizer for continuous casting Expired - Fee Related CN200988090Y (en)