CN1887251A - Cosmetic composition containing tourmaline and its making process - Google Patents

Cosmetic composition containing tourmaline and its making process Download PDF

Info

Publication number
CN1887251A
CN1887251A CN 200510027504 CN200510027504A CN1887251A CN 1887251 A CN1887251 A CN 1887251A CN 200510027504 CN200510027504 CN 200510027504 CN 200510027504 A CN200510027504 A CN 200510027504A CN 1887251 A CN1887251 A CN 1887251A
Authority
CN
China
Prior art keywords
tourmaline
micron
vacuum filtration
white
broken
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510027504
Other languages
Chinese (zh)
Inventor
孙志峰
王宗钢
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Hongkang Science & Technology Development Co Ltd
Original Assignee
Shanghai Hongkang Science & Technology Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Hongkang Science & Technology Development Co Ltd filed Critical Shanghai Hongkang Science & Technology Development Co Ltd
Priority to CN 200510027504 priority Critical patent/CN1887251A/en
Publication of CN1887251A publication Critical patent/CN1887251A/en
Pending legal-status Critical Current

Abstract

The present invention is one kind of composition containing tourmaline and its making process, and the composition for cosmetics is superfine powder with excellent stable dispersivity and capable of absorbing and radiating biological wave at normal temperature, releasing negative ion constantly and generating biocurrent. It has average size below 0.5 micron and has the main component of 3{NaX3Al6(BO3)3Si6O18(OH9F)4}, where X is Mg, Fe, Li or other atoms. The making process includes sorting material, crushing, grinding, vacuum filtering to dewater, drying and other steps.

Description

A kind of tourmalinization cosmetic compositions and manufacture method thereof of containing
Technical field
The present invention is a kind of compositions and manufacture method thereof that contains tourmaline, particularly a kind of ultra-fine tourmaline powder and manufacture method thereof that is applicable to cosmetic field.
Technical background
Tourmaline is a kind of naturally occurring silicates mineral, and its microstructure is special, have charged lastingly, with uranium (radiant), Magnet (magnetic energy) and be called three macro-energy Ores.Its chemical composition:
3{NaX 3Al 6(BO 3)3Si 6O 18(OH 9F) 4}
X is atoms such as Mg, Fe, Li in the formula.According to different X atoms, tourmaline can present from colourless to red, yellow, green, blue, purple, tea, shades of colour such as black.The pure tourmaline of color and luster is a kind of middle-grade gem, is referred to as " tourmaline " again.Wherein white is dravite.Black is iron tourmaline.
From physical chemistry in essence, that tourmaline has is forever charged, emission far infrared and three kinds of effects of trace element stripping, and its permanent charged character further derives character such as anion, interfacial activity.Therefore, it is widely used in the health care cause of industry, agricultural, environmental protection industry and raising people's quality of life.
Because the energy characteristics that tourmaline had, be used for the usefulness that cosmetics can improve the cosmetics effective ingredient greatly, as antioxidation, anti-ultraviolet damage, antiinflammatory removes speckle, preventing aspect the skin allergy medical value is arranged more, can enhance metabolism, improve skin, hair water and oil and various nutrient absorbing.The emulsifying effectiveness of tourmaline can be avoided adding the chemical interface activating agent in cosmetics, can significantly reduce like this because of contacting chemicals and bring skin allergy or damage.
Tourmaline is the harmless natural inorganic material of a kind of safety non-toxic, it is applied in all kinds of cosmetics, can significantly reduce or cancel use to some chemical substance, it collects multiple function and one, its comprehensive function effect is obvious, be the great innovation of series cosmetics, and will be subjected to consumers in general's welcome deeply.Equally at field of textiles, the fabric that contains tourmaline, under the prerequisite that has kept natural cotton fiber moisture absorption, ventilative, soft, smooth characteristics, because its emitting biological ripple (far infrared) at normal temperatures discharges anion, produce characteristic functions such as bioelectric current and antibacterial deodorizing effect, thereby can improve the little of human body and follow, ring is accelerated blood circulation, enhances metabolism, improve human body natural's immunity and vis medicatrix naturae, play the effect of disease resistance.
But, because tourmaline density is big, the hardness height, for 7.2 grades of Mohs, be stiffer than glass and common iron, be processed into the superfine powder in the cosmetics, need utilize certain high novel technique and equipment, this is the primary difficult problem that tourmaline is applied to fields such as cosmetics or weaving.In addition, the white tourmaline of occurring in nature seldom, price is very expensive, how the aphrizite Lycoperdon polymorphum Vitt powder body that content is more is converted into cosmetics used light color or white powder body, will become a kind of breakthrough invention that tourmaline is used.Having, because tourmaline proportion is bigger, is about 3.5 again, and superfine powder is difficult to be uniformly dispersed in liquid phase, and this also is one technological difficulties that tourmaline is applied to cosmetics.
Summary of the invention
The objective of the invention is to overcome the defective that needs technology, propose a kind of tourmalinization cosmetic compositions and manufacture method thereof of containing, particularly a kind of stable dispersive property, the micropowder that is applicable to cosmetic field and manufacture method thereof with excellence.
Purpose of the present invention can be achieved through the following technical solutions:
Described compositions is that a kind of particle mean size is the superfine powder below 0.5 micron, it is characterized in that its main component is 3{NaX 3Al 6(BO 3) 3Si 6O 18(OH 9F) 4, X is atoms such as Mg, Fe, Li in the formula.
Described compositions superfine powder manufacture method is:
Select suitable dravite,, pulverize and wet method is husky grinds, grind to form particle mean size and be 0.5 micron superfine powder through broken.Its preparation technology is as follows:
1. select materials
Comparatively speaking, white tourmaline output is very low, and is often mixing other Ores, so need select the enrichment ore deposit.
2. broken
To select suitable white tourmaline to adopt gyratory crusher to be broken into the bulk of 8~25mm.
3. pulverize
Adopt thunder to cover pulverizer in broken block tourmaline and be ground into 20~40 microns coarse powder.
4. grind
With the white tourmaline coarse powder of having pulverized, adopting sand mill to grind to form particle mean size is 0.5 micron white tourmaline water slurry, adds an amount of dispersant during grinding.
5. vacuum filtration dehydration
White tourmaline water slurry after grinding is carried out the vacuum filtration dehydration.
6. dry
The filter cake of vacuum filtration is placed baking oven, 110 ℃ of dryings of control temperature 3~4 hours.
7. pulverize
Dried white tourmaline is pulverized once more with the general-purpose pulverizer, and the control mean diameter is finished product packing about 0.5 micron.
The dark or schorl at color, can take calcine technology:
Select suitable black iron tourmaline, become the kermesinus tourmaline, form tourmaline powder through super-fine processing again through the high-temperature calcination processing.Its preparation technology is as follows:
1. the pretreatment of aphrizite
Block with selecting suitable aphrizite to be broken into 5~10mm size.
2. pulverize
Adopt thunder illiteracy pulverizer to be ground into 20~40 microns coarse powder the aphrizite of fragmentation.
3. calcination processing
The aphrizite of having pulverized is put into porcelain crucible place 500 ℃~800 ℃ of muffle furnace control temperature, calcined 1~3 hour.
4. grind
Adopting sand mill to grind to form particle mean size the coarse powder after the calcining is 0.5 micron tourmaline water slurry.
5. vacuum filtration dehydration
White tourmaline water slurry after grinding is carried out the vacuum filtration dehydration.
6. dry
The filter cake of vacuum filtration is placed baking oven, 110 ℃ of dryings of control temperature 3~4 hours.
7. pulverize again
Exsiccant tourmaline is pulverized with the general-purpose pulverizer, and the control particle mean size is about 0.5 micron, is finished product and packs.
Compare prior art, the present invention has following outstanding feature:
1, gained superfine white tourmaline powder body of the present invention, Yin Seze are white, remedied the Lycoperdon polymorphum Vitt tourmaline powder and use inconvenient field in cosmetics, can use all kinds of cosmetics.Can meet the need of market to greatest extent and the requirement of consumer.
In essence, that tourmaline has is forever charged, emission far infrared and three kinds of effects of trace element stripping, and its permanent charged character further derives character such as anion, interfacial activity.Because after the ultra-fine processing, its surface area increases, surface energy level also increases, and therefore can bring into play its effect to a greater extent.
During should applying some make up, can improve powder body of the present invention the usefulness of effective ingredient in the cosmetics greatly, as antioxidation, anti-ultraviolet damage, antiinflammatory removes speckle, is preventing aspect the skin allergy medical value is arranged more, can enhance metabolism, improve skin, hair water and oil and various nutrient absorbing.The emulsifying effectiveness of tourmaline can be avoided adding the chemical interface activating agent in cosmetics, can significantly reduce like this because of contacting chemicals and bring skin allergy or damage.
A large number of experiments show that tourmaline powder of the present invention not only can make the water of macromole bunch group diminish, and is penetrated into easily in the tissue, by human body cell is absorbed after adding cosmetics.Can prevent that skin dehydration is aging, promote the absorption of hair nutritional labeling.And, can make the oil component fine dispersion in the cosmetics, prevent cosmetics go bad corruption, layering etc., can add other artificial interfacial agents, can make the grease emulsifying of skin surface, clean easily, make cell hydrophilicization, strengthen the resistance against diseases of human body.
Embodiment
Example one: get 10 kilograms of white tourmaline Ores and be broken into the bulk of 8~25mm, cover pulverizer with thunder and be ground into 20~40 microns coarse powder with gyratory crusher.With coarse powder by tourmaline: the ratio row of water=1: 4 are made into the tourmaline water slurry, with sand mill wet grinding to mean diameter is 0.5 micron tourmaline water slurry, to the dehydration of the slurry of the white appliances gas stony edema after grinding vacuum filtration, place baking oven 110 ℃ of dryings 3.5 hours filter cake.White tourmaline powder after the oven dry is pulverized once more with the general-purpose pulverizer, obtained particle mean size and be 0.5 micron white tourmaline fine powder.
Example two: get 10 kilograms of aphrizite Ores, use the gyratory crusher fragmentation, pulverize with Raymond machine, coarse powder, put in the muffle furnace 500 ℃ of temperature lower calcinations 2 hours, shallow kermesinus tourmaline coarse powder, with coarse powder by tourmaline: the ratio row of water=1: 4 are made into the tourmaline water slurry, with sand mill wet grinding to mean diameter is 0.5 micron tourmaline water slurry, to the light tourmaline water slurry vacuum filtration dehydration after grinding, will consider cake and place baking oven 110 ℃ of dryings 3.5 hours.Light tourmaline powder after the oven dry is pulverized once more with the general-purpose pulverizer, obtained particle mean size and be 0.5 micron light tourmaline fine powder.

Claims (3)

1, a kind of tourmalinization cosmetic compositions that contains is that a kind of particle mean size is the superfine powder below 0.5 micron, it is characterized in that its main component is 3{NaX 3Al 6(BO 3) 3Si 6O 18(OH 9F) 4, X is atoms such as Mg, Fe, Li in the formula.
2, a kind of preparation method that contains the tourmalinization cosmetic compositions is with dravite, through broken, pulverizes and wet method is husky grinds, and grinds to form particle mean size and be 0.5 micron superfine powder, it is characterized in that described technology is:
1. select materials
Select the enrichment ore deposit, select suitable white tourmaline;
2. broken
Adopt gyratory crusher to be broken into the bulk of 8~25mm;
3. pulverize
Adopt thunder to cover pulverizer in broken block tourmaline and be ground into 20~40 microns coarse powder;
4. grind
With the white tourmaline coarse powder of having pulverized, adopting sand mill to grind to form particle mean size is 0.5 micron white tourmaline water slurry, adds an amount of dispersant during grinding;
5. vacuum filtration dehydration
White tourmaline water slurry after grinding is carried out the vacuum filtration dehydration;
6. dry
The filter cake of vacuum filtration is placed baking oven, 110 ℃ of dryings of control temperature 3~4 hours;
7. pulverize
Dried white tourmaline is pulverized once more with the general-purpose pulverizer, and the control mean diameter is finished product packing about 0.5 micron.
3, one contain the preparation method of tourmalinization cosmetic compositions, are with the black iron tourmaline, handle through high-temperature calcination to become the kermesinus tourmaline, form tourmaline powder through super-fine processing again, it is characterized in that described manufacturing process is:
1. the pretreatment of aphrizite
Block with selecting suitable aphrizite to be broken into 5~10mm size;
2. pulverize
Adopt thunder illiteracy pulverizer to be ground into 20~40 microns coarse powder the aphrizite of fragmentation;
3. calcination processing
The aphrizite of having pulverized is put into porcelain crucible place 500 ℃~800 ℃ of muffle furnace control temperature, calcined 1~3 hour;
4. grind
Adopting sand mill to grind to form particle mean size the coarse powder after the calcining is 0.5 micron tourmaline water slurry, adds an amount of dispersant during grinding;
5. vacuum filtration dehydration
White tourmaline water slurry after grinding is carried out the vacuum filtration dehydration;
6. dry
The filter cake of vacuum filtration is placed baking oven, 110 ℃ of dryings of control temperature 3~4 hours;
7. pulverize again
Exsiccant tourmaline is pulverized with the general-purpose pulverizer, and the control particle mean size is about 0.5 micron, is finished product and packs.
CN 200510027504 2005-06-30 2005-06-30 Cosmetic composition containing tourmaline and its making process Pending CN1887251A (en)