CN1837741A - 带有内螺旋加强筋的纤维增强塑料筒及其制备方法 - Google Patents
带有内螺旋加强筋的纤维增强塑料筒及其制备方法 Download PDFInfo
- Publication number
- CN1837741A CN1837741A CN 200610009827 CN200610009827A CN1837741A CN 1837741 A CN1837741 A CN 1837741A CN 200610009827 CN200610009827 CN 200610009827 CN 200610009827 A CN200610009827 A CN 200610009827A CN 1837741 A CN1837741 A CN 1837741A
- Authority
- CN
- China
- Prior art keywords
- cylindrical shell
- reinforcement
- inside spin
- fiber
- resin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (10)