CN1785681A - Eyeglass fitting part having screen printing pattern and technological method of its surface treatment - Google Patents

Eyeglass fitting part having screen printing pattern and technological method of its surface treatment Download PDF

Info

Publication number
CN1785681A
CN1785681A CN 200510034185 CN200510034185A CN1785681A CN 1785681 A CN1785681 A CN 1785681A CN 200510034185 CN200510034185 CN 200510034185 CN 200510034185 A CN200510034185 A CN 200510034185A CN 1785681 A CN1785681 A CN 1785681A
Authority
CN
China
Prior art keywords
pattern
coating
glasses accessory
background color
glasses
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200510034185
Other languages
Chinese (zh)
Other versions
CN100382979C (en
Inventor
高志乐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LONGGANG NANYUE RONGDIAN METAL PRODUCT FACTORY LONGGANG DISTRICT SHENZHEN CITY
Original Assignee
LONGGANG NANYUE RONGDIAN METAL PRODUCT FACTORY LONGGANG DISTRICT SHENZHEN CITY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LONGGANG NANYUE RONGDIAN METAL PRODUCT FACTORY LONGGANG DISTRICT SHENZHEN CITY filed Critical LONGGANG NANYUE RONGDIAN METAL PRODUCT FACTORY LONGGANG DISTRICT SHENZHEN CITY
Priority to CNB2005100341859A priority Critical patent/CN100382979C/en
Publication of CN1785681A publication Critical patent/CN1785681A/en
Application granted granted Critical
Publication of CN100382979C publication Critical patent/CN100382979C/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A glasses' fitting with silk screen printed pattern is composed of basic material and a pattern consisting two plated layers. A technology for preparing said glasses' fitting and treating its surface includes such steps as inputting a chosen pattern to computer, making-up electronic plates, preparing films and silk screen printing impression, electroplating a priming color layer on the basic material of said glass's fitting, silk screen printing, cleaning, baking, electroplating another color layer different from priming color, removing ink oil, washing, and plating a transparent protective layer.

Description

A kind of glasses accessory and surface-treated process thereof with screen printing pattern
Technical field
The present invention relates to glasses accessory and surface treatment thereof, particularly, relate to accessory such as spectacle-frame, nose-bridge frame, village head and leg of spectacles and in the process of above-mentioned accessory surface character silk printing, pattern, trade mark, mark.
Background technology
Existing glasses accessory generally is to adopt spraying, go up the wet goods process of surface treatment lip-deep to glasses accessory of pattern, decorative pattern or brand printing with aesthetic feeling, and this more original process of surface treatment definition is not enough, and very not wear-resisting.Application number is that 02107032.6 Chinese invention patent application discloses a kind of picture frame and processing method thereof with intaglio processed pattern, this method is to utilize laser beam to frame, nose-bridge frame, glasses annexes such as mirror leg carry out the moon and carve processing, thereby form surface-treated layer with pattern, though said method has solved spraying to a certain extent, last wet goods surface treatment is peeled off and wear problems easily, but because its pattern outer surface has the obvious cloudy indenture of carving, surface texture is poor, and cloudy the quarter can be damaged base material, in addition, because the glasses annex is little and meticulous, the exquisite degree of the cloudy needle drawing case of laser still remains to be improved.
Summary of the invention
The technical problem to be solved in the present invention is to design a kind of glasses accessory of screen printing pattern and process that forms screen printing pattern of having at the defective of prior art.
The technical solution used in the present invention is as follows: at the existing glasses accessory surface-treated shortcoming that comprises spectacle-frame, nose-bridge frame, village head and leg of spectacles, the present invention adopts the silk-screen galvanic corrosion technology of the exquisite pattern of easy formation, and the bottom of screen printing pattern plate surface with outside electroplate the surface. form background color coating respectively and be superimposed upon on the background color coating and different second coating of color, thus then by removing part second coating acquisition pattern.Glasses accessory surface-treated galvanic corrosion process of the present invention has two kinds.
First kind of process comprises the steps:
A. with the pattern selected for use input computer, described pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds, and pattern is done to set type to handle makes it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material and electroplate a background color coating earlier;
D. the glasses accessory that is coated with background color coating is placed on and carries out silk-screen acquisition screen printing pattern on the described silk-screen mould;
E. dry the figuratum glasses accessory of silk-screen after the decontamination;
F. the glasses accessory after will drying carries out the electroplating processes second time different with the background color coating color, makes described silk-screen oil pattern be retained in the accessory surface;
G. the pattern stamp-pad ink on the glasses accessory is removed and do last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate color for the second time on the surface of glasses accessory thus is background colour, and recessed background color is the art pattern that lines are drawn.
After described step g, also comprise the steps,
H. electroplate outermost transparency protected coating.
Step h is omissible, but adds that the art pattern that behind the protective clear layer glasses accessory surface will be formed does not does not wear and tear colour-fast.
Drying of above-mentioned steps e is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, and Best Times is 30 minutes, dries that the temperature maintenance in the stove is at 130~150 degree Celsius in the process, and optimum temperature is 140 degree Celsius.
Described screen printing pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds.
Second kind of glasses accessory surface-treated method of the present invention comprises the steps:
A. with the pattern selected for use input computer, described pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds, and pattern is done to set type to handle makes it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material and electroplate a background color coating earlier;
D. glasses accessory is electroplated once more and is obtained second coating different with background color coating;
E. the accessory after will electroplating is placed on and carries out silk-screen acquisition paint patterns on the silk-screen mould;
F. dry the figuratum glasses accessory of silk-screen after the decontamination;
G. the glasses accessory surface is not removed by second coating that paint patterns covers, can not take off to hinder and electroplate the bottom and the oil of winding up the case.
H. the pattern stamp-pad ink on the glasses accessory is removed and does last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate background color for the first time on the surface of glasses accessory thus is background colour, and electroplating color the second time of epirelief is the art pattern that lines are drawn.
As first kind of process, after described step h, also comprise the steps,
I. electroplate outermost transparency protected coating.
Step I is omissible, but adds that the art pattern that behind the protective clear layer glasses accessory surface will be formed does not does not wear and tear colour-fast.
Drying of above-mentioned steps f is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, and Best Times is 30 minutes, dries that the temperature maintenance in the stove is at 130~150 degree Celsius in the process, and optimum temperature is 140 degree Celsius.
Described screen printing pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds.
The layer structure of carrying out the surface-treated glasses accessory through above-mentioned first kind of technology is: comprise the pattern on glasses accessory base material and this base material outer surface, described pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds; Described pattern be by on the background color coating on the described glasses accessory base material and the background color coating, second coating different with background color constituted, the lines of pattern are by removing second coating, appearing the acquisition of background color coating, therefore described pattern is to be background colour with second coating, and background color coating is that lines are formed.
Colour-fast for pattern is not is not worn and torn, on described pattern, also cover a transparency protected coating.
The layer structure of carrying out the surface-treated glasses accessory through above-mentioned second kind of technology is: the pattern on glasses accessory base material and this base material outer surface, described pattern comprise the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds; Described pattern be by on the background color coating on the described glasses accessory base material and the background color coating, second coating different with background color constituted, the lines of pattern are to obtain by removing lines second coating in addition, therefore described pattern is to be background colour with background color coating, and second coating that is superimposed upon on the background color coating is that lines are formed.
Colour-fast for pattern is not is not worn and torn, on described pattern, also cover a transparency protected coating.
Compared with prior art, process of the present invention has following advantage: technology is simple, and is bright-colored various, and surperficial adhesion is good.
Description of drawings
Fig. 1 is the flow chart of first kind of process of glasses accessory surface treatment of the present invention;
Fig. 2 is the flow chart of second kind of process of glasses accessory surface treatment of the present invention;
Fig. 3 is the layer structure schematic diagram through glasses accessory behind the process of surface treatment of Fig. 1;
Fig. 4 is the layer structure schematic diagram through glasses accessory behind the process of surface treatment of Fig. 2.
The specific embodiment
The invention will be further described below in conjunction with accompanying drawing and embodiment shown in the drawings.
The present invention is a kind of to other glasses accessory except that glass lens, carry out the surface-treated new process as spectacle-frame, nose-bridge frame, village head and leg of spectacles, the purpose of this process is to form the long-lived exquisite pattern in glasses accessory surface, to improve the added value of eyewear products.Process of the present invention has following two kinds of embodiment.
Embodiment one: glasses accessory surface-treated process as shown in Figure 1.Its step is as follows:
A. with the pattern input computer of selecting for use, pattern is done the composing processing make it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material 1 and electroplate a background color coating 2 earlier;
D. the glasses accessory that is coated with background color coating 2 is placed on and carries out silk-screen acquisition screen printing pattern on the described silk-screen mould;
E. dry the figuratum glasses accessory of silk-screen after the decontamination; Drying is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, and roasting 30 minutes of best stove dries that the temperature maintenance in the stove is at 130~150 degree Celsius in the process, and optimum temperature maintains 140 degree Celsius;
F. the glasses accessory after will drying carries out the electroplating processes second time different with background color coating 2 colors, forms second coating 4, makes described silk-screen oil pattern be retained in the accessory surface;
G. the pattern stamp-pad ink on the glasses accessory is removed and do last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate color for the second time on the surface of glasses accessory thus is background colour, and recessed background color is the art pattern 3 that lines are drawn.
H. electroplate outermost transparency protected coating 5, the art pattern 3 that the glasses accessory surface is formed does not does not wear and tear colour-fast.
So far the surface treatment of glasses accessory finishes.The layer structure of the glasses accessory that screen printing pattern is arranged after above-mentioned artistic face is handled as shown in Figure 3.Comprise: the pattern 3 on glasses accessory base material 1 and this base material 1 outer surface, described pattern 3 be by on the background color coating 2 on the described glasses accessory base material 1 and the background color coating 2, second coating 4 different with background color constituted, the lines of pattern 3 are by removing second coating 4, appearing 2 acquisitions of background color coating, therefore described pattern 3 is to be background colour with second coating 4, and background color coating 2 is formed for lines.Also be coated with transparency protected coating 5 on the described pattern 3, this protective coating 5 makes pattern 3 not frayed in the process of using glasses accessory, and colour-fast.
Embodiment two: glasses accessory surface-treated process as shown in Figure 2.Its step is as follows:
A. with the pattern input computer of selecting for use, pattern is done the composing processing make it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material 1 and electroplate a background color coating 2 earlier;
D. glasses accessory is electroplated once more and is obtained second coating 4 different with background color coating;
E. the accessory after will electroplating is placed on and carries out silk-screen acquisition paint patterns on the silk-screen mould;
F. dry the figuratum glasses accessory of silk-screen after the decontamination; Drying is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, and roasting 30 minutes of best stove dries that the temperature maintenance in the stove is at 130~150 degree Celsius in the process, and optimum temperature maintains 140 degree Celsius;
G. the glasses accessory surface is not removed by second coating 4 that paint patterns covers, can not take off to hinder and electroplate the bottom 2 and the oil of winding up the case.
H. the pattern stamp-pad ink on the glasses accessory is removed and does last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate background color for the first time on the surface of glasses accessory thus is background colour, and electroplating color the second time of epirelief is the art pattern 3 that lines are drawn;
I. electroplate outermost transparency protected coating 5, the art pattern 3 that the glasses accessory surface is formed does not does not wear and tear colour-fast.
The layer structure of carrying out the surface-treated glasses accessory through the technology of the foregoing description two is: comprise the pattern 3 on glasses accessory base material 1 and this base material 1 outer surface, described pattern 3 be by on the background color coating 2 on the described glasses accessory base material 1 and the background color coating 2, second coating 4 different with background color constituted, the lines of pattern 3 are to obtain by removing lines second coating 4 in addition, therefore described pattern 3 is to be background colour with background color coating 2, is superimposed upon that second coating 4 on the background color coating 2 forms for lines; Also cover a transparency protected coating 5 on described pattern 3, this protective coating 5 does not does not wear and tear patterned layer 3 in the process of using glasses accessory colour-fast, as shown in Figure 4.
Screen printing pattern of the present invention comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds.

Claims (10)

1, a kind of in glasses accessory surface-treated process, described glasses accessory comprises spectacle-frame, nose-bridge frame, village head and leg of spectacles, it is characterized in that this method comprises the steps:
A. with the pattern selected for use input computer, described pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds, and pattern is done to set type to handle makes it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material (1) and electroplate a background color coating (2) earlier;
D. the glasses accessory that is coated with background color coating (2) is placed on and carries out silk-screen acquisition screen printing pattern on the described silk-screen mould;
E. dry the figuratum glasses accessory of silk-screen after the decontamination;
F. the glasses accessory after will drying carries out and the different electroplating processes second time of background color coating (2) color, forms second coating (4), makes described silk-screen oil pattern be retained in the accessory surface;
G. the pattern stamp-pad ink on the glasses accessory is removed and does last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate color for the second time on the surface of glasses accessory thus is background colour, and recessed background color is the art pattern (3) that lines are drawn.
2, glasses accessory surface-treated process according to claim 1 is characterized in that: after described step g, also comprises the steps,
H. electroplate outermost transparency protected coating (5), the art pattern (3) that the glasses accessory surface is formed does not does not wear and tear colour-fast.
3, glasses accessory surface-treated process according to claim 1 is characterized in that: drying of described step e is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, and the best is 30 minutes; Dry temperature maintenance in the stove in the process at 130~150 degree Celsius, optimum temperature is 140 degree Celsius.
4, a kind of in glasses accessory surface-treated process, described glasses accessory comprises spectacle-frame, nose-bridge frame, village head and leg of spectacles, it is characterized in that this method comprises the steps:
A. with the pattern selected for use input computer, described pattern comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds, and pattern is done to set type to handle makes it more exquisite;
B. the pattern of handling setting type carries out the film to handle and make the silk-screen mould of described pattern stand-by;
C. needs are made surface-treated glasses accessory base material (1) and electroplate a background color coating (2) earlier;
D. glasses accessory is electroplated once more and is obtained second coating (4) different with background color coating;
E. the accessory after will electroplating is placed on and carries out silk-screen acquisition paint patterns on the silk-screen mould;
F. dry the figuratum glasses accessory of silk-screen after the decontamination;
G. the glasses accessory surface is not removed by second coating (4) that paint patterns covers, electroplate bottom (2) but can not take off to hinder;
H. the pattern stamp-pad ink on the glasses accessory is removed and does last cleaning, should avoid when removing stamp-pad ink taking off and hinder ground and electrodeposited coating, forming to electroplate background color for the first time on the surface of glasses accessory thus is background colour, and electroplating color the second time of epirelief is the art pattern (3) that lines are drawn.
5, glasses accessory surface-treated process according to claim 4 is characterized in that: after described step h, also comprises the steps,
I. electroplate outermost transparency protected coating (5), the art pattern (3) that the glasses accessory surface is formed does not does not wear and tear colour-fast.
6, glasses accessory surface-treated process according to claim 4, it is characterized in that: drying of described step f is that the glasses accessory after the decontamination cleaning was put into stove roasting 25~35 minutes, the best is 30 minutes, dry temperature maintenance in the stove in the process at 130~150 degree Celsius, optimum temperature is 140 degree Celsius.
7, a kind of glasses accessory that utilizes the described process of claim 1 to make, comprise the pattern (3) on glasses accessory base material (1) and this base material (1) outer surface, described pattern (3) comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds; It is characterized in that:
Described pattern (3) be by on the background color coating (2) on the described glasses accessory base material (1) and the background color coating (2), second coating (4) different with background color constituted, the lines of pattern (3) are by removing second coating (4), appearing background color coating (2) acquisition, therefore described pattern (3) is to be background colour with second coating (4), and background color coating (2) is formed for lines.
8, the glasses accessory that screen printing pattern is arranged according to claim 7; it is characterized in that: also cover a transparency protected coating (5) on described pattern (3), this protective coating (5) does not does not wear and tear patterned layer (3) in the process of using glasses accessory colour-fast.
9, a kind of glasses accessory that utilizes the described process of claim 4 to make, comprise the pattern (3) on glasses accessory base material (1) and this base material (1) outer surface, described pattern (3) comprises the combination of a kind of in art pattern, decorative pattern, literal, trade mark, the mark or some kinds; It is characterized in that:
Described pattern (3) be by on the background color coating (2) on the described glasses accessory base material (1) and the background color coating (2), second coating (4) different with background color constituted, the lines of pattern (3) are to obtain by removing lines second coating (4) in addition, therefore described pattern (3) is to be background colour with background color coating (2), is superimposed upon that second coating (4) on the background color coating (2) forms for lines.
10, the glasses accessory that screen printing pattern is arranged according to claim 9; it is characterized in that: also cover a transparency protected coating (5) on described pattern (3), this protective coating (5) does not does not wear and tear patterned layer (3) in the process of using glasses accessory colour-fast.
CNB2005100341859A 2005-04-15 2005-04-15 Eyeglass fitting part having screen printing pattern and technological method of its surface treatment Expired - Fee Related CN100382979C (en)