CN1782237A - 防渗和保水的方法 - Google Patents
防渗和保水的方法 Download PDFInfo
- Publication number
- CN1782237A CN1782237A CN 200510093354 CN200510093354A CN1782237A CN 1782237 A CN1782237 A CN 1782237A CN 200510093354 CN200510093354 CN 200510093354 CN 200510093354 A CN200510093354 A CN 200510093354A CN 1782237 A CN1782237 A CN 1782237A
- Authority
- CN
- China
- Prior art keywords
- water
- clay
- basis
- weight portion
- rich
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
一种防渗和保水的方法,包括以下步骤:(1)、拨开表层土壤20~50cm,并将新露出来的地面整平、压实;(2)、在搅拌装置中放入轻粘土或重粘土和水,其中轻粘土或重粘土与水的体积比为1∶1~1∶2,搅拌均匀且沉淀后,令其上半层流入步骤(1)整平、压实的地面上,形成5~8cm的隔离层;(3)、将步骤(1)中拨开的土回填至隔离层上方。其目的是提供一种成本低,防渗、保水效果显著的防渗和保水的方法。
Description
技术领域
本发明涉及一种防渗和保水的方法,以改良水田、池塘、湖泊、旱地和盐碱地的防渗和保水特性。
背景技术
在水资源日益紧张的今天,减少水资源的浪费对保障国家经济的发展和人们的正常生活具有非常重要的意义,尤其是对于农业、林业和渔业生产,但现有的许多农田、池塘、湖泊由于地下土质结构的问题,使得农田、池塘、湖泊中的大量水资源通过渗漏流失掉,造成水资源的大量浪费,严重影响当地经济的发展和人们的正常生活。
发明内容
本发明的目的是提供一种成本较低,防渗、保水效果显著的水田、池塘、湖泊、旱地和盐碱地防渗和保水的方法。
本发明防渗和保水的方法,在用于治理旱地时包括以下步骤:
(1)、拨开表层土壤20~50cm,并将新露出来的地面整平、压实;
(2)、在搅拌装置中放入轻粘土或重粘土和水,其中轻粘土或重粘土与水的体积比为1∶1~1∶2,搅拌均匀且沉淀后,令其上半层流入步骤(1)整平、压实的地面上,形成5~8cm的隔离层;
(3)将步骤(1)中拨开的土回填至隔离层上方。
本发明防渗和保水的方法,在用于水田、池塘和湖泊时,该方法包括以下步骤:
(1)、将需要治理的地表面整平、压实;
(2)、在步骤(1)的基础上再铺一层5~8cm的轻粘土或重粘土与细砂的混合物用来制作隔离层,其中轻粘土或重粘土的重量份为7~9,细砂的重量份为1~3;
(3)、在步骤(2)的基础上放水浸泡,使水面没过其表面并浸透;
(4)、在步骤(3)的基础上,使用水耙轮搅拌,搅拌均匀后沉淀至水清。
本发明防渗和保水的方法,在用于水田、池塘或湖泊时,该方法还包括以下步骤:
(5)、在步骤(4)的基础上注入一定深度的水观察,若发现有水渗漏,再铺上2~5cm的轻粘土或重粘土;
(6)、在步骤(5)的基础上放水浸泡,令水面没过其表面并浸透;
(7)、在步骤(6)的基础上使用水耙轮搅拌,搅拌均匀后沉淀至水清。
本发明防渗和保水的方法,在用于水田、池塘和湖泊时,还包括以下步骤:
(8)、对四周的边围进行整理,使其成为20°-40°的斜坡;
(9)、在步骤(8)的基础上在四周的边围上均匀的涂抹3~5cm的泥浆,其中泥浆采用轻粘土或重粘土加水和成;
(10)、在步骤(9)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(11)、在步骤(10)的基础上,在四周边围再涂抹1~3cm的泥浆,其中泥浆采用轻粘土或重粘土加水和成;
(12)、在步骤(11)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(13)、在步骤(12)的基础上,对斜坡进行湿法养护10-20天。
本发明防渗和保水的方法,其中所述轻粘土或重粘土中还添加有氯化钠和生石灰,其中轻粘土或重粘土的重量份为1000~10000,氯化钠的重量份为0.001~1,生石灰的重量份为0.1~2。
本发明防渗和保水的方法,在需要治理的地表面以上或以下形成一定厚度的隔离层,实施起来比较简单,成本低,防渗、保水效果显著。
下面对本发明的用多功能隔离层防渗和保水的方法的具体实施方式作进一步详细说明。
具体实施方式
实施例1旱地治理
包括以下步骤:
(1)、拨开表层土壤20cm、30cm或50cm,并将新露出来的地面整平、压实;
(2)、在搅拌装置中放入轻粘土和水,其中重粘土与水的体积比为1∶1或1∶1.5或1∶2,搅拌均匀且沉淀后,令其上半层流入步骤(1)整平、压实的地面上,形成5cm或7cm或8cm的隔离层;
(3)将步骤(1)中拨开的土回填至隔离层上方。
其中所述步骤(1)中重粘土中还可以添加有氯化钠,其中轻粘土重量份为1000或2000或3000或4000或5000或6000或7000或8000或9000或10000,氯化钠的重量份为0.001或0.01或0.05或0.09或0.1或0.3或0.6或1。
本实施例的方法也可以用于治理水田、池塘或湖泊。
实施例2池塘治理
把池塘的水放干后,进行以下步骤:
(1)、将池塘地表面整平、压实;
(2)、在步骤(1)的基础上再铺一层7cm或8cm的轻粘土与细砂的混合物用来制作隔离层,其中轻粘土的重量份为9或8,细砂的重量份为1或2;
(3)、在步骤(2)的基础上放水浸泡,使水面没过其表面并浸透;
(4)、在步骤(3)的基础上,使用水耙轮搅拌,搅拌均匀后沉淀至水清。
(5)、在步骤(4)的基础上注入一定深度的水观察,若发现有水渗漏,再铺上2cm或4cm的轻粘土;
(6)、在步骤(5)的基础上放水浸泡,令水面没过其表面并浸透;
(7)、在步骤(6)的基础上使用水耙轮搅拌,搅拌均匀后沉淀至水清。
(8)、对池塘四周的边围进行整理,使其成为20°或30°或40°的斜坡;
(9)、在步骤(8)的基础上在四周的边围上均匀的涂抹3cm或4cm或5cm的泥浆,其中泥浆采用轻粘土加水和成;
(10)、在步骤(9)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(11)、在步骤(10)的基础上,在四周边围再涂抹1cm或2cm或3cm的泥浆,其中泥浆采用轻粘土或重粘土加水和成;
(12)、在步骤(11)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(13)、在步骤(12)的基础上,对斜坡进行湿法养护10天或12天或15天或16天或18天或20天。
其中所述步骤(1)中轻粘土中还可以添加有化钠,其中轻粘土重量份为1000或2000或3000或4000或5000或6000或7000或8000或9000或10000,氯化钠的重量份为0.001或0.01或0.05或0.09或0.1或0.3或0.6或1。
本实施例的方法也可以用于治理水田、湖泊。
Claims (6)
1.一种用于旱地和盐碱地的防渗和保水方法,其特征在于:
(1)、拨开表层土壤20~50cm,并将新露出来的地面整平、压实;
(2)、在搅拌装置中放入轻粘土或重粘土和水,其中轻粘土或重粘土与水的体积比为1∶1~1∶2,搅拌均匀且沉淀后,令其上半层流入步骤(1)整平、压实的地面上,形成5~8cm的隔离层;
(3)将步骤(1)中拨开的土回填至隔离层上方。
2.一种防渗和保水方法,其特征在于:该方法包括以下步骤:
(1)、将需要治理的地表面整平、压实;
(2)、在步骤(1)的基础上再铺一层5~8cm的轻粘土或重粘土与细砂的混合物,其中轻粘土或重粘土的重量份为7~9,细砂的重量份为1~3;
(3)、在步骤(2)的基础上放水浸泡,使水面没过其表面并浸透;
(4)、在步骤(3)的基础上,使用水耙轮搅拌,搅拌均匀后沉淀至水清。
3.根据权利要求2所述防渗和保水方法,其特征在于:还包括以下步骤:
(5)、在步骤(4)的基础上注入一定深度的水观察,若发现有水渗漏,再铺上2~5cm的轻粘土或重粘土;
(6)、在步骤(5)的基础上放水浸泡,令水面没过其表面并浸透;
(7)、在步骤(6)的基础上使用水耙轮搅拌,搅拌均匀后沉淀至水清。
4.根据权利要求3所述防渗和保水方法,其特征在于:该方法包括以下步骤:
(8)、对四周的边围进行整理,使其成为20°-40°的斜坡;
(9)、在步骤(8)的基础上在四周的边围上均匀的涂抹3~5cm的泥浆,其中泥浆采用轻粘土或重粘土加水和成;
(10)、在步骤(9)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(11)、在步骤(10)的基础上,在四周边围再涂抹1~3cm的泥浆,其中泥浆采用轻粘土或重粘土加水和成;
(12)、在步骤(11)的基础上,待涂抹的泥浆晒干至龟裂后进行夯实;
(13)、在步骤(12)的基础上,对斜坡进行湿法养护10-20天。
5.根据权利要求1所述的防渗和保水的方法,其特征在于:所述轻粘土或重粘土中还添加有氯化钠和生石灰,其中轻粘土或重粘土的重量份为1000~10000,氯化钠的重量份为0.001~1,生石灰的重量份为0.1~2。
6.根据权利要求2或3或4所述的防渗和保水的方法,其特征在于:所述轻粘土或重粘土中还添加有氯化钠和生石灰,其中轻粘土或重粘土的重量份为1000~10000,氯化钠的重量份为0.001~1,生石灰的重量份为0.1~2。