CN1704354A - 漂浮晶及漂浮液的配制方法 - Google Patents

漂浮晶及漂浮液的配制方法 Download PDF

Info

Publication number
CN1704354A
CN1704354A CN 200410019476 CN200410019476A CN1704354A CN 1704354 A CN1704354 A CN 1704354A CN 200410019476 CN200410019476 CN 200410019476 CN 200410019476 A CN200410019476 A CN 200410019476A CN 1704354 A CN1704354 A CN 1704354A
Authority
CN
China
Prior art keywords
floating
crystalline substance
flotation fluid
seawater
human body
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200410019476
Other languages
English (en)
Other versions
CN1321914C (zh
Inventor
陈侠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin University of Science and Technology
Original Assignee
Tianjin University of Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin University of Science and Technology filed Critical Tianjin University of Science and Technology
Priority to CNB2004100194766A priority Critical patent/CN1321914C/zh
Publication of CN1704354A publication Critical patent/CN1704354A/zh
Application granted granted Critical
Publication of CN1321914C publication Critical patent/CN1321914C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明是提供一种生产工艺简单、成本低廉的漂浮晶及漂浮液的生产方法。本发明漂浮晶包括硫酸镁2.5%-15%、氯化钠40.0%-1.0%、氯化钾4.06%-18%、氯化镁30%-75%、溴化钠5%-0.01%。将漂浮晶适量加入自来水或15°Br’以下的海水中即可制成无色透明的漂浮液,并能使人体自然漂浮。用之可以在室内外建设大型人工死海或小型漂浮浴池,且一次配制后通过本发明的附带净化技术可使水质保持清澈透明,不需再加漂浮晶即可长期使用。

Description

漂浮晶及漂浮液的配制方法
                              技术领域
本发明涉及海洋卤水化工技术领域,更具体的说,是涉及一种漂浮浴(人工死海)中漂浮晶及漂浮液的配制方法。
                              背景技术
在进行海洋化工的研究中发现澄澈溶液中的K+、Na+、Ca2+、Mg2+、SO4 2-、Br-、CI-等离子在合适浓度下,能通过人体的皮肤进行吸收可促进人体的新陈代谢及微循环,并对人们的过度疲劳、失眠健忘、平衡失调、以及皮肤病等有明显的缓解作用,且用它们可以配制成无色透明的液体,使人体自然漂浮,比天然的死海更具优越性。目前的现有技术中此方面尚属空白。
                              发明内容
本发明的目的是为了填补现有技术中的空白,提供一种生产工艺简单、成本低廉的漂浮晶及利用漂浮晶产品适量加入自来水或15°Br’以下的海水中即可配制成能使正常人体自然漂浮的漂浮液的方法。
本发明漂浮晶,通过下述技术方案予以实现,包括以下组分(按重量百分比组成):硫酸镁2.5%-15%、氯化钠40.0%-1.0%、氯化钾4.06%-18%、氯化镁30%-75%、溴化钠5%-0.01%。
本发明漂浮晶还包括组分硫酸铜0.01%-0.06%。
本发明漂浮液的配制方法,包括下述步骤:首先向自来水或15°Br’以下的海水中添加如权利要求1所述的漂浮晶,配制成高密度溶液,其浓度为23~28°Br’;然后经过超滤或多介质过滤;最后经过净化消毒杀菌,即可得到能使人体自然漂浮的漂浮液。
本发明溶液中的K+、Na+、Ca2+、Mg2+、SO4 2-、Br-、CI-等离子在合适浓度下,能通过人体的皮肤进行吸收,可促进人体的新陈代谢及微循环,并对人们的过度疲劳、失眠健忘、平衡失调、以及皮肤病等有明显的缓解作用,且用它们可以配制成无色透明的液体,使人体自然漂浮,比天然的死海更具优越性。本发明溶液不仅能自然漂浮,且对人体及皮肤无刺激性,能促进人体代谢和微循环。
使用本发明方法可以生产漂浮晶产品,并可在室内外建设大型人工死海或小型漂浮浴池,且一次配制后通过本发明中的净化技术不需再加漂浮晶即可以长期使用。
                         具体实施方式
下面结合实施例对本发明做进一步描述。
实施例1:适用于淡水的固体漂浮晶(1#)的配制:
按下列比例配制:
物质名称               (质量%)
MgSO4                 9.82
NaCl                   36.18
KCl                    12.06
MgCl2                 41.37
NaBr                   0.56
CuSO4                 0.01
用实施例1的漂浮晶配制1m3的漂浮液时,需用漂浮晶286kg加入915kg自来水中溶解,最后经过ClO2(按产品说明使用)消毒杀菌,即可得到能使人体自然漂浮的漂浮液。
实施例2:适用于海水的固体漂浮晶(2#)的配制:以3.0至6.0°Be’海水为溶剂配制时,需加主要物质:
物质名称             (质量%)
MgSO4               10.6
NaCl                 31.8
KCl                  9.6
MgCl2               47.4
NaBr                 0.59
CuSO4               0.01
ClO2               (按产品说明使用)
配制漂浮液:配制1立方米漂浮液,可向0.92立方米3.0至6.0°Be’海水中添加漂浮晶(2#)262-236kg,配制成浓度为25°Br’的溶液;然后经过超滤或多介质过滤;最后经过净化消毒杀菌,即可得到能使人体自然漂浮的漂浮液。
实施例3:适用于海水的固体漂浮晶(3#)的配制:以7.0°Be’至11.0°Be’海水为溶剂配制时,需加主要物质:
物质名称                     (质量%)
MgSO4                       12.1
NaCl                         24.3
KCl                          12.1
MgCl2                       48.6
NaBr                         0.03
CuSO4                       0.02
ClO2                       (按产品说明使用)
配制漂浮液:配制1立方米漂浮液,可向0.94立方米7.0°Be’至11.0°Be’海水中添加漂浮晶(3#)234-180kg,配制成浓度为25°Br’左右的溶液;然后经过超滤或多介质过滤;最后经过净化消毒杀菌,即可得到能使人体自然漂浮的漂浮液。
实施例4:漂浮晶(4#)适用于用12至15°Be’卤水作为溶剂配制:
物质名称                     质量%
MgSO4                       14.2
NaCl                         1.15
KCl                          15.6
MgCl2                       69.0
NaBr                         0.02
CuSO4                       0.03
ClO2                       (按产品说明使用)
配制漂浮液:如配制1立方米漂浮液,可向9.7立方米12°Be’至15.0°Be’海水中添加漂浮晶(4#)176-146kg,配制成浓度为25°Br’溶液;然后经过超滤或多介质过滤;最后经过净化消毒杀菌,即可得到能使人体自然漂浮的漂浮液。

Claims (3)

1.一种漂浮晶,其特征是,包括以下组分按重量百分比组成:硫酸镁2.5%-15%、氯化钠40.0%-1.0%、氯化钾4.06%-18%、氯化镁30%-75%、溴化钠5%-0.01%。
2.根据权利要求1所述的漂浮晶,其特征是,还包括组分硫酸铜0.01%-0.06%。
3.一种漂浮液的配制方法,其特征是,包括下述步骤:首先向自来水、海水或15°Br以下的卤水中添加如权利要求1所述的漂浮品,配制成高密度溶液,其浓度为23~28°Br’;然后经过超滤或多介质过滤;最后经过净化消毒杀菌,即可得到能使人体自然漂浮的漂浮液。
CNB2004100194766A 2004-06-04 2004-06-04 漂浮晶及漂浮液的配制方法 Expired - Fee Related CN1321914C (zh)