CN1586854A - 把混凝土粗骨料冷却到0℃到-18℃的方法 - Google Patents
把混凝土粗骨料冷却到0℃到-18℃的方法 Download PDFInfo
- Publication number
- CN1586854A CN1586854A CN 200410055419 CN200410055419A CN1586854A CN 1586854 A CN1586854 A CN 1586854A CN 200410055419 CN200410055419 CN 200410055419 CN 200410055419 A CN200410055419 A CN 200410055419A CN 1586854 A CN1586854 A CN 1586854A
- Authority
- CN
- China
- Prior art keywords
- cooling
- coarse aggregate
- temperature
- concrete
- cooled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
在混凝土拌和楼外建立足够大的冷却仓中,用-6℃以下到-35℃的冷空气做冷却介质,冷却粗骨料一定时间,经过一次冷却就把混凝土粗骨料的温度从10℃到40℃多冷却到0℃到-18℃,或者用0℃左右或者更低或者更高的空气做冷却介质,在混凝土拌和楼外建立足够大的冷却仓中先对粗骨料冷却15分钟或者更短或者更长的时间后,再换用-8℃到-35℃的冷空气做冷却介质,在同一冷却仓中,再一次冷却粗骨料,经过这一次冷却,才把混凝土粗骨料的温度冷却到0℃到-18℃。
Description
一、技术领域
本发明涉及一种混凝土粗骨料的冷却方法。
二、技术背景
目前为了把温度10℃到40℃多的混凝土粗骨料冷却到0℃到-9℃,都要经过两次冷却,在混凝土拌和楼外,用-6℃冷空气或者2℃--4℃冷水做冷却介质,先对粗骨料进行一次冷却,把粗骨料温度冷却到4℃到8℃后,再在混凝土拌和楼内的骨料仓中,用-8℃到-14℃冷空气对粗骨料再一次冷却,在两个冷却地点,经过两次冷却,才能把粗骨料温度冷却到0℃到-9℃,第二次冷却粗骨料的地点,是选择在混凝土拌和楼内的骨料仓中进行,在混凝土拌和楼内骨料仓中进行粗骨料冷却时粗骨料冷却的温度降低幅度达到7.5℃到15℃,著名的巴西伊泰普水电站和世界最大的三峡水电站施工时都是采用这种两次冷却粗骨料方法。这种两次冷却粗骨料方法中,第一次冷却粗骨料时,冷却介质温度比较高,就不可能经过第一次冷却粗骨料后,把粗骨料冷却到0℃到-9℃,就一定要采用第二次冷却粗骨料,而这种两次粗骨料冷却方法中,第二次冷却粗骨料的地点,选择在混凝土拌和楼内的骨料仓中进行,由于混凝土拌和楼内的骨料仓容积都比较小,虽然第二次的冷却介质温度降低到-8℃到-14℃,要使粗骨料降低温度幅度达到7.5℃到15℃,混凝土拌和楼的生产能力要降低很多才能达到,当混凝土拌和楼生产能力比较高时,粗骨料的终温就严重超温,造成预冷混凝土的终温严重超温。
三、发明内容
本发明的目的,是在冷却粗骨料时,不要降低或者只要降低10%左右的混凝土拌和楼铭牌生产能力,就能够用冷空气做冷却介质,在一处冷却仓中,把混凝土粗骨料的温度从10℃到40℃多冷却到0℃到-18℃的混凝土粗骨料冷却方法。
四、具体实施方式
用-6℃以下到-35℃的冷空气做冷却介质,在混凝土拌和楼外建立足够大的粗骨料冷却仓中,冷却粗骨料一定时间,经过一次冷却就把混凝土粗骨料的温度从10℃到40℃多冷却到0℃到-18℃,或者用0℃左右或者更低或者更高温度的空气做冷却介质,在混凝土拌和楼外建立足够大的冷却仓中先对粗骨料冷却15分钟或者更短或者更长时间后,再换用-8℃到-35℃的冷空气做冷却介质,在同一冷却仓中,再一次冷却粗骨料,经过这一次冷却,才把粗骨料的温度冷却到0℃到-18℃,两次用两种温度不同的冷空气冷却粗骨料,粗骨料是不换冷却仓不换冷却地点的,更换的只是温度不同的冷空气。先用单个球体冷却方法的公式计算出达到粗骨料终温的冷却介质温度和冷却时间的几组组合,再经过试验,确定每一种粗骨料冷却时采用的冷却介质温度、冷却介质流量和冷却时间长短,根据确定的冷却时间长短和冷却粗骨料要求的生产能力,计算出冷却仓的需要容积,确定所有参数时,要加20%到50%的富余量。混凝土拌和楼内骨料仓,只承担2℃到5℃的粗骨料降低温度幅度,或者不承担粗骨料的降低温度,混凝土拌和楼内骨料仓另外两个任务,是做冷却好粗骨料的保温仓和调节仓。
五、有益效果
冷却粗骨料时不要降低到或者很少降低混凝土拌和楼的生产能力,而且粗骨料冷却后的终温合格率达到90%以上。
Claims (3)
1、在冷却粗骨料时,不要降低或者只要降低10%左右的混凝土拌和楼铭牌生产能力,就能够用冷空气做冷却介质,在一处冷却仓中,把混凝土粗骨料的温度从10℃到40℃多冷却到0℃到-18℃的混凝土粗骨料冷却方法。
2、根据权利要求1,用-6℃以下到-35℃的冷空气做冷却介质,在混凝土拌和楼外建立足够大的粗骨料冷却仓中,冷却粗骨料一定时间,经过一次冷却就把混凝土粗骨料的温度从10℃到40℃多冷却到0℃到-18℃。
3、根据权利要求1,用0℃左右或更低或者更高温度的空气做冷却介质,在混凝土拌和楼外建立足够大的冷却仓中先对粗骨料冷却15分钟或者更短或者更长的时间后,再换用-8℃到-35℃的冷空气做冷却介质,在同一冷却仓中,再一次冷却粗骨料,经过这次冷却才把混凝土粗骨料的温度冷却到0℃到-18℃。