CN1356178A - Reverse floatation depressant of iron ore and its preparing process - Google Patents

Reverse floatation depressant of iron ore and its preparing process Download PDF

Info

Publication number
CN1356178A
CN1356178A CN 01106060 CN01106060A CN1356178A CN 1356178 A CN1356178 A CN 1356178A CN 01106060 CN01106060 CN 01106060 CN 01106060 A CN01106060 A CN 01106060A CN 1356178 A CN1356178 A CN 1356178A
Authority
CN
China
Prior art keywords
iron ore
starch
inhibitor
naoh
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 01106060
Other languages
Chinese (zh)
Other versions
CN1141184C (en
Inventor
徐井春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB011060603A priority Critical patent/CN1141184C/en
Publication of CN1356178A publication Critical patent/CN1356178A/en
Application granted granted Critical
Publication of CN1141184C publication Critical patent/CN1141184C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

A reverse floatation depress ant of iron ore is prepared from starch, chloroacetic acid, methanol, NaOH, sodium carbonate and water through mixing chloroacetic acid with sodium carbonate, adding starch, stirring, adding the mixed solution of methanol, NaOH and water, and stirring. Its advantages include low dosage, simple preparing process, and high grade of ore concentrate.

Description

Iron ore antifloating inhibitor and preparation method thereof
The present invention relates to a kind of iron ore antifloating inhibitor and preparation method thereof.
Iron ore antifloating inhibitor adopts modified starch more in the prior art, as causticization starch, CMS etc.Have following defective in production application: reagent consumption is big, the cost height; The process for preparation complexity need be heated, the high preparation of hear rate back starch is perishable, causes waste big; It is low to sort efficient, index error, cost height.
The objective of the invention is to study a kind of novel iron ore antifloating inhibitor, make its consumption in production application low, suppress the efficient height, be easy to preparation, anti-rotten, reduce medicament expense usefulness to reach, refer to that height sorts efficient.
Iron ore antifloating inhibitor of the present invention is achieved through the following technical solutions:
This inhibitor is made up of starch, monoxone, methyl alcohol, NaOH, soda ash and water, and the weight proportion of various components is: starch: monoxone: methyl alcohol: NaOH: soda ash: water=100: 15~17: 19~23: 7~9: 9~11: 0.7~1.8.Its best proportioning is a starch: monoxone: methyl alcohol: NaOH: soda ash: water=100: 16: 22: 8: 10: 1.5.
Preparation process of the present invention is: at first monoxone and soda ash stirring and evenly mixing, add then and stir 5~10 minutes in the starch; Again the mixed solution after methyl alcohol, NaOH and water-soluble the separating is added wherein, stirred 10~15 minutes; Be warming up to 65~67 ℃, be incubated 2.5 hours, products therefrom is iron ore antifloating inhibitor of the present invention after pulverizing.
Iron ore antifloating inhibitor of the present invention has following feature: suppress can prepare under efficient height, the consumption normal temperature simple, the saving energy consumption of making up a prescription; Suppress the efficient height, improve concentrate grade 0.3~0.5%,
As follows for specific embodiments of the invention: after getting monoxone 80Kg, soda ash 50gK stirring and evenly mixing; Pour in the container that 500Kg starch is housed, stirred 5~10 minutes; Again the mixed liquor after the NaOH of 40Kg (solid caustic soda) and 110Kg methyl alcohol and the 4.5Kg water stirring and dissolving is added in the starch bowl, stirred 13 minutes; Last steam is heated to 65~66 ℃, is incubated 2.5 hours, and products therefrom is iron ore antifloating inhibitor of the present invention after crushed.
The present invention with the starch contrast, can reduce consumption 45~50% with existing; Preparation need not middle temperature And secondary agitation, simplified the technology of making up a prescription; Concentrate grade improves more than 0.5%, and is difficult for becoming Matter (can reach more than 20 days summer)

Claims (2)

1, a kind of iron ore antifloating inhibitor, be primarily characterized in that this inhibitor is made up of starch, monoxone, methyl alcohol, NaOH, soda ash and water, the weight proportion of various components is: starch: monoxone: methyl alcohol: NaOH: soda ash: water==100: 15~17: 19~23: 7~9: 9~11: 0.7~1.8.
2, a kind of iron ore antifloating inhibitor according to claim 1 is characterized in that its preparation process is: at first behind monoxone and the soda ash stirring and evenly mixing, add in the starch and stirred 5~10 minutes; Again methyl alcohol, NaOH and the water-soluble mixed solution of separating are added wherein, stirred 15 minutes; Be warming up to 65~67 ℃ afterwards, be incubated and be iron ore antifloating inhibitor of the present invention after 2.5 hours products therefroms are pulverized.
CNB011060603A 2001-01-11 2001-01-11 Reverse floatation depressant of iron ore and its preparing process Expired - Fee Related CN1141184C (en)