CN115044942A - Starting sheet cathode and using method thereof - Google Patents

Starting sheet cathode and using method thereof Download PDF

Info

Publication number
CN115044942A
CN115044942A CN202210758232.8A CN202210758232A CN115044942A CN 115044942 A CN115044942 A CN 115044942A CN 202210758232 A CN202210758232 A CN 202210758232A CN 115044942 A CN115044942 A CN 115044942A
Authority
CN
China
Prior art keywords
wedge
section
casing
shaped
electrodeposition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN202210758232.8A
Other languages
Chinese (zh)
Other versions
CN115044942B (en
Inventor
陈瑞山
李开杰
朱兵兵
李珊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinchuan Group Nickel Cobalt Co ltd
Lanzhou Jinchuan Advangced Materials Technology Co ltd
Original Assignee
Lanzhou Jinchuan Advangced Materials Technology Co ltd
Jinchuan Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lanzhou Jinchuan Advangced Materials Technology Co ltd, Jinchuan Group Co Ltd filed Critical Lanzhou Jinchuan Advangced Materials Technology Co ltd
Priority to CN202210758232.8A priority Critical patent/CN115044942B/en
Publication of CN115044942A publication Critical patent/CN115044942A/en
Application granted granted Critical
Publication of CN115044942B publication Critical patent/CN115044942B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a cathode of a starting sheet and a using method thereof, belongs to the field of hydrometallurgy electrodeposition equipment, and solves the problem that a lifting lug shearing process is required in the traditional electrodeposition method. The invention comprises a conductive rod, a conductive sheet, a first shell and a second shell, wherein the conductive sheet comprises an annular section, a connecting section and a wedge-shaped section, the annular section is sleeved on the conductive rod, the wedge-shaped section is attached and connected with the inner wall of the lower end of the first shell, the upper parts of the first shell and the second shell are buckled outside the annular section, an inserting plate is arranged in the second shell, a wedge-shaped block is arranged at the lower end of the inserting plate, the wedge-shaped block is opposite to the wedge-shaped section, and a starting sheet is clamped between the wedge-shaped block and the wedge-shaped section. The using method comprises the following steps: lifting the inserting plate upwards to enable the wedge-shaped block to be staggered with the wedge-shaped section; placing a starting sheet between the wedge-shaped block and the wedge-shaped section; pushing down the inserting plate, clamping the starting sheet and starting electrodeposition; and after the electrodeposition is finished, lifting the plugboard upwards and taking down the starting sheet. The method can ensure the perfect product appearance of the electrodeposition product and improve the production quality.

Description

Starting sheet cathode and using method thereof
Technical Field
The invention belongs to the field of hydrometallurgy electrodeposition equipment, and particularly relates to a cathode of a starting sheet and a using method thereof.
Background
The negative plate is required to be manufactured in the traditional electrodeposition production, the negative plate consists of a conductive rod, a lifting lug, a copper suspension wire and a starting sheet, the lifting lug is required to be manufactured by a special lifting lug shearing machine and punched so as to be convenient for the insertion of the copper suspension wire, and the manufactured lifting lug penetrates through the conductive rod after being bent and is riveted and hung on the conductive rod by the copper suspension wire. Because the finished product of electrodeposition has lug and hole and can influence the selling price, so the finished product of electrodeposition need transfer to the finished product equipment, carry out operations such as lug shearing and packing, not only make manufacturing cost rise, also make intensity of labour increase.
Disclosure of Invention
The invention aims to provide a starting sheet cathode to solve the problem that a traditional electrodeposition method needs a lug shearing process.
Another object of the present invention is to provide a method for using the cathode of the starting sheet.
The technical scheme of the invention is as follows: the utility model provides a starting sheet negative pole, including conducting rod and conducting strip, still include first casing and second casing, the conducting strip is including the cyclic annular section that from top to bottom connects gradually, linkage segment and wedge section, cyclic annular section cover is established on the conducting rod, the wedge section is connected with the laminating of first casing lower extreme inner wall, first casing and second casing upper portion lock are outside and pass through bolt-up connection at cyclic annular section, be equipped with the picture peg in the second casing, the picture peg can remove for the second casing, the picture peg upper end is located outside the second casing, the picture peg lower extreme is equipped with the wedge, the wedge is relative with wedge section position, the starting sheet centre gripping is between wedge and wedge section.
As a further improvement of the invention, the opposite faces of the wedge-shaped block and the wedge-shaped section are respectively provided with rough knurling to increase the friction force.
As a further improvement of the invention, the upper end of the inserting plate is provided with a handle, so that the inserting plate can be operated conveniently.
A method for using a cathode of a starting sheet comprises the following steps:
A. lifting the inserting plate upwards to make the wedge-shaped block staggered with the wedge-shaped section;
B. placing a starting sheet between the wedge-shaped block and the wedge-shaped section;
C. pushing the inserting plate downwards to enable the wedge-shaped block and the wedge-shaped section to clamp the starting sheet, and starting electrodeposition operation;
D. after the electrodeposition is finished, the flashboard is lifted upwards, and the starting sheet can be taken down.
The invention has the beneficial effects that: the cathode of the starting sheet is simple in structure, the starting sheet is fixed on the conductive rod in a clamping mode, the starting sheet does not need to be punched, pierced and hung, the appearance of an electrodeposition product can be guaranteed to be intact, after electrodeposition is finished, the electrodeposition product does not need to be transferred to finished equipment for removing ears, shearing and other operations, the production cost is saved, and the production quality is improved. The invention has simple use method and strong reliability, reduces the labor intensity and improves the production efficiency.
Drawings
FIG. 1 is a schematic perspective view of a cathode of a starting sheet according to the present invention;
FIG. 2 is a schematic diagram of a cathode of a starting sheet according to the present invention;
fig. 3 is a view a-a in fig. 2.
In the figure: 1-a first housing; 2-a second housing; 3, conducting strips; 31-a ring segment; 32-a connecting segment; 33-a wedge-shaped section; 4-a wedge-shaped block; 5-a conductive rod; 6-bolt; 7-starting a pole piece; 8-inserting plates; 9-handle.
Detailed Description
The present invention will be described in further detail with reference to the accompanying drawings.
As shown in fig. 1-3, a cathode of a starting sheet, including a conductive rod 5 and a conductive sheet 3, further including a first casing 1 and a second casing 2, the conductive sheet 3 includes a ring section 31, a connection section 32 and a wedge section 33, which are sequentially connected from top to bottom, the ring section 31 is sleeved on the conductive rod 5, the wedge section 33 is attached to the inner wall of the lower end of the first casing 1, the upper portions of the first casing 1 and the second casing 2 are fastened outside the ring section 31 and fastened and connected by a bolt 6, a board 8 is disposed in the second casing 2, the board 8 can move relative to the second casing 2, the upper end of the board 8 is disposed outside the second casing 2, the lower end of the board 8 is disposed with a wedge block 4, the wedge block 4 is opposite to the wedge section 33, and the starting sheet 7 is clamped between the wedge block 4 and the wedge section 33.
The opposite faces of the wedge-shaped block 4 and the wedge-shaped section 33 are provided with a rough knurling respectively.
The upper end of the inserting plate 8 is provided with a handle 9.
A plurality of sets of the first case 1 and the second case 2 may be provided on one conductive rod 5.
The first shell 1, the second shell 2 and the wedge block 4 are all made of corrosion resistant material. The conductive sheet 3 is made of pure copper.
A method for using a cathode of a starting sheet comprises the following steps:
A. lifting the inserting plate 8 upwards to enable the wedge-shaped block 4 to be staggered with the wedge-shaped section 33;
B. placing the starter piece 7 between the wedge block 4 and the wedge segment 33;
C. the inserting plate 8 is pushed downwards to enable the wedge-shaped block 4 and the wedge-shaped section 33 to clamp the starting plate 7, and electrodeposition operation is started;
D. after the electrodeposition is finished, the flashboard 8 is lifted upwards, and the starting sheet 7 can be taken down.
At the in-process of electrodeposition, the weight of starting sheet 7 can constantly increase, and gravity action will make starting sheet 7 have the trend of lapse, and this can stimulate wedge 4 lapse to make wedge 4 and wedge section 33 clamp starting sheet 7 more and more firmly, avoided the risk of falling, safe and reliable.
The cathode of the starting sheet has a simple structure, is convenient to maintain, saves the operations of transferring the electrodeposition product to finished product equipment for removing ears, shearing and the like on the basis of ensuring the intact appearance of the electrodeposition product, effectively improves the production quality, saves the production cost and reduces the labor intensity.

Claims (4)

1. A cathode for a starter sheet comprising a conductive rod (5) and a conductive sheet (3), characterized in that: still include first casing (1) and second casing (2), conducting strip (3) are including ring segment (31), linkage segment (32) and wedge section (33) that from top to bottom connect gradually, ring segment (31) cover is established on conducting rod (5), wedge section (33) are connected with the laminating of first casing (1) lower extreme inner wall, first casing (1) and second casing (2) upper portion lock are outside and through bolt (6) fastening connection in ring segment (31), be equipped with picture peg (8) in second casing (2), picture peg (8) can remove for second casing (2), picture peg (8) upper end is located outside second casing (2), picture peg (8) lower extreme is equipped with wedge (4), wedge (4) are relative with wedge section (33) position, begin pole piece (7) centre gripping between wedge (4) and wedge section (33).
2. The cathode as claimed in claim 1, wherein: the opposite surfaces of the wedge-shaped block (4) and the wedge-shaped section (33) are respectively provided with a rough knurl.
3. A cathode as claimed in claim 1 or 2, wherein: the upper end of the inserting plate (8) is provided with a handle (9).
4. A method of using the starter sheet cathode of any one of claims 1 to 3, comprising the steps of:
A. the flashboard (8) is lifted upwards to make the wedge-shaped block (4) and the wedge-shaped section (33) staggered;
B. placing a starter piece (7) between the wedge block (4) and the wedge section (33);
C. the inserting plate (8) is pushed downwards to enable the wedge-shaped block (4) and the wedge-shaped section (33) to clamp the starting sheet (7) and start electrodeposition operation;
D. after the electrodeposition is finished, the flashboard (8) is lifted upwards, and the starting sheet (7) can be taken down.
CN202210758232.8A 2022-06-30 2022-06-30 Starting sheet cathode and application method thereof Active CN115044942B (en)