CN113455745A - Material for heating non-combustion cigarette shell and preparation method of cigarette shell - Google Patents

Material for heating non-combustion cigarette shell and preparation method of cigarette shell Download PDF

Info

Publication number
CN113455745A
CN113455745A CN202110751104.6A CN202110751104A CN113455745A CN 113455745 A CN113455745 A CN 113455745A CN 202110751104 A CN202110751104 A CN 202110751104A CN 113455745 A CN113455745 A CN 113455745A
Authority
CN
China
Prior art keywords
shell
glue dipping
inner core
dipping
glue
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202110751104.6A
Other languages
Chinese (zh)
Inventor
梁源
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Altria Client Services LLC
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN202110751104.6A priority Critical patent/CN113455745A/en
Publication of CN113455745A publication Critical patent/CN113455745A/en
Priority to PCT/US2022/035658 priority patent/WO2023278656A1/en
Pending legal-status Critical Current

Abstract

The invention discloses a material for heating a non-burning cigarette shell, which comprises the following material components of plant cellulose and microcrystalline cellulose, wherein the use weight ratio of the plant cellulose to the microcrystalline cellulose is 10:1-80: 1; the shell is tubular, the head end of the shell is closed, the tail end of the shell is transparent, and the shell is manufactured by a glue dipping die through a glue dipping method for multiple times and then is processed; the outer shell comprises an outer sleeve and an inner core, and the outer sleeve and the inner core are processed and formed after being dipped for multiple times by a glue dipping die. The invention provides a novel heating non-combustible cigarette capable of being used in a heating mode, which is used as a cigarette substitute to heat tobacco without combustion, smoke generated after heating is supplied to a user for smoking, harmful substances contained in the smoke generated by heating are far lower than those in the smoke generated by combustion of the tobacco, and the harm degree of the tobacco to the user and the surrounding environment is reduced while the experience feeling of the user is guaranteed.

Description

Material for heating non-combustion cigarette shell and preparation method of cigarette shell
Technical Field
The invention relates to the technical field of cigarettes, in particular to a material for heating a non-burning cigarette shell and a preparation method of the cigarette shell.
Background
Cigarettes are the most common tobacco consumer products at present, and when the cigarettes ignite cut tobacco, aerosol with nicotine, tobacco cracking substances, additional spices and the like is generated, wherein the nicotine is a component which mainly brings pleasure and addiction to smokers. When the common cigarette releases nicotine, the aerosol of the common cigarette contains various harmful substances generated during combustion and cracking, including carbon monoxide, crotonaldehyde, tobacco-specific nitrosamines (TSNAs), benzopyrene and the like, and has certain health hazard to human bodies.
Electronic cigarettes have been developed rapidly in recent years, but electronic cigarettes are electronic products simulating cigarettes by heating and atomizing liquid tobacco tar or semisolid tobacco paste with heating wires, and have the same appearance, smoke, taste and sensation as cigarettes. The electronic cigarette is a product which is powered by a rechargeable lithium polymer battery to drive an atomizer, nicotine and the like are changed into steam through heating tobacco tar in an oil tank, and then a user can suck the electronic cigarette.
Research shows that the content of harmful substances in smoke generated by heating and non-burning tobacco is 80% lower than that of the traditional cigarette, because the heating temperature of the tobacco is far lower than the burning temperature of the tobacco, the release of the harmful substances is limited to a great extent, and therefore, the treatment mode of heating and non-burning tobacco products reduces the harm to smokers due to smoking, and attracts attention of all parties.
Disclosure of Invention
The invention aims to provide a novel non-combustible and heatable material for heating a non-combustible cigarette shell and a preparation method of the cigarette shell.
In order to achieve the purpose, the invention provides the following technical scheme:
a material for heating a non-combustible cigarette shell comprises the following material components of plant cellulose and microcrystalline cellulose, wherein the use weight ratio of the plant cellulose to the microcrystalline cellulose is 10:1-80: 1; the plant cellulose and the microcrystalline cellulose are mixed according to a proportion to form a mixture, 10 parts by weight of the mixture is taken and put into 50 parts by weight of purified water heated to 90 ℃, the mixture is stirred by a homogenizer and kept warm for 1 hour, then the mixture is kept stand for 2 hours at the temperature of 30-60 ℃, then 50 parts by weight of 99% alcohol is added, and the mixture is homogenized and dissolved again to form a liquid shell material.
The scheme adopts the mixture of the plant cellulose (HPMC) and the microcrystalline cellulose as the manufacturing material of the heating non-combustion cigarette shell, the heating non-combustion cigarette shell manufactured by the material can bear the high temperature of 350 ℃ without the defects of carbonization, air leakage and the like, if only the shell manufactured by the plant cellulose is adopted, the shell manufactured by the material can only ensure that the defects of carbonization, air leakage and the like can not appear under the condition of not exceeding 200 ℃, the tobacco is heated below 200 ℃, the generated smoke is too little, the experience feeling of a user is poor, the traditional cigarette can not be completely replaced, the tobacco is heated by the heating temperature of about 300 ℃, the tobacco can be enabled to generate smoke close to the smoke generated by combustion, and the experience feeling of the user is strong.
A method for preparing a casing of a heating non-combustible cigarette, the casing is tubular, the head end of the casing is closed, the tail end of the casing is transparent, the casing is processed after being manufactured by a glue dipping die through a multiple glue dipping method, the method comprises the following steps,
preparing a glue dipping die, wherein the glue dipping die is made of silica gel, the outer surface of the glue dipping die is arranged corresponding to the inner wall of the shell, the tail part of the glue dipping die is provided with a fixed end and a blind hole, the blind hole penetrates through the fixed end and extends into the glue dipping die, a pluggable hard core rod is arranged in the blind hole, and the tail end of the hard core rod is positioned outside the glue dipping die;
preparing a liquid shell material;
dipping glue, namely dipping the glue dipping mould into a liquid shell material, taking out the glue dipping mould, and drying and solidifying the glue dipping mould by using a dehumidifier to form a shell;
repeatedly dipping the glue, after the shell material on the outer side of the glue dipping mold is solidified, dipping the glue dipping mold into the liquid shell material again, taking out the glue dipping mold, and thickening the shell by utilizing drying and solidification of a dehumidifier;
repeating the gum dipping at least once again;
demoulding, namely fixing the fixed end of the glue dipping mould immovably, pushing the hard core rod to move towards the blind hole, reducing the outer diameter of the glue dipping mould while generating deformation and elongation under the pressure of the hard core rod, and realizing demoulding with the glue dipping mould because a shell formed on the outer side of the glue dipping mould does not deform along with the glue dipping mould;
and carrying out laser cutting on the shell, cutting off the redundant length of the shell and punching holes at the appointed position of the shell.
The shell of the scheme is manufactured by adopting a mould glue dipping method for multiple times and then is processed and formed, the size of the shell is similar to that of a common cigarette, the thickness of the shell is about 0.1 mm, the scheme adopts an elastic material silica gel capable of extending and deforming to manufacture the glue dipping mould, a blind hole and a hard core rod are arranged in the glue dipping mould, the drying and solidification are carried out after the glue dipping is carried out each time to form the shell, during demoulding, the fixed end (such as a boss) of the glue dipping mould is fixed, for example, the glue dipping mould penetrates through the fixed plate, but the fixed end cannot penetrate through the fixed plate, the fixed end of the glue dipping mould is pressed by a pressing plate with a hole, then the hard core rod is pushed into the blind hole to apply pressure to the glue dipping mould, so that the glue dipping mould is stretched and thinned under the action of pressure, the elasticity of the shell material is poor, the shell cannot be stretched and thinned along with the glue dipping mould, and the mould can fall off to realize demoulding; the shell of the scheme is light and thin, and is suitable for pressure-free processing by laser.
Preferably, the shell include overcoat, inner core, the overcoat be the tubulose, overcoat head end seal, the tail end can hold the inner core and insert, the inner core be the tubulose, the inner core include tip confined insert anterior segment, the open back end that inserts of tip, insert and be equipped with tobacco accommodation space between anterior segment tip and the overcoat head end, insert and be equipped with the air gap between anterior segment lateral wall and the overcoat inside wall, insert back end lateral surface and the overcoat inside wall closely cooperate fixedly, the overcoat lateral wall on be equipped with a plurality of inlet ports with the air gap intercommunication, the inner core insert the anterior segment tip and be equipped with a plurality of air vents, inlet port, air gap, air vent, inner core pipeline, inner core insert the back end portion and form flue gas channel.
The scheme adopts a thin tubular outer sleeve and an inner core to combine a novel cigarette, and the outer sleeve and the inner core are respectively dipped in glue for multiple times by a glue dipping die to generate and then are processed and formed; the inner core is inserted and fixed in the outer sleeve, tobacco is placed in the tobacco containing space, the rear ends of the inner core and the outer sleeve are used as a suction port of a user, and an air inlet of the outer sleeve is not directly communicated with the suction port (the outer side surface of the inserted rear section of the inner core is tightly matched and fixed with the inner side wall of the outer sleeve to play a sealing role) and needs to be communicated through a smoke channel; when the cigarette heating device is used, the cigarette heating device is used together with a heater, the cigarette head end formed by combining the outer sleeve and the inner core is inserted into the tubular heating cavity of the heater, the tobacco containing space is completely inserted into the heater, the heater switch is turned on to heat, the heating temperature is 230-.
Preferably, the inner core is inserted into the outer side face of the rear section and is tightly matched and fixed with the inner side wall of the outer sleeve through locking grains, the locking grains comprise a first groove and a second groove which are respectively arranged on the inner core and the outer sleeve, and the inner side face of the first groove is attached to the outer side face of the second groove in shape. According to the scheme, the sealing and fixing of the inner core and the outer sleeve are realized through the lock grains, the first groove and the second groove are sunken in the same direction, and when the inner core is inserted into the outer sleeve, the sunken parts of the two grooves are tightly superposed, so that the inner core and the outer sleeve are positioned and fixed, and the ventilation gap is sealed; the first groove and the second groove are not limited to one groove, and two or three grooves can be formed.
Preferably, in the liquid casing material, the ratio of the plant cellulose to the microcrystalline cellulose is 50:1 by weight, 1 kg of the mixture of the plant cellulose and the microcrystalline cellulose is taken and added into 5 kg of purified water at 90 ℃, the mixture is placed in a homogenizer for heat preservation and stirring for 1 hour, after the mixture is completely preserved at 45 ℃, the mixture is kept stand for 2 hours, then 5 kg of 99% alcohol is added, and the mixture is homogenized and dissolved again to form the liquid casing material.
Preferably, the dipping step is repeated for 5 times, and the thickness of the shell is increased by 0.02 mm each time.
Preferably, a plurality of glue dipping molds are fixed on the mold fixing plate together, and the tail end of the hard core rod is positioned outside the mold fixing plate.
Preferably, the outer sleeve and the inner core are transparent tubes.
Compared with the prior art, the invention has the beneficial effects that: the novel heating non-combustible cigarette capable of being used in a heating mode serves as a cigarette substitute, tobacco is heated and non-combustible, smoke generated after heating is supplied to a user for smoking, harmful substances contained in the smoke generated by heating are far lower than those in the smoke generated by burning the tobacco, and the harm degree of the tobacco to the user and the surrounding environment is reduced while the experience feeling of the user is guaranteed.
Drawings
Fig. 1 is a schematic view of a structure of the jacket of the present invention.
Fig. 2 is a schematic view of a structure of the core of the present invention.
Fig. 3 is a schematic cross-sectional structure of the present invention.
Fig. 4 is a schematic structural diagram of the jacket mold of the present invention.
Fig. 5 is a schematic structural view of the core mold of the present invention.
In the figure: 1-outer shell 2-inner core 3-tobacco containing space 4-ventilation gap
5-first groove 6-second groove 7-outer sleeve mold 8-inner core mold
9-fixed end 10-hard core rod 11-air inlet
21-insertion into the front section 22-insertion into the rear section 23-ventilation.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all embodiments, and all other embodiments obtained by a person of ordinary skill in the art without creative efforts based on the embodiments of the present invention belong to the protection scope of the present invention.
The invention provides a technical scheme that:
a material for heating a non-combustible cigarette shell comprises the following material components of plant cellulose and microcrystalline cellulose, wherein the use weight ratio of the plant cellulose to the microcrystalline cellulose is 10:1-80: 1; mixing plant cellulose and microcrystalline cellulose in proportion to form a mixture, taking 10 parts by weight of the mixture, putting the mixture into 50 parts by weight of purified water heated to 90 ℃, stirring by a homogenizer while keeping the temperature for 1 hour, standing for 2 hours at the temperature of 30-60 ℃, then adding 50 parts by weight of 99% alcohol, and homogenizing and dissolving again to form the liquid shell material.
A method for preparing a casing of a cigarette without burning by heating comprises making the casing into a tubular shape, sealing the head end of the casing, penetrating the tail end of the casing, and processing the casing to obtain a finished casing product after the casing is made by a glue dipping mold for multiple times by a glue dipping method (namely, liquid casing material is dipped);
in the liquid shell material, the use weight ratio of the plant cellulose to the microcrystalline cellulose is 50:1, 1 kg of a mixture of the plant cellulose and the microcrystalline cellulose is taken and added into 5 kg of purified water at 90 ℃, the mixture is placed in a homogenizer for heat preservation and stirring for 1 hour, after the mixture is finished, the mixture is kept at 45 ℃ and stands for 2 hours, then 5 kg of 99% alcohol is added, and the mixture is homogenized and dissolved again to form the liquid shell material;
referring to the attached drawings 1-3, a shell comprises an outer sleeve 1 and an inner core 2, the outer sleeve 1 is tubular, the head end of the outer sleeve 1 is closed, the tail end of the outer sleeve 1 can be inserted with the inner core 2, the inner core 2 is tubular, the inner core 2 comprises an insertion front section 21 with a closed end part and an insertion rear section 22 with an open end part, a tobacco containing space 3 is arranged between the end part of the insertion front section 21 and the head end of the outer sleeve 1, a ventilation gap 4 is arranged between the outer side wall of the insertion front section 21 and the inner side wall of the outer sleeve 1, the outer side surface of the insertion rear section 22 is tightly matched and fixed with the inner side wall of the outer sleeve 1, a plurality of air inlets 11 communicated with the ventilation gap 4 are arranged on the side wall of the outer sleeve 1, a plurality of air vents 23 are arranged on the end part of the insertion front section 21 of the inner core 2, and the air inlets 11, the ventilation gap 4, the ventilation holes 23, a pipeline of the inner core 2 and the end part of the insertion rear section 22 form a smoke channel;
the outer side surface of the inner core 2 inserted into the rear section 22 is closely matched and fixed with the inner side wall of the outer sleeve 1 through locking grains, the locking grains comprise a first groove 5 and a second groove 6 which are respectively arranged on the inner core 2 and the outer sleeve 1, and the inner side surface of the first groove 5 is fitted with the outer side surface shape of the second groove 6;
referring to fig. 4-5, the glue dipping mold is made of silica gel and comprises an outer sleeve mold 7 and an inner core mold 8, the outer surface of the glue dipping mold corresponds to the inner wall of the shell, a fixed end 9 and a blind hole are arranged at the tail of the glue dipping mold, the blind hole penetrates through the fixed end 9 and extends into the glue dipping mold, a pluggable hard core rod 10 is arranged in the blind hole, and the tail end of the hard core rod 10 is positioned outside the glue dipping mold;
the outer shell 1 and the inner core 2 are transparent tubes.
The specific using process is as follows: the manufacturing of the outer shell comprises the respective manufacturing and processing of the outer sleeve 1 and the inner core 2, and comprises the following steps,
preparing a glue dipping die outer sleeve die 7 and an inner core die 8 which are suitable for the outer sleeve 1 or the inner core 2;
preparing a liquid shell material;
dipping glue, namely dipping the glue dipping mould into a liquid shell material, taking out the glue dipping mould, and drying and solidifying the glue dipping mould by using a dehumidifier to form a shell;
repeatedly dipping the glue, after the shell material on the outer side of the glue dipping mold is solidified, dipping the glue dipping mold into the liquid shell material again, taking out the glue dipping mold, and thickening the shell by utilizing drying and solidification of a dehumidifier;
carrying out repeated gum dipping for three times, wherein the generated outer shell is an outer shell or an inner core, the thickness of the outer shell is about 1 mm, and a first groove or a second groove is formed in the outer shell or the inner core;
demoulding, namely fixing the fixed end 9 of the glue dipping mould, pushing the hard core rod 10 to move towards the blind hole, reducing the outer diameter of the glue dipping mould while generating deformation and elongation under the pressure of the hard core rod 10, and realizing demoulding with the glue dipping mould because a shell formed on the outer side of the glue dipping mould does not deform along with the glue dipping mould;
carrying out laser cutting on the shell, cutting off the redundant length of the shell, and punching holes at the appointed position of the shell to form an air inlet hole 11 on the outer sleeve 1 or an air vent 23 on the inner core 2;
through testing, the shell product can bear the high temperature of 350 ℃ without defects of carbonization, air leakage and the like.
By overcoat 1, in the new-type heating incombustible cigarette that inner core 2 made up into, tobacco accommodation space 3 is arranged in to the tobacco, be located 1 head end of overcoat, during this scheme of use product, insert 1 head end of overcoat in the tubulose heating chamber of heater, tobacco accommodation space 3 inserts in the heater completely, open the heater switch and heat, when the user inhales, the air is from inlet port 11, ventilation gap 4 gets into tobacco accommodation space 3, carry the flue gas that the tobacco was produced after being heated through air vent 23, inner core 2 pipeline, inner core 2 inserts 22 tip in back end and is inhaled the food.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.

Claims (8)

1. A material for heating a cigarette casing which does not burn, characterized in that: comprises the following material components of plant cellulose and microcrystalline cellulose, wherein the ratio of the plant cellulose to the microcrystalline cellulose by weight is 10:1-80: 1;
the plant cellulose and the microcrystalline cellulose are mixed according to a proportion to form a mixture, 10 parts by weight of the mixture is taken and put into 50 parts by weight of purified water heated to 90 ℃, the mixture is stirred by a homogenizer and kept warm for 1 hour, then the mixture is kept stand for 2 hours at the temperature of 30-60 ℃, then 50 parts by weight of 99% alcohol is added, and the mixture is homogenized and dissolved again to form a liquid shell material.
2. A preparation method of a cigarette shell which is not combusted by heating is characterized in that: the shell is tubular, the head end of the shell is closed, the tail end of the shell is transparent, the shell is manufactured by adopting a glue dipping die for multiple times of glue dipping method and then processed, the method comprises the following steps,
preparing a glue dipping die, wherein the glue dipping die is made of silica gel, the outer surface of the glue dipping die is arranged corresponding to the inner wall of the shell, the tail part of the glue dipping die is provided with a fixed end and a blind hole, the blind hole penetrates through the fixed end and extends into the glue dipping die, a pluggable hard core rod is arranged in the blind hole, and the tail end of the hard core rod is positioned outside the glue dipping die;
preparing a liquid shell material;
dipping glue, namely dipping the glue dipping mould into a liquid shell material, taking out the glue dipping mould, and drying and solidifying the glue dipping mould by using a dehumidifier to form a shell;
repeatedly dipping the glue, after the shell material on the outer side of the glue dipping mold is solidified, dipping the glue dipping mold into the liquid shell material again, taking out the glue dipping mold, and thickening the shell by utilizing drying and solidification of a dehumidifier;
repeating the gum dipping at least once again;
demoulding, namely fixing the fixed end of the glue dipping mould immovably, pushing the hard core rod to move towards the blind hole, reducing the outer diameter of the glue dipping mould while generating deformation and elongation under the pressure of the hard core rod, and realizing demoulding with the glue dipping mould because a shell formed on the outer side of the glue dipping mould does not deform along with the glue dipping mould;
and carrying out laser cutting on the shell, cutting off the redundant length of the shell and punching holes at the appointed position of the shell.
3. The method for producing a casing for a heat-nonflammable cigarette according to claim 2, wherein: the shell include overcoat, inner core, the overcoat be the tubulose, overcoat head end seal, the tail end can hold the inner core and insert, the inner core be the tubulose, the inner core include tip confined insert anterior segment, the open back end that inserts of tip, insert and be equipped with tobacco accommodation space between anterior segment tip and the overcoat head end, insert and be equipped with the air gap between anterior segment lateral wall and the overcoat inside wall, insert back end lateral surface and the inseparable cooperation of overcoat inside wall fixed, the overcoat lateral wall on be equipped with a plurality of inlet ports with the air gap intercommunication, the inner core insert the anterior segment tip and be equipped with a plurality of air vents, inlet port, air gap, air vent, inner core pipeline, inner core insert the back end tip and form flue gas channel.
4. The method for producing a casing for a heat non-combustible cigarette according to claim 3, wherein: the inner core inserts the back end lateral surface and passes through the lock line closely to cooperate fixedly with the overcoat inside wall, the lock line including locating first recess, the second recess on inner core and the overcoat respectively, first recess medial surface and the laminating of second recess lateral surface shape.
5. The method for producing a casing for a heat-nonflammable cigarette according to claim 2, wherein: in the liquid shell material, the ratio of the plant cellulose to the microcrystalline cellulose is 50:1 by weight, 1 kg of a mixture of the plant cellulose and the microcrystalline cellulose is taken and added into 5 kg of purified water at 90 ℃, the mixture is placed in a homogenizer for heat preservation and stirring for 1 hour, after the mixture is finished, the mixture is kept at 45 ℃ and stands for 2 hours, then 5 kg of 99% alcohol is added, and the mixture is homogenized and dissolved again to form the liquid shell material.
6. The method for producing a casing for a heat-nonflammable cigarette according to claim 2, wherein: the gum dipping step is repeated for 5 times, and the shell is thickened by 0.02 mm each time.
7. The method for producing a casing for a heat-nonflammable cigarette according to claim 2, wherein: the glue dipping molds are fixed on the mold fixing plate together, and the tail ends of the hard core rods are positioned outside the mold fixing plate.
8. The method for producing a casing for a heat non-combustible cigarette according to claim 3, wherein: the outer sleeve and the inner core are transparent tubes.
CN202110751104.6A 2021-07-02 2021-07-02 Material for heating non-combustion cigarette shell and preparation method of cigarette shell Pending CN113455745A (en)