CN113211670B - Mixing roll capable of preventing rubber from being scorched - Google Patents

Mixing roll capable of preventing rubber from being scorched Download PDF

Info

Publication number
CN113211670B
CN113211670B CN202110421570.8A CN202110421570A CN113211670B CN 113211670 B CN113211670 B CN 113211670B CN 202110421570 A CN202110421570 A CN 202110421570A CN 113211670 B CN113211670 B CN 113211670B
Authority
CN
China
Prior art keywords
extrusion
rod
rubber
delay
mixing box
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202110421570.8A
Other languages
Chinese (zh)
Other versions
CN113211670A (en
Inventor
李玉滨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wenling Bosheng Plastic Co Ltd
Original Assignee
Wenling Bosheng Plastic Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wenling Bosheng Plastic Co ltd filed Critical Wenling Bosheng Plastic Co ltd
Priority to CN202110421570.8A priority Critical patent/CN113211670B/en
Publication of CN113211670A publication Critical patent/CN113211670A/en
Application granted granted Critical
Publication of CN113211670B publication Critical patent/CN113211670B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to the technical field of mixing, and discloses a mixing mill capable of preventing rubber from being scorched, which comprises a mixing box, wherein extrusion is arranged inside the mixing box, a supporting rod is rotatably connected inside the extrusion , a bearing wheel is meshed and connected with the side surface of the supporting rod, a metal plate is fixedly connected to the side surface of the supporting rod and positioned at one side far away from the bearing wheel, a delay rod is rotatably connected to one side of a conductive block far away from the supporting rod, a one-way extrusion block is arranged on the surface of the extrusion rod, a blocking rod is arranged on the side surface of the one-way extrusion block, a water bag is arranged inside the extrusion , and a hose is fixedly connected to the surface of the water bag. This can avoid rubber by mixing roll of scalding burnt uses through the cooperation of mercury pipe with the water pocket to reached and reached before extrusion surface temperature reaches the degree of scalding green rubber, automatically cooled down extrusion , prevented that the green rubber from being scalded burnt effect.

Description

Mixing roll capable of preventing rubber from being scorched
Technical Field
The invention relates to the technical field of mixing, in particular to a mixing mill capable of preventing rubber from being scorched.
Background
Mixing is a process of mixing raw rubber or plasticated raw rubber and an ingredient into mixed rubber by a rubber mixing mill, is the most important production process for rubber processing, is essentially the process of uniformly dispersing the ingredient in the raw rubber, has the granular ingredient in a dispersion phase and the raw rubber in a continuous phase, and is essential for the rubber manufacturing.
When rubber is mixed, raw rubber needs to be put between the extruders , meanwhile, additives such as an active agent are added, in the process, the extruders generate violent extrusion friction with the raw rubber, so that the surface of the extruders is high in temperature, and when the surface temperature of the extruders reaches a certain value, the contact part of the raw rubber and the extruders is scorched, so that the quality of the produced rubber is reduced.
Disclosure of Invention
Technical problem to be solved
Aiming at the defects of the prior art, the invention provides the mixing mill capable of preventing rubber from being scorched, which has the advantages of automatically cooling the extrusion before the surface temperature of the extrusion reaches the degree of scorching raw rubber, preventing the raw rubber from being scorched and the like, and solves the problem that the extrusion can not be cooled before the surface temperature of the extrusion reaches the degree of scorching raw rubber, so that the raw rubber is scorched.
(II) technical scheme
In order to realize the purpose of automatically cooling the extrusion and preventing the crude rubber from being scorched before the surface temperature of the extrusion reaches the degree of scorching crude rubber, the invention provides the following technical scheme: the mixing roll capable of avoiding rubber from being scorched comprises a mixing roll, wherein extrusion is arranged inside the mixing roll, a supporting rod is connected to the inner part of the extrusion in a rotating manner, a bearing wheel is connected to the side surface of the supporting rod in a meshed manner, a metal plate is fixedly connected to the side surface of the supporting rod and located on one side far away from the bearing wheel, a conductive rod is arranged on one side, far away from the mixing roll, of the metal plate, a conductive block is arranged on the side surface of the conductive rod in an alternating manner, a delay rod is connected to one side, far away from the supporting rod, of the conductive block in a rotating manner, a delay tube is connected to the side surface of the delay rod in a meshed manner, a mercury tube is arranged inside the extrusion , a mercury plate is connected to the inner part of the mercury tube in a sliding manner, an extrusion rod is fixedly connected to one side, close to the center, of the mercury plate, an one-way extrusion block is arranged on the surface of the extrusion rod, a water bag is arranged inside the extrusion , and a hose is fixedly connected to the surface of the water bag.
Preferably, the inside of extrusion is seted up the diversion channel.
Preferably, the side of the supporting rod is provided with a limiting spring.
Preferably, the delay rod and the delay tube are engaged in a direction approaching the mixing box in one direction, so that the metal plate is inserted between the conductive rods when being reset, and the bearing wheel cannot be rotated.
Preferably, the one-way extrusion block and the blocking rod are clamped in a one-way direction close to the center direction to store the extrusion force of the extrusion rod on the water bag.
Preferably, a supporting spring is arranged in the water bag, and the water bag is automatically reset to pump liquid water back when the extrusion rod does not extrude the water bag any more.
Preferably, a condenser is arranged inside the water bag, so that the liquid water in the water bag is kept at a low temperature.
Preferably, the hose is communicated with the water guide groove.
(III) advantageous effects
Compared with the prior art, the invention provides the mixing mill capable of preventing rubber from being scorched, and the mixing mill has the following beneficial effects:
1. this can avoid rubber by mixing roll that scalds burnt, cooperation through mercury pipe and water pocket is used, before the temperature on extrusion surface is close to reaching the degree that scalds burnt crude rubber, through the inflation of mercury in the mercury pipe, make the extrusion pole produce the extrusion to the water pocket, liquid water pours into the guiding gutter through the hose in the water pocket, the completion is to the cooling of extrusion , thereby reached and reached before the extrusion surface temperature reaches the degree that scalds burnt crude rubber, automatically to the cooling of extrusion , prevent that crude rubber from being scalded burnt effect.
2. This can avoid rubber by mixing roll that scalds burnt, cooperation through metal sheet and socket wheel is used, when the temperature on extrusion surface is close to the temperature that can scald burnt crude rubber, explain that the extrusion force between extrusion and the crude rubber reaches certain size, rotate through the socket wheel this moment and drive the carriage bar and remove to keeping away from mixing box direction, reduce the extrusion force between extrusion and the crude rubber, thereby reached before extrusion surface temperature reaches the degree that scalds burnt crude rubber, the effect of the extrusion force between extrusion and the crude rubber is reduced automatically.
Drawings
FIG. 1 is a schematic cross-sectional view of the entire structure of the present invention;
FIG. 2 is a schematic view of the structure and the conductive rod connection mechanism of the present invention;
FIG. 3 is a schematic cross-sectional view of a structural extrusion of the present invention;
FIG. 4 is a schematic cross-sectional view of a water bladder with the structure of the present invention;
FIG. 5 is a schematic cross-sectional view of a mercury tube according to the present invention;
FIG. 6 is a schematic view of the connection between the one-way extrusion block and the blocking rod according to the present invention.
In the figure: 1. mixing box; 2. pressing ; 3. a support bar; 4. a receiving wheel; 5. a metal plate; 6. a conductive rod; 7. a conductive block; 8. a delay bar; 9. a delay tube; 10. a mercury tube; 11. a mercury plate; 12. an extrusion stem; 13. a unidirectional extrusion block; 14. a blocking rod; 15. a water bag; 16. a hose; 17. a water diversion groove.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Referring to fig. 1-6, a mixer capable of preventing rubber from being scorched comprises a mixing box 1, wherein the mixing box 1 is made of stainless steel, which can effectively prevent equipment from being corroded, greatly prolongs the service life of the equipment, reduces the production cost, and plays an indispensable role in enterprises, extrusion 2 is arranged inside the mixing box 1, a supporting rod 3 is rotatably connected inside the extrusion 2, a limit spring is arranged on the side surface of the supporting rod 3, a receiving wheel 4 is engaged and connected on the side surface of the supporting rod 3, a metal plate 5 is fixedly connected on the side surface of the supporting rod 3 and on the side far away from the receiving wheel 4, a conductive rod 6 is arranged on the side surface of the metal plate 5 far away from the mixing box 1, a conductive block 7 is inserted into the side surface of the conductive rod 6, a delay rod 8 is rotatably connected on the side of the conductive block 7 far away from the supporting rod 3, the delay rod 8 is engaged with a delay tube 9 in a direction close to the mixing box 1, therefore, when the metal plate 5 is reset, the metal plate is inserted between the conducting rods 6, the receiving wheel 4 cannot be rotated, the side surface of the delay rod 8 is meshed and connected with the delay tube 9, the mercury tube 10 is arranged inside the extrusion 2, the mercury plate 11 is connected inside the mercury tube 10 in a sliding manner, one side, close to the center, of the mercury plate 11 is fixedly connected with the extrusion rod 12, the surface of the extrusion rod 12 is provided with the one-way extrusion block 13, the one-way extrusion block 13 is clamped with the blocking rod 14 in the one-way direction to the direction close to the center to accumulate the extrusion force of the extrusion rod 12 on the water bag 15, the side surface of the one-way extrusion block 13 is provided with the blocking rod 14, the blocking rod 14 is made of stainless steel and can effectively prevent equipment from being corroded, the water bag 15 is arranged inside the extrusion 2, the supporting spring is arranged inside the water bag 15, the condenser is arranged inside the water bag 15 to keep the liquid water in the water bag 15 at a low temperature, the surface of the water bag 15 is fixedly connected with the hose 16, the hose 16 is communicated with the water guide groove 17, and the water guide groove 17 is formed in the extrusion 2.
The working principle is that when the raw rubber is mixed, the motor is started, the extrusion 2 rotates, the raw rubber is put into the extrusion 2, and when the additive is put into the extrusion 352, the mixing starts.
The temperature of the extrusion 2 is gradually increased along with the progress of mixing, heat is gradually transferred to the mercury in the mercury tube 10 inside the extrusion 2, so that the mercury is heated and expanded to extrude the mercury plate 11, however, as the unidirectional extrusion block 13 arranged on the surface of the extrusion rod 12 on the side surface of the mercury plate 11 is blocked by the blocking rod 14, the extrusion rod 12 does not move immediately, as the surface temperature of the extrusion 2 changes, when the temperature approaches the temperature of the scorching raw rubber, the unidirectional extrusion block 13 goes over the blocking rod 14, so that the extrusion rod 12 moves rapidly towards the center of the extrusion 2 to extrude the water sac 15, the water sac 15 is extruded to fill the liquid water inside the water sac 15 into the diversion groove 17 through the hose 16, as the condenser exists in the water sac 15, the temperature of the liquid water in the water sac 15 is far lower than the temperature of the extrusion 2, so that the temperature of the extrusion 2 is rapidly reduced after the liquid water enters the diversion groove 17, the temperature of the surface of the extrusion 2 is rapidly reduced, so that the extrusion 2 is automatically cooled before the surface temperature of the extrusion 2 reaches the degree of burning the crude rubber, and the crude rubber is prevented from being burnt.
When the temperature of the surface of the extrusion 2 is close to the temperature capable of burning raw rubber, it is indicated that the extrusion force between the extrusion 2 and the raw rubber reaches a certain value, at this time, along with the increase of the extrusion force, the support rod 3 is driven by the extrusion to move in the direction away from the mixing box 1, and further the metal plate 5 is driven to be inserted between the conductive rods 6, so that the motor for controlling the receiving wheel 4 is electrified, the receiving wheel 4 rotates to move the support rod 3 engaged with the receiving wheel in the direction away from the mixing box 1, and the extrusion 2 moves along with the receiving wheel, and therefore, the extrusion force between the extrusion 2 and the raw rubber is reduced.
When the bracing piece 3 moved the certain distance, can lead to the fact the extrusion to conducting block 7, and then release conducting rod 6's side with conducting block 7, make take over wheel 4 and lose power, and bracing piece 3 resets fast under the effect that the side set up spacing spring, and the delay rod 8 of conducting block 7 side needs and the transmission of 9 meshing of delay tube, the event can not lead to taking over wheel 4 to rotate when inserting between conducting rod 6 when metal sheet 5 resets yet, thereby reached and reached before extrusion 2 and the gluey degree of raw extrusion between extrusion of raw rubber reach extrusion 2 surface temperature, the effect of automatic reduction extrusion and raw rubber.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.

Claims (4)

1. A mixer capable of avoiding scorching of rubber, comprising a mixing box (1), characterized in that: the mixing box is characterized in that an extrusion roller (2) is arranged in the mixing box (1), a support rod (3) is rotatably connected in the extrusion roller (2), a bearing wheel (4) is connected to the side surface of the support rod (3) in a meshed manner, a metal plate (5) is fixedly connected to the side surface of the support rod (3) and located on one side far away from the bearing wheel (4), a conductive rod (6) is arranged on one side of the metal plate (5) far away from the mixing box (1), a conductive block (7) is arranged on the side surface of the conductive rod (6) in an inserted manner, a delay rod (8) is rotatably connected to one side of the conductive block (7) far away from the support rod (3), a delay tube (9) is connected to the side surface of the delay rod (8) in a meshed manner, a mercury tube (10) is arranged in the extrusion roller (2), a mercury plate (11) is slidably connected to the inside of the mercury tube (10), and an extrusion rod (12) is fixedly connected to one side of the mercury plate (11) close to the center, a one-way extrusion block (13) is arranged on the surface of the extrusion rod (12), a blocking rod (14) is arranged on the side surface of the one-way extrusion block (13), a water bag (15) is arranged inside the extrusion roller (2), and a hose (16) is fixedly connected to the surface of the water bag (15);
a water diversion groove (17) is formed in the squeezing roller (2); a limiting spring is arranged on the side surface of the supporting rod (3); the delay rod (8) and the delay pipe (9) are meshed in a direction close to the mixing box (1) in a one-way manner; the one-way extrusion block (13) and the blocking rod (14) are clamped in a one-way direction close to the center.
2. A mixer capable of preventing scorch from occurring in rubber according to claim 1, wherein: and a supporting spring is arranged in the water bag (15).
3. A mixer capable of preventing scorch from occurring in rubber according to claim 2, wherein: a condenser is arranged in the water bag (15).
4. A mixer capable of preventing scorch from occurring in rubber according to claim 3, wherein: the hose (16) is communicated with the water guide groove (17).
CN202110421570.8A 2021-04-20 2021-04-20 Mixing roll capable of preventing rubber from being scorched Active CN113211670B (en)