CN112679193A - Method for making micro-element slow-release kettle - Google Patents

Method for making micro-element slow-release kettle Download PDF

Info

Publication number
CN112679193A
CN112679193A CN202110146342.4A CN202110146342A CN112679193A CN 112679193 A CN112679193 A CN 112679193A CN 202110146342 A CN202110146342 A CN 202110146342A CN 112679193 A CN112679193 A CN 112679193A
Authority
CN
China
Prior art keywords
outer layer
inner layer
materials
layer material
kettle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202110146342.4A
Other languages
Chinese (zh)
Inventor
张勇
刘洋
李江波
沈军福
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Superhigh Environmental Protection Technology Co ltd
Original Assignee
Shanghai Superhigh Environmental Protection Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Superhigh Environmental Protection Technology Co ltd filed Critical Shanghai Superhigh Environmental Protection Technology Co ltd
Priority to CN202110146342.4A priority Critical patent/CN112679193A/en
Publication of CN112679193A publication Critical patent/CN112679193A/en
Pending legal-status Critical Current

Abstract

The invention relates to a method for manufacturing a trace element slow-release kettle, which comprises the steps of respectively preparing materials, mixing the materials and mechanically rolling into mud materials for later use by taking purple sand mud and phlogopite as outer layer materials of a kettle body and taking diatom minerals, medical stone, tourmaline, wooden fish stone, loess stone powder and kaolin as inner layer materials. The method comprises the steps of taking an inner layer material, spreading the inner layer material, spreading an outer layer material, placing the inner layer material on the outer layer material, combining the inner layer material and the outer layer material into a combined body by utilizing manual moderate kneading, enabling the inner layer mineral material to be tightly combined with the outer layer purple sand material, manufacturing a purple sand kettle body, enabling the kettle body to be internally provided with a trace element slow release layer which is fully distributed with a micropore structure, fully improving the mechanical property of a composite material, enhancing the strength of the internal micropore structure, and then drying in the shade, roasting, cooling and burning to obtain the purple sand slow release kettle. The microelement slow release pot is used for infusing tea water, tea is placed in the pot, and microelements and the tea water are released in the infusing process.

Description

Method for making micro-element slow-release kettle
Technical Field
The invention relates to a teapot containing trace elements, in particular to a manufacturing method of a trace element slow-release teapot.
Background
The trace elements are important substances for guaranteeing the health of people, and the trace elements necessary for human bodies are as follows: phosphorus, sulfur, potassium, sodium, chlorine, magnesium, iron, zinc, fluorine, rubidium, strontium, copper, iodine, selenium, manganese, cobalt and the like, and the trace elements play an extremely important role in important physiological processes of growth and development, reproductive inheritance, immunity and the like of a human body. Scientifically and properly supplement various trace elements necessary for human body, can regulate physiological function, promote metabolism, improve memory and invigorate human energy.
At present, a lot of products for supplementing trace elements exist in the market, and the products mainly comprise deep-sea fish oil soft capsules, and the range of the trace elements of the products is narrow; for example, the plant soybean, sunflower seed oil, gelatin, glycerin, lemon and the like contain a plurality of trace elements, but the plant varieties are too many to be supplemented in a targeted manner; and for example, Chinese wolfberry, tuckahoe, astragalus, angelica, liquorice and ginseng in the traditional Chinese medicinal materials contain rich trace elements necessary for human bodies, and because the trace elements belong to medical medicinal materials, doctors must prepare prescription medicines according to the physical conditions of all people to supplement. Therefore, how to develop a nourishing product capable of better promoting the absorption of trace elements by human body is a problem to be solved by researchers.
In view of this, the research and development of a trace element product which is convenient to take and easy to carry and can promote the rapid absorption of human bodies becomes a new target sought by scientific researchers in the field.
Disclosure of Invention
The invention aims to provide a method for manufacturing a trace element slow-release kettle, which comprises the steps of taking purple sand mud and phlogopite as outer layer materials of a kettle body, taking diatom minerals, medical stones, tourmaline, wooden fish stones, loess stone powder and kaolin as inner layer materials, respectively carrying out burdening, material mixing and machine rolling to obtain mud materials for later use, and then combining the mud materials into a combined body by hand and moderate kneading to enable the mineral materials of the inner layer to be tightly combined with the purple sand materials of the outer layer to manufacture the purple sand kettle body with the appearance, wherein a trace element slow-release layer with a microporous structure is fully distributed in the kettle body, so that the mechanical property of the combined material is fully improved, the strength of the microporous structure in the kettle body is enhanced, and the problem that the purple sand kettle produced according to the traditional technology.
The technical solution of the invention is as follows:
a method for preparing a microelement slow release kettle comprises taking purple sand mud and phlogopite as outer layer materials of a kettle body, taking diatom minerals, medical stone, tourmaline, wooden fish stone, loess stone powder and kaolin as inner layer materials, respectively blending, mixing and mechanically rolling into mud materials for later use;
spreading an inner layer of standby material, wherein the spreading thickness of the inner layer of material is 1.5-2.5 mm, and the spreading length and width of the inner layer of material are respectively 2 mm with lower tolerance according to the diameter of the kettle body;
spreading an outer layer of standby material, wherein the spreading thickness of the outer layer of material is 1-2 mm, and the spreading length and width of the outer layer of material are respectively limited by an upper tolerance of 1 mm according to the diameter of the kettle body;
the inner layer material is placed on the outer layer material after the outer layer material is laid flat, the inner layer material and the outer layer material are combined into a combined body by manual moderate kneading, so that the mineral material of the inner layer and the purple sand material of the outer layer are tightly combined to manufacture the purple sand kettle body with the appearance, the interior of the kettle body is provided with a trace element slow-release layer which is fully distributed with a micropore structure, and the purple sand slow-release kettle is manufactured by drying in the shade, roasting, cooling and burning.
The inner layer material thickness is optimally 2 mm.
The thickness of the outer layer material is optimally 1.5 mm.
According to the manufacturing method of the trace element slow-release kettle, purple sand mud and phlogopite are used as outer layer materials of a kettle body, diatom minerals, medical stones, tourmaline, wooden fish stones, loess stone powder and kaolin are used as inner layer materials, the materials are respectively proportioned, mixed and mechanically rolled into mud materials for later use, then the mud materials are combined into a combined body through manual moderate kneading, the mineral materials in the inner layer and the purple sand materials in the outer layer are tightly combined, the purple sand kettle body with the appearance is manufactured, and a trace element slow-release layer with a microporous structure is fully distributed in the kettle body, so that the mechanical property of the composite material is fully improved, the strength of the microporous structure in the composite material is enhanced, and the purple sand kettle has the functions of being rich in trace elements, convenient to soak and can promote the rapid.
The microelement slow release kettle manufactured by the method can be used for soaking tea water drunk by human bodies, provides a new option for selecting daily microelement supplement health-care products, and has important application value.
Drawings
FIG. 1 is a schematic view of the structure of a slow release kettle for trace elements manufactured by the method of the present invention.
Fig. 2 is a schematic top view of the microelement slow-release pot shown in fig. 1.
Fig. 3 is an enlarged schematic view of a portion a in fig. 1.
Reference numerals:
1 is an outer layer material, and 2 is an inner layer material.
Detailed Description
The present invention will be described in detail below with reference to the accompanying drawings and examples.
Referring to fig. 1 to 3, the invention provides a method for manufacturing a microelement slow release kettle, which comprises the steps of respectively carrying out batching, material mixing and machine rolling on purple sand mud and phlogopite as outer layer materials 1 of a kettle body and diatom minerals, medical stones, tourmaline, wooden fish stones, loess stone powder and kaolin as inner layer materials 2 to obtain mud materials for later use.
Spreading the inner layer material for later use, wherein the spreading thickness of the inner layer material 2 is 1.5-2.5 mm, and the optimal thickness of the inner layer material is 2 mm. The spreading length and width of the inner layer material are respectively 2 mm with the lower tolerance according to the diameter of the kettle body.
And then taking an outer layer standby material to spread, wherein the spreading thickness of the outer layer material 1 is 1-2 mm, and the optimal thickness of the outer layer material is 1.5 mm. The spreading length and width of the outer layer material are respectively limited by the upper tolerance of 1 mm according to the diameter of the kettle body.
After the outer layer material is spread, as shown in figure 3, the inner layer material 2 is placed on the outer layer material 1, the inner layer material and the outer layer material are combined into a combined body by manual moderate kneading, so that the mineral material of the inner layer and the purple sand material of the outer layer are tightly combined to manufacture the purple sand kettle body with the appearance, and the interior of the kettle body is provided with a trace element slow release layer which is fully distributed with a micropore structure.
Then drying in the shade, roasting and cooling, and finally, roasting to prepare the purple sand slow-release teapot.
The appearance of the microelement slow release teapot manufactured by the method is a dark-red enameled pottery, and the interior of the teapot is provided with the microelement slow release layer which is fully distributed with a micropore structure, so that the mechanical property of the composite material is fully improved, the strength of the micropore structure in the teapot is enhanced, and the teapot has the functions of being rich in microelements, convenient to soak and take and capable of promoting the quick absorption of a human body.
The microelement slow-release pot is used for infusing tea water, tea is placed in the pot, and microelements and tea water are released in the infusion process, so that a new option is provided for selecting daily microelement supplement health care products.
Of course, those skilled in the art will recognize that the above-described embodiments are illustrative only and not intended to be limiting, and that changes, modifications, etc. to the above-described embodiments are intended to fall within the scope of the appended claims, provided they fall within the true spirit and scope of the present invention.

Claims (3)

1. A manufacturing method of a microelement slow release kettle is characterized in that: respectively mixing and mechanically rolling purple sand mud and phlogopite as outer layer materials of the kettle body and diatom minerals, medical stone, tourmaline, wooden fish stone, loess stone powder and kaolin as inner layer materials into mud materials for later use;
spreading an inner layer of standby material, wherein the spreading thickness of the inner layer of material is 1.5-2.5 mm, and the spreading length and width of the inner layer of material are respectively 2 mm with lower tolerance according to the diameter of the kettle body;
spreading an outer layer of standby material, wherein the spreading thickness of the outer layer of material is 1-2 mm, and the spreading length and width of the outer layer of material are respectively limited by an upper tolerance of 1 mm according to the diameter of the kettle body;
the inner layer material is placed on the outer layer material after the outer layer material is laid flat, the inner layer material and the outer layer material are combined into a combined body by manual moderate kneading, so that the mineral material of the inner layer and the purple sand material of the outer layer are tightly combined to manufacture the purple sand kettle body with the appearance, the interior of the kettle body is provided with a trace element slow-release layer which is fully distributed with a micropore structure, and the purple sand slow-release kettle is manufactured by drying in the shade, roasting, cooling and burning.
2. The method for manufacturing a microelement slow release pot according to claim 1, wherein: the inner layer material thickness is optimally 2 mm.
3. The method for manufacturing a microelement slow release pot according to claim 1, wherein: the thickness of the outer layer material is optimally 1.5 mm.
CN202110146342.4A 2021-02-03 2021-02-03 Method for making micro-element slow-release kettle Pending CN112679193A (en)