CN112517235B - Method for improving comprehensive utilization of durite tailings - Google Patents

Method for improving comprehensive utilization of durite tailings Download PDF

Info

Publication number
CN112517235B
CN112517235B CN202011318989.2A CN202011318989A CN112517235B CN 112517235 B CN112517235 B CN 112517235B CN 202011318989 A CN202011318989 A CN 202011318989A CN 112517235 B CN112517235 B CN 112517235B
Authority
CN
China
Prior art keywords
tailings
durite
fine
concentration
overflow
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202011318989.2A
Other languages
Chinese (zh)
Other versions
CN112517235A (en
Inventor
傅卫东
李金祥
徐�明
杨正贤
马浩山
许向阳
王成伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Jinhong New Material Co ltd
Original Assignee
Jiangsu Jinhong New Material Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Jinhong New Material Co ltd filed Critical Jiangsu Jinhong New Material Co ltd
Priority to CN202011318989.2A priority Critical patent/CN112517235B/en
Publication of CN112517235A publication Critical patent/CN112517235A/en
Application granted granted Critical
Publication of CN112517235B publication Critical patent/CN112517235B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for improving comprehensive utilization of durite tailings, which comprises the following steps: the method comprises the following steps of carrying out graded desliming on the durite tailings by a two-stage spiral classifier, selecting and screening the diopside in the tailings, enabling overflow products subjected to the graded desliming twice to flow into a high-efficiency thickener for concentration, returning overflow of the thickener to an on-site production process flow for use as circulating water, conveying underflow of the thickener to a hydrocyclone by a slurry pump for graded desliming, wherein the overflow products are slurry containing mud, carrying out compression and dehydration by a plate and frame filter press to realize dry discharge of the tailings, returning the water subjected to the compression and dehydration to a circulating water tank for use as the circulating water, and being simple in the whole process flow, low in energy consumption and low in production cost, capable of recovering useful minerals in the durite to the maximum extent, and capable of achieving the recovery rates of more than 95% for garnet and diopside, and carrying out dry discharge on the tailings; has no influence on the environment, and realizes the modern production without tail, waste and pollution.

Description

Method for improving comprehensive utilization of durite tailings
Technical Field
The invention belongs to the technical field of mineral separation, and particularly relates to a method for improving comprehensive utilization of durite tailings.
Background
The tailings treatment is an important part of the comprehensive utilization of resources. A large amount of domestic tailings usually have the characteristics of poor quality, fine quality and impurity, particularly, the common mineral separation process and equipment of certain difficultly-separated tailings are difficult to efficiently recover, the maximum recovery of useful minerals cannot be realized, a plurality of mining enterprises do not have the strength of tailing recleaning plants, the economic level and mineral separation technology limit in the early development stage of enterprises, most of the selection plants adopt a rough operation mode, so that a plurality of valuable minerals are discarded along with the tailings, the discharge of the tailings is increased, the great waste of mine resources is caused, improper utilization of the tailings not only occupies the land and causes the waste of resources, but also brings serious pollution and harm to the living environment of people, and the environment is deteriorated. How to realize the modern production without tail, waste and pollution to achieve the purpose of promoting the comprehensive treatment of mine environment is also an important subject of common concern of China and all countries in the world.
The associated minerals in the tailings have large stock and high value. Natural ores are basically symbiotic and associated with multiple minerals, and the value of useful minerals in tailings cannot be underestimated. The main substances in the durite tailings are fine-grained garnet, green glow and fine-grained slime, the recycling of useful minerals in the tailings is mainly influenced by primary slime and secondary slime generated in production, the fine-grained garnet is a high-quality cutting abrasive for cutting precise instruments and parts with high precision requirements, the fine abrasive can improve the cutting precision, the green glow is a main raw material of building materials such as wall tiles and the like, and the tailings can be used as pit filling materials and building materials after being treated, so that the comprehensive utilization of tailings resources is improved, the sustainable utilization of resources is facilitated, and the pressure of environmental pollution is reduced.
Disclosure of Invention
The invention aims to provide a method for improving comprehensive utilization of the durite tailings so as to solve the problems in the background technology.
In order to achieve the purpose, the invention provides the following technical scheme: a method for improving comprehensive utilization of durite tailings comprises the following steps:
the method comprises the following steps: major ore fine-grade garnet, green pyroxene and slime of the durite tailings are subjected to size mixing to form 10-15% low-concentration ore pulp;
step two: the low-concentration durite tailing pulp enters a No. 1 spiral classifier for desliming classification, an overflow product is mainly slime with the concentration lower than 15%, and return sand is pulp with the concentration more than 50% and consists of fine garnet, green pyroxene and a small amount of slime;
step three: the returned sand obtained in the second step is subjected to size mixing to form 20-25% of low-concentration ore pulp, and then enters a No. 2 spiral classifier for secondary desliming and classification, wherein the main material of the returned sand subjected to classification and desliming is green pyroxene, and overflow products are fine-grained garnet and slime with lower concentration;
step four: step two and step three, the overflow products of No. 1 and No. 2 ore washers enter a high-efficiency thickener for thickening, the concentration of the ore pulp is improved, and the overflow water of the thickener returns to the production flow to form circulating water for reuse;
step five: the concentration of the bottom flow product of the high-efficiency thickener is 45 percent, the bottom flow product is conveyed to a swirler by a slurry pump for graded desliming, two products can be obtained after grading, the overflow product is mainly slime, and the settled sand is mainly fine-grained garnet;
step six: conveying the overflow product of the step five to a filter press by a slurry pump for filter pressing, wherein the water content of the filter-pressed product is lower than 10%, the filter-pressed product can be directly conveyed to a backfilling pit of a mining pit or used as a raw material of a building material, and the filter-pressed water is returned to the process flow to be used as circulating water;
step seven: the settled sand produced by the six cyclones is mainly fine-grained garnet, a filter is adopted for filtering to form 10% fine-grained garnet fine sand, the fine-grained garnet fine sand is returned to the process flow for retreatment, and the filtered water is returned to the process flow to be used as circulating water.
Preferably, the spiral classifier in step two and step three is a high weir type double spiral classifier with a diameter of 1.2 meters.
Preferably, the high-efficiency thickener in the fourth step is an NXZ-30 high-efficiency thickener with the diameter of 30 meters.
Preferably, the cyclone in the fifth step is a cyclone with the model number of FX-350, the diameter of the sand settling nozzle is 70mm, and the diameter of the overflow port is 100 mm.
Preferably, the filter press in step six is a plate and frame filter press.
Preferably, the filter in step seven is a plate disc filter.
Compared with the prior art, the invention has the beneficial effects that: the invention aims to effectively recover fine-grained garnet and green pyroxene in the tailings, improve the resource utilization rate, further treat slime in the tailings and realize dry discharge of the tailings, and the method has low production cost and truly realizes 'tailless, waste-free and pollution-free' modern production of a selected factory; the whole process flow is simpler, the energy consumption is lower, the production cost is low, useful minerals in the ores are recovered to the maximum extent, and the environment is not polluted.
Drawings
FIG. 1 is a flow diagram of a beneficiation process in an embodiment of the present invention;
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Example 1
Referring to fig. 1, the present invention provides a technical solution: a method for improving the comprehensive utilization rate of the durite tailings comprises the following steps:
the method comprises the following steps: carrying out size mixing on the main ore of the durenite tailings, namely fine-grained garnet, green pyroxene and slime to form 10-15% low-concentration ore pulp;
step two: the low-concentration durite tailing pulp enters a No. 1 spiral classifier for desliming classification, an overflow product is mainly slime with the concentration lower than 15%, and return sand is pulp with the concentration more than 50% and consists of fine garnet, green pyroxene and a small amount of slime;
step three: the returned sand obtained in the second step is subjected to size mixing to form 20-25% of low-concentration ore pulp, and then enters a No. 2 spiral classifier for secondary desliming and classification, wherein the main material of the returned sand subjected to classification and desliming is green pyroxene, and overflow products are fine-grained garnet and slime with lower concentration;
step four: step two and step three, the overflow products of No. 1 and No. 2 ore washers enter a high-efficiency thickener for thickening, the concentration of the ore pulp is improved, and the overflow water of the thickener returns to the production flow to form circulating water for reuse;
step five: the concentration of the bottom flow product of the high-efficiency thickener is 45 percent, the bottom flow product is conveyed to a swirler by a slurry pump for graded desliming, two products can be obtained after grading, the overflow product is mainly slime, and the settled sand is mainly fine-grained garnet;
step six: conveying the overflow product of the step five to a filter press by a slurry pump for filter pressing, wherein the water content of the filter-pressed product is lower than 10%, the filter-pressed product can be directly conveyed to a backfilling pit of a mining pit or used as a raw material of a building material, and the filter-pressed water is returned to the process flow to be used as circulating water;
step seven: the settled sand produced by the six cyclones is mainly fine-grained garnet, a filter is adopted for filtering to form 10% fine-grained garnet fine sand, the fine-grained garnet fine sand is returned to the process flow for retreatment, and the filtered water is returned to the process flow to be used as circulating water.
In this embodiment, preferably, the spiral classifier in the second step and the third step is a high weir type single spiral classifier with a diameter of 1.2 m, the installation inclination angle of the spiral classifier is smaller, and the groove body of the spiral classifier is lengthened compared with that of a common spiral classifier, so that the spiral classifier has the advantages of large treatment capacity and high efficiency of classification and desliming.
In this embodiment, preferably, the high-efficiency thickener in the fourth step is an NXZ-30 high-efficiency thickener with a diameter of 30 meters, and has a large diameter, a large treatment capacity, a good concentration effect, and low power consumption.
In this embodiment, the cyclone in step five is preferably FX-350 in size, the sand settling nozzle is 70mm in diameter, and the overflow port is 100mm in diameter, and the cyclone has the advantages of no moving parts in the cyclone, simple structure and convenient use. Compared with other classification separation equipment, the cyclone has higher classification efficiency which can reach more than 80 percent, and the classification granularity of the cyclone is fine, thus meeting the requirements of industrial production; in addition, the cyclone has low manufacturing cost, less material consumption and more economic value.
In this embodiment, preferably, the filter press in the sixth step is a plate and frame filter press, which has a simpler structure, is easy to operate, runs stably, and has a flexible selection range of filter area and a small floor area; has strong adaptability to materials.
In this embodiment, preferably, the filter in the seventh step is a plate disc type filter, and the disc type filter has the advantages of thorough filtration, high working efficiency, long service life, simple structure, easy operation, and stable operation.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.

Claims (5)

1. A method for improving comprehensive utilization of durite tailings is characterized by comprising the following steps: the method comprises the following steps:
the method comprises the following steps: carrying out size mixing on the main ore of the durenite tailings, namely fine-grained garnet, green pyroxene and slime to form 10-15% low-concentration ore pulp;
step two: the low-concentration durite tailing pulp enters a No. 1 spiral classifier for desliming classification, overflow products mainly comprise ore mud with the concentration lower than 15%, return sand is ore pulp with the concentration more than 50% and consists of fine garnet, green pyroxene and a small amount of ore mud;
step three: the returned sand obtained in the second step is subjected to size mixing to form 20-25% of low-concentration ore pulp, and then enters a No. 2 spiral classifier for secondary desliming and classification, wherein the main material of the returned sand subjected to classification and desliming is green pyroxene, and overflow products are fine-grained garnet and slime with lower concentration;
step four: step two and step three overflow products of No. 1 and No. 2 ore washers enter a high-efficiency thickener for thickening, the concentration of ore pulp is improved, and overflow water of the thickener returns to a production and abortion flow to form circulating water for reuse;
step five: the concentration of the bottom flow product of the efficient thickener is 45 percent, the bottom flow product is conveyed to a swirler by a slurry pump for graded desliming, and two products are obtained after grading, wherein the overflow product is mainly slime, and the settled sand is mainly fine-grained garnet;
step six: conveying the overflow product of the step five to a filter press by a slurry pump directly for filter pressing, wherein the water content of the filter-pressed product is lower than 10%, directly conveying the product to a mining pit for backfilling the pit or using the product as a raw material of a building material, and returning the filter-pressed water to the process flow for using as circulating water;
step seven: the settled sand generated by the six cyclones is mainly fine-grained garnet, a filter is adopted for filtering to form 10% of fine-grained garnet fine sand, the fine sand returns to the process flow for retreatment, and the filtered water returns to the process flow and is used as circulating water;
the spiral classifier in the second step is a high weir type double-spiral classifier with the diameter of 1.2 meters.
2. The method for improving comprehensive utilization of the durite tailings according to claim 1, wherein the method comprises the following steps: the high-efficiency thickener in the fourth step is an NXZ-30 high-efficiency thickener with the diameter of 30 meters.
3. The method for improving comprehensive utilization of the durite tailings according to claim 1, wherein the method comprises the following steps: the cyclone in the step five is the cyclone with the model number of FX-350, the diameter of the sand settling nozzle is 70mm, and the diameter of the overflow port is 100 mm.
4. The method for improving comprehensive utilization of durite tailings according to claim 1, wherein the method comprises the following steps: and the filter press in the sixth step is a plate and frame filter press.
5. The method for improving comprehensive utilization of durite tailings according to claim 1, wherein the method comprises the following steps: the filter in the seventh step is a plate disc type filter.
CN202011318989.2A 2020-11-23 2020-11-23 Method for improving comprehensive utilization of durite tailings Active CN112517235B (en)