CN1124815A - 油田配注作业施工的暂堵技术 - Google Patents
油田配注作业施工的暂堵技术 Download PDFInfo
- Publication number
- CN1124815A CN1124815A CN 93114648 CN93114648A CN1124815A CN 1124815 A CN1124815 A CN 1124815A CN 93114648 CN93114648 CN 93114648 CN 93114648 A CN93114648 A CN 93114648A CN 1124815 A CN1124815 A CN 1124815A
- Authority
- CN
- China
- Prior art keywords
- consumption
- blanking plug
- diverting agent
- agent
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明涉及一种用于油田配注作业施工的暂堵技术,属于油田化学应用领域,使用该技术可免去配注作业施工中投捞堵塞器的工序,主要技术特征是:用暂堵剂先将水嘴堵死,装入堵塞器内,随配水器下入井内,待封隔器坐封后一定时间内,暂堵剂全部分散溶解后即可正常配注,从而减少施工周期和劳动强度。暂堵剂由无机盐、半乳甘露糖、胶粘剂、增塑剂、固化剂、稀释剂及填料组成,具有适应温度范围广、强度适宜等特征,能满足施工要求。
Description
本发明涉及一种用于油田注水井配注作业施工的暂堵技术,属于油田化学应用领域。
油田分层注水是在注水井中下入封隔器将各油层分隔开,并在各注水层段装有偏心配水器,配水器由工作筒和堵塞器组成,堵塞器位于工作筒内,堵塞器内装有水嘴,靠水嘴的大小来控制各注水层的注水量。本发明之前注水井配注作业施工时,需将堵塞器内的水嘴先装死嘴子,随配水器下入井内,待封隔器坐封后,需将堵塞器捞出,把死嘴子换成不同直径的水嘴,再将堵塞器投送到工作筒内,以达到分层配水的目的,这样施工周期长,劳动强度大,且投捞堵塞器时,易造成井下落物而必须重新作业。本发明的构思是使用一种暂堵剂,先将水嘴封堵,在地面装入堵塞器内,将其投入工作筒,然后下入井内,待封隔器坐封后的一定时间内,暂堵剂全部分散溶解,然后可转入正常注水,配注作业施工中免去投捞堵塞器的工序,从而减少施工周期和劳动强度。
目前已有的暂堵剂用于压裂封堵炮眼,它分为油溶性和水溶性两种,均属堆积堵塞,该暂堵剂堵塞时间短,一般不超过3小时,暂堵剂适应的温度低于地层原始温度,适应的强度低,堵剂本身不受剪切力,该种暂堵剂不适用于配注作业施工。
用于配注作业施工的暂堵剂,粘在水嘴下方,置于堵塞器滤网内只有1立方厘米的空间内,用量少,且要求适应温度为40-60℃,堵塞时间为10-15小时,承压20MPa,待封隔器坐封后,该暂堵剂在24-30小时内可全部分散溶解,压力对堵剂是一个剪切的破坏力。
本发明的目的在于避免上述已有技术的不足之处,而提供一种暂堵剂,及其使用方法。
本发明的目的可通过以下技术方案而达到:该暂堵剂由无机盐、半乳甘露糖,胶粘剂、固化剂、增塑剂、稀释剂及填料所组成。暂堵剂配方及各组份重量百分比如下:
无机盐为氯化钠或氯化钙,用量27.0%;
半乳甘露糖为田菁或爪胶,用量28.0%;该成份用来控制溶速;
胶粘剂为环氧树脂,用量8.0%;可控制胶结程度,达到不同使用温度范围;
810水下环氧固化剂,用量3.5%;
增塑剂为邻苯二甲酸二丁脂,用量1%;
稀释剂为乙醇或丙酮,用量5.5%,用于稀释胶粘剂并与备组份混匀;
填料为270目石英砂,用量27%,可调解溶速,使其与胶粘剂形成承压主体。
将配方中的各组份混合后,搅拌均匀,在模具中砸制成圆柱体,在恒温箱内恒温后即可使用。
下面给出本发明的一个最佳实施例:
暂堵剂配方和各组份重量百分比为:
氯化钠:田菁:环氧树脂:810水下环氧固化剂:邻苯二甲酸二丁脂:乙醇:270目石英砂=27%∶28%∶8%∶3.5%∶1%∶5.5%∶27% 。
将以上配方中各组份按重量百分比混合后,在Φ12mm模具中砸制成高10mm的圆柱体,在恒温箱内恒温40℃,经8小时后即可使用。使用时将暂堵剂用金属胶粘在水嘴下方,然后随配注管柱下入井内,封隔器坐封后,暂堵剂在24-30小时内全部分散溶解,完成暂堵作用。
本发明的优点是:构思新颖,在配注作业施工中免去投捞堵塞器的工序,大大降低了作业工人的劳动强度,提高作业施工效率,并有利于安全施工;该暂堵技术使用的暂堵剂能满足现场施工要求,即能保证封隔器正常坐封,又可保证正常配注;暂堵剂配方中各组份无毒、对空气无污染,暂堵剂成形操作简单,具有适应温度范围广、强度适宜、堵得住、解得开等特征。本发明为注水井配注作业施工提供了一种新的配套技术。
Claims (2)
1、本发明属于油田化学应用领域,称为油田配注作业施工的暂堵技术,本发明之前,油田注水井配注作业施工时,需将堵塞器内的水嘴先装死嘴子,随配水器下入井内,待封隔器坐封后,将堵塞器捞出,把死嘴子换成不同直径的水嘴,再将堵塞器投送到工作筒内,本发明的特征在于:用暂堵剂先将水嘴封堵后,装入堵塞器内,随配水器下入井内,待封隔器坐封后的一定时间内,暂堵剂全部分散溶解,免去作业施工中投捞堵塞器的工序。
2、如权利要求1所述的暂堵技术,其特征在于:所说的暂堵剂由无机盐,半乳甘露糖、胶粘剂、固化剂、增塑剂、稀释剂及填料所组成,暂堵剂配方及各组份重量百分比如下:
无机盐为氯化钠或氯化钙,用量27.0%;
半乳甘露糖为田菁或爪胶,用量28.0%;
胶粘剂为环氧树脂,用量8.0%;
810水下环氧固化剂,用量3.5%;
增塑剂为邻苯二甲酸二丁脂,用量1%;
稀释剂为乙醇或丙酮,用量5.5%;
填料为270目石英砂,用量27%。