CN112157776A - Processing method of reinforced solid wood floor board - Google Patents
Processing method of reinforced solid wood floor board Download PDFInfo
- Publication number
- CN112157776A CN112157776A CN202011093920.4A CN202011093920A CN112157776A CN 112157776 A CN112157776 A CN 112157776A CN 202011093920 A CN202011093920 A CN 202011093920A CN 112157776 A CN112157776 A CN 112157776A
- Authority
- CN
- China
- Prior art keywords
- curing
- paint
- sanding
- solid wood
- wood floor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention belongs to the technical field of wood floor processing, and particularly relates to a processing method of a reinforced solid wood floor board, which comprises the following steps: the method comprises the following steps: selecting and processing materials; selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate; step two: controlling the water content; stacking the plates with the specifications together, and placing the plates in the sun for high-temperature exposure to ensure that the water content in the plates is 15-25%; step three: processing a plate; the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening; step four: the board paint process can accurately master the water content in the solid wood floor, and effectively prevents the solid wood floor from cracking, deforming and falling off due to paint on the surface after being used for a long time, so that the service life of the solid wood floor is influenced.
Description
Technical Field
The invention relates to the technical field of wood floor processing, in particular to a processing method of a reinforced solid wood floor board.
Background
The wood floor is a ground decoration material formed by drying and processing natural wood, is also called a log floor, is a floor directly processed by wood, has the texture of natural growth of wood, is a poor thermal conductor, can play a role of being warm in winter and cool in summer, has comfortable foot feeling and safe use, and is an ideal material for ground decoration of bedrooms, living rooms, study rooms and the like.
However, when the existing processing method of the reinforced solid wood floor board is used for producing and processing the board, the moisture in the board can not be accurately controlled, so that the produced wood floor board is easy to deform, and the paint falls and cracks after being used for a long time, thereby influencing the service life of the wood floor board.
Disclosure of Invention
The invention aims to provide a processing method of a reinforced solid wood floor board, which aims to solve the problem that the service life of the wood floor board is influenced because the water content in the board cannot be accurately mastered when the wood floor board is produced by the existing board processing method in the background technology, and the produced board is easy to drop paint, crack and the like after being used for a long time.
In order to achieve the purpose, the invention provides the following technical scheme: the processing method of the reinforced solid wood floor board comprises the following steps:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun for high-temperature exposure to ensure that the water content in the plates is 15-25%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
the method comprises the following steps of repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, applying sealing base paint, drying and curing, applying base paint, UV curing, sanding, applying base color, UV curing, applying base paint, UV curing, sanding, applying back paint, UV curing, rolling finish paint, spraying paint, UV curing, applying high-performance finish paint, UV curing, color separation and the like, spraying codes, packaging, performing selective inspection according to standards, obtaining qualified products and leaving factories.
Preferably, the board is exposed to high temperature for 2-3 weeks.
Preferably, the length of the solid wood floor board is 40cm-50 cm.
Preferably, the thickness of the solid wood floor is 2cm-3 cm.
Preferably, the width of the solid wood board is 10cm-13 cm.
Compared with the prior art, the invention has the beneficial effects that:
through the common cooperation of selected materials processing, control water content, panel processing and panel paint technology, can accurately master the inside water content of solid wood floor, prevent effectively that solid wood floor from after long-time the use, the condition that fracture, deformation and surface paint dropped appears, influence solid wood floor's life.
Drawings
FIG. 1 is a flow chart of the processing method of the reinforced solid wood floor board.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
In the description of the present invention, it is to be understood that the terms "upper", "lower", "front", "rear", "left", "right", "top", "bottom", "inner", "outer", and the like, indicate orientations or positional relationships based on the orientations or positional relationships shown in the drawings, are merely for convenience in describing the present invention and simplifying the description, and do not indicate or imply that the device or element being referred to must have a particular orientation, be constructed and operated in a particular orientation, and thus, should not be construed as limiting the present invention.
Referring to fig. 1, the present invention provides a technical solution: the processing method of the reinforced solid wood floor board comprises the following steps:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun for high-temperature exposure to ensure that the water content in the plates is 15-25%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, sealing base paint, drying and curing, priming paint, UV curing, sanding, priming paint coating, UV curing, sanding, priming color coating, UV curing, priming paint coating, UV curing, sanding, back paint coating, UV curing, rolling finish paint, paint spraying, UV curing, high-performance finish paint, UV curing, color separation and the like, code spraying, packaging, performing selective inspection according to standards, obtaining qualified products and leaving a factory;
exposing the plate to the sun at high temperature for 2-3 weeks;
the length of the solid wood floor board is 40cm-50 cm;
the thickness of the solid wood floor is 2cm-3 cm;
the width of the solid wood board is 10cm-13 cm.
Example 1:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun to be exposed at high temperature to ensure that the water content in the plates is 15%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
the method comprises the following steps of repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, applying sealing base paint, drying and curing, applying base paint, UV curing, sanding, applying base color, UV curing, applying base paint, UV curing, sanding, applying back paint, UV curing, rolling finish paint, spraying paint, UV curing, applying high-performance finish paint, UV curing, color separation and the like, spraying codes, packaging, performing selective inspection according to standards, obtaining qualified products and leaving factories.
Example 2:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun to be exposed at high temperature to ensure that the water content in the plates is 20%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
the method comprises the following steps of repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, applying sealing base paint, drying and curing, applying base paint, UV curing, sanding, applying base color, UV curing, applying base paint, UV curing, sanding, applying back paint, UV curing, rolling finish paint, spraying paint, UV curing, applying high-performance finish paint, UV curing, color separation and the like, spraying codes, packaging, performing selective inspection according to standards, obtaining qualified products and leaving factories.
Example 3:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun to be exposed at high temperature to ensure that the water content in the plates is 25%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
the method comprises the following steps of repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, applying sealing base paint, drying and curing, applying base paint, UV curing, sanding, applying base color, UV curing, applying base paint, UV curing, sanding, applying back paint, UV curing, rolling finish paint, spraying paint, UV curing, applying high-performance finish paint, UV curing, color separation and the like, spraying codes, packaging, performing selective inspection according to standards, obtaining qualified products and leaving factories.
While there have been shown and described the fundamental principles and essential features of the invention and advantages thereof, it will be apparent to those skilled in the art that the invention is not limited to the details of the foregoing exemplary embodiments, but is capable of other specific forms without departing from the spirit or essential characteristics thereof; the present embodiments are therefore to be considered in all respects as illustrative and not restrictive, the scope of the invention being indicated by the appended claims rather than by the foregoing description, and all changes which come within the meaning and range of equivalency of the claims are therefore intended to be embraced therein, and any reference signs in the claims are not intended to be construed as limiting the claim concerned.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.
Claims (5)
1. The processing method of the reinforced solid wood floor board is characterized by comprising the following steps:
the method comprises the following steps: selecting and processing materials;
selecting wood with straight part of stems and thick diameter from the original wood, and splitting, sawing and trimming to form a specification plate;
step two: controlling the water content;
stacking the plates with the specifications together, and placing the plates in the sun for high-temperature exposure to ensure that the water content in the plates is 15-25%;
step three: processing a plate;
the dried plate is subjected to plate piece inspection, sanding, color separation, repair, sanding again, back groove opening, end socket tenon opening and longitudinal tenon opening;
step four: a board paint process;
the method comprises the following steps of repairing the processed plate, soaking anti-cracking oil, coloring and sealing the groove tenon, sanding, filling putty, UV curing, sanding, attaching base oil, drying and curing, applying sealing base paint, drying and curing, applying base paint, UV curing, sanding, applying base color, UV curing, applying base paint, UV curing, sanding, applying back paint, UV curing, rolling finish paint, spraying paint, UV curing, applying high-performance finish paint, UV curing, color separation and the like, spraying codes, packaging, performing selective inspection according to standards, obtaining qualified products and leaving factories.
2. The method of claim 1, wherein the method comprises the steps of: the panels are exposed to the sun at elevated temperatures for 2-3 weeks.
3. The method of claim 1, wherein the method comprises the steps of: the length of the solid wood floor board is 40cm-50 cm.
4. The method of claim 1, wherein the method comprises the steps of: the thickness of the solid wood floor is 2cm-3 cm.
5. The method of claim 1, wherein the method comprises the steps of: the width of the solid wood board is 10cm-13 cm.