CN111196693A - Light foam concrete for backfilling sunken toilet - Google Patents
Light foam concrete for backfilling sunken toilet Download PDFInfo
- Publication number
- CN111196693A CN111196693A CN202010018353.XA CN202010018353A CN111196693A CN 111196693 A CN111196693 A CN 111196693A CN 202010018353 A CN202010018353 A CN 202010018353A CN 111196693 A CN111196693 A CN 111196693A
- Authority
- CN
- China
- Prior art keywords
- parts
- foam concrete
- cement
- fly ash
- methyl cellulose
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses light foam concrete for backfilling a sunken toilet, which comprises the following components in parts by weight: 60-140 parts of cement, 60-140 parts of fly ash, 30-60 parts of slag micro powder, 1-1.6 parts of vegetable protein agent, 1-1.6 parts of suspending agent, 1-1.6 parts of hydroxypropyl methyl cellulose ether, 1-2.5 parts of foam stabilizer, 1-1.6 parts of polyvinyl alcohol fiber and 1-1.6 parts of calcium formate. According to the invention, through optimizing the proportion of each component, the lightweight foam concrete can be directly stirred and formed without foaming equipment, and in addition, through introducing additives with multiple functions, the foam concrete has the unique functions of high fluidity, good uniformity, excellent waterproof effect and high later strength.
Description
Technical Field
The invention relates to the technical field of building materials, in particular to light foam concrete for backfilling a sunken toilet.
Background
The water seepage of the toilet is always a chronic disease of common diseases of building quality, the existing sinking toilet is basically backfilled with ceramsite, but the ceramsite only solves the problem of light weight, does not contribute to water resistance and water resistance, and the calcination of the ceramsite also generates smoke dust which is very harmful to the environment, and the country eliminates the high-pollution materials.
The foam concrete is a novel material, which is composed of a large number of tiny unconnected air holes, has the advantages of light weight, sound insulation, water resistance and pipeline protection, and has the advantages of good waterproof effect, strong bonding force with a base surface, high construction speed and the like when being applied to the backfill of a toilet.
The foam concrete is prepared by taking cement, slag derivative and fly ash as cementing materials and adding high molecular materials such as methyl cellulose ether, polyvinyl alcohol fiber, plant protein foaming agent, suspending agent, foam stabilizer and the like, and can be directly prepared into a porous light material with the apparent density of 350-550Kg/m3 by adopting a high-speed stirring mode.
The foaming amount and the anti-settling segregation are the key and difficult points of the technology. The foaming amount is too small, the apparent density of the finished product is high, and the foaming agent is too large, so that corner collapse and low strength of the finished product are easily caused. Segregation settling is to keep the slurry separated from the cementitious material in the middle of the hardening process to ensure that the slurry concentrations at the bottom and top are completely consistent.
Disclosure of Invention
Aiming at the defects in the prior art, the invention provides light foam concrete for backfilling a sunken toilet.
In order to achieve the purpose, the invention adopts the technical scheme that: comprises the following components in parts by weight: 60-140 parts of cement, 60-140 parts of fly ash, 30-60 parts of slag micro powder, 1-1.6 parts of vegetable protein agent, 1-1.6 parts of suspending agent, 1-1.6 parts of hydroxypropyl methyl cellulose ether, 1-2.5 parts of foam stabilizer, 1-1.6 parts of polyvinyl alcohol fiber and 1-1.6 parts of calcium formate.
Preferably, the light foam concrete for backfilling of the sinking toilet comprises the following components in parts by weight: 60 parts of cement, 60 parts of fly ash, 30 parts of slag micro powder, 1 part of vegetable protein agent, 1 part of suspending agent, 1 part of hydroxypropyl methyl cellulose ether, 1 part of foam stabilizer, 1 part of polyvinyl alcohol fiber and 1 part of calcium formate.
Preferably, the light foam concrete for backfilling of the sinking toilet comprises the following components in parts by weight: 80 parts of cement, 80 parts of fly ash, 40 parts of slag micro powder, 1.2 parts of a vegetable protein agent, 1.2 parts of a suspending agent, 1.2 parts of hydroxypropyl methyl cellulose ether, 1.5 parts of a foam stabilizer, 1.2 parts of polyvinyl alcohol fiber and 1.2 parts of calcium formate.
Preferably, the light foam concrete for backfilling of the sinking toilet comprises the following components in parts by weight: 110 parts of cement, 110 parts of fly ash, 50 parts of slag micro powder, 1.4 parts of a vegetable protein agent, 1.4 parts of a suspending agent, 1.4 parts of hydroxypropyl methyl cellulose ether, 2 parts of a foam stabilizer, 1.4 parts of polyvinyl alcohol fiber and 1.4 parts of calcium formate.
Preferably, the light foam concrete for backfilling of the sinking toilet comprises the following components in parts by weight: 140 parts of cement, 140 parts of fly ash, 60 parts of slag micro powder, 1.6 parts of a vegetable protein agent, 1.6 parts of a suspending agent, 1.6 parts of hydroxypropyl methyl cellulose ether, 2.5 parts of a foam stabilizer, 1.6 parts of polyvinyl alcohol fiber and 1.6 parts of calcium formate.
The invention has the following beneficial effects: according to the invention, through optimizing the proportion of each component, the lightweight foam concrete can be directly stirred and formed without foaming equipment, and in addition, through introducing additives with multiple functions, the foam concrete has the unique functions of high fluidity, good uniformity, excellent waterproof effect and high later strength.
Detailed Description
The following detailed description of the preferred embodiments of the present invention is provided to enable those skilled in the art to more readily understand the advantages and features of the present invention, and to clearly and unequivocally define the scope of the present invention.
Example 1
A light foam concrete for backfilling a sunken toilet comprises the following components in parts by weight: comprises the following components in parts by weight: 60 parts of cement, 60 parts of fly ash, 30 parts of slag micro powder, 1 part of vegetable protein agent, 1 part of suspending agent, 1 part of hydroxypropyl methyl cellulose ether, 1 part of foam stabilizer, 1 part of polyvinyl alcohol fiber and 1 part of calcium formate.
Example 2
A light foam concrete for backfilling a sunken toilet comprises the following components in parts by weight: 80 parts of cement, 80 parts of fly ash, 40 parts of slag micro powder, 1.2 parts of a vegetable protein agent, 1.2 parts of a suspending agent, 1.2 parts of hydroxypropyl methyl cellulose ether, 1.5 parts of a foam stabilizer, 1.2 parts of polyvinyl alcohol fiber and 1.2 parts of calcium formate.
Example 3
A light foam concrete for backfilling a sunken toilet comprises the following components in parts by weight: 110 parts of cement, 110 parts of fly ash, 50 parts of slag micro powder, 1.4 parts of a vegetable protein agent, 1.4 parts of a suspending agent, 1.4 parts of hydroxypropyl methyl cellulose ether, 2 parts of a foam stabilizer, 1.4 parts of polyvinyl alcohol fiber and 1.4 parts of calcium formate.
Example 4
A light foam concrete for backfilling a sunken toilet comprises the following components in parts by weight: 140 parts of cement, 140 parts of fly ash, 60 parts of slag micro powder, 1.6 parts of a vegetable protein agent, 1.6 parts of a suspending agent, 1.6 parts of hydroxypropyl methyl cellulose ether, 2.5 parts of a foam stabilizer, 1.6 parts of polyvinyl alcohol fiber and 1.6 parts of calcium formate.
The fly ash adopted by the invention is a byproduct of thermal power plant dust collection, exists in the form of vitreous minerals, has a ball effect and an alkali excitation effect, and is beneficial to improving the fluidity and later strength of the foam concrete. The slag differential is an industrial byproduct of slag of a steel plant after water quenching, contains high silica wool glass body, and greatly improves the rheological property and later strength of the foam concrete. The vegetable protein foaming agent mainly controls the content of smile pores, is a main additive of the foamed concrete, and fundamentally changes the water retention and segregation resistance functions of the foamed concrete by the application of a suspending agent, a foam stabilizer and hydroxypropyl methyl cellulose, thereby preparing a finished product with stable quality.
The above description is only for the purpose of illustrating the preferred embodiments of the present invention and is not to be construed as limiting the invention, and any modifications, equivalents, improvements and the like that fall within the spirit and principle of the present invention are intended to be included therein.
Claims (5)
1. A light foam concrete for backfilling a sunken toilet is characterized by comprising the following components in parts by weight: 60-140 parts of cement, 60-140 parts of fly ash, 30-60 parts of slag micro powder, 1-1.6 parts of vegetable protein agent, 1-1.6 parts of suspending agent, 1-1.6 parts of hydroxypropyl methyl cellulose ether, 1-2.5 parts of foam stabilizer, 1-1.6 parts of polyvinyl alcohol fiber and 1-1.6 parts of calcium formate.
2. The light foam concrete for the backfill of the sinking toilet according to claim 1, is characterized by comprising the following components in parts by weight: 60 parts of cement, 60 parts of fly ash, 30 parts of slag micro powder, 1 part of vegetable protein agent, 1 part of suspending agent, 1 part of hydroxypropyl methyl cellulose ether, 1 part of foam stabilizer, 1 part of polyvinyl alcohol fiber and 1 part of calcium formate.
3. The light foam concrete for the backfill of the sinking toilet according to claim 1, is characterized by comprising the following components in parts by weight: 80 parts of cement, 80 parts of fly ash, 40 parts of slag micro powder, 1.2 parts of a vegetable protein agent, 1.2 parts of a suspending agent, 1.2 parts of hydroxypropyl methyl cellulose ether, 1.5 parts of a foam stabilizer, 1.2 parts of polyvinyl alcohol fiber and 1.2 parts of calcium formate.
4. The light foam concrete for the backfill of the sinking toilet according to claim 1, is characterized by comprising the following components in parts by weight: 110 parts of cement, 110 parts of fly ash, 50 parts of slag micro powder, 1.4 parts of a vegetable protein agent, 1.4 parts of a suspending agent, 1.4 parts of hydroxypropyl methyl cellulose ether, 2 parts of a foam stabilizer, 1.4 parts of polyvinyl alcohol fiber and 1.4 parts of calcium formate.
5. The light foam concrete for the backfill of the sinking toilet according to claim 1, is characterized by comprising the following components in parts by weight: 140 parts of cement, 140 parts of fly ash, 60 parts of slag micro powder, 1.6 parts of a vegetable protein agent, 1.6 parts of a suspending agent, 1.6 parts of hydroxypropyl methyl cellulose ether, 2.5 parts of a foam stabilizer, 1.6 parts of polyvinyl alcohol fiber and 1.6 parts of calcium formate.