CN110497634A - Ice bucket preparation method - Google Patents

Ice bucket preparation method Download PDF

Info

Publication number
CN110497634A
CN110497634A CN201810474036.1A CN201810474036A CN110497634A CN 110497634 A CN110497634 A CN 110497634A CN 201810474036 A CN201810474036 A CN 201810474036A CN 110497634 A CN110497634 A CN 110497634A
Authority
CN
China
Prior art keywords
ice bucket
double face
shell
face slab
liner
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810474036.1A
Other languages
Chinese (zh)
Inventor
孟国庆
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FTI Group Holding Co Ltd
PEIN GROUP (HOLDING) CORP
Original Assignee
PEIN GROUP (HOLDING) CORP
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by PEIN GROUP (HOLDING) CORP filed Critical PEIN GROUP (HOLDING) CORP
Priority to CN201810474036.1A priority Critical patent/CN110497634A/en
Publication of CN110497634A publication Critical patent/CN110497634A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of ice bucket preparation methods comprising the steps of: ABS resin layer is fitted in PC resin plate to form double face slab;Double face slab is adsorbed in the surface of shaping dies by thermal softening, and via vacuum suction to form hard shell and hardcoat;Heat-preservation cotton and liner are linked to hard shell and hardcoat sequentially to form the shell and lid that a liner is covered in heat-preservation cotton;Finally, lid is movably connected on shell to form ice bucket, whereby, ice bucket preparation method of the present invention can produce the hard-shelled ice bucket of tool, ice can be kept the temperature come to store food or drink by making ice bucket not only, moreover it is possible to the situation that food of the anti-stop bit inside ice bucket and drink collide.

Description

Ice bucket preparation method
Technical field
The present invention relates to a kind of for manufacturing the preparation method of ice bucket, it is especially a kind of using specific material and preparation method come Manufacture the preparation method of ice bucket.
Background technique
Fishing and camping are the interest of many people, and ice bucket can all be prepared with camping fan to store fishing by generally going fishing It obtains, food or drink and other items, however, the mode that is made of ice bucket is by emission forming machine by polypropylene at present (Polypropylene, abbreviation PP) is projected and is formed, still, the ice bucket being made of polypropylene have intolerant to fall also intolerant to The shortcomings that hitting, and then when shock of the ice bucket by strength, ice bucket is easy breakage, seriously leads to not continue to use, cause just It must repair or buy again another ice bucket.
Summary of the invention
The hard-shelled ice bucket of tool can be produced the main purpose of the present invention is to provide a kind of, and then ice bucket can not only be kept the temperature Ice is protected to store food or drink, moreover it is possible to prevent food or drink the ice bucket impacted inside the case where.
For up to the purpose, the present invention provides a kind of ice bucket preparation method, characterized by comprising:
One sheet fabrication step: an ABS resin plate is fitted in into a PC resin layer to form a pair of deck panels;
One shell forming step: heating the double face slab, softens the double face slab to form one and can be carried out deformation Softening double face slab, and to the softening double face slab carry out vacuum suction, so that the softening double face slab is adsorbed in one one-tenth A hard shell and a hardcoat for three-dimensional shape is presented to be formed for the surface of shape mold;
One heat-preservation cotton: being respectively arranged at the inside of the hard shell and the inside of the hardcoat by one inside procedure of processing, then Two liners are connected to the hard shell and the hardcoat to allow the liner to be covered in the heat-preservation cotton, and then form a shell Body and a lid;And
One connecting step: the lid is movably connected on the shell to form an ice bucket.
The ice bucket preparation method, wherein the sheet fabrication step further include: provide multiple by ABS resin institute structure At resin particle, and the multiple resin particle is heated, make the multiple resin particle by thermal softening common shape The resin fluid that half solid fraction is presented at one, and the resin fluid is squeezed and forms the ABS resin plate.
The ice bucket preparation method, in which: the resin particle is in 200~230 DEG C of processing environment by thermal softening.
The ice bucket preparation method, in which: the double face slab is in 150~200 DEG C of processing environment by thermal softening.
The ice bucket preparation method, in which: the ice bucket preparation method also includes a liner forming step, the liner Forming step includes:
Waterproof sheet is cut into a bottom sheet body, a wall surface sheet body and a ring slice;
The wall surface sheet body is crimped and vertically adjacent in the edge of the bottom sheet body, then by the two, hot pressing carrys out phase each other It connects;And
The apical margin that the ring slice level is placed in the wall surface sheet body is adjacent, then hot pressing comes mutually each other by the two Connect and compose the liner.
The ice bucket preparation method, in which: the temperature of hot pressing is 50 DEG C.
The method have the characteristics that heat-preservation cotton and liner are sequentially connected to inside hard shell and inside hardcoat to form shell With lid, and shell Moveable assembled in lid to complete ice bucket, there is hard shell and hardcoat whereby, outside ice bucket, and ice bucket is interior Portion has heat-preservation cotton and liner, so that ice bucket has outer hard interior soft characteristic, and then ice bucket can not only keep the temperature ice to store food Object or drink, moreover it is possible to prevent food or drink the ice bucket impacted inside the case where.
Detailed description of the invention
Fig. 1 is the step block diagram of ice bucket preparation method of the present invention;
Fig. 2A and Fig. 2 B is the schematic diagram of sheet fabrication step in the first preferred embodiment;
Fig. 3 is the schematic diagram of liner forming step in the first preferred embodiment;
Fig. 4 A and Fig. 4 B is the schematic diagram of the first shell forming step in the first preferred embodiment;
Fig. 5 is the schematic diagram of the first inside procedure of processing in the first preferred embodiment;
Fig. 6 A and Fig. 6 B is the schematic diagram of second housing forming step in the first preferred embodiment;
Fig. 7 is the schematic diagram of the second inside procedure of processing in the first preferred embodiment;
Fig. 8 is the schematic diagram of connecting step in the first preferred embodiment;
Fig. 9 A and Fig. 9 B is the schematic diagram of sheet fabrication step in the second preferred embodiment.
Description of symbols: 1- ice bucket preparation method;10- pumping board machine;101- screw rod;102- die orifice;11- vacuum forming Machine;The first shaping dies of 111-;112- group connects frame;113- heating mechanism;The second shaping dies of 114-;20-ABS resin particle; 201-ABS resin fluid;202-ABS resin plate;21-PC resin layer;22-PC resin particle;221-PC resin fluid; 222-PC resin plate;The first double face slab of 30-;301- first softens double face slab;The second double face slab of 31-;311- second Soften double face slab;40- bottom sheet body;41- wall surface sheet body;42- ring slice;43- connection sheet body;44- covers sheet body;45- Accommodating space;The first liner of 46-;The second liner of 47-;50- hard shell;The first heat-preservation cotton of 501-;51- hardcoat;511- second is kept the temperature Cotton;60- shell;61- lid;70- ice bucket;S1- sheet fabrication step;S2- liner forming step;The first shell of S3- forming step Suddenly;The first inside S4- procedure of processing;S5- second housing forming step;The second inside S6- procedure of processing;S7- connecting step.
Specific embodiment
The present invention is further described with attached drawing combined with specific embodiments below, the advantages and features of the present invention will be with Description and it is apparent.
It please refers to shown in Fig. 1, Fig. 2A and Fig. 2 B, in the first preferred embodiment, ice bucket preparation method 1 of the present invention is mainly matched Unify pumping board machine 10, a cycle machine (not shown) and a vacuum former 11 to use, firstly, pumping board machine 10 starts to be added Heat allows the temperature of screw rod 101 to be heated to 200~230 DEG C so that a screw rod 101 for being set to pumping board machine 10 is gradually warmed up, then, By multiple ABS resin particles 20, (acrylonitrile-butadiene-styrene copolymer, ABS are Acrylonitrile Butadiene The acronym of Styrene) it is put into the inside of pumping board machine 10, and screw rod 101 starts to be rotated, and allows multiple ABS resins Grain 20 is moved and screw rod 101 rotated towards the die orifice 102 that one is formed in pumping board machine 10, when multiple ABS trees When rouge particle 20 is by screw rod 101, ABS resin particle 20 by thermal softening, allows multiple ABS under 200~230 DEG C of processing environment The ABS resin fluid 201 of half solid fraction of a presentation is collectively formed in resin particle 20, and ABS resin fluid 201 is flowed to die orifice 102 It is squeezed and forms an ABS resin plate 202, then, ABS resin plate 202 is fitted in one with color or decorative pattern PC resin layer 21 (polycarbonate, PC are the abbreviations of Polycarbonate), and simultaneously to ABS resin plate 202 and PC resin Layer 21 is cut to form one first double face slab 30 and one second double face slab 31, whereby, the first and second double face slab 30,31 are made of ABS resin plate 202 and PC resin layer 21, however, both ABS resin plate 202 and PC resin layer 21 The first and second double face slab 30,31 is collectively formed and only facilitates purposes of discussion, not restricted first and second double face slab 30,31 plates one Surely it to be made of ABS resin plate 202 and PC resin layer 21, that is, both first and second double face slabs 30,31 can be by ABS tree Rouge plate 202 is formed with the ABS resin layer with color pattern, whereby, that is, completes a sheet fabrication step S1.
In this embodiment, since ABS resin particle 20 is to be made under 200~230 DEG C of processing environment by thermal softening ABS resin particle 20 will not be burnt because temperature is excessively high, be avoided that indirectly ABS resin fluid 201 lose soffening with it is tough Property, also, ABS resin particle 20 will not can not form the ABS resin fluid 201 of half solid fraction because temperature is too low, indirectly Lead to not shape ABS resin plate 202, in other words, when screw rod 101 heats and causes more than 230 DEG C, ABS resin particle 20 can be there is a situation where burning, and then ABS resin fluid 201 can lose soffening and toughness, also, after screw rod 101 heats Temperature when being not above 200 DEG C, multiple ABS resin particles 20 can not form ABS resin fluid 201.
It please refers to shown in Fig. 1 and Fig. 3, when Yu Jinhang sheet fabrication step S1, can synchronize and carry out a liner forming step S2, Firstly, cutting a waterproof sheet (not shown) to form the neither same bottom sheet body 40 of shape size, a wall surface each other Sheet body 41, a ring slice 42, a connecting piece body 43 and a covering sheet body 44, then cycle machine is electrically connected at outside one Power supply allows cycle machine to start conductive heater because external power supply is electrically connected to 50 DEG C, next, curling wall surface sheet body 41, and curly wall surface sheet body 41 will be presented vertically adjacent in the edge of the bottom sheet body 40, then, cycle machine is by wall Dough sheet body 41 with 50 DEG C of temperature hot pressing in the outer rim of bottom sheet body 40 so that both bottom sheet body 40 and wall surface sheet body 41 are altogether With forming an accommodating space 45, then come, ring slice 42 with connect both sheet bodies 43 equally with 50 DEG C of temperature hot pressing in wall surface Sheet body 41 is to form first liner 46 that three-dimensional shape is presented, as shown, ring slice 42 is in wall surface sheet body 41 and even Between contact pin body 43, and the apical margin that 42 level of ring slice is placed in wall surface sheet body 41 is adjacent, also, ring slice 42 with connect Both sheet bodies 43 are formed in wall surface sheet body 41 in one end far from bottom sheet body 40, in addition, covering sheet body 44 independently forms one is in Second liner 47 of existing sheet, so that the shape of the second liner 47 is different from the first liner 46.
It please refers to shown in Fig. 1, Fig. 4 A and Fig. 4 B, followed by the first shell forming step S3, by one first finishing die Tool 111 is installed on vacuum former 11, then the first double face slab 30 is assembled in the group that one is set to vacuum former 11 and connects frame 112, then, the heating mechanism 113 for being assembled in vacuum former 11 by one begins to warm up heating, and the first double face slab 30 is allowed to pass through Heating mechanism 113 and in the heating environment between 150~200 DEG C by thermal softening with formed one can be carried out deformation first softening Double face slab 301, then, group connect frame 112 towards the movement of the first shaping dies 111, make vacuum former 11 double to the first softening Deck panels 301 carry out vacuum suction, make the first softening double face slab 301 be adsorbed in the outer surface of the first shaping dies 111 at The hard shell 50 of three-dimensional shape is presented in shape one, in preferred embodiment, after hard shell 50 is cooling, is cut hard shell 50 to cut Except the flash for being formed in hard shell 50, also, 21, the PC resin layer outermosts in hard shell 50, and ABS resin plate 202 hard The most inner side of shell 50, so that the color pattern of PC resin layer 21 is formed in the outer surface of hard shell 50.
It please refers to shown in Fig. 1 and Fig. 5, prepares multiple the first soft heat-preservation cottons 501, and multiple first heat-preservation cottons 501 are solid Due to the interior surface of hard shell 50, in this embodiment, one of them the first heat-preservation cotton 501 is fixed on the bottom of hard shell 50, and Remaining first heat-preservation cotton 501 is fixed on four side all around of hard shell 50, next, the first liner 46 is covered in the first guarantor Warm cotton 501, and hard shell 50 is connected to form a shell 60, one first inside procedure of processing S4 is completed whereby, in this embodiment In, the bottom sheet body 40 of the first liner 46 is covered in one of them first heat-preservation cotton 501, and the wall surface sheet body of the first liner 46 41 are covered in remaining first heat-preservation cotton 501, also, the hardness of the first heat-preservation cotton 501 is less than hard shell 50.
Please refer to shown in Fig. 1, Fig. 6 A and Fig. 6 B, complete sheet fabrication step S1 after, in addition to carry out the first shell at Except shape step S3, it is necessary to carry out a second housing forming step S5, a shape is different from the of the first shaping dies 111 Two shaping dies 114 are installed on vacuum former 11, then the group that the second double face slab 31 is assembled in vacuum former 11 is connect frame 112, then, the heating mechanism 113 of vacuum former 11, which is begun to warm up, to be warming up between 150~200 DEG C, allows heating mechanism 113 Second double face slab 31 is heated, the second double face slab 31 is made to can be carried out the second of deformation because heat softens to form one Soften double face slab 311, then, group connects frame 112 towards the movement of the second shaping dies 114, after allowing 11 pairs of vacuum former to soften Second softening double face slab 311 carry out vacuum suction, so that the second softening double face slab 311 is adsorbed in the second shaping dies 114 Outer surface to shape the hardcoat 51 of a presentation three-dimensional shape, in preferred embodiment, after hardcoat 51 is cooling, to hardcoat 51 into Row cutting is formed in the flash of hardcoat 51 to cut off, also, 21, the PC resin layer outermosts in hardcoat 51, and ABS resin Plate 202 most inner sides in hardcoat 51, so that the color pattern of PC resin layer 21 is formed in the outer surface of hardcoat 51.
It please refers to shown in Fig. 1 and Fig. 7, prepares the second heat-preservation cotton 511 that a property is identical to the first heat-preservation cotton 501, and the Two heat-preservation cottons 511 are fixed on the inside of hardcoat 51, then the second liner 47 is linked to hardcoat 51, and the second liner 47 is allowed to be covered in Two heat-preservation cottons 511 are located at the second heat-preservation cotton 511 between hardcoat 51 and the second liner 47, and whereby, the second liner 47, second is protected A lid 61 is collectively formed with 51 three of hardcoat to complete one second inside procedure of processing S6 in warm cotton 511.
It please refers to shown in Fig. 1 and Fig. 8, finally carries out connecting step S7, lid 61 is movably connected on shell 60 to be formed One ice bucket 70, also, due to the mutual Moveable assembled of both lid 61 and shell 60, it is lifted so that lid 61 can be carried out to turn over, in addition, ice 70 outside of bucket has hard shell 50 and hardcoat 51, and the inside of ice bucket 70 has in the first and second heat-preservation cotton 501,511 and first and second Gallbladder 46,47, so that the outside of ice bucket 70 has outer hard interior soft characteristic, and then ice bucket 70 can not only keep the temperature ice to store food Or drink, moreover it is possible to it is resistance to fall crashworthiness, it is opposite to prevent food or drink 70 impacted inside of ice bucket the case where.
It please refers to shown in Fig. 1, Fig. 9 A and Fig. 9 B, in the second preferred embodiment, exists with the difference of the first preferred embodiment In sheet fabrication step S1, other steps flow charts are identical to the first preferred embodiment, and then in this embodiment, in addition to plate plus Except the rapid S1 of work step, will no longer it be described in detail for other steps.
As shown, pumping board machine 10 starts to be heated, so that the screw rod 101 of pumping board machine 10 is heated to 200~230 DEG C, Then, multiple PC resin particles 22 (polycarbonate, PC are the abbreviations of Polycarbonate) are put into the inside of pumping board machine 10, Multiple PC resin particles 22 are allowed to be moved and screw rod 101 rotated towards the die orifice 102 of pumping board machine 10, when multiple When PC resin particle 22 is by screw rod 101, PC resin particle 22, by thermal softening, allows more under 200~230 DEG C of processing environment The PC resin fluid 221 of half solid fraction of a presentation is collectively formed in a PC resin particle 22, and PC resin fluid 221 is flowed to die orifice 102 are squeezed and form a PC resin plate 222, then, PC resin plate 222 are fitted in PC resin layer 21, and simultaneously PC resin plate 222 and PC resin layer 21 are cut to form the first double face slab 30 and the second double face slab 31, by This, the first and second double face slab 30,31 is made of PC resin plate 222 and PC resin layer 21, however, PC resin plate 222 The first and second double face slab 30,31 is collectively formed with 21 the two of PC resin layer and only facilitates purposes of discussion, not restricted first and second Double face slab 30,31 plates have to be made of PC resin plate 222 and PC resin layer 21, that is, the first and second double face slab 30, Both 31 can be made of PC resin plate 222 with the ABS resin layer with color pattern, and whereby, i.e. completion sheet fabrication walks Rapid S1.
After completing sheet fabrication step S1, when Yu Jinhang the first and second shell forming step S3, S5, PC resin is just utilized First and second double face slab 30,31 composed by plate 222 and PC resin layer 21 carries out vacuum suction to form hard shell 50 and hardcoat 51。
Above explanation and examples are merely exemplary, it is not intended to limit the scope of the present invention in any way.This field Technical staff should be understood that without departing from the spirit and scope of the invention can details to technical solution of the present invention and Form is modified or is replaced, but these modifications and replacement are fallen within the protection scope of the present invention.

Claims (6)

1. a kind of ice bucket preparation method, characterized by comprising:
One sheet fabrication step: an ABS resin plate is fitted in into a PC resin layer to form a pair of deck panels;
One shell forming step: heating the double face slab, softens the double face slab to form one and can be carried out the soft of deformation Change double face slab, and vacuum suction is carried out to the softening double face slab, the softening double face slab is made to be adsorbed in a finishing die A hard shell and a hardcoat for three-dimensional shape is presented to be formed for the surface of tool;
One heat-preservation cotton: being respectively arranged at the inside of the hard shell and the inside of the hardcoat by one inside procedure of processing, then by two Liner is connected to the hard shell and the hardcoat to allow the liner to be covered in the heat-preservation cotton, so formed a shell with One lid;And
One connecting step: the lid is movably connected on the shell to form an ice bucket.
2. ice bucket preparation method according to claim 1, which is characterized in that the sheet fabrication step further include: provide Multiple resin particles being made of ABS resin, and the multiple resin particle is heated, make the multiple resin particle The resin fluid of half solid fraction of a presentation is collectively formed by thermal softening, and the resin fluid is squeezed and forms the ABS Resin plate.
3. ice bucket preparation method according to claim 2, it is characterised in that: the resin particle 200~230 DEG C plus By thermal softening in work environment.
4. ice bucket preparation method according to claim 1, it is characterised in that: the double face slab 150~200 DEG C plus By thermal softening in work environment.
5. ice bucket preparation method according to claim 4, it is characterised in that: the ice bucket preparation method also includes a liner Forming step, the liner forming step includes:
Waterproof sheet is cut into a bottom sheet body, a wall surface sheet body and a ring slice;
The wall surface sheet body is crimped and vertically adjacent in the edge of the bottom sheet body, then hot pressing mutually interconnects each other by the two It connects;And
The apical margin that the ring slice level is placed in the wall surface sheet body is adjacent, then hot pressing is connected with each other each other by the two Constitute the liner.
6. ice bucket preparation method according to claim 5, it is characterised in that: the temperature of hot pressing is 50 DEG C.
CN201810474036.1A 2018-05-17 2018-05-17 Ice bucket preparation method Pending CN110497634A (en)