CN110257894A - The unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment - Google Patents

The unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment Download PDF

Info

Publication number
CN110257894A
CN110257894A CN201910479680.2A CN201910479680A CN110257894A CN 110257894 A CN110257894 A CN 110257894A CN 201910479680 A CN201910479680 A CN 201910479680A CN 110257894 A CN110257894 A CN 110257894A
Authority
CN
China
Prior art keywords
support plate
aluminium foil
fixedly mounted
slot
electrolytic cell
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201910479680.2A
Other languages
Chinese (zh)
Other versions
CN110257894B (en
Inventor
王斌
邹利华
李冬英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shaoyang University
Original Assignee
Shaoyang University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shaoyang University filed Critical Shaoyang University
Priority to CN201910479680.2A priority Critical patent/CN110257894B/en
Publication of CN110257894A publication Critical patent/CN110257894A/en
Application granted granted Critical
Publication of CN110257894B publication Critical patent/CN110257894B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention provides a kind of unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment of mesohigh.The unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment, comprising: support plate;Elevating mechanism, the elevating mechanism setting is on the supporting plate;Two side plates, two side plates are fixedly mounted on the top of the support plate;Slot is fed, the feed slot is fixedly mounted on the top of the support plate;Electrolytic cell, the electrolytic cell are fixedly mounted on the top of the support plate;Multiple titanium plate electrodes, multiple titanium plate electrodes are arranged in the feed slot;Multiple graphite electrodes, multiple graphite electrodes are arranged in the electrolytic cell;Two filling mechanism, two filling mechanism are fixedly mounted on the top of the support plate, and the present invention has rational design, can handle sour gas, reduce the cleaning that sour gas damage health of people also facilitates titanium plate electrode and graphite electrode.

Description

The unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment
Technical field
The present invention relates to aluminium foil corrosion field more particularly to a kind of unleaded aluminium foil for electrolytic capacitor corrosion feeds of mesohigh Device.
Background technique
A kind of thermoprint material for directly rolling flakiness with metallic aluminium of aluminium foil, the effect of hot stamping effects and pure silver foil thermoprint It is similar, therefore also known as white alloy foil, a kind of medium-high voltage aluminum electrolytic capacitor aluminium foil corrosion feeder equipment exists in the prior art, including For containing the feed slot and electrolytic cell and live-roller, titanium plate electrode, graphite electrode and DC power supply of electrolyte, the titanium Plate electrode is dipped in the electrolyte of feed slot and is electrically connected with the anode of DC power supply, and the graphite electrode is dipped in the electricity of electrolytic cell It is electrically connected in solution liquid and with the cathode of DC power supply;The live-roller is respectively provided in the slot of feed slot and electrolytic cell and outside slot, The aluminium foil is wound on live-roller, and can continuously enter electrolytic cell from feed slot along live-roller, has been prevented using conventional conductive The sparking that often occurs when roller conduction, spot, striped, conductive rollers are corroded to influence the bad phenomenons such as electrolyte, improve Aluminium foil quality.
But electrolyte is generally acid solution and can generate acidity during acid solution corrodes aluminium foil Gas, these gases are absorbed by the body for a long time to generate harm to the health of people, and electrode assembly can also be pasted after using Solution, cleaning up are simultaneously inconvenient.
Therefore, it is necessary to provide a kind of unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment solution of mesohigh above-mentioned technology Problem.
Summary of the invention
The present invention provides a kind of unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment of mesohigh, solves sour gas damage The problem of evil health of people and electrode assembly cleaning inconvenience.
In order to solve the above technical problems, the unleaded aluminium foil for electrolytic capacitor corrosion feed dress of mesohigh provided by the invention It sets, comprising: support plate;Elevating mechanism, the elevating mechanism setting is on the supporting plate;Two side plates, two side plates are solid Dingan County is mounted in the top of the support plate;Slot is fed, the feed slot is fixedly mounted on the top of the support plate;Electrolytic cell, The electrolytic cell is fixedly mounted on the top of the support plate;Multiple titanium plate electrodes, multiple titanium plate electrodes are arranged described It feeds in slot;Multiple graphite electrodes, multiple graphite electrodes are arranged in the electrolytic cell;Two filling mechanism, two The filling mechanism is fixedly mounted on the top of the support plate;Cover board, the cover board are arranged in the feed slot and electrolytic cell Top, multiple titanium plate electrodes and multiple graphite electrodes are fixedly connected with the bottom of the cover board;Multiple transmissions Roller, multiple live-rollers are separately positioned in the slot of the feed slot and the electrolytic cell and outside slot;Aluminium foil, the aluminium foil are set It sets on multiple live-rollers;Sour gas average mechanism, the sour gas average mechanism are arranged on the cover board.
Preferably, it is opened up at the top of the support plate there are two the second through-hole, the is equipped in two second through-holes Two bearings, the outer ring of two second bearings are fixedly connected with the inner wall of two second through-holes respectively, and two described Fixation is set in two rotating bars the inner ring of two bearings respectively.
Preferably, the bottom four corners position of the support plate is fixedly installed with supporting leg.
Preferably, the bottom of the feed slot and the electrolytic cell is fixedly installed with drain pipe, two drain pipes Run through support plate, and is equipped with valve on two drain pipes.
Preferably, the side of the support plate is equipped with two-direction switch.
Compared with the relevant technologies, the unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment tool of mesohigh provided by the invention It has the advantages that:
The present invention provides a kind of unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment of mesohigh, during corrosion, Sour gas can be generated, blower is started, blower will feed the gas in slot and electrolytic cell and be inhaled by air-suction cover, air inlet pipe and hose Enter into the first cabinet, filter plate neutralizes sour gas, and graphite electrode and the least significant end of titanium plate electrode is made to leave electrolysis Then slot and feed slot carry out cleaning wiping to titanium plate electrode and graphite electrode with water or with tool, more convenient, this Device facilitates the cleaning of electrode assembly, can also reduce harm of the sour gas to operator's health, more Practical, the present invention has rational design, can handle sour gas, reduces sour gas damage health of people and also facilitates titanium The cleaning of plate electrode and graphite electrode.
Detailed description of the invention
Fig. 1 is the structural schematic diagram that the unleaded aluminium foil for electrolytic capacitor of mesohigh provided by the invention corrodes feeder equipment;
Fig. 2 is the enlarged structure schematic diagram of part A in Fig. 1;
Fig. 3 is the schematic diagram of filling mechanism described in Fig. 1;
Fig. 4 faces schematic cross-sectional view for the first cabinet shown in FIG. 1;
Fig. 5 is the backsight structural representation of the first cabinet shown in FIG. 1.
Figure label: 1, support plate, 2, motor, 3, two-groove belt pulley, 4, rotating bar, 5, single slot belt pulley, 6, belt, 7, Feed slot, 8, titanium plate electrode, 9, graphite electrode, 10, side plate, 11, aluminium foil, 12, live-roller, 13, cover board, 14, arch tube, 15, Air-suction cover, 16, blower, 17, air inlet pipe, the 18, first cabinet, 19, filter plate, 20, exhaust pipe, the 21, second cabinet, 22, go out liquid Pipe, 23, the pump housing, 24, liquor box, 25, electrolytic cell, 26, hose, 27, connecting tube.
Specific embodiment
The invention will be further described with embodiment with reference to the accompanying drawing.
First embodiment
Please refer to Fig. 1 and Fig. 2, wherein Fig. 1 is that the unleaded aluminium foil for electrolytic capacitor of mesohigh provided by the invention is rotten Lose the structural schematic diagram of feeder equipment;Fig. 2 is the enlarged structure schematic diagram of part A in Fig. 1.The unleaded electrolytic capacitor of mesohigh is used Aluminium foil corrosion feeder equipment, comprising: support plate 1;Elevating mechanism, the elevating mechanism are arranged in support plate 1;Two side plates 10, two side plates 10 are fixedly mounted on the top of the support plate 1;Slot 7 is fed, the feed slot 7 is fixedly mounted on The top of the support plate 1;Electrolytic cell 25, the electrolytic cell 25 are fixedly mounted on the top of the support plate 1;Multiple titanium plate electricity Pole 8, multiple titanium plate electrodes 8 are arranged in the feed slot 7;Multiple graphite electrodes 9, multiple graphite electrodes 9 are arranged In the electrolytic cell 25;Two filling mechanism, two filling mechanism are fixedly mounted on the top of the support plate 1; The top of the feed slot 7 and electrolytic cell 25, multiple titanium plate electrodes 8 and multiple institutes is arranged in cover board 13, the cover board 13 Graphite electrode 9 is stated to be fixedly connected with the bottom of the cover board 13;Multiple live-rollers 12, multiple live-rollers 12 are respectively set In the slot of the feed slot 7 and the electrolytic cell 25 and outside slot;Aluminium foil 11, the aluminium foil 11 are arranged in multiple live-rollers On 12;Sour gas average mechanism, the sour gas average mechanism are arranged on the cover board 13.
The top of the support plate 1 is opened up there are two the second through-hole, is equipped with second bearing in two second through-holes, The outer ring of two second bearings is fixedly connected with the inner wall of two second through-holes respectively, two second bearings Fixation is set in two rotating bars 4 inner ring respectively.
The bottom four corners position of the support plate 1 is fixedly installed with supporting leg.
The bottom of the feed slot 7 and the electrolytic cell 25 is fixedly installed with drain pipe, and two drain pipes pass through Perforating branches fagging 1, and valve is equipped on two drain pipes.
The side of the support plate 1 is equipped with two-direction switch.
The working principle of the unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment of mesohigh provided by the invention is as follows:
The model HY2-60 of two-direction switch, two-direction switch, motor 2 and external power supply are successively electrically connected structure by conducting wire At closed circuit, the top of cover board 13 offers multiple avoid holes, for making aluminium foil 11 that can pass through cover board in transmission process 13, it feeds slot 7 and there are two live-roller 12 respectively in electrolytic cell 25, it is electric when being passed through sour corrosion in feed slot 7 and electrolytic cell 25 When solving liquid, it can make to be immersed in sour corrosion electrolyte by the aluminium foil 11 of live-roller 12 in feed slot 7 and electrolytic cell 25,
Step 1: titanium plate electrode 8 is electrically connected with the anode of direct current, graphite electrode 9 and the cathode of direct current are electrically connected It connects, the fixed particle of sodium hydroxide is placed in filter plate 19;
Step 2: being passed through sour corrosion electrolyte in liquor box 24, start the pump housing 23, the pump housing 23 is by connecting tube 27 and goes out Sour corrosion electrolyte is extracted into feed slot 7 and electrolytic cell 25 by liquid pipe 22, is made in electrode solution submergence feed slot 7 and electrolytic cell 25 Live-roller 12, be then driven aluminium foil 11, aluminium foil 11 is corroded.
Second embodiment:
Please refer to Fig. 2, Fig. 3, Fig. 4 and Fig. 5, wherein Fig. 2 is the enlarged structure schematic diagram of part A in Fig. 1;Fig. 3 is The schematic diagram of filling mechanism described in Fig. 1;Fig. 4 faces schematic cross-sectional view for the first cabinet shown in FIG. 1;Fig. 5 is Fig. 1 Shown in the first cabinet backsight structural representation.The unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment, the liter Descending mechanism includes motor 2, single slot 5, two belts 6 of belt pulley of the rotating bar 4, two of two-groove belt pulley 3, two, and the motor 2 is solid Dingan County is mounted in the bottom of the support plate 1, and the fixation of two-groove belt pulley 3 is set on the output shaft of the motor 2, two institutes State rotating bar 4, two rotating bars 4 are rotatably installed in the support plate 2, and two rotating bars 4 with it is described Cover board 13 is threadedly coupled, and fixation is set in two rotating bars 4 two single slot belt pulleys 5 respectively, two skins Band 6 is respectively wound around between two single slot belt pulleys 5 and the two-groove belt pulley 3, is opened up in two rotating bars 4 There is one section of external screw thread, the top of the cover board 13 is opened up there are two threaded hole, and two rotating bars 4 extend through described in two Threaded hole is simultaneously mutually screwed with the inner wall of two threaded holes, and two side plate 10 sides close to each other are fixedly installed with Two fixed blocks, the top of four fixed blocks offer first through hole, are equipped with first in four first through hole Bearing, the outer ring of four first bearings are fixedly connected with the inner wall of four first through hole respectively, and four described first Fixation is set in two rotating bars 4 inner ring of bearing respectively.
The sour gas average mechanism include two air-suction covers 15, arch tube 14, blower 16, hose 26, air inlet pipe 17, First cabinet 18, filter plate 19, exhaust pipe 20, two air-suction covers 15 are fixedly mounted on the bottom of the cover board 13, and Two air-suction covers 15 are located at the surface of the feed slot 7 and the electrolytic cell 25, the fixed peace of the arch tube 14 Mounted in the top of the cover board 13, and the arch tube 14 is connected with two air-suction covers 15, the fixed peace of the blower 16 Mounted in the top of the cover board 13, the air inlet pipe 17 is fixedly connected between the blower 16 and the arch tube 14, described First cabinet 18 is fixedly mounted on any one of side plate 10, the hose 26 be fixedly connected on the blower 16 with it is described Between first cabinet 18, the filter plate 19 is fixedly mounted on the inner wall of first cabinet 18, and the exhaust pipe 20 is fixed It is mounted on the side outer wall of first cabinet 18, and the exhaust pipe 20 is connected with first cabinet 18, described The side of one cabinet 18 is hinged with hermatic door, and hermatic door is equipped with door handle.
Two filling mechanism include two 23, two liquor boxs of the pump housing of outlet tube 22, two of the second cabinet 21, two 24, two connecting tubes 27, two second cabinets 21 and two liquor boxs 24 are fixedly mounted on the support plate 1 Top, two pump housings 23 are respectively and fixedly installed in the bottom interior wall of two second cabinets 21, and liquid is gone out described in two Pipe 22 is respectively and fixedly installed on the feed slot 7 and the electrolytic cell 25, and two outlet tubes 22 respectively with two institutes It states the pump housing 23 to be fixedly connected, two connecting tubes 27 are respectively fixedly connected in two liquor boxs 24 and two pump housings Between 23.
During corrosion, sour gas can be generated, starts blower 16, blower 16 will be fed in slot 7 and electrolytic cell 25 Gas be drawn into the first cabinet 18 by air-suction cover 15, air inlet pipe 17 and hose 26, filter plate 19 carries out sour gas It neutralizes;
After corrosion, external pipe and drain pipe are connected, and valve is opened, and sour corrosion electrolyte is discharged, and starting is fallen Clockwise switch is activated motor 2, and motor 2 drives two-groove belt pulley 3 to rotate, and two-groove belt pulley 3 drives two by two belts 6 A list slot belt pulley 5 rotates, and two single slot belt pulleys 5 drive two rotating bars 4 to rotate synchronously, and two rotating bars 4 drive cover board 13 increase, and cover board 13 drives titanium plate electrode 8 and graphite electrode 9 to increase, and leave graphite electrode 9 and the least significant end of titanium plate electrode 8 Then electrolytic cell 25 and feed slot 7 carry out cleaning wiping to titanium plate electrode 8 and graphite electrode 9 with water or with tool, compared with For convenience, the present apparatus facilitates the cleaning of electrode assembly, can also reduce sour gas to operator's health Harm, it is more practical.
Compared with the relevant technologies, the unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment tool of mesohigh provided by the invention It has the advantages that:
The unleaded aluminium foil for electrolytic capacitor corrosion feeder equipment of mesohigh can generate sour gas during corrosion, Start blower 16, blower 16 will feed slot 7 and suck with the gas in electrolytic cell 25 by air-suction cover 15, air inlet pipe 17 and hose 26 Into the first cabinet 18, filter plate 19 neutralizes sour gas, leaves graphite electrode 9 and the least significant end of titanium plate electrode 8 Then electrolytic cell 25 and feed slot 7 carry out cleaning wiping to titanium plate electrode 8 and graphite electrode 9 with water or with tool, compared with For convenience, the present apparatus facilitates the cleaning of electrode assembly, can also reduce sour gas to operator's health Harm, more practical, the present invention has rational design, can handle sour gas, reduces sour gas and damages health of people Also the cleaning of titanium plate electrode 8 and graphite electrode 9 is facilitated.
The above description is only an embodiment of the present invention, is not intended to limit the scope of the invention, all to utilize this hair Equivalent structure or equivalent flow shift made by bright specification and accompanying drawing content is applied directly or indirectly in other relevant skills Art field, is included within the scope of the present invention.

Claims (8)

1. the unleaded aluminium foil for electrolytic capacitor of mesohigh corrodes feeder equipment characterized by comprising
Support plate;
Elevating mechanism, the elevating mechanism setting is on the supporting plate;
Two side plates, two side plates are fixedly mounted on the top of the support plate;
Slot is fed, the feed slot is fixedly mounted on the top of the support plate;
Electrolytic cell, the electrolytic cell are fixedly mounted on the top of the support plate;
Multiple titanium plate electrodes, multiple titanium plate electrodes are arranged in the feed slot;
Multiple graphite electrodes, multiple graphite electrodes are arranged in the electrolytic cell;
Two filling mechanism, two filling mechanism are fixedly mounted on the top of the support plate;
The top of the feed slot and electrolytic cell, multiple titanium plate electrodes and multiple stones is arranged in cover board, the cover board Electrode ink is fixedly connected with the bottom of the cover board;
Multiple live-rollers, multiple live-rollers are separately positioned in the slot of the feed slot and the electrolytic cell and outside slot;
Aluminium foil, the aluminium foil are arranged on multiple live-rollers;
Sour gas average mechanism, the sour gas average mechanism are arranged on the cover board.
2. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that institute Stating elevating mechanism includes motor, two-groove belt pulley, two rotating bars, two single slot belt pulleys, two belts, and the motor is fixed It is mounted on the bottom of the support plate, the two-groove belt pulley fixation is set on the output shaft of the motor, turns described in two Lever, two rotating bars are rotatably installed in the support plate, and two rotating bars with the cover board screw thread Connection, fixation is set in two rotating bars two single slot belt pulleys respectively, and two belts are respectively wound around Between two single slot belt pulleys and the two-groove belt pulley, one section of external screw thread, institute are offered in two rotating bars State and opened up at the top of cover board there are two threaded hole, two rotating bars extend through two threaded holes and with described in two The inner wall of threaded hole mutually screws, and two side plates side close to each other is fixedly mounted there are two fixed block, described in four The top of fixed block offers first through hole, and first bearing, four first axles are equipped in four first through hole The outer ring held is fixedly connected with the inner wall of four first through hole respectively, and the inner ring of four first bearings distinguishes fixing sleeve It is located in two rotating bars.
3. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that institute Stating sour gas average mechanism includes two air-suction covers, arch tube, blower, hose, air inlet pipe, the first cabinet, filter plate, exhaust Pipe, two air-suction covers are fixedly mounted on the bottom of the cover board, and two air-suction covers are located at the feed The surface of slot and the electrolytic cell, the arch tube are fixedly mounted on the top of the cover board, and the arch tube and two The air-suction cover is connected, and the blower is fixedly mounted on the top of the cover board, and the air inlet pipe is fixedly connected on the wind Between machine and the arch tube, first cabinet is fixedly mounted on any one of side plate, and the hose is fixedly connected Between the blower and first cabinet, the filter plate is fixedly mounted on the inner wall of first cabinet, the row Tracheae is fixedly mounted on the side outer wall of first cabinet, and the exhaust pipe is connected with first cabinet, described The side of first cabinet is hinged with hermatic door, and hermatic door is equipped with door handle.
4. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that two A filling mechanism include two the second cabinets, two outlet tubes, two pump housings, two liquor boxs, two connecting tubes, two Second cabinet and two liquor boxs are fixedly mounted on the top of the support plate, and two pump housings are fixed respectively It is mounted in the bottom interior wall of two second cabinets, two outlet tubes are respectively and fixedly installed to the feed slot and institute It states on electrolytic cell, and two outlet tubes are fixedly connected with two pump housings respectively, two connecting tubes are fixed respectively It is connected between two liquor boxs and two pump housings.
5. the unleaded aluminium foil for electrolytic capacitor of 2 mesohigh according to claim corrodes feeder equipment, which is characterized in that institute It states and is opened up at the top of support plate there are two the second through-hole, be equipped with second bearing in two second through-holes, two described the The outer ring of two bearings is fixedly connected with the inner wall of two second through-holes respectively, and the inner ring of two second bearings is solid respectively Surely it is set in two rotating bars.
6. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that institute The bottom four corners position for stating support plate is fixedly installed with supporting leg.
7. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that institute The bottom for stating feed slot and the electrolytic cell is fixedly installed with drain pipe, and two drain pipes run through support plate, and two Valve is equipped on a drain pipe.
8. the unleaded aluminium foil for electrolytic capacitor of mesohigh according to claim 1 corrodes feeder equipment, which is characterized in that institute The side for stating support plate is equipped with two-direction switch.
CN201910479680.2A 2019-06-04 2019-06-04 Aluminum foil corrosion feeder for medium-high voltage lead-free electrolytic capacitor Active CN110257894B (en)