Prior art keywords
pitch
rubber
rubber powder
asphalt
modified
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910279895.XA
Other languages
Chinese (zh)
Inventor
高翔
于彩霞
钱季洁
侯萧
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanjing Polytechnic Institute
Original Assignee
Nanjing Polytechnic Institute
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing Polytechnic Institute filed Critical Nanjing Polytechnic Institute
Priority to CN201910279895.XA priority Critical patent/CN109957255A/en
Publication of CN109957255A publication Critical patent/CN109957255A/en
Pending legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L95/00Compositions of bituminous materials, e.g. asphalt, tar, pitch
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L2201/00Properties
    • C08L2201/08Stabilised against heat, light or radiation or oxydation

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Civil Engineering (AREA)
  • Materials Engineering (AREA)
  • Structural Engineering (AREA)
  • Health & Medical Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Medicinal Chemistry (AREA)
  • Polymers & Plastics (AREA)
  • Organic Chemistry (AREA)
  • Road Paving Structures (AREA)
  • Compositions Of Macromolecular Compounds (AREA)

Abstract

The present invention relates to a kind of preparation methods of pitch, specifically, being a kind of preparation method of rubber modified asphalt.It mainly include matrix pitch and rubber powder, the pitch selects 90# road asphalt, the rubber powder that the rubber powder selection higher damaged tire of oblique natural gum content is process, the rubber powder fineness is between -60 mesh of 30 mesh, the matrix pitch is matched by weight with rubber powder, rubber powder: pitch=20:100, modifying agent: pitch=10:100, stabilizer: pitch=9:100.Waste-tyre rubber-powder is used to pitch to be modified, greatly reduce social black pollution, realize the purpose for energy-saving and emission-reduction of turning waste into wealth, there is stronger heat-resisting quantity simultaneously, improve the viscosity of pitch, improve the cryogenic property of pitch, reduce pavement cracking, anti-aging, anti-oxidant and thermal stability is increased for pitch, and since the excellent elasticity of rubber for tire also provides flexible and endurance and anti-crack ability in biggish temperature range for bituminous pavement, to extend 1 ~ 3 times of service life of road surface.

Description

A kind of preparation method of rubber modified asphalt
Technical field
The present invention relates to a kind of preparation methods of pitch, specifically, being a kind of preparation method of rubber modified asphalt.
Background technique
Rubber modified asphalt (Asphalt Rubber, abbreviation AR) is a kind of rubber powder made of waste tire, as changing Property agent is added in matrix pitch, in a special special installation, through a series of works such as high temperature, additive and shear-mixed With manufactured novel high-quality composite material.The service life on road surface can be made to improve, reduce noise, mitigate vibration, improve heat surely Qualitative and Thermal cracking improves freezing.
China builds road and SBS modified pitch is widely used at present, and SBS is expensive, with skyrocketing for oil price, The price of SBS is up to 22000 yuan/ton.And waste-tyre rubber-powder price only has 3000 yuan/ton, through calculating, per 100 km can be reduced 25,000,000 yuan of road surface cost.
Summary of the invention
In order to solve the above-mentioned technical problem, waste-tyre rubber-powder is used for pitch and is modified by the present invention, is significantly reduced Social black pollution, realizes the purpose for energy-saving and emission-reduction of turning waste into wealth.
To achieve the goals above, the specific technical solution that the present invention uses is as follows:
A kind of preparation method of rubber modified asphalt, which is characterized in that mainly include matrix pitch and rubber powder, the pitch choosing The rubber powder being process with 90# road asphalt, the rubber powder selection higher damaged tire of oblique natural gum content, the rubber Rubber powder fineness is between -60 mesh of 30 mesh, and the matrix pitch is matched by weight with rubber powder, rubber powder: pitch=20:100 changes Property agent: pitch=10:100, stabilizer: pitch=9:100, the preparation method of the rubber modified asphalt the following steps are included:
(1) prepare rubber modified bitumen: pitch is matched by weight with rubber powder, rubber powder: pitch=20:100, by pitch and glue Be put into heating tank after powder mixing, temperature risen to 170 °C, the pitch after will heat up is by modifying agent: pitch proportion is added and is modified Agent, when addition, feed while stirring;
(2) carry out effectively mixing repeatedly: starting colloid merges variable-frequency control pump, and the asphalt after preparing in step 1 is led to Colloid mill unification is crossed to place into agitator tank after, after the material has all merged, closing machine;
(3) stabilizer is added: according to the proportion by the asphalt after grinding altogether in step 2, stabilizer: pitch=9:100 is added steady Determine agent, carries out total mill again according to step 2, after number reaches 3-6 times, test to the modified pitch after total mill, Zhi Daoda To desired indicator;
(4) it develops: the rubber modified asphalt processed is put into progress later period development in holding vessel, development time is 1-2 hours, Obtain qualified rubber modified asphalt.
The present invention is further improved, and the rubber modified asphalt is modified the storage time in situation no more than 24 at the scene Hour.
The present invention is further improved, and the storage temperature of the rubber modified asphalt is at 150-160 °C.
Beneficial effects of the present invention: waste-tyre rubber-powder is used for pitch and is modified by the present invention, greatly reduces society Meeting black pollution, realizes the purpose for energy-saving and emission-reduction of turning waste into wealth, while having stronger heat-resisting quantity, improves the glutinous of pitch Degree improves the cryogenic property of pitch, reduces pavement cracking, increases anti-aging, anti-oxidant and thermal stability, Er Qieyou for pitch Flexible and endurance and anti-crack also are provided for bituminous pavement in biggish temperature range in the excellent elasticity of rubber for tire Ability, to extend 1 ~ 3 times of service life of road surface.
Specific embodiment
In order to deepen the understanding of the present invention, below in conjunction with embodiment, the invention will be described in further detail, the reality It applies example for explaining only the invention, protection scope of the present invention is not constituted and limited.
A kind of preparation method of rubber modified asphalt, which is characterized in that mainly include matrix pitch and rubber powder, the drip Blueness selects 90# road asphalt, the rubber powder that the rubber powder selection higher damaged tire of oblique natural gum content is process, institute Rubber powder fineness is stated between -60 mesh of 30 mesh, the matrix pitch is matched by weight with rubber powder, rubber powder: pitch=20: 100, modifying agent: pitch=10:100, stabilizer: pitch=9:100, the preparation method of the rubber modified asphalt include following step It is rapid:
(1) prepare rubber modified bitumen: pitch is matched by weight with rubber powder, rubber powder: pitch=20:100, by pitch and glue Be put into heating tank after powder mixing, temperature risen to 170 °C, the pitch after will heat up is by modifying agent: pitch proportion is added and is modified Agent, when addition, feed while stirring;
(2) carry out effectively mixing repeatedly: starting colloid merges variable-frequency control pump, and the asphalt after preparing in step 1 is led to Colloid mill unification is crossed to place into agitator tank after, after the material has all merged, closing machine;
(3) stabilizer is added: according to the proportion by the asphalt after grinding altogether in step 2, stabilizer: pitch=9:100 is added steady Determine agent, carries out total mill again according to step 2, after number reaches 3-6 times, test to the modified pitch after total mill, Zhi Daoda To desired indicator;
(4) it develops: the rubber modified asphalt processed is put into progress later period development in holding vessel, development time is 1-2 hours, Obtain qualified rubber modified asphalt.
In the present embodiment, the rubber modified asphalt was modified the storage time in situation no more than 24 hours at the scene.
In the present embodiment, the storage temperature of the rubber modified asphalt is at 150-160 °C.
Basic principles and main features and advantage of the invention have been shown and described above.The technical staff of the industry should Understand, the present invention is not limited to the above embodiments, and the above embodiments and description only describe originals of the invention Reason, without departing from the spirit and scope of the present invention, various changes and improvements may be made to the invention, these changes and improvements It all fall within the protetion scope of the claimed invention.The claimed scope of the invention is by appended claims and its equivalent circle It is fixed.

Claims (3)

1. a kind of preparation method of rubber modified asphalt, which is characterized in that mainly include matrix pitch and rubber powder, the pitch 90# road asphalt is selected, the rubber powder that the rubber powder selection higher damaged tire of oblique natural gum content is process is described Rubber powder fineness is between -60 mesh of 30 mesh, and the matrix pitch is matched by weight with rubber powder, rubber powder: pitch=20:100, Modifying agent: pitch=10:100, stabilizer: pitch=9:100, the preparation method of the rubber modified asphalt the following steps are included:
Prepare rubber modified bitumen: pitch is matched by weight with rubber powder, rubber powder: pitch=20:100 mixes pitch and rubber powder Be put into heating tank after conjunction, temperature risen to 170 °C, the pitch after will heat up is by modifying agent: modifying agent is added in pitch proportion, It feeds while stirring when addition;
Carry out effectively mixing repeatedly: starting colloid merges variable-frequency control pump, and the asphalt after preparing in step 1 is passed through glue Body places into agitator tank after merging one time, after the material has all merged, closing machine;
Stabilizer is added: according to the proportion by the asphalt after grinding altogether in step 2, stabilizer: pitch=9:100, which is added, to be stablized Agent carries out total mill again according to step 2, after number reaches 3-6 times, tests to the modified pitch after total mill, until reaching Desired indicator;
Development: being put into progress later period development in holding vessel for the rubber modified asphalt processed, and development time is 1-2 hours, is obtained To qualified rubber modified asphalt.
2. a kind of preparation method of rubber modified asphalt according to claim 1, which is characterized in that the modified rubber drip The green storage time being modified in situation at the scene was no more than 24 hours.
3. a kind of preparation method of rubber modified asphalt according to claim 2, which is characterized in that the modified rubber The storage temperature of pitch is at 150-160 °C.
CN201910279895.XA 2019-04-09 2019-04-09 A kind of preparation method of rubber modified asphalt Pending CN109957255A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201910279895.XA CN109957255A (en) 2019-04-09 2019-04-09 A kind of preparation method of rubber modified asphalt

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201910279895.XA CN109957255A (en) 2019-04-09 2019-04-09 A kind of preparation method of rubber modified asphalt

Publications (1)

Publication Number Publication Date
CN109957255A true CN109957255A (en) 2019-07-02

Family

ID=67025887

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201910279895.XA Pending CN109957255A (en) 2019-04-09 2019-04-09 A kind of preparation method of rubber modified asphalt

Country Status (1)

Country Link
CN (1) CN109957255A (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110387130A (en) * 2019-07-15 2019-10-29 南京科技职业学院 A kind of preparation method of rubber powder asphalt
CN111440456A (en) * 2020-04-23 2020-07-24 中交路桥建设有限公司 SBS rubber powder modified asphalt, preparation method and pavement construction method thereof
CN112111164A (en) * 2020-08-26 2020-12-22 盐城工学院 Method for refining asphalt for road construction

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107916005A (en) * 2017-12-05 2018-04-17 佛山市高明区明城镇新能源新材料产业技术创新中心 A kind of environment-friendly rubber asphalt and preparation method thereof
CN108219487A (en) * 2017-12-30 2018-06-29 中铁十八局集团第五工程有限公司 A kind of rubber powder modified asphalt and preparation method thereof
CN109181328A (en) * 2018-09-28 2019-01-11 南京科技职业学院 A kind of preparation method of composite modified asphalt

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107916005A (en) * 2017-12-05 2018-04-17 佛山市高明区明城镇新能源新材料产业技术创新中心 A kind of environment-friendly rubber asphalt and preparation method thereof
CN108219487A (en) * 2017-12-30 2018-06-29 中铁十八局集团第五工程有限公司 A kind of rubber powder modified asphalt and preparation method thereof
CN109181328A (en) * 2018-09-28 2019-01-11 南京科技职业学院 A kind of preparation method of composite modified asphalt

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110387130A (en) * 2019-07-15 2019-10-29 南京科技职业学院 A kind of preparation method of rubber powder asphalt
CN111440456A (en) * 2020-04-23 2020-07-24 中交路桥建设有限公司 SBS rubber powder modified asphalt, preparation method and pavement construction method thereof
CN112111164A (en) * 2020-08-26 2020-12-22 盐城工学院 Method for refining asphalt for road construction

Similar Documents

Publication Publication Date Title
CN109957255A (en) A kind of preparation method of rubber modified asphalt
CN106800787B (en) A kind of high-temperature storage property high-viscosity high-elasticity modified pitch and preparation method thereof
CN106242378B (en) Hot in-plant reclaimed asphalt mixture and preparation method thereof
CA2797305C (en) Rubber asphalt and preparation method thereof
EP3467045A1 (en) Plant mix warm regenerated asphalt mixture and preparation method therefor
CN103756341A (en) High-toughness waste rubber asphalt and preparation method thereof
CN104312173A (en) Rubber composite modified asphalt and preparation method thereof
CN102234188B (en) Method for preparing environment-friendly warm mix asphalt
CN102329102A (en) Hot-mix-cold-laid SBS (styrene butadiene styrene) modified asphalt mixture
CN110387130A (en) A kind of preparation method of rubber powder asphalt
CN104119032A (en) A regenerating method of an SBS asphalt mixture with a high RAP mixing amount
CN113698139A (en) High-mixing-amount RAP hot mix plant recycling modified asphalt mixture and preparation method thereof
CN112029306A (en) Preparation method of epoxy modified emulsified asphalt with shape memory performance
CN109456604A (en) A kind of high-performance modified emulsified asphalt and preparation method thereof
CN108517127B (en) Coal direct liquefaction residue hard hot asphalt grouting material and preparation method thereof
CN109575618A (en) A kind of compound rock asphalt tracking-resisting modifier of graphene and preparation method thereof
CN109650781A (en) A kind of high frictional resistance thin overlay asphalt of middle low temperature warm mix and preparation method thereof
CN105131618A (en) Road seam filling asphalt material, and preparation method and applications thereof
CN102634062A (en) Method for preparing high-tenacity reclaimed rubber by adding coupling agent
CN109534722A (en) A kind of high-performance reclaimed bituminous pavement cold-repairing material and preparation method thereof
CN104556820B (en) Interfacial modifier capable of improving pitch-aggregate performance and preparation method thereof
CN103013142A (en) Waste tire rubber powder plant asphalt material and preparation method thereof
CN112374806A (en) Glass fiber rubber modified asphalt mixture and preparation method thereof
CN116768531A (en) High-blending-amount TB rubber modified asphalt mixture and preparation method thereof
CN110256745A (en) A kind of modified pitch composite particles and preparation method thereof based on waste rubber powder

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20190702