CN109746175A - Solid wood furniture spraying process - Google Patents

Solid wood furniture spraying process Download PDF

Info

Publication number
CN109746175A
CN109746175A CN201711093480.0A CN201711093480A CN109746175A CN 109746175 A CN109746175 A CN 109746175A CN 201711093480 A CN201711093480 A CN 201711093480A CN 109746175 A CN109746175 A CN 109746175A
Authority
CN
China
Prior art keywords
spraying
solid wood
spraying process
wood furniture
plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711093480.0A
Other languages
Chinese (zh)
Inventor
刘能江
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dujiangyan Rui To Furniture Co Ltd
Original Assignee
Dujiangyan Rui To Furniture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dujiangyan Rui To Furniture Co Ltd filed Critical Dujiangyan Rui To Furniture Co Ltd
Priority to CN201711093480.0A priority Critical patent/CN109746175A/en
Publication of CN109746175A publication Critical patent/CN109746175A/en
Pending legal-status Critical Current

Abstract

The present invention discloses a kind of solid wood furniture spraying process, comprising the following steps: Step 1: choosing solid wood board, and excision forming;Step 2: the plate after cutting is sent into 120 DEG C -150 DEG C of limewash, boiling 3h-5h;Step 3: in 120 DEG C -150 DEG C of at a temperature of drying plate;Step 4: when plate humidity is to stop drying in 6%-11%;Step 5: assembled furniture molding and spray-applied primer, dry 30min-50min after spraying;Step 6: intermediate layer paint is sprayed in primed surface, dry 60min-70min after spraying;Step 7: spraying upper layer in paint surface is painted in middle level, dry 10min-20min after spraying.A variety of spraying process that the present invention uses, significantly improve the mechanical performance and glossiness of coating, to improve the wearability of coating, impact resistance and protect color gloss retention.

Description

Solid wood furniture spraying process
Technical field
The invention belongs to Furniture manufacturing fields, and in particular to a kind of solid wood furniture spraying process.
Background technique
Traditional paint is aided with various auxiliary agents and pigment using vegetable oil, synthetic resin as main film forming substance, and when use need to add Entering the organic solvent dilutings such as toluene, dimethylbenzene, base-material, which is that the small molecule appearance in synthetic resin is easily absorbed by the body, to damage, And solvent is toluene, dimethylbenzene is even more morbid substance, is also required to expend mass energy, material, discharge when producing these solvents A large amount of waste residues and toxic gas, it is totally unfavorable to environment.
Summary of the invention
The technical problems to be solved by the invention are in view of the above shortcomings of the prior art, to provide a kind of solid wood furniture spray Technique is applied, can be carried out effectively spraying, guarantees the effect of spraying.
The technical scheme adopted by the invention is that: a kind of solid wood furniture spraying process, comprising the following steps:
Step 1: choosing solid wood board, and excision forming;
Step 2: the plate after cutting is sent into 120 DEG C -150 DEG C of limewash, boiling 3h-5h;
Step 3: in 120 DEG C -150 DEG C of at a temperature of drying plate;
Step 4: when plate humidity is to stop drying in 6%-11%;
Step 5: assembled furniture molding and spray-applied primer, dry 30min-50min after spraying;
Step 6: intermediate layer paint is sprayed in primed surface, dry 60min-70min after spraying;
Step 7: spraying upper layer in paint surface is painted in middle level, dry 10min-20min after spraying.
In one embodiment, in step 2, temperature is 150 DEG C, digestion time 5h.
In one embodiment, in step 3, drying temperature is 150 DEG C.
In one embodiment, in step 4, plate humidity is 11%.
In one embodiment, in step 5, drying time 50min.
In one embodiment, in step 6, drying time 70min.
In one embodiment, in step 7, drying time 20min.
The beneficial effects of the present invention are: a variety of spraying process of use significantly improve the mechanical performance and gloss of coating Degree, to improve the wearability of coating, impact resistance and protect color gloss retention.
Specific embodiment
Below in conjunction with specific embodiment, invention is further described in detail.
A kind of solid wood furniture spraying process, comprising the following steps:
Step 1: choosing solid wood board, and excision forming;
Step 2: the plate after cutting is sent into 120 DEG C -150 DEG C of limewash, boiling 3h-5h;
Step 3: in 120 DEG C -150 DEG C of at a temperature of drying plate;
Step 4: when plate humidity is to stop drying in 6%-11%;
Step 5: assembled furniture molding and spray-applied primer, dry 30min-50min after spraying;
Step 6: intermediate layer paint is sprayed in primed surface, dry 60min-70min after spraying;
Step 7: spraying upper layer in paint surface is painted in middle level, dry 10min-20min after spraying.
In the present embodiment, in step 2, temperature is 150 DEG C, digestion time 5h.
In the present embodiment, in step 3, drying temperature is 150 DEG C.
In the present embodiment, in step 4, plate humidity is 11%.
In the present embodiment, in step 5, drying time 50min.
In the present embodiment, in step 6, drying time 70min.
In the present embodiment, in step 7, drying time 20min.
A variety of spraying process that the present invention uses, significantly improve the mechanical performance and glossiness of coating, to improve painting Wearability, impact resistance and the guarantor's color gloss retention of layer.
A specific embodiment of the invention above described embodiment only expresses, the description thereof is more specific and detailed, but simultaneously Limitations on the scope of the patent of the present invention therefore cannot be interpreted as.It should be pointed out that for those of ordinary skill in the art For, without departing from the inventive concept of the premise, various modifications and improvements can be made, these belong to guarantor of the invention Protect range.

Claims (7)

1. a kind of solid wood furniture spraying process, it is characterised in that: the following steps are included:
Step 1: choosing solid wood board, and excision forming;
Step 2: the plate after cutting is sent into 120 DEG C -150 DEG C of limewash, boiling 3h-5h;
Step 3: in 120 DEG C -150 DEG C of at a temperature of drying plate;
Step 4: when plate humidity is to stop drying in 6%-11%;
Step 5: assembled furniture molding and spray-applied primer, dry 30min-50min after spraying;
Step 6: intermediate layer paint is sprayed in primed surface, dry 60min-70min after spraying;
Step 7: spraying upper layer in paint surface is painted in middle level, dry 10min-20min after spraying.
2. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 2, temperature is 150 DEG C, is steamed Boiling the time is 5h.
3. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 3, drying temperature 150 ℃。
4. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 4, plate humidity be 11%。
5. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 5, drying time is 50min。
6. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 6, drying time is 70min。
7. solid wood furniture spraying process according to claim 1, it is characterised in that: in step 7, drying time is 20min。
CN201711093480.0A 2017-11-08 2017-11-08 Solid wood furniture spraying process Pending CN109746175A (en)