CN109698351A - It is a kind of to improve the additive for covering paper adsorptivity - Google Patents
It is a kind of to improve the additive for covering paper adsorptivity Download PDFInfo
- Publication number
- CN109698351A CN109698351A CN201811598538.1A CN201811598538A CN109698351A CN 109698351 A CN109698351 A CN 109698351A CN 201811598538 A CN201811598538 A CN 201811598538A CN 109698351 A CN109698351 A CN 109698351A
- Authority
- CN
- China
- Prior art keywords
- sio
- powder
- pure water
- board surface
- polar board
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The object of the present invention is to provide the additives that paper adsorptivity is covered in a kind of raising, by 30% SiO2Grind into powder and the mixing dispersion into 70% pure water, the polar board surface that smear is crossed sprays the evenly dispersed pure water for having SiO2 powder, then is covered with one layer of paper to polar board surface, polar board surface is wrapped, SiO2The nm of the d of powder≤75, such absorption property is more preferable, and evenly dispersed has SiO2The pure water of powder needs to be stirred mixing at any time and guarantees its adsorptivity, in this way to pole plate without negative effect, the adhesiveness for applying paperboard can be improved, scrap to reduce pole plate, suitable for production.
Description
Technical field
The present invention relates to the additives that accumulator plate process field more particularly to a kind of raising cover paper adsorptivity.
Background technique
Battery is usually will use in people's life, and wherein battery includes lead-acid accumulator, lead acid storage battery
It include pole plate in pond.Pole plate is formed using lead liquid casting, and pole plate needs to apply cream later, then carries out leaching acid.Sour work will be drenched at present
Sequence is cancelled, and is changed to be covered with one layer of paper in polar board surface, to reduce spent acid, the pollution of scrap lead cream.But in process of production often
It will appear paper bonding loosely, it is easy to fall off, and increase pole plate and scrap.Therefore solving the problems, such as this just seems particularly significant.
Summary of the invention
To solve the above problems, the present invention provides a kind of additive for improving and covering paper adsorptivity, by 30% SiO2It is ground into
Powder and the mixing dispersion into 70% pure water, the polar board surface that smear is crossed spray the evenly dispersed pure water for having SiO2 powder, then
One layer of paper is covered with to polar board surface, polar board surface is wrapped, SiO2The nm of the d of powder≤75, such absorption property is more preferable, and
And evenly dispersed there is SiO2The pure water of powder needs to be stirred mixing at any time and guarantees its adsorptivity, in this way to pole plate without negative shadow
It rings, the adhesiveness for applying paperboard can be improved, scrap, solve the problems in the background art to reduce pole plate.
The object of the present invention is to provide the additives that paper adsorptivity is covered in a kind of raising, include the material of following content: SiO2
30% and 70% pure water;
By 30% SiO2Grind into powder is sieved later, puts into 70% pure water, is stirred later, so that SiO2Powder
End is dispersed in pure water;There is SiO for the sprinkling of polar board surface that smear is crossed is evenly dispersed2The pure water of powder, so that pole plate table
EDS maps are dispersed with SiO2The pure water of powder is finally covered with one layer of paper in polar board surface, polar board surface is wrapped.
Further improvement lies in that: the SiO2The nm of the d of powder≤75.
Further improvement lies in that: described evenly dispersed have SiO2Need of the pure water of powder before being sprayed onto polar board surface at any time
It is stirred mixing, so that SiO2Powder scatter in pure water.
Beneficial effects of the present invention: the present invention is by 30% SiO2Grind into powder and the mixing dispersion into 70% pure water,
The polar board surface that smear is crossed sprays the evenly dispersed pure water for having SiO2 powder, then is covered with one layer of paper to polar board surface, by pole plate
Surface wraps, SiO2The nm of the d of powder≤75, such absorption property is more preferable, and evenly dispersed has SiO2The pure water of powder needs
It to be stirred mixing at any time and guarantees its adsorptivity, in this way to pole plate without negative effect, the adhesiveness for applying paperboard can be improved, from
And reduce pole plate and scrap, suitable for production.
Specific embodiment
In order to deepen the understanding of the present invention, the present invention will be described in further detail with reference to the examples below, the embodiment
For explaining only the invention, it is not intended to limit the scope of the present invention..
The present embodiment provides the additives that paper adsorptivity is covered in a kind of raising, include the material of following content: SiO230% He
70% pure water;
By 30% SiO2Grind into powder is sieved later, puts into 70% pure water, is stirred later, so that SiO2Powder
End is dispersed in pure water;There is SiO for the sprinkling of polar board surface that smear is crossed is evenly dispersed2The pure water of powder, so that pole plate table
EDS maps are dispersed with SiO2The pure water of powder is finally covered with one layer of paper in polar board surface, polar board surface is wrapped.
The SiO2The nm of the d of powder=75.Described evenly dispersed have SiO2The pure water of powder before being sprayed onto polar board surface with
When needs be stirred mixing so that SiO2Powder scatter in pure water.
By 30% SiO2Grind into powder and the mixing dispersion into 70% pure water, the polar board surface that smear is crossed spray equal
The even pure water for being dispersed with SiO2 powder, then one layer of paper is covered with to polar board surface, polar board surface is wrapped, SiO2The d of powder≤
75 nm, such absorption property is more preferable, and evenly dispersed has SiO2The pure water of powder needs to be stirred mixing at any time and guarantees it
Adsorptivity can be improved the adhesiveness for applying paperboard, scrap to reduce pole plate in this way to pole plate without negative effect, be suitable for life
In production.
Claims (3)
1. a kind of improve the additive for covering paper adsorptivity, it is characterised in that: include the material of following content: SiO230% and 70%
Pure water;
By 30% SiO2Grind into powder is sieved later, puts into 70% pure water, is stirred later, so that SiO2Powder
It is dispersed in pure water;There is SiO for the sprinkling of polar board surface that smear is crossed is evenly dispersed2The pure water of powder, so that polar board surface
It is distributed with and is dispersed with SiO2The pure water of powder is finally covered with one layer of paper in polar board surface, polar board surface is wrapped.
2. a kind of as described in claim 1 improve the additive for covering paper adsorptivity, it is characterised in that: the SiO2D≤75 of powder
nm。
3. a kind of improve covers the additive of paper adsorptivity as described in claim 1, it is characterised in that: described evenly dispersed have SiO2
Needs of the pure water of powder before being sprayed onto polar board surface at any time are stirred mixing, so that SiO2Powder scatter in pure water
In.