CN109352132A - Control the method that inner and outer ring difference of height deforms after low pressure ring type partition welds - Google Patents

Control the method that inner and outer ring difference of height deforms after low pressure ring type partition welds Download PDF

Info

Publication number
CN109352132A
CN109352132A CN201811240280.8A CN201811240280A CN109352132A CN 109352132 A CN109352132 A CN 109352132A CN 201811240280 A CN201811240280 A CN 201811240280A CN 109352132 A CN109352132 A CN 109352132A
Authority
CN
China
Prior art keywords
partition
outer ring
welding
ring
difference
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811240280.8A
Other languages
Chinese (zh)
Inventor
张辰鸾
王冬雪
邹艳哲
杨飞鹏
王广成
高作为
康禹
苏志成
张仁军
孔令福
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Harbin Turbine Co Ltd
Original Assignee
Harbin Turbine Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Harbin Turbine Co Ltd filed Critical Harbin Turbine Co Ltd
Priority to CN201811240280.8A priority Critical patent/CN109352132A/en
Publication of CN109352132A publication Critical patent/CN109352132A/en
Pending legal-status Critical Current

Abstract

The method that inner and outer ring difference of height deforms after low pressure ring type partition welds is controlled, it is related to a kind of method of control inner and outer ring difference of height deformation, and in particular to a method of inner and outer ring difference of height deforms after control low pressure ring type partition welds.The present invention is in order to solve the problem of partition due to the big unstable quality of weld industry difficulty.Step of the invention is Step 1: assemble in diaphragm inner ring and partition outer ring;Step 2: drawing round wires and pitch lines in partition inner ring, round wires and pitch lines are drawn on partition outer ring;Step 3: assembling guide vane between partition inner ring and partition inner ring, and check whether fitted position complies with standard;Step 4: the steam output side weld seam of welding diaphragm;Step 5: partition steam output side is loaded upward;Step 6: welding diaphragm steam admission side weld seam;Step 7: completing partition welding, check whether each size of partition and weld size comply with standard.The invention belongs to steam turbine equipment fields.

Description

Control the method that inner and outer ring difference of height deforms after low pressure ring type partition welds
Technical field
The present invention relates to a kind of methods of control inner and outer ring difference of height deformation, and in particular to a kind of control low pressure ring type partition The method that inner and outer ring difference of height deforms after welding, belongs to steam turbine equipment field.
Background technique
Conventional Steam Turbine low pressure ring type partition is made of partition outer ring, partition inner ring, guide vane, and argon arc welding is used after assembly It is welded, position while welding is respectively at the position that guide vane is connect with partition outer ring, partition inner ring.When partition erection welding, first will Steam output side is upward, after assembling guide vane, welds steam output side weld seam, then workpiece is attached to welding steam admission side weld seam on positioner.Due to Low voltage partition plate general size is larger, and welding capacity is also larger, and biggish heat input causes partition postwelding to shrink, and causes throat dimension super Difference, partition inner and outer rings difference of height is inconsistent, occurs axial phenomenon of grinding one's teeth when often closing half after partition welding.This kind of partitions by Big, the unstable quality in weld industry difficulty.
Summary of the invention
The present invention is solves the problem of that partition due to the big unstable quality of weld industry difficulty, and then proposes to control The method that inner and outer ring difference of height deforms after the welding of low pressure ring type partition.
The technical solution adopted by the present invention to solve the above problem is as follows: specific step is as follows for the method for the invention:
Step 1: assemble in diaphragm inner ring and partition outer ring;
Step 2: drawing round wires and pitch lines in partition inner ring, round wires and pitch lines are drawn on partition outer ring;
Step 3: assembling guide vane between partition inner ring and partition inner ring, and check whether fitted position complies with standard;
Step 4: the steam output side weld seam of welding diaphragm;
Step 5: partition steam output side is loaded upward;
Step 6: welding diaphragm steam admission side weld seam;
Step 7: completing partition welding, check whether each size of partition and weld size comply with standard.
Further, guarantee that horizontal error is not more than 0.5mm during assemble in diaphragm inner ring and partition outer ring in step 1, And ensure that partition inner ring and partition outer ring are concentric.
Further, in step 2 with leveling ruler, advise and mark horizontal middle separated time respectively in partition inner ring and partition outer ring And vertical middle separated time, and horizontal middle separated time and vertical middle separated time extend respectively on the end face of partition inner ring and partition outer ring;Every Plate inner ring and the pitch of partition outer ring will uniformly correspond to adjustment, finally draw quasi- pitch lines, and stamp foreign dotting punch respectively.
Further, in step 4 by the way of argon arc welding welding diaphragm steam output side weld seam.
Further, centering partition center of gravity in step 5, with cushion block by the partition inner ring and partition outer ring of partition lagging edge Difference in height filling-in guarantees that flatness complies with standard;Every half block partition is evenly arranged 5~8 cushion blocks, and cushion block point is welded in partition On ring.
Further, in step 6 by the way of argon arc welding welding diaphragm steam admission side weld seam, partition integral solder sequence The quadrant area symmetrical wheel flow point group welding divided when by assembly, weld seam remain downhand position.
The beneficial effects of the present invention are: the present invention is easy to use, practical, location control is accurate, weld industry The features such as being obviously improved.The present invention effectively controls the inner and outer ring difference in height after the welding of low pressure ring type partition, and partition is effectively prevent to close Axial direction after half is ground one's teeth, to improve partition quality.
Detailed description of the invention
Fig. 1 is conventional power unit low pressure ring type partition schematic diagram.
Specific embodiment
Specific embodiment 1: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment The method for connecing rear inner and outer ring difference of height deformation is achieved by the steps of:
Step 1: assemble in diaphragm inner ring 1 and partition outer ring 2;
Step 2: drawing round wires and pitch lines in partition inner ring 1, round wires and pitch lines are drawn on partition outer ring 2;
Step 3: assembling guide vane between partition inner ring 1 and partition inner ring 1, and check whether fitted position complies with standard;
Step 4: the steam output side weld seam of welding diaphragm;
Step 5: partition steam output side is loaded upward;
Step 6: welding diaphragm steam admission side weld seam;
Step 7: completing partition welding, check whether each size of partition and weld size comply with standard.
Specific embodiment 2: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment Guarantee level is missed in the process for assemble in diaphragm inner ring 1 and partition outer ring 2 in the step of connecing the method for rear inner and outer ring difference of height deformation one Difference is not more than 0.5mm, and ensures that partition inner ring 1 and partition outer ring 2 are concentric.
Specific embodiment 3: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment In the step of connecing the method for rear inner and outer ring difference of height deformation two with leveling ruler, advise and drawn respectively in partition inner ring 1 and partition outer ring 2 Horizontal middle separated time and vertical middle separated time out, and horizontal middle separated time and vertical middle separated time extend respectively to outside partition inner ring 1 and partition On the end face of ring 2;Partition inner ring 1 and the pitch of partition outer ring 2 will uniformly correspond to adjustment, finally draw quasi- pitch lines, and beat respectively Loading dotting punch.
Specific embodiment 4: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment In the step of connecing the method for rear inner and outer ring difference of height deformation four by the way of argon arc welding welding diaphragm steam output side weld seam.
Specific embodiment 5: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment Centering partition center of gravity in the step of connecing the method for rear inner and outer ring difference of height deformation five, with cushion block by the partition inner ring of partition lagging edge 1 and the 2 difference in height filling-in of partition outer ring, guarantee that flatness complies with standard;Every half block partition is evenly arranged 5~8 cushion blocks, and cushion block Point is welded in partition inner ring 1.
Specific embodiment 6: embodiment is described with reference to Fig. 1, control low pressure ring type partition weldering described in present embodiment Welding diaphragm steam admission side weld seam, partition are whole by the way of argon arc welding in the step of connecing the method for rear inner and outer ring difference of height deformation six The quadrant area symmetrical wheel flow point group welding divided when body welding sequence is by assembly, weld seam remain downhand position.
The above described is only a preferred embodiment of the present invention, be not intended to limit the present invention in any form, though So the present invention has been disclosed as a preferred embodiment, and however, it is not intended to limit the invention, any technology people for being familiar with this profession Member, without departing from the scope of the present invention, when the technology contents using the disclosure above are modified or are modified For the equivalent embodiment of equivalent variations, but without departing from the technical solutions of the present invention, according to the technical essence of the invention, Within the spirit and principles in the present invention, any simple modifications, equivalent substitutions and improvements to the above embodiments etc., still Belong within the protection scope of technical solution of the present invention.

Claims (6)

1. controlling the method that inner and outer ring difference of height after the welding of low pressure ring type partition deforms, it is characterised in that: the control low-voltage ring The method that inner and outer ring difference of height deforms after the welding of formula partition is achieved by the steps of:
Step 1: assemble in diaphragm inner ring (1) and partition outer ring (2);
Step 2: drawing round wires and pitch lines on partition inner ring (1), round wires and pitch lines are drawn on partition outer ring (2);
Step 3: assembling guide vane between partition inner ring (1) and partition inner ring (1), and check whether fitted position complies with standard;
Step 4: the steam output side weld seam of welding diaphragm;
Step 5: partition steam output side is loaded upward;
Step 6: welding diaphragm steam admission side weld seam;
Step 7: completing partition welding, check whether each size of partition and weld size comply with standard.
2. the method that inner and outer ring difference of height deforms after the welding of control low pressure ring type partition, feature exist according to claim 1 In: guarantee that horizontal error is not more than 0.5mm in step 1 during assemble in diaphragm inner ring (1) and partition outer ring (2), and ensure every Plate inner ring (1) and partition outer ring (2) are concentric.
3. the method that inner and outer ring difference of height deforms after the welding of control low pressure ring type partition, feature exist according to claim 1 In: in step 2 with leveling ruler, advise marked respectively in partition inner ring (1) and partition outer ring (2) horizontal middle separated time and it is vertical in Separated time, and horizontal middle separated time and vertical middle separated time extend respectively on the end face of partition inner ring (1) and partition outer ring (2);Partition Inner ring (1) and the pitch of partition outer ring (2) will uniformly correspond to adjustment, finally draw quasi- pitch lines, and stamp sample dotting punch respectively.
4. the method that inner and outer ring difference of height deforms after the welding of control low pressure ring type partition, feature exist according to claim 1 In: in step 4 by the way of argon arc welding welding diaphragm steam output side weld seam.
5. the method that inner and outer ring difference of height deforms after the welding of control low pressure ring type partition, feature exist according to claim 1 In: centering partition center of gravity in step 5 is mended the partition inner ring (1) of partition lagging edge and partition outer ring (2) difference in height with cushion block It is flat, guarantee that flatness complies with standard;Every half block partition is evenly arranged 5~8 cushion blocks, and cushion block point is welded on partition inner ring (1).
6. the method that inner and outer ring difference of height deforms after the welding of control low pressure ring type partition, feature exist according to claim 1 In: in step 6 by the way of argon arc welding welding diaphragm steam admission side weld seam, divided when partition integral solder sequence is by assembly The symmetrical wheel flow point group welding of quadrant area, weld seam remains downhand position.
CN201811240280.8A 2018-10-23 2018-10-23 Control the method that inner and outer ring difference of height deforms after low pressure ring type partition welds Pending CN109352132A (en)