CN109112558A - A kind of Environment protection type metal rust inhibitor - Google Patents
A kind of Environment protection type metal rust inhibitor Download PDFInfo
- Publication number
- CN109112558A CN109112558A CN201710485614.7A CN201710485614A CN109112558A CN 109112558 A CN109112558 A CN 109112558A CN 201710485614 A CN201710485614 A CN 201710485614A CN 109112558 A CN109112558 A CN 109112558A
- Authority
- CN
- China
- Prior art keywords
- parts
- environment protection
- protection type
- type metal
- metal rust
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of Environment protection type metal rust inhibitors; component including following parts by weight: 5-7 parts of zinc sulfate; 3-5 parts of amides vapor phase inhibitor, 4-6 parts of sodium propionate, 2-4 parts of complexing agent, 1-3 parts of surfactant, 3-5 parts of kaolin, 7-9 parts of fatty alcohol polyoxyethylene ether, 6-8 parts of diethanol amine, 5-7 parts of modified silicone resin, 4-6 parts, 1-3 parts of octadecylamine of N oleoyl propylhomoserin octadecylamine salt; 4-6 parts of sodium alkyl sulfonate, 100-300 parts of deionized water.Environment protection type metal rust inhibitor of the present invention, formula is scientific and reasonable, and antirust, degreasing dirt-removing power are strong, has no adverse effects, and will not generate foam to non-ferrous metal, spillover will not be generated under high pressure;With excellent contact rustless property and good volatile rust prevention effect.
Description
Technical field
The present invention relates to chemical products fields, and in particular to a kind of Environment protection type metal rust inhibitor.
Background technique
The corrosion of metal is frequently problem in production and living, and metal rusting not only makes metal works itself outside
Shape, color and mechanical performance etc. are destroyed, and more mainly decline its quality of item.In China every year because metal becomes rusty
The steel of erosion account for the 20% of steel total output, and there are about 30% equipment to scrap because of corrosion, both pollute environment, there is a large amount of moneys of waste
Source and energy consumption.The metal that the whole world is scrapped due to corrosion every year accounts for about the 20%-40% of world's metal annual production, wherein steel
The corrosion of iron accounts for the half of corrosion of metal, and the wasting of resources is extremely serious.It is each that metal is widely used in machinery, automobile, household electrical appliances, building etc.
Industry reduces corrosion waste to improve metallicity, needs to surface rust protection processing.Antirust agent have it is safe, easy to operate,
The advantages that low in cost.Existing antirust agent is all made of base oil and oil-soluble inhibitor, can only play contact antirust
Function does not reach those at the position of antirust agent, then cannot form effective corrosion protection.
Summary of the invention
Goal of the invention: to overcome the shortcomings of the existing technology, the present invention is directed to provide a kind of Environment protection type metal rust inhibitor.
Technical solution: in order to solve the above technical problems, the present invention adopts the following technical scheme:
A kind of Environment protection type metal rust inhibitor, the component including following parts by weight: 5-7 parts of zinc sulfate, amides volatile rust prevention
3-5 parts of agent, 4-6 parts of sodium propionate, 2-4 parts of complexing agent, 1-3 parts of surfactant, 3-5 parts of kaolin, fatty alcohol polyoxyethylene ether
7-9 parts, 6-8 parts of diethanol amine, 5-7 parts of modified silicone resin, 4-6 parts, 1-3 parts of octadecylamine of N oleoyl propylhomoserin octadecylamine salt, alkyl
4-6 parts of sodium sulfonate, 100-300 parts of deionized water.
It further, further include 5-7 parts of monoethanolamine benzoate.
It further, further include 8-10 parts of macromolecule film former.
The unmentioned technology of the present invention is the prior art.
The utility model has the advantages that Environment protection type metal rust inhibitor of the present invention, formula is scientific and reasonable, and antirust, degreasing dirt-removing power are strong, to having
Non-ferrous metal has no adverse effects, and will not generate foam, and spillover will not be generated under high pressure;With excellent contact antirust
Performance and good volatile rust prevention effect.
Specific embodiment
For a better understanding of the present invention, below with reference to the embodiment content that the present invention is furture elucidated, but it is of the invention
Content is not limited solely to the following examples.
Embodiment 1
A kind of Environment protection type metal rust inhibitor, the component including following parts by weight: 5 parts of zinc sulfate, amides vapor phase inhibitor 3
Part, 4 parts of sodium propionate, 2 parts of complexing agent, 1 part of surfactant, 3 parts of kaolin, 7 parts of fatty alcohol polyoxyethylene ether, diethanol amine 6
Part, 5 parts of modified silicone resin, 4 parts, 1 part of octadecylamine of N oleoyl propylhomoserin octadecylamine salt, 4 parts of sodium alkyl sulfonate, deionized water 100
Part;5 parts of monoethanolamine benzoate;8 parts of macromolecule film former.
Environment protection type metal rust inhibitor of the present invention, formula is scientific and reasonable, and antirust, degreasing dirt-removing power are strong, to non-ferrous metal without
Adverse effect, and foam will not be generated, spillover will not be generated under high pressure;With excellent contact rustless property and
Good volatile rust prevention effect.
Embodiment 2
A kind of Environment protection type metal rust inhibitor, the component including following parts by weight: 7 parts of zinc sulfate, amides vapor phase inhibitor 5
Part, 6 parts of sodium propionate, 4 parts of complexing agent, 3 parts of surfactant, 5 parts of kaolin, 9 parts of fatty alcohol polyoxyethylene ether, diethanol amine 8
Part, 7 parts of modified silicone resin, 6 parts, 3 parts of octadecylamine of N oleoyl propylhomoserin octadecylamine salt, 6 parts of sodium alkyl sulfonate, deionized water 300
Part;7 parts of monoethanolamine benzoate;10 parts of macromolecule film former.
Embodiment 3
A kind of Environment protection type metal rust inhibitor, the component including following parts by weight: 6 parts of zinc sulfate, amides vapor phase inhibitor 4
Part, 5 parts of sodium propionate, 3 parts of complexing agent, 2 parts of surfactant, 4 parts of kaolin, 8 parts of fatty alcohol polyoxyethylene ether, diethanol amine 7
Part, 6 parts of modified silicone resin, 5 parts, 2 parts of octadecylamine of N oleoyl propylhomoserin octadecylamine salt, 5 parts of sodium alkyl sulfonate, deionized water 200
Part;6 parts of monoethanolamine benzoate;9 parts of macromolecule film former.
The above is only the preferred embodiment of the present invention, it should be pointed out that: those skilled in the art are come
It says, without departing from the principle of the present invention, can also be adjusted to each facility locations, these adjustment also should be regarded as this hair
Bright protection scope.
Claims (3)
1. a kind of Environment protection type metal rust inhibitor, it is characterised in that: the component including following parts by weight: 5-7 parts of zinc sulfate, amides
3-5 parts of vapor phase inhibitor, 4-6 parts of sodium propionate, 2-4 parts of complexing agent, 1-3 parts of surfactant, 3-5 parts of kaolin, poly alkyl alcohol
7-9 parts of ethylene oxide ether, 6-8 parts of diethanol amine, 5-7 parts of modified silicone resin, 4-6 parts of N oleoyl propylhomoserin octadecylamine salt, octadecylamine 1-
3 parts, 4-6 parts of sodium alkyl sulfonate, 100-300 parts of deionized water.
2. Environment protection type metal rust inhibitor as described in claim 1, it is characterised in that: further include 5-7 parts of monoethanolamine benzoate.
3. Environment protection type metal rust inhibitor as described in claim 1, it is characterised in that: further include 8-10 parts of macromolecule film former.