CN108927920A - A kind of energy conservation metal fingerprint and preparation method thereof - Google Patents
A kind of energy conservation metal fingerprint and preparation method thereof Download PDFInfo
- Publication number
- CN108927920A CN108927920A CN201810851733.4A CN201810851733A CN108927920A CN 108927920 A CN108927920 A CN 108927920A CN 201810851733 A CN201810851733 A CN 201810851733A CN 108927920 A CN108927920 A CN 108927920A
- Authority
- CN
- China
- Prior art keywords
- part body
- left part
- right part
- inner sidewall
- pedestal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of energy saving metal fingerprint and preparation method thereof, it includes pedestal, and in the bottom end of arm body and by being welded and fixed, the top of arm body is welded with connection palmar hand for the top holding of pedestal;Connecting palmar hand includes finger section, left part body and right part body, finger section includes former and later two metacarpus and five finger sections, the top that the front and rear of five finger sections is molded over two metacarpus goes out, the side of thumb and the side of little finger in five finger sections form mounting groove, the lower part of left part body and the lower weld of right part body form palm interconnecting piece, the top sidewall of left part body and right part body has the palm side wall interconnecting piece upwardly extended, the palm side wall interconnecting piece sleeve of left part body and right part body is in corresponding mounting groove, two palm side wall interconnecting pieces and finger section splice and are welded to form main palmar hand, main palmar hand and palm interconnecting piece composition connection palmar hand.It makes simply, and convenient welding, secured intensity is high, and the service life is long.
Description
Technical field:
The present invention relates to glove mould equipment technical field, more specifically to a kind of energy saving metal fingerprint and its production side
Method.
Background technique:
Existing fingerprint production method is to be split into two halves using fingerprint ontology along its longitudinal direction, and half is palmar aspect part,
The other half is hand back portion.Palmar aspect part forms a complete fingerprint after fixing with hand back portion make-up.Its surface
For best bright finish.Problem of the prior art:
(1) palmar aspect part can only realize local welding with after hand back portion make-up, and fourchette position can not weld, securely strong
It is poor to spend, and the service life is short.
(2) highly polished, dip effect is poor, cannot achieve the production of butyronitrile, emgloves.
Summary of the invention:
The purpose of the present invention is overcoming the deficiencies of the prior art and provide a kind of energy saving metal fingerprint and preparation method thereof, it is made
Simply, convenient welding, secured intensity is high, and the service life is long.
The solution to the technical problem of the present invention is as follows:
A kind of energy conservation metal fingerprint, it includes pedestal, and the top holding of pedestal is in the bottom end of arm body and solid by welding
Fixed, the top of arm body is welded with connection palmar hand;
Connection palmar hand includes finger section, left part body and right part body, and finger section includes former and later two metacarpus and five finger sections, and five
The top that the front and rear of a finger section is molded over two metacarpus goes out, the side of the thumb in five finger sections and little finger
Side form mounting groove, the lower part of left part body and the lower weld of right part body form palm interconnecting piece, left part body and the right side
The top sidewall of portion's body has the palm side wall interconnecting piece upwardly extended, the palm side wall interconnecting piece sleeve of left part body and right part body
In corresponding mounting groove, main palmar hand is spliced and are welded to form to two palm side wall interconnecting pieces and finger section, main palmar hand and
Palm interconnecting piece composition connection palmar hand.
Raised positioning region is formed on the inner sidewall of the relative wall of two palm side wall interconnecting pieces, raised positioning region is pressed against
On the inner sidewall of corresponding mounting groove.
At the inner sidewall of the relative wall of the lower part of the left part body and right part body, formed on the inner sidewall of left part body
Location hole forms positioning protrusion on the inner sidewall of right part body, and positioning protrusion sleeve is in location hole.
The lower part of the inner sidewall of the left part body and right part body forms lower convex portion, and lower convex portion is pressed against arm body
Inside top wall on.
The lower part of the arm body forms major diameter set portion, and pedestal holding is in major diameter set portion, the bottom of pedestal
Lateral wall has radially extending edges, and radially extending edges are pressed against on the bottom surface in diameter set portion.
A kind of production method making energy saving metal fingerprint, it is characterised in that: it the following steps are included:
(1), design is made according to the fingerprint of required production and is divided into finger section, left part body, right part body, hand centered on fingerprint center
Arm body and pedestal use corresponding finger section mold, left part mould, right part mould, arm body mould by die casting machine
Finger section, left part body, right part body, arm body and pedestal is respectively prepared in tool and base mould;
(2), finger section, left part body, right part body, arm body and pedestal are spliced, so that pedestal holding is in the big of arm body
In diameter set portion, by the positioning protrusion sleeve formed on the inner sidewall of right part body in the location hole of left part body, by left part body
The lower convex portion formed with the lower part of the inner sidewall of right part body protrudes into the top of arm body and is pressed against arm body
On inside top wall, the protrusion that will be formed on the inner sidewall of the relative wall of left part body and the palm side wall interconnecting piece of right part body
Positioning region is pressed against on the inner sidewall of corresponding mounting groove, and finger section is clamped between two palm side wall interconnecting pieces;
(3), it will be welded between all parts spliced;
(4), the commissure of welding is processed by shot blasting;
(5), the surface for the component that step (4) are completed is subjected to spray treatment as needed, is completed the production.
780 ± 30 ° of the melt temperature of the die casting machine die casting dwell time 18 seconds, opens the 20 seconds time of mould.
Polishing in the step (4) is using sanding machine either engraving machine engraving.
The welding of the step (3) uses 300W -1500W laser welder.
Spray treatment in the step (5) operates in spray painting room, sprays nano material, is sprayed into fiber crops as needed
Face or flower face.
Protrusion effect of the invention is:
Compared with prior art, it makes simple, and convenient welding, secured intensity is high, and the service life is long.
Detailed description of the invention:
Fig. 1 is the structural schematic diagram of fingerprint of the invention;
Fig. 2 is the decomposition texture schematic diagram of fingerprint of the invention;
Fig. 3 is the partial sectional view of the decomposing state of fingerprint of the invention.
Specific embodiment:
The present invention will be described in detail with specific preferred embodiment with reference to the accompanying drawing, so that advantages and features of the invention
It can be easier to be readily appreciated by one skilled in the art, these embodiments are only the purpose illustrated, it is no intended to model of the invention
It encloses and is defined.
Embodiment, as shown in Fig. 1 to Fig. 3, a kind of energy conservation metal fingerprint, it includes pedestal 1, and the top holding of pedestal 1 exists
In the bottom end of arm body 2 and by being welded and fixed, the top of arm body 2 is welded with connection palmar hand 3;
Connecting palmar hand 3 includes finger section 31, left part body 32 and right part body 33, and finger section 31 includes former and later two 311 Hes of metacarpus
Five finger sections 312, the top that the front and rear of five finger sections 312 is molded over two metacarpus 311 go out, five finger sections
The side of thumb in 312 and the side of little finger form mounting groove 313, the lower part of left part body 32 and right part body 33
There is the top sidewall of lower weld composition palm interconnecting piece 34, left part body 32 and right part body 33 the palm side wall upwardly extended to connect
35 sleeve of palm side wall interconnecting piece of socket part 35, left part body 32 and right part body 33 is in corresponding mounting groove 313, two palmar sides
Main palmar hand 36, main palmar hand 36 and the composition connection of palm interconnecting piece 34 are spliced and are welded to form to wall interconnecting piece 35 and finger section 31
Palmar hand 3.
Raised positioning region 351, protrusion positioning are formed on the inner sidewall of the relative wall of two palm side wall interconnecting pieces 35
Portion 351 is pressed against on the inner sidewall of corresponding mounting groove 313.
At the inner sidewall of the relative wall of the lower part of the left part body 32 and right part body 33, on the inner sidewall of left part body 32
Location hole 321 is formed, positioning protrusion 331 is formed on the inner sidewall of right part body 33,331 sleeve of positioning protrusion is in location hole
In 321.
The lower part of the inner sidewall of the left part body 32 and right part body 33 forms lower convex portion 37, and lower convex portion 37 is pressed against
On the inside top wall of arm body 2.
The lower part of the arm body 2 forms major diameter set portion 21, and 1 holding of pedestal is in major diameter set portion 21, pedestal 1
Bottom outside wall there are radially extending edges 11, radially extending edges 11 are pressed against on the bottom surface in diameter set portion 21.
A kind of production method making energy saving metal fingerprint, it the following steps are included:
(1), design is made according to the fingerprint of required production and is divided into finger section 31, left part body 32, right part centered on fingerprint center
Body 33, arm body 2 and pedestal 1 use corresponding finger section mold, left part mould, right part mould, hand by die casting machine
Finger section 31, left part body 32, right part body 33, arm body 2 and pedestal (1) is respectively prepared in arm set mould and base mould;
(2), finger section 31, left part body 32, right part body 33, arm body 2 and pedestal 1 are spliced, so that 1 holding of pedestal is in arm
In the major diameter set portion 21 of body 2, by 331 sleeve of positioning protrusion formed on the inner sidewall of right part body 33 in left part body 32
In location hole 321, the lower convex portion 37 that the lower part of left part body 32 and the inner sidewall of right part body 33 forms is protruded into arm body 2
Top in and be pressed against on the inside top wall of arm body 2, by the palm side wall interconnecting piece of left part body 32 and right part body 33
The raised positioning region 351 formed on the inner sidewall of 35 relative wall is pressed against on the inner sidewall of corresponding mounting groove 313, hand
Finger portion 31 is clamped between two palm side wall interconnecting pieces 35;
(3), it will be welded between all parts spliced;
(4), the commissure of welding is processed by shot blasting;
(5), the surface for the component that step (4) are completed is subjected to spray treatment as needed, is completed the production.
780 ± 30 ° of the melt temperature of the die casting machine die casting dwell time 18 seconds, opens the 20 seconds time of mould.
Polishing in the step (4) is using sanding machine either engraving machine engraving.
The welding of the step (3) uses 300W -1500W laser welder.
Spray treatment in the step (5) operates in spray painting room, sprays nano material, is sprayed into fiber crops as needed
Face or flower face.
Pitted skin is made in it or various colored faces can be used for producing the gloves of the materials such as butyronitrile, latex, PVC.
Wherein pitted skin using 0.8-1.6mm spray steel ball equipment spray convex-concave pitted skin or mold on carve complete, and spend face be
Finger section mold, left part mould, right part mould, arm sleeve mould surface on carve various decorative patterns, carry out die casting
When, the finger section 31 that is directly prepared into, left part body 32, right part body 33, arm body 2 outside wall surface straight forming have decorative pattern.
Wherein, connect palmar hand 3 in each siding with a thickness of 0.95 ± 0.25mm.
The siding of arm body 2 with a thickness of 1.2 ± 0.15mm.
The above embodiments are only used to illustrate the present invention, and not limitation of the present invention, in relation to the common of technical field
Technical staff can also make a variety of changes and modification without departing from the spirit and scope of the present invention, therefore institute
There is equivalent technical solution to also belong to scope of the invention, scope of patent protection of the invention should be defined by the claims.
Claims (10)
1. a kind of energy conservation metal fingerprint, it is characterised in that: it includes pedestal (1), and the top holding of pedestal (1) is in arm body
(2) in bottom end and by being welded and fixed, the top of arm body (2) is welded with connection palmar hand (3);
Connecting palmar hand (3) includes finger section (31), left part body (32) and right part body (33), and finger section (31) includes former and later two
Metacarpus (311) and five finger sections (312), the front and rear of five finger sections (312) are molded over the top of two metacarpus (311)
Portion goes out, and the side of thumb and the side of little finger in five finger sections (312) form mounting groove (313), left part body
(32) lower weld of lower part and right part body (33) forms palm interconnecting piece (34), the top of left part body (32) and right part body (33)
Portion's side wall has the palm side wall interconnecting piece (35) upwardly extended, the palm side wall interconnecting piece of left part body (32) and right part body (33)
(35) sleeve in corresponding mounting groove (313), splice and weld group by two palm side wall interconnecting pieces (35) and finger section (31)
At main palmar hand (36), main palmar hand (36) and palm interconnecting piece (34) composition connection palmar hand (3).
2. a kind of energy saving metal fingerprint according to claim 1, it is characterised in that: the phase of two palm side wall interconnecting pieces (35)
To forming on the inner sidewall of wall surface raised positioning region (351), raised positioning region (351) is pressed against corresponding mounting groove (313)
Inner sidewall on.
3. a kind of energy saving metal fingerprint according to claim 1, it is characterised in that: the left part body (32) and right part body (33)
Lower part relative wall inner sidewall at, formed on the inner sidewall of left part body (32) location hole (321), right part body (33)
Inner sidewall on form positioning protrusion (331), positioning protrusion (331) sleeve is in location hole (321).
4. a kind of energy saving metal fingerprint according to claim 1, it is characterised in that: the left part body (32) and right part body (33)
The lower part of inner sidewall form lower convex portion (37), lower convex portion (37) is pressed against on the inside top wall of arm body (2).
5. a kind of energy saving metal fingerprint according to claim 1, it is characterised in that: the lower part of the arm body (2) forms
There is major diameter set portion (21), in major diameter set portion (21), the bottom outside wall of pedestal (1) has radial prolong for pedestal (1) holding
It stretches side (11), radially extending edges (11) are pressed against on the bottom surface in diameter set portion (21).
6. a kind of production method for making any one of claims 1 to 5 energy conservation metal fingerprint, it is characterised in that: it include with
Lower step:
(1), according to the fingerprint of required production be made design be divided into centered on fingerprint center finger section (31), left part body (32),
Right part body (33), arm body (2) and pedestal (1) use corresponding finger section mold, left part mould, the right side by die casting machine
Finger section (31), left part body (32), right part body (33), arm is respectively prepared in portion's mould, arm sleeve mould and base mould
Body (2) and pedestal (1);
(2), finger section (31), left part body (32), right part body (33), arm body (2) and pedestal (1) are spliced, so that pedestal
(1) holding is in the major diameter set portion (21) of arm body (2), the positioning protrusion that will be formed on the inner sidewall of right part body (33)
(331) sleeve is in the location hole (321) of left part body (32), by the lower part of left part body (32) and the inner sidewall of right part body (33) at
The lower convex portion (37) that type has is protruded into the top of arm body (2) and is pressed against on the inside top wall of arm body (2), will
The protrusion formed on the inner sidewall of the relative wall of the palm side wall interconnecting piece (35) of left part body (32) and right part body (33) is fixed
Position portion (351) is pressed against on the inner sidewall of corresponding mounting groove (313), and finger section (31) is clamped in two palm side wall interconnecting pieces
(35) between;
(3), it will be welded between all parts spliced;
(4), the commissure of welding is processed by shot blasting;
(5), the surface for the component that step (4) are completed is subjected to spray treatment as needed, is completed the production.
7. the production method of energy conservation metal fingerprint according to claim 6, it is characterised in that: the die casting machine die casting is melted
780 ± 30 ° of material temperature degree, the dwell time 18 seconds, open the 20 seconds time of mould.
8. the production method of energy conservation metal fingerprint according to claim 6, it is characterised in that: the throwing in the step (4)
Gloss sanding machine either engraving machine engraving.
9. the production method of energy conservation metal fingerprint according to claim 6, it is characterised in that: the welding of the step (3)
Using 300W -1500W laser welder.
10. the production method of energy conservation metal fingerprint according to claim 6, it is characterised in that: the spray in the step (5)
It applies processing to operate in spray painting room, sprays nano material, be sprayed into pitted skin or flower face as needed.