CN1088886A - 一种硫磺冶炼工艺和设备 - Google Patents

一种硫磺冶炼工艺和设备 Download PDF

Info

Publication number
CN1088886A
CN1088886A CN 93101075 CN93101075A CN1088886A CN 1088886 A CN1088886 A CN 1088886A CN 93101075 CN93101075 CN 93101075 CN 93101075 A CN93101075 A CN 93101075A CN 1088886 A CN1088886 A CN 1088886A
Authority
CN
China
Prior art keywords
sulphur
settling pocket
reaction chamber
equipment
smelting technology
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 93101075
Other languages
English (en)
Inventor
高书友
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 93101075 priority Critical patent/CN1088886A/zh
Publication of CN1088886A publication Critical patent/CN1088886A/zh
Pending legal-status Critical Current

Abstract

本发明属于用硫铁矿冶炼硫磺技术领域。利用 在尾气中喷入碱性液体,使冶炼中产生的SO2和 H2S气体发生反应,解决环境污染问题,并提高硫磺 收得率。

Description

本发明属于硫磺冶炼技术领域。
现有硫磺冶炼技术中,大量采用土窑冶炼。由于冶炼过程产生大量的SO2和H2S气体排放,造成了严重的环境污染,炉群周围10公里的地方,寸土不生。同时生产效率低,一般品位16%左右的硫铁矿,吨矿石硫磺所得为4%左右,已有资料报道的“密闭还原净化法”冶炼技术,只是加长了排烟道,虽然比土窑冶炼降低了SO2及H2S排放,但并未从根本解决,而且投资较大。
本发明的目的就是为了克服上述已有技术的不足,提出一种新的炼磺工艺及设备,使SO2、H2S排放完全达到国家标准。硫磺收得率高于已有技术。
本发明的解决方案是:在H2S、SO2排空前,增加一个反应室,反应室中喷入硷性液体,使SO2、H2S在硷性气氛中发生氧化还反应,反应生成的硫在其后的沉降室沉降。
下面结合附图和实施例进一步说明本技术方案。
附图一是工艺流程图。
附图二是反应室、沉降室结构图。
冶炼炉(1)炉内硫铁矿及燃料(例如煤)用常规方式堆装点燃后,产生的H2S、SO2、S(气态)从导磺管(2)进入磺箱(3)。为了使气态S冷却沉降,磺箱(3)设计为多级串联,气态S降温后结晶成固态单质S,沉降在磺箱(3)内,供取出精炼。SO2、H2S经过总烟道(4)进入反应室(5)。反应室(5)的顶部装有若干个喷头(6),硷性液体(例如石灰水)从喷头(6)形成雾状喷出,随着SO2、H2S经过过渡烟道(7)进入沉降室(8)、SO2、H2S在硷性气氛中发生氧化还原反应,生成S和H2O。
S及其它杂质沉降在沉降室(8),定期打开沉降室的密封口取出分离,精炼。
为了使SO2、H2S充分反应,沉降室采取多级串联,每级的烟道口(9)开口位置交错,使SO2、H2S,雾状Ca(OH)充分混合,在平面内形成附图(三)所示运动轨迹,竖直面内形成附图(四)所示运动轨道。
未反应完的残余SO2、H2S,水蒸气经过尾烟道(10)从烟囱(11)排放,Ca(OH)液体从反应室,沉降室底部回收使用。

Claims (4)

1、一种用硫铁矿冶炼硫磺工艺,包括冶炼炉,磺箱、反应室、沉降室,其特征是在反应室喷入雾状硷性液体,使H2S和SO2在硷性气氛中产生氧化还原反应。
2、根据权利要求1所述的磺箱,其特征是采取至少二级以上多级串联。
3、根据权利要求1所述的沉降室,其特征是采取至少二级以上多级串级。
4、根据权利要求1和3所述的沉降室,其特征是每级沉降室烟道口位置上下,左右交义排列。
CN 93101075 1993-01-02 1993-01-02 一种硫磺冶炼工艺和设备 Pending CN1088886A (zh)