CN108724552A - The bonding process of liquid-state silicon gel and stainless steel adapting piece - Google Patents

The bonding process of liquid-state silicon gel and stainless steel adapting piece Download PDF

Info

Publication number
CN108724552A
CN108724552A CN201810418884.0A CN201810418884A CN108724552A CN 108724552 A CN108724552 A CN 108724552A CN 201810418884 A CN201810418884 A CN 201810418884A CN 108724552 A CN108724552 A CN 108724552A
Authority
CN
China
Prior art keywords
stainless steel
adapting piece
steel adapting
liquid
silicon gel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810418884.0A
Other languages
Chinese (zh)
Inventor
周波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Development In Science And Technology Co Ltd Of Suzhou Cathay
Original Assignee
Development In Science And Technology Co Ltd Of Suzhou Cathay
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Development In Science And Technology Co Ltd Of Suzhou Cathay filed Critical Development In Science And Technology Co Ltd Of Suzhou Cathay
Priority to CN201810418884.0A priority Critical patent/CN108724552A/en
Publication of CN108724552A publication Critical patent/CN108724552A/en
Pending legal-status Critical Current

Abstract

The present invention provides the bonding process of liquid-state silicon gel and stainless steel adapting piece, include the following steps:1)Cleaning;2)Baking;3)Gluing;4)Secondary baking;5)Vulcanization;6)Post-cure;7)Deburring;8)Full inspection.The present invention selects suitable glue, and stainless steel adapting piece and liquid-state silicon gel are bonded, pass through sulfidation twice, bonding strength can be increased to maximum, the waterproof seal for increasing connector also greatly reduces product obscission, and the expulsion rate of silica gel is made to drop to 1% by 15%.

Description

The bonding process of liquid-state silicon gel and stainless steel adapting piece
Technical field
The present invention relates to mobile phone connector bonding technology fields, the more particularly to bonding of liquid-state silicon gel and stainless steel adapting piece Technique.
Background technology
Mobile phone connector is that on the outside then gluing passes through liquid-state silicon gel sulfidization molding, liquid-state silicon gel and stainless to stainless steel part The bonding of steel part can play the role of sealing, dustproof and waterproof, so requiring the cementation of junction very high.If connection The cementation insufficient strength at place, just will appear fall off, leak a series of problems, such as, these problems are ten for the use of mobile phone Divide serious.Existing processing technology can not ensure the adhesion strength of stainless steel adapting piece and liquid-state silicon gel so that subsequently make Occur silica gel repeatedly in fall off lower phenomenon, has seriously affected the experience of user.
Invention content
In order to overcome the deficiencies of existing technologies, the present invention provides a kind of bonding work of liquid-state silicon gel and stainless steel adapting piece Skill can avoid the appearance of existing issue by the technique.
To achieve the goals above, the present invention provides following technical scheme:
The bonding process of liquid-state silicon gel and stainless steel adapting piece, includes the following steps:
1)Cleaning:Stainless steel adapting piece is put into alcohol and is cleaned, quantity 1000pcs, the time keeps 2 ~ 5min;Stainless steel is connected The appearance of fitting is dirty to be washed, and generally use directly impregnates and stirs the greasy dirt for making stainless steel adapting piece appearance several times.
2)Baking:By cleaned stainless steel adapting piece be put into temperature be carried out in 105 ± 5 DEG C of oven baking 15 ~ 30min;Alcohol is vapored away by high temperature, subsequent glue-line is made to will not fall off;
3)Gluing:In the stainless steel adapting piece surrounding gluing roasted;The glue is directly to buy, using manually-operated mode Gluing, the glue-line are not generate obscission in order to which stainless steel adapting piece and liquid-state silicon gel to be bonded together;
4)Secondary baking:By the stainless steel adapting piece of coated glue be put into temperature be carried out in 105 ± 5 DEG C of oven baking 30 ± 5min;Glue-line baking is dried;
5)Vulcanization:The stainless steel adapting piece that baking finishes is put into mold, injecting liquid-state silicon gel by the runner of mold will produce Product are sulfided into cavity shape;Make to be enclosed with liquid-state silicon gel on the outside of stainless steel adapting piece by mold and forms fixed shape;
6)Post-cure:The product vulcanizated is put into oven and carries out post-cure, oven temperature is 135 ± 5 DEG C;Revulcanization The intensity for increasing liquid-state silicon gel, makes its vulcanization more thoroughly be unlikely to deform;
7)Deburring:The good product of post-cure is subjected to appearance detection, and is cleared up extra flash by deburring jig; The flash of product is removed by deburring jig;
8)Full inspection:Product after deburring is detected the product machined using microscope detection appearance and size.
Further, the step 5)In curing temperature be 120 ~ 130 DEG C, vulcanization time be 30 seconds.
Further, the step 7)The time of middle post-cure is 30 ± 5min.
Further, the step 1)In alcohol be room temperature.
Advantageous effect caused by the present invention is:Suitable glue is selected, stainless steel adapting piece and liquid-state silicon gel are bonded Get up, by sulfidation twice, adhesion strength can be increased to maximum, increase the waterproof seal of connector, also greatly Ground reduces product obscission, and the expulsion rate of silica gel is made to drop to 1% by 15%.
Specific implementation mode
The preferred embodiments of the present invention will be described in detail below so that advantages and features of the invention can be easier to by It will be appreciated by those skilled in the art that so as to make a clearer definition of the protection scope of the present invention.
Embodiment one:
The bonding process of liquid-state silicon gel and stainless steel adapting piece, includes the following steps:
1)Cleaning:Stainless steel adapting piece is put into alcohol and is impregnated and stir several times, quantity 1000pcs, the time keeps 2min;It will The appearance of stainless steel adapting piece is dirty to be washed;
2)Baking:Cleaned stainless steel adapting piece is put into the oven that temperature is 100 DEG C and carries out baking 30min;Pass through height Temperature vapors away alcohol, and subsequent glue-line is made to will not fall off;
3)Gluing:In the stainless steel adapting piece surrounding gluing roasted;The glue is directly to buy, using manually-operated mode Gluing, the glue-line are not generate obscission in order to which stainless steel adapting piece and liquid-state silicon gel to be bonded together;
4)Secondary baking:The stainless steel adapting piece of coated glue is put into the oven that temperature is 100 DEG C and carries out baking 35min;It will Glue-line baking is dried;
5)Vulcanization:The stainless steel adapting piece that baking finishes is put into mold, injecting liquid-state silicon gel by the runner of mold will produce Product are sulfided into cavity shape, and curing temperature is 120 DEG C, continues 30 seconds;Make to be enclosed with liquid on the outside of stainless steel adapting piece by mold State silica gel simultaneously forms fixed shape;
6)Post-cure:The product vulcanizated is put into oven and carries out post-cure, oven temperature is 130 DEG C, and the time is lasting 35min;Revulcanization increases the intensity of liquid-state silicon gel, its vulcanization is made more thoroughly to be unlikely to deform;
7)Deburring:The good product of post-cure is subjected to appearance detection, and is cleared up extra flash by deburring jig; The flash of product is removed by deburring jig;
8)Full inspection:Product after deburring is detected the product machined using microscope detection appearance and size.
Embodiment two:
The bonding process of liquid-state silicon gel and stainless steel adapting piece, includes the following steps:
1)Cleaning:Stainless steel adapting piece is put into alcohol and is impregnated and stir several times, quantity 1000pcs, the time keeps 5min;It will The appearance of stainless steel adapting piece is dirty to be washed;
2)Baking:Cleaned stainless steel adapting piece is put into the oven that temperature is 110 DEG C and carries out baking 15min;Pass through height Temperature vapors away alcohol, and subsequent glue-line is made to will not fall off;
3)Gluing:In the stainless steel adapting piece surrounding gluing roasted;The glue is directly to buy, using manually-operated mode Gluing, the glue-line are not generate obscission in order to which stainless steel adapting piece and liquid-state silicon gel to be bonded together;
4)Secondary baking:The stainless steel adapting piece of coated glue is put into the oven that temperature is 110 DEG C and carries out baking 25min;It will Glue-line baking is dried;
5)Vulcanization:The stainless steel adapting piece that baking finishes is put into mold, injecting liquid-state silicon gel by the runner of mold will produce Product are sulfided into cavity shape, and curing temperature is 130 DEG C, continues 30 seconds;Make to be enclosed with liquid on the outside of stainless steel adapting piece by mold State silica gel simultaneously forms fixed shape;
6)Post-cure:The product vulcanizated is put into oven and carries out post-cure, oven temperature is 140 DEG C, continues 25min; Revulcanization increases the intensity of liquid-state silicon gel, its vulcanization is made more thoroughly to be unlikely to deform;
7)Deburring:The good product of post-cure is subjected to appearance detection, and is cleared up extra flash by deburring jig; The flash of product is removed by deburring jig;
8)Full inspection:Product after deburring is detected using microscope detection appearance and size to the product machined
Liquid-state silicon gel is bonded on stainless steel adapting piece by using the technique, bonding strength is ensure that, makes falling off for silica gel Rate drops to 1% by 15%.
The above description is merely a specific embodiment, but scope of protection of the present invention is not limited thereto, any Those skilled in the art within the technical scope disclosed by the invention, can without the variation that creative work is expected or It replaces, should be covered by the protection scope of the present invention.Therefore, protection scope of the present invention should be limited with claims Subject to fixed protection domain.

Claims (4)

1. the bonding process of liquid-state silicon gel and stainless steel adapting piece, which is characterized in that include the following steps:
Cleaning:Stainless steel adapting piece is put into alcohol and is cleaned, quantity 1000pcs, the time keeps 2 ~ 5min;
Baking:Cleaned stainless steel adapting piece is put into the oven that temperature is 105 ± 5 DEG C and carries out 15 ~ 30min of baking;
Gluing:In the stainless steel adapting piece surrounding gluing roasted;
Secondary baking:By the stainless steel adapting piece of coated glue be put into temperature be carried out in 105 ± 5 DEG C of oven baking 30 ± 5min;
Vulcanization:The stainless steel adapting piece that baking finishes is put into mold, liquid-state silicon gel is injected by product by the runner of mold It is sulfided into cavity shape;
Post-cure:The product vulcanizated is put into oven and carries out post-cure, oven temperature is 135 ± 5 DEG C;
Deburring:The good product of post-cure is subjected to appearance detection, and is cleared up extra flash by deburring jig;
Full inspection:Product after deburring is using microscope detection appearance and size.
2. the bonding process of liquid-state silicon gel according to claim 1 and stainless steel adapting piece, which is characterized in that the step 5)In curing temperature be 120 ~ 130 DEG C, vulcanization time be 30 seconds.
3. the bonding process of liquid-state silicon gel according to claim 1 and stainless steel adapting piece, which is characterized in that the step 7)The time of middle post-cure is 30 ± 5min.
4. the bonding process of liquid-state silicon gel according to claim 1 and stainless steel adapting piece, which is characterized in that the step 1)In alcohol be room temperature.
CN201810418884.0A 2018-05-04 2018-05-04 The bonding process of liquid-state silicon gel and stainless steel adapting piece Pending CN108724552A (en)