CN108703482A - A kind of preparation method and product of the horn comb with sterilization - Google Patents

A kind of preparation method and product of the horn comb with sterilization Download PDF

Info

Publication number
CN108703482A
CN108703482A CN201810280500.3A CN201810280500A CN108703482A CN 108703482 A CN108703482 A CN 108703482A CN 201810280500 A CN201810280500 A CN 201810280500A CN 108703482 A CN108703482 A CN 108703482A
Authority
CN
China
Prior art keywords
comb
horn
blank
hair
processing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810280500.3A
Other languages
Chinese (zh)
Inventor
陈再伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Renhuai Only Corner Processing Plant
Original Assignee
Renhuai Only Corner Processing Plant
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Renhuai Only Corner Processing Plant filed Critical Renhuai Only Corner Processing Plant
Priority to CN201810280500.3A priority Critical patent/CN108703482A/en
Publication of CN108703482A publication Critical patent/CN108703482A/en
Pending legal-status Critical Current

Abstract

The product prepared the present invention relates to a kind of preparation method of horn comb with sterilization and using this method, the preparation method are included sorting, raw material cleaning, cutting sorting, thermocompression forming, draw sample processing, tooth punching processing and polishing treatment.The horn comb prepared using the method for the invention, long-time service can be dredged through dredging collateral, promote head blood circulation, can efficiently reduce and eliminate alopecia, disconnected hair, dandruff, phenomena such as preventing hair malnutrition and lead to long white hair, yellow hair and alopecia;At the same time it can also effectively kill the various germs adhered on scalp or hair, realize quickly to the disinfection of scalp or hair, ensure the long-term health of people's scalp and hair and salubrious, it is not only with health role, also there is sterilization, meet very much modern Man's Demands.In addition, also having widened the application range of ox horn, its added value can be improved, different consumer demands can be met, be very suitable for promoting and applying.

Description

A kind of preparation method and product of the horn comb with sterilization
Technical field
The invention belongs to the preparing technical fields of horn comb in daily necessities, and in particular to one kind having disinfection The preparation method of the horn comb of effect and the product prepared using this method.
Background technology
Comb is the tool of combing hair, is one of indispensable apparatus in people's daily life, people are made at present There are mainly three types of combs, respectively plastic comb, wood comb and cutin comb.Wherein plastic comb is chemical material heat Die casting is made, and energy consumption is big in process of producing product and generates pollution, and chemical material is in direct contact hair during product use Scalp, and it is easy to produce static electricity, departing from health environment-friendly requirement, meanwhile, in the preparation process of plastic comb, due to chemical substance Easily remain on comb, people cause withered hair, jaundice, scalp itch when combing one's hair, constantly afterwards can be to human body using one section It is harmful.And wood comb can not only play electrostatic, but without health-care effect.And cutin comb is typically all to use horn comb, ox horn Comb is elaborated by hand using traditional technique using ox horn as raw material.Since ox horn itself is a kind of Chinese medicine of preciousness There is material clearing heat and detoxicating, phencyclidine, blood pressure lowering, curing rheumatism to control the medicinal efficacy that stone is led in leaching.
Combed one's hair using natural horn comb, have many health-care effects, can be non-sticky with de-sludging, solution itch without pain, it is gentle and Hair is not hung;Also accelerate scalp blood circulation, strengthen immunity;There is clear hot and cold blood, antipruritic to prevent electrostatic, no simultaneously Alopecia, debris removing hair care, relaxing tendons and activating collaterals, mind-tranquilizing brain-strengthening promote the unique health-care effects such as natural on-off cycles of hair growth.Therefore, it uses sooner or later daily Horn comb is combed one's hair, and can be dredged through dredging collateral, be promoted head blood circulation, can be efficiently reduced and be eliminated alopecia, disconnected hair, dandruff, prevent Only hair malnutrition and phenomena such as lead to long white hair, yellow hair and alopecia.However, after comb uses repeatedly, just have each Kind of microbial pathogens and fungi generate, the propagation and sprawling of these germs will jeopardize scalp, hair, brain and body it is strong Health.And silver is ideal sterilization, antiviral material, has efficient, wide spectrum, safety and without characteristics such as drug resistances.Due to comb with Daily life is closely related, and as people's living standards continue to improve and the continuous of modern aesthetic idea are widened, People expect a kind of not only with health role, and can keep its natural essence, while the also comb with sterilization Son, this by be the current development of Jiao Zhi techniques processing enterprise a direction, the application range of ox horn can be widened in this way, together When can also meet different consumer demands.
Invention content
The technical problem to be solved by the present invention is in view of the deficiencies of the prior art, provide a kind of raw material to be easy to get, prepare Comb it is not only with health role, moreover it is possible to keep the natural essence of original ox horn lines and color, while also there is disinfection to kill The horn comb of bacterium effect, can further widen the application range of ox horn, can meet different consumer demands, specifically A kind of this kind of method of preparation method and utilization of the horn comb with sterilization prepares the horn comb of gained.
In order to solve the above technical problems, the technical solution adopted by the present invention is:A kind of ox horn with sterilization The preparation method of comb, the preparation method comprise the technical steps that:
(1) sorting:It selects shape and thickness is suitable for making the ox horn of comb as raw material;
(2) raw material cleans:Clear water immersion is first used to clean ox horn raw material good selected in step (1), to remove Ox horn raw material is put into clear water reserviors and impregnates 60~90 minutes, impregnated through clear water by stain;Warm water immersion is used to carry out disinfection again Deodorization processing is placed in disinfection deodorization processing in warm water after taking-up, at 40~60 minutes, soaking temperature control existed for soaking time control 40~50 DEG C, most afterwards through naturally cooling to room temperature, and 3~May, naturally dry are placed under normal temperature condition;
(3) sorting is cut:Cutting process will be carried out by ox horn raw material after natural drying in step (2), not by ox horn both ends It is usable to cut away, that is, insignificant problem solid section and the part relatively thin with ox head contact position are cut away, is then stretched to along the insignificant problem The direction of ox head carries out cutting, ox horn is therefrom splitted using longitudinal profile mode, to make slabbing comb blank;
(4) thermocompression forming:The comb blank of gained in step (3) is first subjected to sofening treatment, comb blank is first put into temperature In 120~130 DEG C of conduction oils, to carry out heating and softening processing, the sofening treatment time is 6~8 minutes;It then will be after softening Comb blank, which is put into constant temperature hot-press arrangement, carries out hot-pressing processing, flattens exhibition directly with 15~20 tons of pressure, is kept at least 40 points Clock makes the comb blank of bending flatten, and comb blank is down to normal temperature and pressure after hot-pressing processing, and comb blank is straight through flattening exhibition After sizing, naturally dry;
(5) sample processing is drawn:By in step (4) after thermocompression forming gained comb blank, draw and the matched shape of comb size Shape, and remove extra tailing, the groove formed in the ox horn growth course on comb blank is then polished into light It is sliding, it is spare to obtain comb blank;
(6) tooth punching is handled:The comb blank of gained in step (5) is placed on progress tooth punching processing in gulleting machine, is wanted according to design It asks cutting processing to go out the broach of dissimilar tooth form, forms different broach by the different tooth punchings of comb size, depth, tooth pitch, then The right-angle side rounding of broach is formed into knuckle-tooth structure again;
(7) polishing treatment:After the broach of gained in step (6) is first passed through corase grinding and fine grinding, then it is processed by shot blasting.
Further, the preparation method of a kind of horn comb with sterilization of the present invention, wherein in institute During stating step (4) thermocompression forming, wherein when carrying out hot-pressing processing in constant temperature hot-press arrangement, to the comb after softening Spray contains the solution of sterilization in blank, and the solution is Nano silver solution, wherein a concentration of the 15 of the solution ~20%, for the grain size of silver particles between 80~100 nanometers, solution spray amount is 3~5 times of comb billet weight;In comb In blank flattening process, by spray Nano silver solution, make in the comb blank after silver particles fully penetrated to softening.
Further, the preparation method of a kind of horn comb with sterilization of the present invention, wherein in institute During stating step (7) polishing treatment, the corase grinding is polished using the sand paper of 200~300 mesh, and fine grinding uses 600~800 purposes Sand paper is polished, and the polishing treatment is processed by shot blasting using polishing machine, is applied on polishing wheel with antiscuffing paste, to by essence Comb after mill carries out last polishing treatment using antiscuffing paste.
The present invention also provides a kind of horn combs with sterilization prepared according to the above method.
Using a kind of preparation method of the horn comb with sterilization of the present invention, with prior art phase Than advantage is:By being carried out after cleaning twice to selected ox horn raw material, and 3 are placed under normal temperature condition After~May, then carry out subsequent processing, in this way can guarantee the horn comb for preparing have it is indeformable, do not crack and not broken teeth Advantage.Meanwhile when carrying out hot-pressing processing in constant temperature hot-press arrangement, into the comb blank after softening, spray nano silver is molten Liquid can make by spray Nano silver solution in the comb blank after silver particles fully penetrated to softening.Using side of the present invention Horn comb prepared by method, long-time service can be dredged through dredging collateral, promote head blood circulation, can be efficiently reduced and be eliminated alopecia, break Hair, dandruff, phenomena such as preventing hair malnutrition and lead to long white hair, yellow hair and alopecia;Meanwhile when broach and scalp or head During hair contact, the various germs adhered on scalp or hair can also be fast and effeciently killed, are realized quickly to scalp Or the disinfection of hair, it ensure that the long-term health of people's scalp and hair and salubrious, it is not only with health role, also have Sterilization meets modern Man's Demands very much.In addition, also having widened the application range of ox horn, its added value can be improved, Different consumer demands can be met, be very suitable for promoting and applying.
Specific implementation mode
In order to more fully explain the implementation of the present invention, further illustrated the present invention below in conjunction with specific embodiment.Institute It gives an actual example and is served only for explaining the present invention, rather than limit the scope of the present invention.
Embodiment 1:
A kind of preparation method of the horn comb with sterilization, the preparation method comprise the technical steps that:
(1) sorting:It selects shape and thickness is suitable for making the ox horn of comb as raw material;
(2) raw material cleans:Clear water immersion is first used to clean ox horn raw material good selected in step (1), to remove Ox horn raw material is put into clear water reserviors and impregnates 60~75 minutes, impregnated through clear water by stain;Warm water immersion is used to carry out disinfection again Deodorization processing is placed in disinfection deodorization processing in warm water after taking-up, at 40~50 minutes, soaking temperature control existed for soaking time control 40~50 DEG C, most afterwards through naturally cooling to room temperature, and after placing March under normal temperature condition, through naturally dry;
(3) sorting is cut:Cutting process will be carried out by ox horn raw material after natural drying in step (2), not by ox horn both ends It is usable to cut away, that is, insignificant problem solid section and the part relatively thin with ox head contact position are cut away, is then stretched to along the insignificant problem The direction of ox head carries out cutting, ox horn is therefrom splitted using longitudinal profile mode, to make slabbing comb blank;
(4) thermocompression forming:The comb blank of gained in step (3) is first subjected to sofening treatment, comb blank is first put into temperature In 120~125 DEG C of conduction oils, to carry out heating and softening processing, the sofening treatment time is 7~8 minutes;It then will be after softening Comb blank, which is put into constant temperature hot-press arrangement, carries out hot-pressing processing, flattens exhibition directly with 15 tons of pressure, is kept at least 40 minutes, made The comb blank of bending flattens, and comb blank is down to normal temperature and pressure after hot-pressing processing, and comb blank opens up straight sizing through flattening Afterwards, naturally dry;When carrying out hot-pressing processing wherein in constant temperature hot-press arrangement, sprayed into the comb blank after softening The solution containing sterilization is noted, the solution is Nano silver solution, wherein a concentration of the 15% of the solution, silver particles Grain size between 80~90 nanometers, solution spray amount is 3 times of comb billet weight;In comb blank flattening process, By spray Nano silver solution, make in the comb blank after silver particles fully penetrated to softening;
(5) sample processing is drawn:By in step (4) after thermocompression forming gained comb blank, draw and the matched shape of comb size Shape, and remove extra tailing, the groove formed in the ox horn growth course on comb blank is then polished into light It is sliding, it is spare to obtain comb blank;
(6) tooth punching is handled:The comb blank of gained in step (5) is placed on progress tooth punching processing in gulleting machine, is wanted according to design It asks cutting processing to go out the broach of dissimilar tooth form, forms different broach by the different tooth punchings of comb size, depth, tooth pitch, then The right-angle side rounding of broach is formed into knuckle-tooth structure again;
(7) polishing treatment:After the broach of gained in step (6) is first passed through corase grinding and fine grinding, then it is processed by shot blasting.It is described thick Mill is polished using the sand paper of 200 mesh, and fine grinding is polished using the sand paper of 600 mesh, and the polishing treatment is polished using polishing machine Processing, is applied to antiscuffing paste on polishing wheel, and last polishing treatment is carried out using antiscuffing paste to the comb after fine grinding.
Embodiment 2:
A kind of preparation method of the horn comb with sterilization, the preparation method comprise the technical steps that:
(1) sorting:It selects shape and thickness is suitable for making the ox horn of comb as raw material;
(2) raw material cleans:Clear water immersion is first used to clean ox horn raw material good selected in step (1), to remove Ox horn raw material is put into clear water reserviors and impregnates 70~80 minutes, impregnated through clear water by stain;Warm water immersion is used to carry out disinfection again Deodorization processing is placed in disinfection deodorization processing in warm water after taking-up, at 45~55 minutes, soaking temperature control existed for soaking time control 43~48 DEG C, most afterwards through naturally cooling to room temperature, and after placing April under normal temperature condition, through naturally dry;
(3) sorting is cut:Cutting process will be carried out by ox horn raw material after natural drying in step (2), not by ox horn both ends It is usable to cut away, that is, insignificant problem solid section and the part relatively thin with ox head contact position are cut away, is then stretched to along the insignificant problem The direction of ox head carries out cutting, ox horn is therefrom splitted using longitudinal profile mode, to make slabbing comb blank;
(4) thermocompression forming:The comb blank of gained in step (3) is first subjected to sofening treatment, comb blank is first put into temperature In 120~130 DEG C of conduction oils, to carry out heating and softening processing, the sofening treatment time is 6~7 minutes;It then will be after softening Comb blank, which is put into constant temperature hot-press arrangement, carries out hot-pressing processing, flattens exhibition directly with 18 tons of pressure, is kept at least 40 minutes, made The comb blank of bending flattens, and comb blank is down to normal temperature and pressure after hot-pressing processing, and comb blank opens up straight sizing through flattening Afterwards, naturally dry;When carrying out hot-pressing processing wherein in constant temperature hot-press arrangement, sprayed into the comb blank after softening The solution containing sterilization is noted, the solution is Nano silver solution, wherein a concentration of the 18% of the solution, silver particles Grain size between 85~95 nanometers, solution spray amount is 4 times of comb billet weight;In comb blank flattening process, By spray Nano silver solution, make in the comb blank after silver particles fully penetrated to softening;
(5) sample processing is drawn:By in step (4) after thermocompression forming gained comb blank, draw and the matched shape of comb size Shape, and remove extra tailing, the groove formed in the ox horn growth course on comb blank is then polished into light It is sliding, it is spare to obtain comb blank;
(6) tooth punching is handled:The comb blank of gained in step (5) is placed on progress tooth punching processing in gulleting machine, is wanted according to design It asks cutting processing to go out the broach of dissimilar tooth form, forms different broach by the different tooth punchings of comb size, depth, tooth pitch, then The right-angle side rounding of broach is formed into knuckle-tooth structure again;
(7) polishing treatment:After the broach of gained in step (6) is first passed through corase grinding and fine grinding, then it is processed by shot blasting, it is described thick Mill is polished using the sand paper of 300 mesh, and fine grinding is polished using the sand paper of 800 mesh, and the polishing treatment is polished using polishing machine Processing, is applied to antiscuffing paste on polishing wheel, and last polishing treatment is carried out using antiscuffing paste to the comb after fine grinding.
Embodiment 3:
A kind of preparation method of the horn comb with sterilization, the preparation method comprise the technical steps that:
(1) sorting:It selects shape and thickness is suitable for making the ox horn of comb as raw material;
(2) raw material cleans:Clear water immersion is first used to clean ox horn raw material good selected in step (1), to remove Ox horn raw material is put into clear water reserviors and impregnates 80~90 minutes, impregnated through clear water by stain;Warm water immersion is used to carry out disinfection again Deodorization processing is placed in disinfection deodorization processing in warm water after taking-up, at 50~60 minutes, soaking temperature control existed for soaking time control 45~50 DEG C, most afterwards through naturally cooling to room temperature, and after placing May under normal temperature condition, through naturally dry;
(3) sorting is cut:Cutting process will be carried out by ox horn raw material after natural drying in step (2), not by ox horn both ends It is usable to cut away, that is, insignificant problem solid section and the part relatively thin with ox head contact position are cut away, is then stretched to along the insignificant problem The direction of ox head carries out cutting, ox horn is therefrom splitted using longitudinal profile mode, to make slabbing comb blank;
(4) thermocompression forming:The comb blank of gained in step (3) is first subjected to sofening treatment, comb blank is first put into temperature In 120~130 DEG C of conduction oils, to carry out heating and softening processing, the sofening treatment time is 7~8 minutes;It then will be after softening Comb blank, which is put into constant temperature hot-press arrangement, carries out hot-pressing processing, flattens exhibition directly with 20 tons of pressure, is kept at least 40 minutes, made The comb blank of bending flattens, and comb blank is down to normal temperature and pressure after hot-pressing processing, and comb blank opens up straight sizing through flattening Afterwards, naturally dry;When carrying out hot-pressing processing wherein in constant temperature hot-press arrangement, sprayed into the comb blank after softening The solution containing sterilization is noted, the solution is Nano silver solution, wherein a concentration of the 20% of the solution, silver particles Grain size between 90~100 nanometers, solution spray amount is 5 times of comb billet weight;In comb blank flattening process, By spray Nano silver solution, make in the comb blank after silver particles fully penetrated to softening;
(5) sample processing is drawn:By in step (4) after thermocompression forming gained comb blank, draw and the matched shape of comb size Shape, and remove extra tailing, the groove formed in the ox horn growth course on comb blank is then polished into light It is sliding, it is spare to obtain comb blank;
(6) tooth punching is handled:The comb blank of gained in step (5) is placed on progress tooth punching processing in gulleting machine, is wanted according to design It asks cutting processing to go out the broach of dissimilar tooth form, forms different broach by the different tooth punchings of comb size, depth, tooth pitch, then The right-angle side rounding of broach is formed into knuckle-tooth structure again;
(7) polishing treatment:After the broach of gained in step (6) is first passed through corase grinding and fine grinding, then it is processed by shot blasting, it is described thick Mill is polished using the sand paper of 200 mesh, and fine grinding is polished using the sand paper of 800 mesh, and the polishing treatment is polished using polishing machine Processing, is applied to antiscuffing paste on polishing wheel, and last polishing treatment is carried out using antiscuffing paste to the comb after fine grinding.
Example the above is only the implementation of the present invention is not intended to limit the scope of the invention, every to utilize this hair Equivalent structure or equivalent flow shift made by bright description is applied directly or indirectly in other relevant technology necks Domain is included within the scope of the present invention.

Claims (4)

1. a kind of preparation method of the horn comb with sterilization, it is characterised in that:The preparation method includes as follows Processing step:
(1) sorting:It selects shape and thickness is suitable for making the ox horn of comb as raw material;
(2) raw material cleans:Clear water immersion is first used to clean ox horn raw material good selected in step (1), to remove Ox horn raw material is put into clear water reserviors and impregnates 60~90 minutes, impregnated through clear water by stain;Warm water immersion is used to carry out disinfection again Deodorization processing is placed in disinfection deodorization processing in warm water after taking-up, at 40~60 minutes, soaking temperature control existed for soaking time control 40~50 DEG C, most afterwards through naturally cooling to room temperature, and 3~May, naturally dry are placed under normal temperature condition;
(3) sorting is cut:Cutting process will be carried out by ox horn raw material after natural drying in step (2), not by ox horn both ends It is usable to cut away, that is, insignificant problem solid section and the part relatively thin with ox head contact position are cut away, is then stretched to along the insignificant problem The direction of ox head carries out cutting, ox horn is therefrom splitted using longitudinal profile mode, to make slabbing comb blank;
(4) thermocompression forming:The comb blank of gained in step (3) is first subjected to sofening treatment, comb blank is first put into temperature In 120~130 DEG C of conduction oils, to carry out heating and softening processing, the sofening treatment time is 6~8 minutes;It then will be after softening Comb blank, which is put into constant temperature hot-press arrangement, carries out hot-pressing processing, flattens exhibition directly with 15~20 tons of pressure, is kept at least 40 points Clock makes the comb blank of bending flatten, and comb blank is down to normal temperature and pressure after hot-pressing processing, and comb blank is straight through flattening exhibition After sizing, naturally dry;
(5) sample processing is drawn:By in step (4) after thermocompression forming gained comb blank, draw and the matched shape of comb size Shape, and remove extra tailing, the groove formed in the ox horn growth course on comb blank is then polished into light It is sliding, it is spare to obtain comb blank;
(6) tooth punching is handled:The comb blank of gained in step (5) is placed on progress tooth punching processing in gulleting machine, is wanted according to design It asks cutting processing to go out the broach of dissimilar tooth form, forms different broach by the different tooth punchings of comb size, depth, tooth pitch, then The right-angle side rounding of broach is formed into knuckle-tooth structure again;
(7) polishing treatment:After the broach of gained in step (6) is first passed through corase grinding and fine grinding, then it is processed by shot blasting.
2. a kind of preparation method of horn comb with sterilization according to claim 1, it is characterised in that: During step (4) thermocompression forming, wherein when carrying out hot-pressing processing in constant temperature hot-press arrangement, to the comb after softening Spray contains the solution of sterilization in sub- blank, and the solution is Nano silver solution, wherein the solution is a concentration of 15~20%, for the grain size of silver particles between 80~100 nanometers, solution spray amount is 3~5 times of comb billet weight;It is combing In sub- blank flattening process, by spray Nano silver solution, make in the comb blank after silver particles fully penetrated to softening.
3. a kind of preparation method of horn comb with sterilization according to claim 1, it is characterised in that: During step (7) polishing treatment, the corase grinding is polished using the sand paper of 200~300 mesh, and fine grinding uses 600~800 mesh Sand paper polishing, the polishing treatment is processed by shot blasting using polishing machine, is applied on polishing wheel with antiscuffing paste, to passing through Comb after fine grinding carries out last polishing treatment using antiscuffing paste.
4. the horn comb with sterilization prepared according to any one of claims 1 to 3 the method.
CN201810280500.3A 2018-04-02 2018-04-02 A kind of preparation method and product of the horn comb with sterilization Pending CN108703482A (en)