CN108593891A - The quick method of indirect determination moisture content in a kind of construction of airfield runway high roadbed - Google Patents

The quick method of indirect determination moisture content in a kind of construction of airfield runway high roadbed Download PDF

Info

Publication number
CN108593891A
CN108593891A CN201810540193.8A CN201810540193A CN108593891A CN 108593891 A CN108593891 A CN 108593891A CN 201810540193 A CN201810540193 A CN 201810540193A CN 108593891 A CN108593891 A CN 108593891A
Authority
CN
China
Prior art keywords
moisture content
filling body
water
waddy
construction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810540193.8A
Other languages
Chinese (zh)
Inventor
张伟
杨聪
鲁丙奎
刘崴
廖红玉
刘明周
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China First Metallurgical Group Co Ltd
Original Assignee
China First Metallurgical Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China First Metallurgical Group Co Ltd filed Critical China First Metallurgical Group Co Ltd
Priority to CN201810540193.8A priority Critical patent/CN108593891A/en
Publication of CN108593891A publication Critical patent/CN108593891A/en
Pending legal-status Critical Current

Abstract

A kind of method of quick indirect determination moisture content in constructing the invention discloses airfield runway high roadbed, including:S1, airfield runway high roadbed construction in, in filling body bury more waddys, waddy top is waiting for exposing certain length above filling body;S2, filling body progress filling body making is treated, Wood moisture detector is set on the top of waddy, passes through the aqueous rate score that Wood moisture detector measures timber;The soil moisture content of filling body is calculated;S3, the natural moisture content for measuring various fillers in high roadbed construction, calculate the water ultimately joined, embankment construction are made to reach optimum moisture content;S4, water is ultimately joined according to what is be calculated, the mode for adding water or being exposed to the sun is taken to filling body, adjusts soil moisture content, reaches optimum moisture content;S5, filling body is rolled, and measures the moisture content after rolling, ensure that it reaches optimum moisture content.The present invention is convenient and efficient, has saved the duration, ensure that the construction quality of airfield runway.

Description

The quick method of indirect determination moisture content in a kind of construction of airfield runway high roadbed
Technical field
The present invention relates in civil airport engineering high roadbed construction field more particularly to a kind of construction of airfield runway high roadbed The method of quick indirect determination moisture content.
Background technology
Traditional measurement of water-content coefficient method includes alcohol combustion method, oven drying method.
Alcohol combustion method --- burnt using alcohol in pedotheque the heat released, keeps soil water evaporation dry It is dry, by the difference for front and back quality of burning, calculate the percentage of soil moisture content.
Oven drying method --- the most classical and accurate method, by soil, drying to constant weight at 105~110 DEG C, in soil Various moisture can volatilize away, can directly measure moisture.
But above-mentioned construction method has the shortcomings that respective, alcohol combustion method can take away the dry of sample in the high-temp combustion stage Substance so that metric results are inaccurate, and every part of sample need to do 3 groups of experiments, and experiment takes 30 minutes, and the time is longer.
Although oven drying method is accurate, the test period grows (for 24 hours), and feedback result is slow, seriously affects the construction period.
Above method in the prior art has some limitations or measuring accuracy is relatively low or back-to-back testing knot The fruit time is longer, it is difficult to be suitable for, construction period tight application scenarios high for this required precision of airfield runway.
Invention content
The technical problem to be solved in the present invention is for the defects in the prior art, to provide a kind of airfield runway high roadbed The method of quick indirect determination moisture content in construction.
The technical solution adopted by the present invention to solve the technical problems is:
The present invention provides in a kind of construction of airfield runway high roadbed that quickly the method for indirect determination moisture content, this method include Following steps:
S1, airfield runway high roadbed construction in, high roadbed construction filling body include bottom filling body, Yi Jiyi Filling body is waited for above filling body, more waddys are buried in filling body, and waddy top is waiting for exposing centainly above filling body Length;
It after the completion of S2, waddy are embedded, treat filling body and carries out filling body making, after the completion of making, set on the top of waddy Wood moisture detector is set, the aqueous rate score of timber is measured by Wood moisture detector;And according to moisture content and soil The soil moisture content of filling body is calculated in conversion formula between earth moisture content;
S3, the natural moisture content for measuring various fillers in high roadbed construction, pass through Changes in weather situation, the water absorption of bottom And the windage of filling body moisture when filling that paves calculates the water ultimately joined, and embankment construction is made to reach best aqueous Rate;
S4, water is ultimately joined according to what is be calculated, the mode for adding water or being exposed to the sun is taken to filling body, adjusted soil and contain Water rate, reaches optimum moisture content;
S5, filling body is rolled, and measures the moisture content after rolling, ensure that it reaches optimum moisture content.
Further, the specific method of step S1 of the invention is:
Crushing processing is carried out to construction area, it is 1m that thickness is filled in setting, is layouted according to the grid of 10m*10m, The waddy of 1.2m long, diameter 3cm are inserted into the point laid, lower layer's soil body depth that waddy is squeezed into filling body is 0.1m fills empty paving layer thickness control in 1m, and it is 0.1m that waddy, which is exposed at and fills the length of empty laying or more,.
Further, the specific method of step S2 of the invention is:
By waddy fill the control of empty overlay thickness 1m, and carry out making, after making is completed 2 hours, starts to survey Determine the moisture content that waddy is close to Tu Mianchu, a waddy measures 3 aqueous rate scores, minimum to ensure 30% sampling rate, and takes Sample quantity is no less than 3 waddys.
Further, if the moisture content of waddy is unknown in step S2 of the invention, test is determined by the following method The gear of moisture content:
The wood sample that moisture content is average is taken, be divided into 1-4 grades with Wood moisture detector measures moisture content respectively, and each Shelves measured value is recorded, and the average value of each shelves measured value is taken;Wood sample is sent into baking oven, is contained by oven method measurement Water rate;Then it makes comparisons with 4 cell means, it is corresponding with the immediate numerical value of moisture content that oven method measures in being averaged Gear, subsequent measurements are secured to this gear.
Further, the conversion formula in step S2 of the invention between moisture content and soil moisture content is:
The moisture content of soil=Wood moisture detector measured value+(temperature, which corresponds to increased moisture content+humidity and corresponds to, to be increased Moisture content)/2.
Further, the method tool of the natural moisture content of various fillers in high roadbed construction is measured in step S3 of the invention Body is:
Moisture content W%=(M1+M2+M3) × 100/M when the earthwork paves;
Quality × natural moisture content of M1-raw material;
M2-reaches the water M2=M × Wa%-M1 being added when optimum moisture content;
The optimum moisture content of Wa-mixture;
The lost quality of moisture in M3-construction transport, paving process;
The gross mass of M-mixture.
Further, the method for ultimately joining water is calculated in step S4 of the invention is specially:
Increase and decrease water content=mixture gathers materials natural aqueous quality+moisture loss quality containing water quality-
Relative difference of the moisture content apart from optimum moisture content is calculated according to above-mentioned formula, takes the side for adding water or being exposed to the sun Formula carries out impact-rolling again after adjusting soil moisture content.
The beneficial effect comprise that:Quick indirect determination moisture content in the airfield runway high roadbed construction of the present invention Method, 1, Wood moisture detector it is cheap, it is easy to carry, be suitable for fast-field evaluation timber moisture content.2, lead to It crosses timber and is inserted into the soil body, measure moisture content indirect determination and go out soil moisture content.3, waddy can be effectively played as mark post Control the effect of filling body virtual resurfacing thickness.4, waddy is easy to get and cheap, and cost is small, pollution-free to be influenced on the quality of filling body It is negligible.5, result is fed back at once, can quickly be measured soil moisture content according to relational graph, be saved test period, accelerate Duration improves work efficiency.
Description of the drawings
Present invention will be further explained below with reference to the attached drawings and examples, in attached drawing:
Fig. 1 is the structural schematic diagram of the embodiment of the present invention;
Fig. 2 is the increased moisture content graph of relation of temperature waddy opposite with soil of the embodiment of the present invention;
Fig. 3 is the increased moisture content graph of relation of humidity waddy opposite with soil of the embodiment of the present invention.
Specific implementation mode
In order to make the purpose , technical scheme and advantage of the present invention be clearer, with reference to the accompanying drawings and embodiments, right The present invention is further elaborated.It should be appreciated that described herein, specific examples are only used to explain the present invention, not For limiting the present invention.
Quickly the method for indirect determination moisture content includes following step in the airfield runway high roadbed construction of the embodiment of the present invention Suddenly:
The first step:Embedded waddy is in filling body;
Thickness 1m is filled in crushing region, is layouted according to the grid of 10m*10m, by 1.2m long, the wood of diameter 3cm Rod is inserted into the point laid, and squeezes into lower layer soil body 0.1m, fills empty paving layer thickness control in 1m, exposed 0.1m.
Second step:Filling body making measures moisture content;
Virtual resurfacing thickness (1m) is carried out by waddy to control, making is completed, and starts to measure (waddy is close to Tu Mianchu) after 2 hours Moisture content, a waddy measure 3 aqueous rate scores, at least ensure 30% sampling rate, and no less than 3.
The operating procedure of Wood moisture detector is:
1, battery is loaded onto, " HoLD " key is pressed and is once switched on.
2, it after being switched on, presses " ENTER " key and seeds may be selected, share 4 gear seeds and may be selected.In the light of actual conditions select here It is measured on 2 gears.When measurement, two probes will be inserted into seeds simultaneously.
3, " ENTER " key lockable Wood moisture reading is pressed, while having " HOLD " display in LCD screen, then by then releasing Locking.
4, long-press " HOLD " key will shutdown after 2 seconds.
5, it presses " SET " key, opens backlight, then by then closing backlight;Long-press " SET " key 2S, MAX start to flicker, indicate into Enter parameter setting state, flicker display will be recycled successively by pressing " ENTER " key again at this time:MAX- Wood moistures currently read-DEG C- ℉.Finally press the determination of " SET " key.(1) when MAX flickers, " SET " key is pressed, Wood moisture reading is the maximum value measured; (2) when Wood moisture, which is read, to be flickered, press " SET " key, Wood moisture reading is the current value that measures, (3) when DEG C flickering, It presses " SET ", air themperature unit is selected as degree Celsius;(4) press " SET " key air themperature unit and are selected as China when ℉ flickers Family name's degree;
6, in 2 minutes, if without any button operation and unmeasured Wood moisture, by automatic shutdown.
Determine gear:
If Wood moisture to be measured is unknown, gear can be determined by the following method:
The average wood sample of water intaking point first, measures moisture for 1-4 grades, and each shelves measured value respectively with instrument It records.Sample is immediately sent into baking oven, moisture content is measured by oven method.Then compared with 4 cell means, which The numerical value that gear measures is close, measures later and is secured to this gear.
The moisture content of timber is not also real soil moisture content, it has relationship with Atmosphere temp.and RH, and intermediate there are one Fixed transformational relation, the data measured with moisture detector during being filled according to airport test section earthwork early period are dried with laboratory The data (3000 groups) that case measures are compared, and obtain the curve graph such as Fig. 2 and Fig. 3.
The moisture content of soil=Wood moisture detector+【Increased moisture content (temperature)+increased moisture content (humidity)】/ 2, it is illustrated that on other humidity for not marking, the moisture content value added under temperature conditions uses interpolation method value.
Third walks:The water increased or decreased needed for calculating
The composition of the water content of filling material
In Aerodrome construction, the natural moisture content of various fillers is measured first, is determined and is reached addition needed for optimum moisture content Water, while the windage of filling body moisture determines when being filled by Changes in weather situation, next layer of water absorption and paving The water ultimately joined, the final water content determined before rolling.Water content when only rolling could be reached close to optimum moisture content To best rolling effect.
To sum up analysis is drawn a conclusion:
Water content W%=(M1+M2+M3) × 100/M when the earthwork paves;
Quality × natural moisture content of M1-raw material;
M2-reaches the water M2=M × Wa%-M1 being added when optimum moisture content;
The optimum moisture content of Wa-mixture;
The lost quality (empirically determined according to test section) of moisture in M3-construction transport, paving process;
The gross mass of M-mixture.
4th step:Moisture increases or decreases
Increase and decrease water content=mixture gathers materials natural aqueous quality+moisture loss quality (experience) containing water quality-.According to upper Relative difference of the moisture content apart from optimum moisture content obtained by formula is stated, after taking the mode for adding water to be exposed to the sun to adjust soil moisture content again Carry out impact-rolling.
5th step:Moisture content and compactness are measured after rolling
The mixture moisture of the Accurate Determining of the representative natural moisture content to gather materials and links of constructing scatters and disappears The estimation of amount is to control the key link of water content.Moisture content is surveyed after rolling calculates compactness in order to save test period acceleration Upper layer filling body fills.
The present invention measures the moisture content of filling body using the waddy being inserted into filling body plus Wood moisture detector, than existing The faster convenience of method of field alcohol combustion method and laboratory's baking oven drying, and waddy can be used as the mark that thickness is filled in control Bar has saved the duration, ensure that quality.
It should be understood that for those of ordinary skills, it can be modified or changed according to the above description, And all these modifications and variations should all belong to the protection domain of appended claims of the present invention.

Claims (7)

1. the quick method of indirect determination moisture content in a kind of construction of airfield runway high roadbed, which is characterized in that this method includes Following steps:
S1, in the construction of airfield runway high roadbed, the filling body of high roadbed construction includes the filling body of bottom, and has filled Filling body is waited for above body, more waddys is buried in filling body, waddy top is waiting for exposing certain length above filling body;
It after the completion of S2, waddy are embedded, treat filling body and carries out filling body making, after the completion of making, wood is set on the top of waddy Material moisture detector measures the aqueous rate score of timber by Wood moisture detector;And contained according to moisture content and soil The soil moisture content of filling body is calculated in conversion formula between water rate;
S3, measure high roadbed construction in various fillers natural moisture content, by Changes in weather situation, the water absorption of bottom and The windage of filling body moisture when filling that paves calculates the water ultimately joined, and embankment construction is made to reach optimum moisture content;
S4, water is ultimately joined according to what is be calculated, the mode for adding water or being exposed to the sun is taken to filling body, adjusts soil water-containing Rate reaches optimum moisture content;
S5, filling body is rolled, and measures the moisture content after rolling, ensure that it reaches optimum moisture content.
2. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 1 It is, the specific method of step S1 is:
Crushing processing is carried out to construction area, it is 1m that thickness is filled in setting, is layouted according to the grid of 10m*10m, will The waddy of 1.2m long, diameter 3cm are inserted into the point laid, and it is 0.1m that waddy, which squeezes into lower layer's soil body depth in filling body, Empty paving layer thickness control is filled in 1m, it is 0.1m that waddy, which is exposed at and fills the length of empty laying or more,.
3. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 2 It is, the specific method of step S2 is:
By waddy fill the control of empty overlay thickness 1m, and carry out making, after making is completed 2 hours, starts to measure wood Rod is close to the moisture content of Tu Mianchu, and a waddy measures 3 aqueous rate scores, minimum to ensure 30% sampling rate, and samples number Amount is no less than 3 waddys.
4. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 1 It is, if the moisture content of waddy is unknown in step S2, determines the gear of test moisture content by the following method:
The wood sample that moisture content is average is taken, be divided into 1-4 grades with Wood moisture detector measures moisture content respectively, and each shelves are surveyed Definite value is recorded, and the average value of each shelves measured value is taken;Wood sample is sent into baking oven, is measured by oven method aqueous Rate;Then it makes comparisons with 4 cell means, it is corresponding with the immediate numerical value of moisture content that oven method measures in being averaged Gear, subsequent measurements are secured to this gear.
5. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 1 It is, the conversion formula in step S2 between moisture content and soil moisture content is:
The moisture content of soil=Wood moisture detector measured value+(temperature corresponds to increased moisture content+humidity and corresponds to increased contain Water rate)/2.
6. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 1 It is, the method that the natural moisture content of various fillers in high roadbed construction is measured in step S3 is specially:
Moisture content W%=(M1+M2+M3) × 100/M when the earthwork paves;
Quality × natural moisture content of M1-raw material;
M2-reaches the water M2=M × Wa%-M1 being added when optimum moisture content;
The optimum moisture content of Wa-mixture;
The lost quality of moisture in M3-construction transport, paving process;
The gross mass of M-mixture.
7. the method for quick indirect determination moisture content, feature in airfield runway high roadbed construction according to claim 1 It is, the method that the water finally increased or decreased is calculated in step S4 is specially:
Increase and decrease water content=mixture gathers materials natural aqueous quality+moisture loss quality containing water quality-
Relative difference of the moisture content apart from optimum moisture content is calculated according to above-mentioned formula, takes the mode tune for adding water or being exposed to the sun Impact-rolling is carried out again after section soil moisture content.
CN201810540193.8A 2018-05-30 2018-05-30 The quick method of indirect determination moisture content in a kind of construction of airfield runway high roadbed Pending CN108593891A (en)