CN108454055A - A kind of mold improving PVC spool production stabilities - Google Patents

A kind of mold improving PVC spool production stabilities Download PDF

Info

Publication number
CN108454055A
CN108454055A CN201810575268.6A CN201810575268A CN108454055A CN 108454055 A CN108454055 A CN 108454055A CN 201810575268 A CN201810575268 A CN 201810575268A CN 108454055 A CN108454055 A CN 108454055A
Authority
CN
China
Prior art keywords
mold
die holder
connect
spreader
pvc spool
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810575268.6A
Other languages
Chinese (zh)
Inventor
邓添华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANJING LIANSU TECHNOLOGY INDUSTRIAL Co Ltd
Original Assignee
NANJING LIANSU TECHNOLOGY INDUSTRIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANJING LIANSU TECHNOLOGY INDUSTRIAL Co Ltd filed Critical NANJING LIANSU TECHNOLOGY INDUSTRIAL Co Ltd
Priority to CN201810575268.6A priority Critical patent/CN108454055A/en
Publication of CN108454055A publication Critical patent/CN108454055A/en
Pending legal-status Critical Current

Abstract

The present invention relates to PVC spool production moulds, more specifically, it is related to a kind of mold improving PVC spool production stabilities, include the linkage section of solution, linkage section is connect with shunting die holder, and shunting die holder is combined with several extrusion dies, extrusion die is equipped with die holder, extrusion die is equipped with the spreader of the taper coordinated with die holder, and spreader cooperatively forms distributary division with die holder, and distributary division is gradually tapered up along melt flow direction;Spreader by equipped with flat segments connect with mold core, mold core with shrink set cooperatively forms contraction flow region, contraction flow region is gradually tapered up along melt flow direction;Mold core cooperatively forms setting section with mouth mold, and setting section is equipped with the tapered portion gradually tapered up and flat part, the outlet end of setting section are connect with coolant jacket.Mould flow passage structure design with optimization, effectively reduces solution die swelling power, comprehensive to promote production stability.

Description

A kind of mold improving PVC spool production stabilities
Technical field
The present invention relates to PVC spool production moulds, more particularly, to a kind of mould improving PVC spool production stabilities Tool.
Background technology
Production spool generally goes out four production model using one in the market, to reach higher production efficiency, but therewith Come, some problems also occurs in production in product, and most distinct issues are exactly:Tubing production stability difference, high rejection rate , production cost is increased, is unfavorable for the raising of production stability and reduces product rejection rate.
Invention content
The present invention is at least one defect overcome described in the above-mentioned prior art, and it is steady to provide a kind of raising PVC spools production Qualitative mold has the mould flow passage structure design of optimization, effective reduction solution die swelling power comprehensive to promote production stabilization Property.
In order to solve the above technical problems, the technical solution adopted by the present invention is:It is a kind of to improve PVC spool production stabilities Mold, wherein include the linkage section of solution, linkage section is connect with shunting die holder, and shunting die holder is combined with several extrusion dies Tool, extrusion die are equipped with die holder, and extrusion die is equipped with the spreader of the taper coordinated with die holder, and spreader is cooperatively formed with die holder Distributary division, distributary division are gradually tapered up along melt flow direction;Spreader by equipped with flat segments connect with mold core, mold core with receive Contracting set cooperatively forms contraction flow region, and contraction flow region is gradually tapered up along melt flow direction;Mold core cooperatively forms setting section with mouth mold, shapes Portion is equipped with the tapered portion gradually tapered up and flat part, the outlet end of setting section are connect with coolant jacket.
It in the present invention, is connect with shunting die holder by linkage section, solution is imported shunting die holder by linkage section, and shunting die holder connects Several extrusion dies are connected to, solution is imported several extrusion dies by the effect by shunting die holder.Extrusion die be equipped with The spreader of the taper of die holder cooperation, the distributary division that spreader is cooperatively formed with die holder are gradually tapered up along melt flow direction.Point Stream shuttle by equipped with flat segments connect with mold core, solution is flowed by flat segments.Mold core cooperatively forms contraction flow region with set is shunk, Contraction flow region is gradually tapered up along melt flow direction, by the contraction of solution, is reduced the cross-sectional volume of solution, is formed simultaneously certain It stretches, by solution appearance and size gradually by greatly as small transformation so that it is strong to promote solution for the further Dispersion Fusion of molecule between solution Degree.Setting section is equipped with the tapered portion gradually tapered up and flat part, and by tapered portion that solution is gradually thin by thickness drawing, outer diameter is by becoming greatly It is small, gradually stretch.Using flat part, compression compact melt completes melt and is plasticized and is molded in mold.
In one embodiment, spreader is equipped with bullet and fixed part, and bullet cooperatively forms distributary division with die holder, Fixed part is connect with mold core.Bullet with die holder cooperatively form distributary division, melt is split by solid by distributary division Hollow circle, connect to set spreader and is fixed by fixed part with mold core.
In one embodiment, it shrinks set to be connected with mouth mold, contraction flow region is connected with each other with setting section.Shrink set with Mouth mold is connected, and mouth mold is fixed, and realizes that contraction flow region is consistent with the connection of setting section.
Preferably, the contraction of contraction flow region and the shrink-fit of tapered portion are consistent.Contraction flow region shrinks solution, tapered portion Also solution is shunk, ensures stability of the solution in flow process.
In one embodiment, extrusion die is equipped with pressing plate, and pressing plate is connect with mouth mold, and pressing plate coordinates counterpart with set is shunk Mould is fixed.Pressing plate coordinates with set is shunk, and mouth mold is fixed, and realizes the accurate fit of contraction flow region and tapered portion.
In one embodiment, coolant jacket is equipped with outer water jacket, and outer water jacket is connected with coolant jacket made of Heat Conduction Material.It is cold But what is be arranged with is made from a material that be thermally conductive, and avoids accumulation of the heat in coolant jacket.
Preferably, coolant jacket is equipped with the cavity coordinated with PVC spools, and coolant jacket is equipped with helicla flute, is guided by helicla flute Cooling water flows through coolant jacket.
Coolant jacket is equipped with cavity, and PVC spools are accommodated by cavity.Coolant jacket is equipped with helicla flute, and flow flows in helicla flute It crosses, coolant jacket is flowed through by helicla flute guide cooling water.
Preferably, the inner surface for the cavity that coolant jacket is equipped with is equipped with frosting, improves abrasion resistance.
Compared with prior art, the present invention having the characteristics that:The structure design of the mold runner of optimization is realized to mold The mouth mold of the careful design of pressure, connecting shaping section reduces melt die swelling power, meanwhile, it is comprehensive using spiral cooling water cover It closes and promotes production stability.
Description of the drawings
Fig. 1 is overall structure diagram in the embodiment of the present invention.
Fig. 2 is coolant jacket structural schematic diagram in the embodiment of the present invention.
Fig. 3 is extrusion die structural schematic diagram in the embodiment of the present invention.
Specific implementation mode
Attached drawing only for illustration, is not considered as limiting the invention;It is attached in order to more preferably illustrate the present embodiment Scheme certain components to have omission, zoom in or out, does not represent the size of actual product;To those skilled in the art, The omitting of some known structures and their instructions in the attached drawings are understandable.Being given for example only property of position relationship described in attached drawing Illustrate, is not considered as limiting the invention.
Embodiment 1:
As Fig. 1 and as shown in figure 3, the present invention provide it is a kind of improve PVC spool production stabilities mold, include the company of solution Section 1 is connect, solution is connect by linkage section 1 with shunting die holder 2, and the solution outflux of shunting die holder 2 is equipped with extrusion die, this implementation In example, there are four extrusion die is set.
As shown in figure 3, the solution inflow entrance of extrusion die is equipped with die holder 3, die holder 3 is equipped with the cavity of taper, extrusion die Interior to be equipped with spreader 4, spreader 4 is equipped with bullet 41 and fixed part 42.Bullet 41 coordinates with the cavity that die holder 3 is equipped with, shape At distributary division 31, distributary division 31 is gradually tapered up along melt flow direction.
As shown in figure 3, fixed part 42 is connect with mold core 8, it is connect with mold core 8 by fixed part 42 and progress is set to spreader 4 It is fixed.
As shown in figure 3, the solution by distributary division 31 enters contraction flow region 51 by flat segments, contraction flow region 51 is to shrink set 5 The pyramidal structure cooperatively formed with mold core 8, contraction flow region 51 are gradually tapered up along melt flow direction, to molten during melt flow Body is stretched.
As shown in figure 3, mold core 8 cooperatively forms setting section with mouth mold 6, setting section is equipped with 61 peace of tapered portion gradually tapered up Straight portion 81, tapered portion 61 are gradually tapered up along melt flow direction, are squeezed solution, the solution after the extruding of tapered portion 61 Into flat part 81, further compression compact melt completes melt and is plasticized and is molded in mold.
Mold core 8 is equipped with two parts, and a part is divided for the tapered portion 61 coordinated with contraction set 5 and mouth mold 6, what tapered portion 61 was divided The shape structure for shrinking set 5 and 6 part of mouth mold corresponding with size, and then the channel of taper is formed, while can ensure contraction flow region 51 with the connection of the retracted configuration of tapered portion 61, avoid product quality from being affected.;Another part is to be cooled and shaped part, with Flat part 81 coordinates.
In the present embodiment, extrusion die is equipped with pressing plate 7, and pressing plate 7 coordinates with set 5 is shunk, mouth mold 6 is fixed, realizes The accurate fit of contraction flow region 51 and tapered portion 61.
As shown in Fig. 2, coolant jacket 92 is equipped with outer water jacket 91, outer water jacket 91 is connected with coolant jacket 92 made of Heat Conduction Material, PVC spools, which stretch, enters coolant jacket 92.Coolant jacket 92 is equipped with the cavity coordinated with PVC spools, and it is cold that PVC spools enter cavity progress But.Coolant jacket 92 is equipped with helicla flute 93, and coolant jacket 92,93 guide cooling water of helicla flute are flowed through by 93 guide cooling water of helicla flute Rotational flow avoids incrustation scale or other impurity from depositing, has the function that clean automatically.
In the present embodiment, when mold design, need to meet following relationship:The annular space area of spreader 4 is set as V1, mouth mold 6, The annular space area of mold core 8 is V2, and 6 diameter of bore of mouth mold is D, and each discharge area is V3 after shunting die holder 2 shunts, and shunts die holder 2 Longitudinal length is L, and it is d to be cooled to jacket diameter of bore, then:
V1/V3 >=4 and L is inversely proportional with the ratio, L is bigger, and the ratio is then smaller.
10≤V1/V2≤28 and D increases with the increase of the ratio, but need to ensure that D/d ratios are not more than simultaneously 1.05。
Obviously, the above embodiment of the present invention be only to clearly illustrate example of the present invention, and not be pair The restriction of embodiments of the present invention.For those of ordinary skill in the art, may be used also on the basis of the above description To make other variations or changes in different ways.There is no necessity and possibility to exhaust all the enbodiments.It is all this All any modification, equivalent and improvement etc., should be included in the claims in the present invention made by within the spirit and principle of invention Protection domain within.

Claims (8)

1. a kind of mold improving PVC spool production stabilities, which is characterized in that include the linkage section of solution, the connection Section is connect with shunting die holder, and shunting die holder is combined with several extrusion dies, and the extrusion die is equipped with die holder, and extrusion die is set Have a spreader of the taper coordinated with die holder, spreader and die holder cooperatively form distributary division, distributary division along melt flow direction by Taper contracting;The spreader by equipped with flat segments connect with mold core, mold core with shrink set cooperatively forms contraction flow region, the receipts Contracting portion is gradually tapered up along melt flow direction;The mold core cooperatively forms setting section with mouth mold, and the setting section, which is equipped with, gradually to be received The tapered portion and flat part of contracting, the outlet end of the setting section are connect with coolant jacket.
2. the mold according to claim 1 for improving PVC spool production stabilities, which is characterized in that the spreader is set There are bullet and fixed part, the bullet to cooperatively form distributary division with die holder, the fixed part is connect with mold core.
3. the mold according to claim 1 for improving PVC spool production stabilities, which is characterized in that contractions set and Mouth mold is connected, and the contraction flow region is connected with each other with setting section.
4. the mold according to claim 3 for improving PVC spool production stabilities, which is characterized in that the contraction flow region It shrinks consistent with the shrink-fit of tapered portion.
5. the mold according to claim 1 for improving PVC spool production stabilities, which is characterized in that the extrusion die Equipped with pressing plate, the pressing plate is connect with mouth mold, and pressing plate is fixed mouth mold with set cooperation is shunk.
6. the mold according to claim 1 for improving PVC spool production stabilities, which is characterized in that the cooling is arranged There are outer water jacket, the outer water jacket to be connected with coolant jacket made of Heat Conduction Material.
7. the mold according to claim 6 for improving PVC spool production stabilities, which is characterized in that the cooling is arranged There are the cavity coordinated with PVC spools, the coolant jacket to be equipped with helicla flute, coolant jacket is flowed through by helicla flute guide cooling water.
8. the mold according to claim 7 for improving PVC spool production stabilities, which is characterized in that the cooling is arranged The inner surface of some cavitys is equipped with frosting, improves abrasion resistance.
CN201810575268.6A 2018-06-06 2018-06-06 A kind of mold improving PVC spool production stabilities Pending CN108454055A (en)