CN108424749B - 抑尘封土剂 - Google Patents
抑尘封土剂 Download PDFInfo
- Publication number
- CN108424749B CN108424749B CN201810232756.7A CN201810232756A CN108424749B CN 108424749 B CN108424749 B CN 108424749B CN 201810232756 A CN201810232756 A CN 201810232756A CN 108424749 B CN108424749 B CN 108424749B
- Authority
- CN
- China
- Prior art keywords
- sealing agent
- sodium silicate
- dust suppression
- soil sealing
- liquid hardening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
抑尘封土剂,提供了一种抑制扬尘的地膜产品的配制工艺,以硅酸钠水玻璃为原料,通过选料、配料、混料、反应等步骤,向硅酸钠水溶液中逐步添加聚丙烯酸钠和液体硬化剂,使得其能够有效的自硬化成地膜,抑制扬尘封隔土壤,工艺过程简单,配置方便,随配随用,使用方法简单,自然风干,施工不受外界温度风力等环境因素影响,干燥后生成的防尘地膜对环境无害,不影响土壤的后续使用,环保和抑尘效果好。
Description
技术领域
本发明属于化工生产技术领域,具体为一种抑制扬尘的地膜产品的制备方法。
背景技术
为了阻止露天料场或工地现场的扬尘影响附近环境,人们会设置一些环保设施来防止尘土扬起,常采用的措施有在大型料场设置横拉的金属网板墙体包围住料场、在堆放的建筑垃圾上覆盖软质塑料防尘网、在一定范围内铺设地膜等方法,对于地膜来说,在阳光下易风化和氧化,进而失去了本来的效果,还会产生新的污染,同时,酸性喷膜或浆膜,还会对地面带来二次污染,影响该处现场的后续使用。
发明内容
本发明的目的在于提供一种抑尘封土剂的配制工艺,以解决上述问题。
为实现上述目的,本发明提出的技术方案为:
抑尘封土剂,其具体的工艺流程包括以下步骤:
①选料:选取质量分数为40%的硅酸钠溶液作为原料;
②配料:在混合槽中将水和硅酸钠溶液以质量比1:2的比例混合,并在恒温50℃下搅拌均匀;
③混料:在搅拌过程中匀速加入硅酸钠溶液质量3~6%的聚丙烯酸钠,持续搅拌至完全溶解;
④反应:向上述溶液中匀速加入液体硬化剂,搅拌30min至完全溶解,即得成品抑尘封土剂,即可输送至成品储罐中储存和出售。
在本发明中,所述液体硬化剂为硅酸钾,加入量为硅酸钠溶液质量的3~6%。
在本发明中,所述抑尘封土剂的使用方法在于:配好之后6h内直接喷施于地面,待自然干燥后即可生效。
与现有技术相比,本发明选用硅酸钠水玻璃作为产品的原料,工艺过程简单,配置方便,随配随用,使用方法简单,自然风干,施工不受外界温度风力等环境因素影响,干燥后生成的防尘地膜对环境无害,不影响土壤的后续使用,环保和抑尘效果好。
具体实施方式
以下结合具体优选的实施例对本发明作进一步描述,但并不因此而限制本发明的保护范围。
抑尘封土剂,其配制的工艺流程包括以下步骤:①选料:选取市售质量分数为40%的硅酸钠溶液作为原料;②配料:在混合槽中将水和硅酸钠溶液以质量比1:2的比例混合,并在恒温50℃下搅拌均匀;③混料:在搅拌过程中匀速加入硅酸钠溶液质量3~6%的聚丙烯酸钠,持续搅拌至完全溶解;④反应:向上述溶液中匀速加入硅酸钠溶液质量3~6%的液体硬化剂硅酸钾,搅拌30min至完全溶解,即得成品抑尘封土剂,即可输送至成品储罐中储存和出售。
在本发明中,上述抑尘封土剂的使用方法为:配好之后6h内直接喷施于地面,待自然干燥后即可生效,以随配随用为最佳。
在本发明中,以硅酸钠水玻璃作为产品原料,工艺过程简单,配置方便,随配随用,使用方法简单,自然风干,施工不受外界温度风力等环境因素影响,干燥后生成的防尘地膜对环境无害,不影响土壤的后续使用,环保和抑尘效果好。
Claims (2)
1.抑尘封土剂,其特征在于,其具体的工艺流程包括以下步骤:
①选料:选取质量分数为40%的硅酸钠溶液作为原料;
②配料:在混合槽中将水和硅酸钠溶液以质量比1:2的比例混合,并在恒温50℃下搅拌均匀;
③混料:在搅拌过程中匀速加入硅酸钠溶液质量3~6%的聚丙烯酸钠,持续搅拌至完全溶解;
④反应:向上述溶液中匀速加入液体硬化剂,搅拌30min至完全溶解,即得成品抑尘封土剂,即可输送至成品储罐中储存和出售;所述液体硬化剂为硅酸钾,加入量为硅酸钠溶液质量的3~6%。
2.根据权利要求1所述的抑尘封土剂,其特征在于,所述抑尘封土剂的使用方法在于:配好之后6h内直接喷施于地面,待自然干燥后即可生效。