CN108300154A - A kind of static conductive coating and its production method - Google Patents
A kind of static conductive coating and its production method Download PDFInfo
- Publication number
- CN108300154A CN108300154A CN201710961404.0A CN201710961404A CN108300154A CN 108300154 A CN108300154 A CN 108300154A CN 201710961404 A CN201710961404 A CN 201710961404A CN 108300154 A CN108300154 A CN 108300154A
- Authority
- CN
- China
- Prior art keywords
- parts
- conductive coating
- static conductive
- epoxy resin
- chlorosulfonated polyethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of static conductive coatings, are made of according to parts by weight following raw material:Chlorosulfonated polyethylene rubber:20 35 parts;Epoxy resin:50 parts;Conductive mica:15 20 parts;Calcite in powder:30 45 parts;Propylene glycol methyl ether acetate:20 30 parts;Auxiliary agent:25 parts;A kind of production method of static conductive coating, the production method of the static conductive coating include the following steps:S1;It is stirred under normal pressure;S2:Grinding;S3 is packed.Static conductive coating is using the epoxy resin of oil resistivity and excellent anti-corrosion performance as main film-former, make main modifying agent with the generally acknowledged long-life type chlorosulfonated polyethylene rubber in China and foreign countries, conducting pigment, filler, conductive auxiliary agent, solvent etc., the electrostatically conductive oil-tolerant special dual-component anticorrosive paint being prepared through advanced technologies is added.
Description
Technical field
The present invention relates to static conductive coating technical field, specially a kind of static conductive coating and its production method.
Background technology
Static conductive coating is generally acknowledged with China and foreign countries using the epoxy resin of oil resistivity and excellent anti-corrosion performance as main film-former
Long-life type chlorosulfonated polyethylene rubber make main modifying agent, conducting pigment, filler, conductive auxiliary agent, solvent etc. is added, through advanced
The electrostatically conductive oil-tolerant special dual-component anticorrosive paint that technique is prepared., oil, chemical industry, railway, the industries store oil such as traffic
The store oils such as tank, oil pipeline, oil holding slot vehicle, oil tanker, oil transporting appliance inside and outside wall anti-corrosion antistatic protection;Gas tank, sluice,
The anti-corrosion antistatic protection of lower pipeline etc.;The anti-corrosion antistatic protection of the industry devices such as coal mine, aviation, weaving, grain, facility.
Antiseptic property is good.Coating adhesion is strong, and impact resistance is excellent.Permeability resistance is good, and humidity resistance is excellent, water-tolerant.Oil resistance is good.
Coating can for a long time be used in natural gas, coal gas and in the oil products such as gasoline, kerosene, diesel oil, lubricating oil.Electric conductivity is strong.It leads
Electric performance stablity is reliable, and resistivity meets GB6950-2001 Oil Tank static conductive coating technical indicators.Easy to use, room temperature is solid
Change.Bi-component package is not limited by space enrironment, it is only necessary to be stirred evenly after opening bucket, be prepared curing agent in proportion, used
General-purpose construction method, normal temperature cure film forming, and one-pass film-forming is thick.Solvent not chlorine-containing compound, glycol divinyl ether and its
Acetate.
Invention content
The purpose of the present invention is to solve disadvantage existing in the prior art, and a kind of static conductive coating that proposes and its
Production method.
To achieve the above object, the present invention provides the following technical solutions:
A kind of static conductive coating is made of following raw material according to parts by weight:
Chlorosulfonated polyethylene rubber:23 parts;
Epoxy resin:50 parts;
Conductive mica:15 parts;
Calcite in powder:30 parts;
Propylene glycol methyl ether acetate:20 parts;
Auxiliary agent:2 parts;
Preferably, the epoxy resin.
Preferably, the calcite in powder grain size is 1250 mesh.
Preferably, a kind of production method of static conductive coating, the production method of the static conductive coating include the following steps:
S1:It is stirred under normal pressure:Chlorosulfonated polyethylene rubber:23 parts;Epoxy resin:50 parts;Conductive mica:15 parts;Fang Xie
Mountain flour:30 parts;Propylene glycol methyl ether acetate:20 parts;Auxiliary agent:2 parts;It stirs 30 minutes to 50 minutes;
S2:It is ground to fineness 30um into grinder;
S3:Packaging:The product of S2 is packed according to specification requirement.
A kind of static conductive coating provided by the invention, the static conductive coating not only have preferable antiseptic property, Er Qieshi
It is a kind of of low cost, it has excellent performance, full-featured static conductive coating.
Specific implementation mode
Based on the embodiments of the present invention, those of ordinary skill in the art are obtained without making creative work
The every other embodiment obtained, shall fall within the protection scope of the present invention.
Embodiment 1
A kind of static conductive coating is made of following raw material according to parts by weight:
Chlorosulfonated polyethylene rubber:26 parts;
Epoxy resin:50 parts;
Conductive mica:16 parts;
Calcite in powder:33 parts;
Propylene glycol methyl ether acetate:21 parts;
Auxiliary agent:2 parts;
Preferably, the epoxy resin.
Preferably, the calcite in powder grain size is 1250 mesh.
A kind of production method of static conductive coating, the production method of the static conductive coating include the following steps:
S1:It is stirred under normal pressure:Chlorosulfonated polyethylene rubber:26 parts;Epoxy resin:50 parts;Conductive mica:16 parts;Fang Xie
Mountain flour:33 parts;Propylene glycol methyl ether acetate:21 parts;Auxiliary agent:2 parts;It stirs 30 minutes to 50 minutes;
S2:It is ground to fineness 30um into grinder;
S3:Packaging:The product of S2 is packed according to specification requirement.
Embodiment 2
A kind of static conductive coating is made of following raw material according to parts by weight:
Chlorosulfonated polyethylene rubber:30 parts;
Epoxy resin:50 parts;
Conductive mica:17 parts;
Calcite in powder:38 parts;
Propylene glycol methyl ether acetate:25 parts;
Auxiliary agent:3 parts;
Preferably, the epoxy resin.
Preferably, the calcite in powder grain size is 1250 mesh.
A kind of production method of static conductive coating, the production method of the static conductive coating include the following steps:
S1:It is stirred under normal pressure:Chlorosulfonated polyethylene rubber:30 parts;Epoxy resin:50 parts;Conductive mica:17 parts;Fang Xie
Mountain flour:38 parts;Propylene glycol methyl ether acetate:25 parts;Auxiliary agent:3 parts;It stirs 30 minutes to 50 minutes;
S2:It is ground to fineness 30um into grinder;
S3:Packaging:The product of S2 is packed according to specification requirement.
Embodiment 3
The formula of a kind of static conductive coating, the static conductive coating is made of the component comprising following parts by weight:
Chlorosulfonated polyethylene rubber:35 parts;
Epoxy resin:50 parts;
Conductive mica:20 parts;
Calcite in powder:45 parts;
Propylene glycol methyl ether acetate:30 parts;
Auxiliary agent:5 parts;
Preferably, the epoxy resin.
Preferably, the calcite in powder grain size is 1250 mesh.
A kind of production method of static conductive coating, the production method of the static conductive coating include the following steps:
S1:It is stirred under normal pressure:Chlorosulfonated polyethylene rubber:35 parts;Epoxy resin:50 parts;Conductive mica:20 parts;Fang Xie
Mountain flour:45 parts;Propylene glycol methyl ether acetate:30 parts;Auxiliary agent:5 parts;It stirs 30 minutes to 50 minutes;
S2:It is ground to fineness 30um into grinder;
S3:Packaging:The product of S2 is packed according to specification requirement.
It although an embodiment of the present invention has been shown and described, for the ordinary skill in the art, can be with
Understanding without departing from the principles and spirit of the present invention can carry out these embodiments a variety of variations, modification, replace
And modification, the scope of the present invention is defined by the appended.
Claims (6)
1. a kind of static conductive coating, it is characterised in that:It is made of according to parts by weight following raw material:
Chlorosulfonated polyethylene rubber:20-35 parts;
Epoxy resin:50 parts;
Conductive mica:15-20 parts;
Calcite in powder:30-45 parts;
Propylene glycol methyl ether acetate:20-30 parts;
Auxiliary agent:2-5 parts.
2. a kind of static conductive coating according to claim 1, it is characterised in that:It is made of according to parts by weight following raw material:
Chlorosulfonated polyethylene rubber:20 parts;
Epoxy resin:50 parts;
Conductive mica:15 parts;
Calcite in powder:30 parts;
Propylene glycol methyl ether acetate:20 parts;
Auxiliary agent:2 parts.
3. a kind of static conductive coating according to claim 1, it is characterised in that:The epoxy resin.
4. a kind of static conductive coating according to claim 1, it is characterised in that:The calcite in powder grain size is 1250 mesh.
5. a kind of static conductive coating according to claim 1, it is characterised in that:Chlorosulfonated polyethylene rubber.
6. a kind of production method of static conductive coating as described in claim 1, it is characterised in that:The producer of the static conductive coating
Method includes the following steps:
S1:It is stirred under normal pressure:Chlorosulfonated polyethylene rubber:20 parts;Epoxy resin:50 parts;Conductive mica:15 parts;Calcite in powder:
30 parts;Propylene glycol methyl ether acetate:20 parts;Auxiliary agent:2 parts;It stirs 30 minutes to 50 minutes;
S2:It is ground to fineness 30um into grinder;
S3:Packaging:The product of S2 is packed according to specification requirement.