CN108162254A - The included opening stabilizer bar bushing mold of one kind - Google Patents
The included opening stabilizer bar bushing mold of one kind Download PDFInfo
- Publication number
- CN108162254A CN108162254A CN201711316070.8A CN201711316070A CN108162254A CN 108162254 A CN108162254 A CN 108162254A CN 201711316070 A CN201711316070 A CN 201711316070A CN 108162254 A CN108162254 A CN 108162254A
- Authority
- CN
- China
- Prior art keywords
- split block
- block
- split
- stabilizer bar
- catch
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses the included opening stabilizer bar bushing molds of one kind, multigroup half_split block is located between cope plate and lower template, every group of half_split block includes the first half_split block and the second half_split block, first half_split block offers multiple first grooves, first groove, which extends outwardly, is useful for the catch of bushing opening, second half_split block offers multiple second grooves, and the first groove and the second groove form complete bushing die cavity, and mold core is located in die cavity;Bushing rubber material not welding at catch at the time of molding, rubber material is separated to be formed through inside and outside opening, eliminate this procedure that subsequently cuts product, and the prepsetting gap between catch and mold core, mold core is avoided to collide when entering die cavity with catch, simultaneously, spring is equipped between adjacent the first half_split block and the second half_split block, under die opening state, there are gaps between the first half_split block and the second half_split block under spring force effect, more avoid when mold core enters die cavity and collide with catch.
Description
Technical field
The present invention relates to bushing technical field more particularly to a kind of included opening stabilizer bar bushing molds.
Background technology
Stabilizer bar bushing, which is mounted on automobile, is connected stabiliser bar pull rod with vehicle frame, its effect is that barrier unsteadiness of wheels passes
It is delivered on vehicle body, safety and the comfort of automobile can be improved, partially stabilized bushing is with opening, traditional manufacturing method
It is opening to be cut on bushing finished product, but increase procedure of processing, reduces production efficiency, and the opening essence being cut into
Spend low, opening size that different bushings are cut out, position difference are larger.
Invention content
To solve technical problem present in background technology, the present invention proposes a kind of included opening stabilizer bar bushing mold.
A kind of included opening stabilizer bar bushing mold proposed by the present invention, including cope plate, lower template, multiple mold cores and more
Group half_split block;Multigroup half_split block is located between cope plate and lower template, and every group of half_split block includes the first half_split block and second and breathe out
Husband's block, the first half_split block offer multiple first grooves, the first groove inner wall to the catch being externally provided with for being molded bushing opening,
Second half_split block offers multiple second grooves, and it is multiple complete that multiple first grooves and multiple second grooves are symmetrical arranged composition one by one
Whole bushing die cavity, multiple mold cores are located in multiple die cavitys one by one respectively.
Preferably, the interval for anticollision is preset between catch and mold core.
Preferably, spring is equipped between the first half_split block and the second half_split block, the first half_split block and second under die opening state
Half_split block spacing distance.
Preferably, the first half_split block is equipped with locating piece, and the second half_split block is equipped with locating slot, locating piece under molding state
Cooperation is in locating slot.
Preferably, arbitrary second groove offers torn edges slot on one side in the second half_split block close to the first half_split block.
Preferably, multigroup half_split block is arranged in parallel.
Preferably, adjacent first half_split block of two groups of arbitrary neighborhood and the second half_split block are integrally formed.
Preferably, cope plate, which extends outwardly, is useful for the convex block for positioning multigroup half_split block, and convex block is resisted against outermost Hough
On block periphery, convex block leans face as inclined surface with half_split block.
In the present invention, the included opening stabilizer bar bushing mold that is proposed, the first groove and second on the first half_split block
Bushing die cavity is formed after the cooperation of the second groove on half_split block, catch is outward extended in the first groove inner wall and gos deep into die cavity,
Bushing rubber material not welding at catch at the time of molding separates rubber material to be formed through inside and outside opening, after eliminating
Continuous this procedure that cuts product;Since catch is relatively thin, the prepsetting gap between catch and mold core, when avoiding the mold core from entering die cavity with
It collides with catch by catch clashing and breaking;Meanwhile spring is equipped between adjacent the first half_split block and the second half_split block, die sinking
Under state, there are gaps between the first half_split block and the second half_split block under spring force effect, and such catch with putting mold core in advance
Position apart from bigger, more avoid when mold core enters die cavity and collide with catch, in clamping process, the convex block on cope plate
Squeezing half_split block causes half_split block to enter accurate position, and the first half_split block and the second half_split block squeeze spring and finally mutually support
It leans on.
Description of the drawings
Fig. 1 is a kind of exploded perspective view of included opening stabilizer bar bushing mold proposed by the present invention;
Fig. 2 is a kind of half_split block vertical view of included opening stabilizer bar bushing mold proposed by the present invention;
Fig. 3 is a kind of vertical view of included opening single die cavity of stabilizer bar bushing mold proposed by the present invention;
Fig. 4 is a kind of the second half_split block structure diagram of included opening stabilizer bar bushing mold proposed by the present invention;
Fig. 5 is the side view of a kind of included opening stabilizer bar bushing upper mould plate and half_split block proposed by the present invention.
Specific embodiment
As shown in Figs. 1-5, Fig. 1 is a kind of exploded perspective view of included opening stabilizer bar bushing mold proposed by the present invention,
Fig. 2 is a kind of half_split block vertical view of included opening stabilizer bar bushing mold proposed by the present invention, and Fig. 3 is proposed by the present invention one
The vertical view of the included opening single die cavity of stabilizer bar bushing mold of kind, Fig. 4 carry opening stabiliser bar for one kind proposed by the present invention
Second half_split block structure diagram of bush mould, Fig. 5 is on a kind of included opening stabilizer bar bushing mold proposed by the present invention
The side view of template and half_split block.
With reference to Fig. 1-3, a kind of included opening stabilizer bar bushing mold proposed by the present invention, including cope plate 1, lower template 2,
36 mold cores and six groups of half_split blocks 3;Every group of half_split block 3 is set there are six die cavity, and six groups of half_split blocks 3 form 36 moulds altogether
Chamber, 36 mold cores are respectively positioned in 36 die cavitys, and therefore, the mold in the present embodiment once molds molding 30
Six bush moulds;
Six groups of half_split blocks 3 are located between cope plate 1 and lower template 2, and every group of half_split block 3 includes the first half_split block 31 and the
Two half_split blocks 32, the first half_split block 31 are opened up there are six the first groove 311, and the second half_split block 32 opens up that there are six the second grooves
321, six the first grooves 311 and six the second grooves 321 are symmetrical arranged form six complete bushing die cavitys one by one, and mold core is fixed
Position is in the die cavity, also, 311 inner wall of the first groove extends outwardly and is useful for the catch 312 of bushing opening, and catch 312 is along mould
Chamber is axially set, and rubber material is separated to be formed and be passed through by bushing rubber material not welding at catch 312 at the time of molding, catch 312
The opening of bushing axial direction is worn, eliminates this procedure that subsequently cuts product.
Reference Fig. 2, in the present embodiment, the included opening stabilizer bar bushing mold proposed, in a specific embodiment,
First half_split block 31 and the second half_split block 32 are in strip structure, in the concrete structure design of half_split block 3, first group of half_split block 3
The first half_split block 31 of the second half_split block 32 and second group of half_split block 3 be integrally formed, the second half_split block of second group of half_split block 3
32 are integrally formed with the first half_split block 31 of third group half_split block 3, the second half_split block 32 of third group half_split block 3 and the 4th group of Kazakhstan
First half_split block 31 of husband's block 3 is integrally formed, the second half_split block 32 of the 4th group of half_split block 3 and the first of the 5th group of half_split block 3
Half_split block 31 is integrally formed, the second half_split block 32 of the 5th group of half_split block 3 and 31 one of the first half_split block of the 6th group of half_split block 3
Molding, multigroup half_split block 3 are arranged in parallel.
In the present embodiment, catch is relatively thin, and in order to which catch 312 is not collided with mold core, catch 312 shortens 0.2mm, therefore catch
There is the gap of 0.2mm between 312 and mold core, when mold core enters die cavity, due to the gap of this 0.2mm, when mold core enters die cavity
It avoids and is collided with catch 312 by catch clashing and breaking.
With reference to Fig. 2, further in order to avoid mold core and catch 312 collide, the first half_split block 31 in every group of half_split block 3
And second be equipped with spring 4 between half_split block 32, there are gap between the first half_split block 31 and the second half_split block 32 under die opening state,
In this way catch 312 and put in advance mold core position apart from bigger, more avoid and collide when mold core enters die cavity with catch 312,
In specific design method, the both sides of the first half_split block 31 and the second half_split block 32 open up it is jagged, the of every group of half_split block 3
The both sides of one half_split block 31 and the second half_split block 32 are respectively equipped with spring 4, and 4 both ends of spring are born against to be lacked in the first half_split block 31
On mouth and 32 notch of the second half_split block, the first half_split block 31 and the second half_split block 32 are separated 2mm by spring 4.
In order to avoid the first half_split block 31 and the second half_split block 32 misplace in molding, the first half_split block 31 is equipped with
The locating piece 313 of two semi-cylindricals, sets the locating slot 322 there are two semi-cylindrical on the second half_split block 32, under molding state
Just cooperation in locating slot 322, limits the first half_split block 31 and the second half_split block 32 is opposite along half_split block 3 locating piece 313
Length direction moves.
With reference to Fig. 3, in the present embodiment, torn edges slot 323 is offered on one side close to the first half_split block 31 in the second half_split block 32,
Torn edges slot 323 is located at 321 both sides of the second groove, plays the role of torn edges in road reforming process after 323 molding bushing of torn edges slot.
With reference to Fig. 4, cope plate 1, which extends outwardly, is useful for the strip convex block 11 for positioning multigroup half_split block 3,11 inside of convex block
Wall is resisted against on 3 periphery of outermost half_split block, 11 madial wall of convex block and 31 lateral wall phase of the first half_split block in the present embodiment
Against another 11 madial wall of convex block is resisted against, and convex block 11 leans face as inclined surface with half_split block 3, is breathed out in this way in molding
Husband's block 3 more slightly deviates, by inclined surface so that the playback of half_split block 3 is to correct position, and when molding in two convex blocks 11
Side wall and 1 inside of cope plate form trapezoid cross section and closure pressing speed are improved, and avoid and are adjusted repeatedly in clamping process
Half_split block 3.
Included opening stabilizer bar bushing mold in the present embodiment, the first groove 311 and second on the first half_split block 31
Bushing die cavity is formed after the cooperation of second groove 321 on half_split block 32, catch 312 is outward extended with simultaneously in 311 inner wall of the first groove
Go deep into die cavity, bushing rubber material not welding at catch 312 at the time of molding separates rubber material to be formed through inside and outside
Opening, eliminates this procedure that subsequently cuts product;And the prepsetting gap between catch 312 and mold core, avoids mold core from entering
With colliding with catch 312 during die cavity;Meanwhile spring is equipped between adjacent the first half_split block 31 and the second half_split block 32
4, under die opening state, there are gap, such catch between the first half_split block 31 and the second half_split block 32 under the effect of 4 elastic force of spring
312 with put in advance mold core position apart from bigger, more avoid and collide when mold core enters die cavity with catch 312, clamping process
In, the convex block 11 on cope plate 1 squeezes half_split block 3 so that half_split block 3 enters accurate position, and spring 4 progresses into compression shape
State.
The foregoing is only a preferred embodiment of the present invention, but protection scope of the present invention be not limited thereto,
Any one skilled in the art in the technical scope disclosed by the present invention, according to the technique and scheme of the present invention and its
Inventive concept is subject to equivalent substitution or change, should be covered by the protection scope of the present invention.
Claims (8)
1. the included opening stabilizer bar bushing mold of one kind, which is characterized in that including cope plate (1), lower template (2), multiple mold cores
With multigroup half_split block (3);Multigroup half_split block (3) is located between cope plate (1) and lower template (2), and every group of half_split block (3) includes
First half_split block (31) and the second half_split block (32), the first half_split block (31) offer multiple first grooves (311), the first groove
(311) inner wall offers multiple second grooves to the catch (312) being externally provided with for being molded bushing opening, the second half_split block (32)
(321), multiple first grooves (311) and multiple second grooves (321) are symmetrical arranged one by one forms multiple complete bushing die cavitys,
Multiple mold cores are located in multiple die cavitys one by one respectively.
2. included opening stabilizer bar bushing mold according to claim 1, which is characterized in that catch (312) and mold core it
Between preset interval for anticollision.
3. included opening stabilizer bar bushing mold according to claim 1, which is characterized in that the first half_split block (31) and the
Spring (4) is equipped between two half_split blocks (32), the first half_split block (31) and the second half_split block (32) spacing distance under die opening state.
4. included opening stabilizer bar bushing mold according to claim 1, which is characterized in that the first half_split block is set on (31)
Have a locating piece (313), the second half_split block (32) is equipped with locating slot (322), under molding state locating piece (313) cooperation positioning
In slot (322).
5. included opening stabilizer bar bushing mold according to claim 1, which is characterized in that arbitrary second groove (321)
Torn edges slot (323) is offered on one side close to the first half_split block (31) in the second half_split block (32).
6. included opening stabilizer bar bushing mold according to claim 1, which is characterized in that multigroup half_split block (3) is parallel
Setting.
7. it is according to claim 6 it is included opening stabilizer bar bushing mold, which is characterized in that two groups of arbitrary neighborhood it is adjacent
First half_split block (31) and the second half_split block (32) are integrally formed.
8. included opening stabilizer bar bushing mold according to claim 7, which is characterized in that cope plate (1) extends outwardly
It is useful for positioning the convex block (11) of multigroup half_split block (3), convex block (11) is resisted against on outermost half_split block (3) periphery, convex block
(11) face is leant with half_split block (3) as inclined surface.