CN107916053A - One kind is based on ultraviolet light cured furniture waterproof coating priming paint and its production method - Google Patents

One kind is based on ultraviolet light cured furniture waterproof coating priming paint and its production method Download PDF

Info

Publication number
CN107916053A
CN107916053A CN201711338845.1A CN201711338845A CN107916053A CN 107916053 A CN107916053 A CN 107916053A CN 201711338845 A CN201711338845 A CN 201711338845A CN 107916053 A CN107916053 A CN 107916053A
Authority
CN
China
Prior art keywords
parts
component
priming paint
ultraviolet light
waterproof coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711338845.1A
Other languages
Chinese (zh)
Inventor
胡廷政
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xuzhou Longbang Furniture Co Ltd
Original Assignee
Xuzhou Longbang Furniture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xuzhou Longbang Furniture Co Ltd filed Critical Xuzhou Longbang Furniture Co Ltd
Priority to CN201711338845.1A priority Critical patent/CN107916053A/en
Publication of CN107916053A publication Critical patent/CN107916053A/en
Pending legal-status Critical Current

Abstract

One kind is based on ultraviolet light cured furniture waterproof coating priming paint and its production method, belongs to chemical technology field, the component of component in parts by weight includes:4~7 parts of epoxy resin, 75~90 parts of zinc powder, 3~5 parts of siliceous nano assistant, 2~3 parts of anti-settling agent, 5~12 parts of solvent, 15~35 parts of modified polyester acrylate ester, 10~25 parts of monomer, 25~45 parts of filler, 2~7 parts of photoinitiator, 0.8~1.2 part of anti-settling agent, 0.5~0.7 part of defoamer, the cured furniture waterproof coating priming paint of ultraviolet light of the present invention can improve adhesive force, salt spray resistance, better than the priming paint adhesive force of traditional handicraft, it is and easy to operate, it is time-consuming short, greatly improve the efficiency, energy is saved, greatly reduce the discharge of VOC, there is bulge and break-off after avoiding construction.

Description

One kind is based on ultraviolet light cured furniture waterproof coating priming paint and its production method
Technical field
The present invention relates to one kind to be based on ultraviolet light cured furniture waterproof coating priming paint and its production method, belongs to chemical industry Technical field.
Background technology
In the prior art, during the dry film metal Zn content based on epoxy zinc rich primer >=70%, coating adhesion, impact resistance It can be reduced etc. mechanical performance with the raising of Zn content, salt spray resistance can also decrease, and can so influence work progress Coating is easily destroyed by external force and occurs returning rust, increases the workload of repairing, even if coating is not destroyed, finally can also influence to use Service life.
UV-curing technology it be by the automatic roller coat of machinery equipment, showering or spray in furniture plate face, ultraviolet Promote photoinitiator to decompose under the irradiation of light, generate free radicals, initiation resin reaction, a kind of coating of instantaneous solidification film forming, its It is mainly characterized by:Handled by intensive ultraviolet photocuring, color stability, for a long time Chang Xin, is truly realized efficient, environmentally friendly.
The content of the invention
For problem exists in the prior art, used it is an object of the invention to provide one kind based on the cured furniture of ultraviolet light Waterproof coating priming paint and its production method.
To achieve these goals, the technical solution adopted by the present invention is:Applied based on the cured furniture of ultraviolet light with waterproof Film priming paint, the component of the component in parts by weight include:4~7 parts of epoxy resin, 75~90 parts of zinc powder, siliceous nanometer help 3~5 parts of agent, 2~3 parts of anti-settling agent, 5~12 parts of solvent, 15~35 parts of modified polyester acrylate ester, 10~25 parts of monomer, fill out Fill 25~45 parts of agent, 2~7 parts of photoinitiator, 0.8~1.2 part of anti-settling agent, 0.5~0.7 part of defoamer.
Further, the component of the component in parts by weight includes:4 parts of epoxy resin, 75 parts of zinc powder, siliceous nanometer help 3 parts of agent, 2 parts of anti-settling agent, 5 parts of solvent, 15 parts of modified polyester acrylate ester, 10 parts of monomer, 25 parts of filler, photoinitiator 2 Part, 0.8 part of anti-settling agent, 0.5 part of defoamer.
Further, the component of the component in parts by weight includes:7 parts of epoxy resin, 90 parts of zinc powder, siliceous nanometer help 5 parts of agent, 3 parts of anti-settling agent, 12 parts of solvent, 35 parts of modified polyester acrylate ester, 25 parts of monomer, 45 parts of filler, light-initiated 7 Part, 1.2 parts of anti-settling agent, 0.7 part of defoamer.
Based on above-mentioned ultraviolet light cured furniture waterproof coating priming paint production method, it is comprised the concrete steps that:
(1) first by urethane acrylate and modified polyester acrylate ester, monomer, photoinitiator, anti-settling agent and defoamer Stir evenly, add filler in the case of stirring, be distributed to after fineness reaches requirement;
(2) epoxy resin that molecular weight is 200~800 is added to dissolving in the first organic solvent to stir evenly, then first Siliceous nano assistant, anti-settling agent are added in organic solvent, is stirred evenly, stir evenly laggard sand mill be ground to fineness≤ 3.75 μm, the zinc powder for finally adding 800~1200 mesh fully stirs evenly, and obtains zinc-rich steel structure anti-corrosion primer first component, standby With;
(3) the zinc-rich steel structure anti-corrosion bottom that the zinc-rich steel structure anti-corrosion primer first component obtained is obtained with step (2) Paint component B is mixed evenly, and cures 30~45 minutes, obtains being based on the cured furniture waterproof coating priming paint of ultraviolet light.
Compared with prior art, product of the invention, which is based on the cured furniture waterproof coating priming paint of ultraviolet light, to improve Adhesive force, salt spray resistance, better than the priming paint adhesive force of traditional handicraft, and it is easy to operate, time-consuming it is short, substantially increase effect Rate, has saved energy, greatly reduces the discharge of VOC, bulge and break-off occurs after avoiding construction.
Embodiment
The invention will be further described below.
Based on ultraviolet light cured furniture waterproof coating priming paint, the component of the component in parts by weight includes:Epoxy 4~7 parts of resin, 75~90 parts of zinc powder, 3~5 parts siliceous of nano assistant, 2~3 parts of anti-settling agent, 5~12 parts of solvent, modification 15~35 parts of polyester acrylate, 10~25 parts of monomer, 25~45 parts of filler, 2~7 parts of photoinitiator, anti-settling agent 0.8~ 1.2 parts, 0.5~0.7 part of defoamer.
Further, the component of the component in parts by weight includes:4 parts of epoxy resin, 75 parts of zinc powder, siliceous nanometer help 3 parts of agent, 2 parts of anti-settling agent, 5 parts of solvent, 15 parts of modified polyester acrylate ester, 10 parts of monomer, 25 parts of filler, photoinitiator 2 Part, 0.8 part of anti-settling agent, 0.5 part of defoamer.
Further, the component of the component in parts by weight includes:7 parts of epoxy resin, 90 parts of zinc powder, siliceous nanometer help 5 parts of agent, 3 parts of anti-settling agent, 12 parts of solvent, 35 parts of modified polyester acrylate ester, 25 parts of monomer, 45 parts of filler, light-initiated 7 Part, 1.2 parts of anti-settling agent, 0.7 part of defoamer.
Based on above-mentioned ultraviolet light cured furniture waterproof coating priming paint production method, it is comprised the concrete steps that:
(1) first by urethane acrylate and modified polyester acrylate ester, monomer, photoinitiator, anti-settling agent and defoamer Stir evenly, add filler in the case of stirring, be distributed to after fineness reaches requirement;
(2) epoxy resin that molecular weight is 200~800 is added to dissolving in the first organic solvent to stir evenly, then first Siliceous nano assistant, anti-settling agent are added in organic solvent, is stirred evenly, stir evenly laggard sand mill be ground to fineness≤ 3.75 μm, the zinc powder for finally adding 800~1200 mesh fully stirs evenly, and obtains zinc-rich steel structure anti-corrosion primer first component, standby With;
(3) the zinc-rich steel structure anti-corrosion bottom that the zinc-rich steel structure anti-corrosion primer first component obtained is obtained with step (2) Paint component B is mixed evenly, and cures 30~45 minutes, obtains being based on the cured furniture waterproof coating priming paint of ultraviolet light.

Claims (4)

1. it is based on ultraviolet light cured furniture waterproof coating priming paint, it is characterised in that the component of the component in parts by weight Including:4~7 parts of epoxy resin, 75~90 parts of zinc powder, 3~5 parts siliceous of nano assistant, 2~3 parts of anti-settling agent, solvent 5~ 12 parts, it is 15~35 parts of modified polyester acrylate ester, 10~25 parts of monomer, 25~45 parts of filler, 2~7 parts of photoinitiator, anti-settling 0.8~1.2 part of agent, 0.5~0.7 part of defoamer.
2. according to claim 1 be based on ultraviolet light cured furniture waterproof coating priming paint, it is characterised in that described to press The component of parts by weight component includes:4 parts of epoxy resin, 75 parts of zinc powder, 3 parts siliceous of nano assistant, 2 parts of anti-settling agent, machine are molten 5 parts of agent, 15 parts of modified polyester acrylate ester, 10 parts of monomer, 25 parts of filler, 2 parts of photoinitiator, 0.8 part of anti-settling agent, defoamer 0.5 part.
3. according to claim 1 be based on ultraviolet light cured furniture waterproof coating priming paint, it is characterised in that described to press The component of parts by weight component includes:7 parts of epoxy resin, 90 parts of zinc powder, 5 parts siliceous of nano assistant, 3 parts of anti-settling agent, machine are molten 12 parts of agent, 35 parts of modified polyester acrylate ester, 25 parts of monomer, 45 parts of filler, 7 parts light-initiated, 1.2 parts of anti-settling agent, defoamer 0.7 part.
4. being based on above-mentioned ultraviolet light cured furniture waterproof coating priming paint production method, it is comprised the concrete steps that:
(1) first urethane acrylate and modified polyester acrylate ester, monomer, photoinitiator, anti-settling agent and defoamer are stirred Uniformly, filler is added in the case of stirring, is distributed to after fineness reaches requirement;
(2) epoxy resin that molecular weight is 200~800 is added to dissolving in the first organic solvent to stir evenly, then it is organic first Siliceous nano assistant, anti-settling agent are added in solvent, is stirred evenly, laggard sand mill is stirred evenly and is ground to the μ of fineness≤3.75 M, the zinc powder for finally adding 800~1200 mesh fully stir evenly, and obtain zinc-rich steel structure anti-corrosion primer first component, spare;
(3) the zinc-rich steel structure anti-corrosion primer second that the zinc-rich steel structure anti-corrosion primer first component obtained is obtained with step (2) Component is mixed evenly, and cures 30~45 minutes, obtains being based on the cured furniture waterproof coating priming paint of ultraviolet light.
CN201711338845.1A 2017-12-14 2017-12-14 One kind is based on ultraviolet light cured furniture waterproof coating priming paint and its production method Pending CN107916053A (en)