CN107876979A - A kind of power lithium-ion battery liquid injection port seals method for laser welding - Google Patents

A kind of power lithium-ion battery liquid injection port seals method for laser welding Download PDF

Info

Publication number
CN107876979A
CN107876979A CN201710979832.6A CN201710979832A CN107876979A CN 107876979 A CN107876979 A CN 107876979A CN 201710979832 A CN201710979832 A CN 201710979832A CN 107876979 A CN107876979 A CN 107876979A
Authority
CN
China
Prior art keywords
laser
injection port
liquid injection
ion battery
welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710979832.6A
Other languages
Chinese (zh)
Inventor
冯臣相
钟芳琦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangxi Hengdong New Energy Co Ltd
Original Assignee
Jiangxi Hengdong New Energy Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangxi Hengdong New Energy Co Ltd filed Critical Jiangxi Hengdong New Energy Co Ltd
Priority to CN201710979832.6A priority Critical patent/CN107876979A/en
Publication of CN107876979A publication Critical patent/CN107876979A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of power lithium-ion battery liquid injection port to seal method for laser welding, the position beginning and end of laser-beam welding machine welding track being arranged on beyond laser welded seam.Advantages of the present invention:Prevent the phenomenon that the unstable caused laser welded seam of laser-beam welding machine energy when going out laser and closing laser fries hole leakage, ensure that the intersection of beginning and end very overlaps, and improves sealing in the lump;The position that beginning and end need to only fall beyond laser welded seam can be, it is necessary to which the position of accurate starting point and terminal, the laser welded seam distance that beginning and end arrives be simple to operate without accurate.

Description

A kind of power lithium-ion battery liquid injection port seals method for laser welding
Technical field
The present invention relates to a kind of power lithium-ion battery liquid injection port to seal method for laser welding, belongs to lithium battery technology neck Domain.
Background technology
With the continuous progress of lithium-ion-power cell technology, the lithium ion battery of metal shell increasingly turns into main flow, gold Belong to the advantages of housing battery is due to high stability, high security, wide small volume and tolerable temperature scope, it is commercially Occupation rate constantly rises.Lithium battery in the fabrication process, when into battery container inject electrolyte after, due to electrolyte to be maintained Stability and need to be sealed the liquid injection port of battery container, at present generally using being laser welded seal, this kind of technology Efficiency high, good sealing effect, prior art are first to determine the track of weld seam, select some point on weld seam to be used as starting point, swash Light rotates a circle around starting point and reached home, and terminal and starting point overlap, but laser-beam welding machine energy when going out laser and closing laser Measure unstable, fried hole leakage can be caused, therefore the welding of terminal and starting point is unstable, beginning and end on soldered, Weld can be caused laser penetration housing or the complete situation of welded seal occur, it is also possible to the friendship of beginning and end occur Do not overlapped also at boundary, the situation that laser turns off, liquid injection port sealing is undesirable, the phenomenon of leakage occurs.
Chinese patent CN104772567B, discloses the method for laser welding for reducing the starting the arc and receiving arc defect, and this method is At starting the arc end and receive arc end and change interaction angle between laser and mother metal, to regulate and control molten bath and aperture in welding process Form, so as to solve the problems, such as easily to produce defect at starting the arc end and receipts arc end during fusion welding, avoid in starting the arc end and receipts There is the unstable of laser beam welding in arc end, reaches the purpose for improving laser welding reliability, although this kind of method has Certain effect, but want accurate starting the arc end and receive arc end position, and original incident direction, oblique incidence direction, receipts arc incidence Direction, the requirement to purification bonding machine is higher, and intermediate demand translation-angle, practical operation are got up relatively difficult.
The content of the invention
The technical problem to be solved in the present invention, be to provide a kind of intersection for ensureing beginning and end very overlap, Sealing is strong, it is simple to operate, seal laser welding side without the power lithium-ion battery liquid injection port in accurate starting point and final position Method.
The present invention is realized by following proposal:A kind of power lithium-ion battery liquid injection port seals method for laser welding, will swash The beginning and end of photocoagulator welding track is arranged on the position beyond laser welded seam.
By welding program the position beginning and end of laser-beam welding machine welding track being arranged on beyond laser welded seam.
The welding track is made up of laser welded seam, changeover portion and breeze way, and changeover portion is starting point between laser welded seam Track, buffering section laser welded seam is to the track between terminal.
The intersection of the changeover portion and breeze way is some point fallen on laser welded seam.
The changeover portion and breeze way are linear or arc.
The changeover portion and breeze way are the tangent line of laser welded seam.
The laser welded seam falls between sealing valve block and battery container, and beginning and end falls the electricity beyond laser welded seam On the housing of pond.
Liquid injection port is cleaned using laser marking machine before power lithium-ion battery liquid injection port seals laser welding, swashed The laser that light marking machine is sent is as follows according to the circle of laser index carving cleaning track movement one, cleaning in the surrounding of liquid injection port:
Step 1, on laser marking machine CCD is installed and taken pictures detecting system;
Step 2, by CCD take pictures detecting system Automatic-searching liquid injection port and determine laser index carving clean track;
Step 3, the surface whole marking cleaning at laser welded seal position, crystallization electrolyte, foreign matter will be needed by going out laser automatically And surface oxide layer vaporization at high temperature during laser index carving, then taken away by smoke discharging dust removing system;
Step 4, enters the lower section of laser-beam welding machine after step 3 cleaning by streamline, and automatic sealing valve block of placing is carried out Laser welding.
Beneficial effects of the present invention are:
1st, a kind of power lithium-ion battery liquid injection port of present invention sealing method for laser welding by laser-beam welding machine welding track Beginning and end is arranged on the position beyond weld seam, and preventing laser-beam welding machine, energy is unstable causes when going out laser and closing laser Laser welded seam fry hole leakage phenomenon, in the lump ensure beginning and end intersection very overlap, improve sealing;
2nd, a kind of beginning and end of power lithium-ion battery liquid injection port sealing method for laser welding of the present invention need to only fall in laser Position beyond weld seam can be, it is necessary to which the position of accurate starting point and terminal, the laser welded seam distance that beginning and end arrives be without essence Really, it is simple to operate.
Brief description of the drawings
Fig. 1 is a kind of welding track signal that a kind of power lithium-ion battery liquid injection port of the present invention seals method for laser welding Figure.
Fig. 2 is that a kind of another welding track of power lithium-ion battery liquid injection port sealing method for laser welding of the present invention shows It is intended to.
Fig. 3 is the welding track schematic diagram in background information.
In figure:1 is starting point, and 2 be terminal, and 3 be laser welded seam, and 4 be changeover portion, and 5 be breeze way, and 6 be sealing valve block, and 7 are Battery container.
Embodiment
With reference to Fig. 1-3, the present invention is further described, but the scope of the present invention does not limit to the content.
Wherein identical parts are presented with like reference characters.It should be noted that the word used below in description Language "front", "rear", "left", "right", "up" and "down" refer to the direction in accompanying drawing, and word " interior " and " outer " refer respectively to court To or away from particular elements geometric centers direction, and accompanying drawing is compared using very simplified form and accurately using non- Rate, only for the purpose of facilitating and clarifying the purpose of the embodiments of the invention.
For clarity, not describing whole features of practical embodiments, in the following description, known function is not described in detail And structure, because they can make the present invention chaotic due to unnecessary details, it will be understood that opening in any practical embodiments In hair, it is necessary to a large amount of implementation details are made to realize the specific objective of developer, such as according to relevant system or relevant business Limitation, another embodiment is changed into by one embodiment, additionally, it should think that this development is probably complicated and expended Time, but it is only to those skilled in the art routine work.
A kind of power lithium-ion battery liquid injection port seals method for laser welding, by the starting point 1 of laser-beam welding machine welding track The position beyond laser welded seam 3 is arranged on terminal 2.
By welding program the position starting point 1 of laser-beam welding machine welding track and terminal 2 being arranged on beyond laser welded seam 3 Put.
Welding track is made up of laser welded seam 3, changeover portion 4 and breeze way 5, changeover portion 4 be starting point 1 to laser welded seam 3 it Between track, 5 laser welded seams 3 of breeze way arrive terminal 2 between track.
The intersection of changeover portion 4 and breeze way 5 is some point fallen on laser welded seam 3.
Changeover portion 4 and breeze way 5 are linear or arc.
Changeover portion 4 and the tangent line that breeze way 5 is laser welded seam 3.
Laser welded seam 3 falls between sealing valve block 6 and battery container 7, and starting point 1 and terminal 2 fall beyond laser welded seam 3 On battery container 7.
Liquid injection port is cleaned using laser marking machine before power lithium-ion battery liquid injection port seals laser welding, swashed The laser that light marking machine is sent is as follows according to the circle of laser index carving cleaning track movement one, cleaning in the surrounding of liquid injection port:
Step 1, on laser marking machine CCD is installed and taken pictures detecting system;
Step 2, by CCD take pictures detecting system Automatic-searching liquid injection port and determine laser index carving clean track;
Step 3, the surface whole marking cleaning at laser welded seal position, crystallization electrolyte, foreign matter will be needed by going out laser automatically And surface oxide layer vaporization at high temperature during laser index carving, then taken away by smoke discharging dust removing system;
Step 4, enters the lower section of laser-beam welding machine after step 3 cleaning by streamline, and automatic sealing valve block 6 of placing is carried out Laser welding.
Although more detailed elaboration is done to technical scheme and has been enumerated, it will be appreciated that for ability For field technique personnel, modification is made to above-described embodiment or uses equivalent alternative solution, this is to those skilled in the art It is it is clear that these modifications or improvements without departing from theon the basis of the spirit of the present invention, belong to the present invention for member Claimed scope.

Claims (8)

1. a kind of power lithium-ion battery liquid injection port seals method for laser welding, it is characterised in that:Laser-beam welding machine is welded into rail The starting point of mark(1)And terminal(2)It is arranged on laser welded seam(3)Position in addition.
A kind of 2. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 1, it is characterised in that: By welding programming by the starting point of laser-beam welding machine welding track(1)And terminal(2)It is arranged on laser welded seam(3)Position in addition Put.
A kind of 3. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 2, it is characterised in that: The welding track is by laser welded seam(3), changeover portion(4)And breeze way(5)Composition, changeover portion(4)For starting point(1)To Laser Welding Seam(3)Between track, breeze way(5)Position laser welded seam(3)To terminal(2)Between track.
A kind of 4. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 3, it is characterised in that: The changeover portion(4)With breeze way(5)Intersection be to fall in laser welded seam(3)On some point.
A kind of 5. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 3, it is characterised in that: The changeover portion(4)And breeze way(5)For linear or arc.
A kind of 6. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 3, it is characterised in that: The changeover portion(4)And breeze way(5)For laser welded seam(3)Tangent line.
A kind of 7. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 3, it is characterised in that: The laser welded seam(3)Fall in sealing valve block(6)And battery container(7)Between, starting point(1)And terminal(2)Fall in laser welded seam (3)Battery container in addition(7)On.
A kind of 8. power lithium-ion battery liquid injection port sealing method for laser welding according to claim 1, it is characterised in that: Liquid injection port is cleaned using laser marking machine before power lithium-ion battery liquid injection port seals laser welding, laser marking machine The laser sent is as follows according to the circle of laser index carving cleaning track movement one, cleaning in the surrounding of liquid injection port:
Step 1, on laser marking machine CCD is installed and taken pictures detecting system;
Step 2, by CCD take pictures detecting system Automatic-searching liquid injection port and determine laser index carving clean track;
Step 3, the surface whole marking cleaning at laser welded seal position, crystallization electrolyte, foreign matter will be needed by going out laser automatically And surface oxide layer vaporization at high temperature during laser index carving, then taken away by smoke discharging dust removing system;
Step 4, enter the lower section of laser-beam welding machine by streamline after step 3 cleaning, it is automatic to place sealing valve block(6)Enter Row laser welding.
CN201710979832.6A 2017-10-19 2017-10-19 A kind of power lithium-ion battery liquid injection port seals method for laser welding Pending CN107876979A (en)