- Prior art keywords
- housing
- paint
- skin
- spray painting
- oxidation processes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D11/00—Electrolytic coating by surface reaction, i.e. forming conversion layers
- C25D11/02—Anodisation
- C25D11/04—Anodisation of aluminium or alloys based thereon
- C25D11/14—Producing integrally coloured layers
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D11/00—Electrolytic coating by surface reaction, i.e. forming conversion layers
- C25D11/02—Anodisation
- C25D11/04—Anodisation of aluminium or alloys based thereon
- C25D11/16—Pretreatment, e.g. desmutting
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D11/00—Electrolytic coating by surface reaction, i.e. forming conversion layers
- C25D11/02—Anodisation
- C25D11/04—Anodisation of aluminium or alloys based thereon
- C25D11/18—After-treatment, e.g. pore-sealing
-
- H—ELECTRICITY
- H05—ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR
- H05K—PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H05K5/00—Casings, cabinets or drawers for electric apparatus
- H05K5/02—Details
- H05K5/0217—Mechanical details of casings
- H05K5/0243—Mechanical details of casings for decorative purposes
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Microelectronics & Electronic Packaging (AREA)
- Casings For Electric Apparatus (AREA)
Abstract
The embodiment of the present application discloses a kind of method for producing shell, housing and electronic equipment, wherein, method for producing shell includes:First, there is provided a housing, and the outer surface of housing is processed by shot blasting, blasting treatment is carried out to the housing outer surface after polishing;Then, monochromatic oxidation processes are carried out to the housing outer surface after blasting treatment, carrying out spray painting at least once to the housing outer surface after monochromatic oxidation processes is handled, and at least one layer of skin of paint is formed in housing outer surface.The embodiment of the present application can make it that surface of shell is smooth, fingerprint not easy to stick, and housing outer surface can be kept clean and tidy.
Description
Technical field
The application is related to technical field of electronic equipment, and in particular to a kind of method for producing shell, housing and electronic equipment.
Background technology
At present, electronic equipment, the raw material that for example mobile phone, the housing of tablet personal computer prepare processing is usually aluminium, and business
The aluminium being commercially available then due to its rigidity the problems such as can not directly use.Need to carry out multiple working process to raw material aluminium
Shell structure needed for formation.However, after housing processing of the prior art, housing outer surface easily glues fingerprint.
The content of the invention
The embodiment of the present application provides a kind of method for producing shell, housing and electronic equipment, it is possible to reduce housing outer surface
Viscous fingerprint.
In a first aspect, the embodiment of the present application provides a kind of method for producing shell, the housing is used in electronic equipment, described
Method for producing shell includes:
One housing is provided;
The outer surface of the housing is processed by shot blasting;
Blasting treatment is carried out to the housing outer surface after the polishing;
Monochromatic oxidation processes are carried out to the housing outer surface after the blasting treatment;
Spray painting at least once is carried out to the housing outer surface after the monochromatic oxidation processes to handle, in the housing outer surface
Form at least one layer of skin of paint.
Second aspect, the embodiment of the present application also provide a kind of housing, and the housing uses housing making side as described above
Method is formed.
The third aspect, the embodiment of the present application also provide a kind of housing, and applied in electronic equipment, the housing includes relative
The inner surface of setting and outer surface, the housing include concaveconvex structure, oxide layer and the skin of paint formed on the outer surface,
The oxide layer is formed on the concaveconvex structure, and the skin of paint is formed in the oxide layer.
Fourth aspect, the embodiment of the present application additionally provide a kind of electronic equipment, including housing, and the housing is as described above
Housing.
The method for producing shell that the embodiment of the present application provides, first, there is provided a housing, and the outer surface of housing is thrown
Light processing, blasting treatment is carried out to the housing outer surface after polishing;Then, the housing outer surface after blasting treatment is carried out
Monochromatic oxidation processes, spray painting at least once is carried out to the housing outer surface after monochromatic oxidation processes and handled, in housing outer surface shape
Into at least one layer of skin of paint.It can make it that surface of shell is smooth, fingerprint not easy to stick, housing outer surface can be kept whole
It is clean.
Brief description of the drawings
In order to illustrate more clearly of the technical scheme in the embodiment of the present application, make required in being described below to embodiment
Accompanying drawing is briefly described, it should be apparent that, drawings in the following description are only some embodiments of the present application, for
For those skilled in the art, on the premise of not paying creative work, it can also be obtained according to these accompanying drawings other attached
Figure.
Fig. 1 is the structural representation for the electronic equipment that the embodiment of the present application provides.
Fig. 2 is the structural representation for the housing that the embodiment of the present application provides.
Fig. 3 is the structural representation for the bonnet that the embodiment of the present application provides.
Fig. 4 is profiles of the Fig. 3 in A-A directions.
Fig. 5 is another profiles of the Fig. 3 in A-A directions.
Fig. 6 is another profiles of the Fig. 3 in A-A directions.
Fig. 7 is another profiles of the Fig. 3 in A-A directions.
Fig. 8 is another profiles of the Fig. 3 in A-A directions.
Fig. 9 is another profiles of the Fig. 3 in A-A directions.
Figure 10 is another structural representation for the housing that the embodiment of the present application provides.
Figure 11 is another structural representation for the bonnet that the embodiment of the present application provides.
Figure 12 is another structural representation for the electronic equipment that the embodiment of the present application provides.
Figure 13 is the schematic flow sheet for the bonnet preparation method that the embodiment of the present application provides.
Figure 14 is the schematic flow sheet for the spray painting processing that the embodiment of the present application provides.
Embodiment
Below in conjunction with the accompanying drawing in the embodiment of the present application, the technical scheme in the embodiment of the present application is carried out clear, complete
Site preparation describes.Obviously, described embodiment is only some embodiments of the present application, rather than whole embodiments.It is based on
Embodiment in the application, the every other implementation that those skilled in the art are obtained under the premise of creative work is not made
Example, belong to the scope of the application protection.
In the description of the present application, it is to be understood that term " " center ", " longitudinal direction ", " transverse direction ", " length ", " width ",
" thickness ", " on ", " under ", "front", "rear", "left", "right", " vertical ", " level ", " top ", " bottom ", " interior ", " outer ", " up time
The orientation or position relationship of the instruction such as pin ", " counterclockwise " are based on orientation shown in the drawings or position relationship, are for only for ease of
Describe the application and simplify to describe, rather than indicate or imply that signified device or element must have specific orientation, Yi Te
Fixed azimuth configuration and operation, therefore it is not intended that limitation to the application.In addition, term " first ", " second " are only used for
Purpose is described, and it is not intended that instruction or hint relative importance or the implicit quantity for indicating indicated technical characteristic.
Thus, " first " is defined, the feature of " second " can be expressed or implicitly includes one or more feature.
In the description of the present application, " multiple " are meant that two or more, unless otherwise specifically defined.
, it is necessary to illustrate in the description of the present application, unless otherwise clearly defined and limited, term " installation ", " phase
Even ", " connection " should be interpreted broadly, for example, it may be being fixedly connected or being detachably connected, or be integrally connected;Can
To be mechanical connection or electrical connection or can mutually communicate;Can be joined directly together, can also be by between intermediary
Connect connected, can be connection or the interaction relationship of two elements of two element internals.For the ordinary skill of this area
For personnel, the concrete meaning of above-mentioned term in this application can be understood as the case may be.
In this application, unless otherwise clearly defined and limited, fisrt feature second feature it " on " or it " under "
Can directly it be contacted including the first and second features, it is not directly to contact but pass through it that can also include the first and second features
Between other characterisation contact.Moreover, fisrt feature second feature " on ", " top " and " above " to include first special
Sign is directly over second feature and oblique upper, or is merely representative of fisrt feature level height and is higher than second feature.Fisrt feature exists
Second feature " under ", " lower section " and " following " fisrt feature that includes are immediately below second feature and obliquely downward, or be merely representative of
Fisrt feature level height is less than second feature.
Following disclosure provides many different embodiments or example is used for realizing the different structure of the application.In order to
Simplify disclosure herein, hereinafter the part and setting of specific examples are described.Certainly, they are only example, and
And purpose does not lie in limitation the application.In addition, the application can in different examples repeat reference numerals and/or reference letter,
This repetition is for purposes of simplicity and clarity, between itself not indicating discussed various embodiments and/or setting
Relation.In addition, this application provides various specific techniques and material examples, but those of ordinary skill in the art can be with
Recognize the application of other techniques and/or the use of other materials.
The embodiment of the present application provides a kind of method for producing shell, housing and electronic equipment.It will carry out respectively below detailed
Explanation.
In the present embodiment, will be described from the angle of bonnet preparation method, the method for producing shell can form shell
Body, the housing can be set in the electronic device, such as mobile phone, tablet personal computer, palm PC (Personal Digital
Assistant, PDA) etc..
Refer to the structural representation that 1, Fig. 1 is the electronic equipment that the embodiment of the present application provides.The electronic equipment 1 includes shell
Body 10, display screen 20, printed circuit board 30, battery 40.
Referring to Fig. 2, Fig. 2 is the structural representation for the housing that the embodiment of the present application provides.Wherein, the housing 10 can wrap
Cover plate 11, center 12 and bonnet 13 are included, cover plate 11, center 12 and bonnet 13 are mutually combined to form the housing 10, and the housing 10 has
There is the confined space formed by cover plate 11, center 12 and bonnet 13, to accommodate display screen 20, printed circuit board 30, battery 40
Deng device.In certain embodiments, the lid of cover plate 11 is set on center 12, and the lid of bonnet 13 is set on center 12, cover plate 11 and bonnet
13 are located at the opposite face of center 12, and cover plate 11 and bonnet 13 are oppositely arranged, and the confined space of housing 10 is located at cover plate 11 and bonnet
Between 13.
Wherein, cover plate 11 can be transparent glass cover plate.In some embodiments, cover plate 11 can be with such as blue precious
Glass cover-plate made of the materials such as stone.Wherein, center 12 can be metal shell, such as aluminium alloy center 12.Need what is illustrated
It is that the material of the embodiment of the present application center 12 is not limited to this, other manner can also be used, such as:Center 12 can ceramics
Center, glass center.For another example:Center 12 can be plastic cement center.Also such as:Center 12 can be metal and plastic cement phase interworking
The structure of conjunction, plastic portions and being molded on sheet metal can be formed.Wherein, bonnet 13 can be with metal back cover, such as aluminium
Alloy bonnet.
Also referring to Fig. 3, Fig. 3 is the structural representation for the bonnet that the embodiment of the present application provides.The bonnet 13 can wrap
The inner surface 131 being oppositely arranged and outer surface 132 are included, the inner surface 131 of the bonnet 13 forms shell close to center 12 and cover plate 11
The inner surface of body 10, the outer surface 132 of the bonnet 13 is away from center 12 and cover plate 11, the outer surface of formation housing 10.The bonnet
13 can also include volcanic crater 133, and the volcanic crater 133 can install camera.
Also referring to Fig. 4, Fig. 4 is profiles of the Fig. 3 in A-A directions.Bonnet 13a can include bonnet substrate 137,
Oxide layer 134 and skin of paint 136.
Wherein, bonnet substrate 137 can use aluminium, such as aluminium alloy.The bonnet substrate 137 includes the He of inner surface 131
Outer surface 132, the inner surface of the bonnet substrate 137 can be understood as the inner surface of bonnet 13, and the bonnet substrate 137 is outer
Surface can be understood as the outer surface before bonnet is not aoxidized, painted etc..
Wherein, oxide layer 134 is formed on the outer surface 132 of bonnet substrate 137.The oxide layer 134 can be by once
Oxidation forms layer of oxide layer 134.Such as:Monochrome oxidation forms the oxide layer 134, specifically can be by being carried out after oxidation technology
Coloring is formed.It should be noted that in some embodiments, it is also possible to formed using oxidation twice or oxidation more than twice
Multilayer oxide layer.
Such as:Referring to Fig. 5, Fig. 5 is another profiles of the Fig. 3 in A-A directions.Fig. 5 and Fig. 4 difference is:Bonnet
13b oxide layer 134 includes two layers, i.e. the first oxide layer 1341 and the second oxide layer 1342.First oxide layer 1341 is formed
On the outer surface 132 of bonnet substrate 137, the second oxide layer 1342 is formed in the first oxide layer 1341, in certain embodiments,
The part that second oxide layer can be covered only in the first oxide layer.First oxide layer 1341 and the second oxide layer 1342 can
To increase the adhesion with skin of paint 136.Wherein, the sandwich construction on oxide layer, is no longer illustrated one by one herein.One
In a little embodiments, first oxide layer can be colored oxide layer, and the second oxide layer can also be colored oxide layer.First oxygen
The color for changing layer can be different from the color of the second oxide layer, can also be identical.Wherein, skin of paint 136 is formed in oxide layer 134
On, oxide layer 134 is between skin of paint 136 and bonnet substrate 137.In certain embodiments, can be sprayed in oxide layer 134
One layer of paint forms the skin of paint 136.The skin of paint 136 is located at the outermost layer of the outer surface of bonnet 13, and its surface is smooth, no
Fingerprint easy to stick, exterior surface cleaning is smooth after can keeping.
It should be noted that in some embodiments, it is also possible to two layers of paint or more than two layers are sprayed in oxide layer 134
Paint, to form two layers of skin of paint or multilayer skin of paint.Such as:Referring to Fig. 6, Fig. 6 is another sections of the Fig. 3 in A-A directions
Figure.Fig. 6 and Fig. 4 difference is:Bonnet 13c skin of paint 136 includes the first skin of paint 1361 and the second skin of paint 1362.Should
First skin of paint 1361 is formed in oxide layer 134, and second skin of paint 1362 is formed on the first skin of paint 1361.At some
In embodiment, the thickness of the second skin of paint 1362 is more than the thickness of the first skin of paint 1361, further, the second skin of paint 1362
Thickness be twice of thickness of the first skin of paint 1361, for example the thickness of the second skin of paint 1362 is 10um, the first skin of paint
1361 thickness is 5um.It should also be noted that, the second skin of paint 1362 and the first skin of paint 1361 in process of production may
In the presence of certain error amount, for example error amount is 0.5um.The setting of second skin of paint and the first skin of paint thickness can be to bonnet
Outer surface provides preferably protection, and so that is bonded between two layers of skin of paint even closer.
For another example:Referring to Fig. 7, Fig. 7 is another profiles of the Fig. 3 in A-A directions.Fig. 7 and Fig. 4 difference is:Afterwards
Lid 13d skin of paint 136 includes the first skin of paint 1361, the second skin of paint 1362 and the 3rd skin of paint 1363.First paint
Layer 1361 is formed in oxide layer 134, and second skin of paint 1362 is formed on the first skin of paint 1361, the 3rd skin of paint
1363 form on the second skin of paint 1362.Formed in oxide layer 134 two layers or three layers of skin of paint can increase oxide layer and
The adhesion of skin of paint, to the protecting effect of bonnet more preferably.In certain embodiments, the thickness of the 3rd skin of paint 1363 is more than the
Two skin of paints 1362, the thickness of the second skin of paint 1362 are more than the thickness of the first skin of paint 1361.Further, the 3rd skin of paint
1363 thickness is twice of the thickness of the second skin of paint 1362, and the thickness of the second skin of paint 1362 is the first skin of paint 1361
Twice of thickness, for example the thickness of the 3rd skin of paint 1363 is 8um, the thickness of the second skin of paint 1362 are 4um, the first skin of paint
1361 thickness is 2um.
In certain embodiments, the thickness of the 3rd skin of paint 1363, the second skin of paint 1362 and the first skin of paint 1361 according to
Secondary equal thickness is reduced, for example the thickness of the 3rd skin of paint 1363 is 9um, and the thickness of the second skin of paint 1362 is 6um, and first paints
The thickness of layer 1361 is 3um.The setting of 3rd skin of paint, the second skin of paint and the first skin of paint thickness can be to rear exterior surface
Preferably protection is provided, and so that bonded between three layers of skin of paint even closer.
In certain embodiments, the skin of paint can be with transparent setting.It should be noted that when skin of paint is at least two layers
When, wherein at least one layer of skin of paint can be with transparent setting.Further, the transparent setting of all skin of paints.Aoxidized with bonnet
Layer is the appearance face color of bonnet.
In order to increase the adhesion between skin of paint 136 and oxide layer 134, in certain embodiments, referring to Fig. 8, Fig. 8
For another profiles of the Fig. 4 in A-A directions.Fig. 8 and Fig. 4 difference is:Bonnet 13e can also include binder course 135.The knot
Close layer 135 to be formed in oxide layer 134, skin of paint 136 is formed on binder course 135.In certain embodiments, the binder course
135 can be formed in oxide layer 134 using PVD (Physical Vapor Deposition, physical vapour deposition (PVD)) mode
On.The binder course 135 can increase between oxide layer 134 and skin of paint 136 between oxide layer 134 and skin of paint 136
Adhesion.It should be noted that the embodiment of the present application can also other manner oxide layer formed binder course, to increase oxide layer
With the adhesion of skin of paint.
In certain embodiments, referring to Fig. 9, Fig. 9 be Fig. 4 in another profile in A-A directions, Fig. 9 and Fig. 4 difference
It is:The outer surface of bonnet 13f bonnets substrate 137 forms concaveconvex structure 1371, and the concaveconvex structure 1371 can pass through sand-blasting machine
Formed by the way of sandblasting so that the outer surface of bonnet substrate 137 is cleaned, be coarse, and then can increase to be formed and be tied in the bumps
Adhesion on structure 1371 between oxide layer 134 and skin of paint 136.
It should be noted that the structure of the bonnet is not limited to this, such as:Bonnet can include two layers or multilayer aoxidizes
Layer, two layers or multilayer skin of paint.For another example:Bonnet can include two layers or multilayer oxide layer, two layers or multilayer skin of paint and
Binder course.For another example:Bonnet can include two layers or multilayer oxide layer, two layers or multilayer skin of paint and binder course.Need
Bright, the number of plies between oxide layer, binder course and skin of paint changes within the protection domain of the embodiment of the present application,
This is no longer illustrated one by one.
It should be noted that the structure of the embodiment of the present application housing is not limited to this, such as, referring to Fig. 10, Figure 10 is
Another structural representation for the housing that the embodiment of the present application provides.Wherein, the housing 10a shown in Figure 10 includes cover plate 16 and bonnet
17.In certain embodiments, the directly lid of cover plate 16 is set on bonnet 17, and cover plate 16 and bonnet 17 are mutually combined to form the housing
10a, housing 10a have the confined space formed by cover plate 16 and bonnet 17, to accommodate display screen 20, printed circuit board
30th, the device such as battery 40.Compared to the housing 10 shown in Fig. 2, housing 10a does not include center, or perhaps by the center in Fig. 2
12 and bonnet 13 be integrally formed to form the structure of a bonnet 17 (certainly, middle frame structure can also be named as herein).Specifically, it please join
Figure 11 is read, Figure 11 is another structural representation for the bonnet that the embodiment of the present application provides.In certain embodiments, bonnet 17 includes
Inner surface 171 and outer surface 172, inner surface 171 and outer surface 172 are oppositely arranged, and form the whole surface of bonnet 17.The bonnet
17 each Rotating fields can refer to bonnet 13, will not be repeated here.
Wherein, the printed circuit board 30 is installed in the housing 10, and the printed circuit board 30 can be the master of electronic equipment 1
Plate, antenna, motor, microphone, camera, light sensor, receiver and processing can be integrated with printed circuit board 30
The functional units such as device.In certain embodiments, the printed circuit board 30 is fixed in housing 10.Specifically, the printed circuit board
30 can be screwed on center 12 by screw, can also be fitted on using card by the way of buckle on center 12.It should be noted that
The mode that the embodiment of the present application printed circuit board 30 is specifically fixed on center 12 is not limited to this, can with other manner, than
Such as by way of buckle and screw are fixed jointly.
Wherein, the battery 40 is installed in the housing 10, and battery 40 is electrically connected with the printed circuit board 30, with to electronics
Equipment 1 provides power supply.Housing 10 can be as the battery cover of battery 40.Housing 10 covers battery 40 to protect battery 40, specifically
Be that bonnet 13 covers battery 40 to protect battery 40, reduce battery 40 due to electronic equipment 1 collision, fall etc. and be subject to
Damage.
Wherein, the display screen 20 is installed in the housing 10, meanwhile, the display screen 20 is electrically connected on printed circuit board 30,
To form the display surface of electronic equipment 1.The display screen 20 includes viewing area 14 and non-display area 15.The viewing area 14 can
With for showing the picture of electronic equipment 1 or carry out touching manipulation etc. for user.The top area of the non-display area 15 is opened
If for the perforate of sound and light conduction, the functions such as fingerprint module, touch controlled key can be set on the bottom of non-display area 15
Component.Wherein the cover plate 11 is installed on display screen 20, to cover display screen 20, is formed and the identical viewing area of display screen 20
And non-display area, viewing area that specifically can be refering to display screen 20 and non-display area.
It should be noted that the structure of the display screen 20 is not limited to this.For example the display screen can be comprehensive screen or different
Property screen, specifically, refer to Figure 12, Figure 12 is another structural representation for the electronic equipment that the embodiment of the present application provides.Figure 12
In electronic equipment and Fig. 1 in the difference of electronic equipment be:Non-display area 15a is formed directly on display screen 20a,
For example it is arranged to transparent configuration in display screen 20a non-display area 15a, so that optical signal passes through, or directly in display screen
20a non-display area is opened up for structures such as the perforate of light conduction or breach, can be by front camera, photoelectric sensor etc.
Non-display area position is arranged at, so that front camera is taken pictures, photoelectric sensor detects.Viewing area 14a is paved with electronics
Equipment 1a whole surfaces.It should be noted that the device such as housing 10, printed circuit board 30 and battery 40 in electronic equipment 1a
Above content can be referred to, will not be repeated here.
In order to further describe the shell structure of the embodiment of the present application, carried out specifically by taking method for producing shell as an example below
It is bright.It should be noted that method for producing shell can specifically include bonnet preparation method, center preparation method.Housing system below
Make method to illustrate by taking bonnet preparation method as an example, it is to be understood that the embodiment of the present application method for producing shell is simultaneously unlimited
In bonnet.
Also referring to Figure 13, Figure 13 is the schematic flow sheet for the bonnet preparation method that the embodiment of the present application provides.After this
Lid preparation method comprises the following steps:
In a step 101, there is provided a bonnet.The bonnet can be metal material, such as aluminium, further, such as aluminium
Alloy.It should be noted that the bonnet can be directly commercially available, sheet fabrication can also be obtained, such as to aluminium alloy plate
The PROCESS FOR TREATMENTs such as material is forged and pressed, timeliness obtain.
Wherein, the bonnet can include inner surface and the outer surface being oppositely arranged, and the bonnet and its inner surface, outer surface can
Refering to above content, will not be repeated here.
In a step 102, the outer surface of bonnet is processed by shot blasting.So that rear exterior surface is smooth.
In certain embodiments, can be real to rear exterior surface by the way of machinery, chemistry, electrochemistry or ultrasonic wave etc.
Now polish.To cause the reduction of bonnet surface roughness, to obtain bright, flat surface rear exterior surface.Wherein, chemical polishing
Mode is to carry out regular dissolving to rear exterior surface to reach smooth.Wherein, electrochemical polish mode is by bonnet appearance
Face is negative electrode as anode, insoluble petal, and the two poles of the earth are immersed in electrolytic cell simultaneously, leads to direct current and produces selective anode
Solution, so that the increase of bonnet exterior surface gloss degree is big.The mode wherein mechanically polished is by exterior surface after cutting so that
Exterior surface plastic deformation removes the convex portion after polishing and obtains even surface afterwards.The mode of wherein ultrasonic polishing is to put bonnet
Enter in abrasive suspension and be placed in together in ultrasound field, by the oscillation action of ultrasonic wave, abrasive material is ground in workpiece surface
Polishing.
In certain embodiments, before being processed by shot blasting to the outer surface of bonnet, first rear exterior surface can be entered
Row grinding process, then the rear exterior surface after grinding process is processed by shot blasting again, makes polishing better so that
Exterior surface is more smooth afterwards.Here, it should be noted that the grinding process can be understood as to thick before polishing plus
Work.I.e., it is possible to first carry out once thick polishing to rear exterior surface, then once carefully polished, complete polishing.
In step 103, blasting treatment is carried out to the rear exterior surface after polishing.
In certain embodiments, blasting treatment is carried out to the rear exterior surface after polishing, can be in rear exterior surface
Concaveconvex structure is formed, the concaveconvex structure can increase the adhesion between oxide layer and skin of paint.The wherein concaveconvex structure can be with
Refering to above content, will not be repeated here.
At step 104, monochromatic oxidation processes are carried out to the rear exterior surface after blasting treatment.Specifically, the step 104
Specifically include:Oxidation processes are carried out to the rear exterior surface after blasting treatment, to form oxide layer;And to oxidation processes after
Exterior surface carries out coloring treatment afterwards, with the color of exterior surface after the formation in oxide layer.
In certain embodiments, monochromatic oxidation processes can be carried out to the rear exterior surface after blasting treatment, to form oxygen
Change layer, or perhaps oxide-film, and carry out coloring treatment after oxidation, and then form required appearance color, such as red,
Blueness etc..
It should be noted that in some embodiments, it is also possible to after blasting treatment rear exterior surface carry out twice or
Oxidation processes more than twice, to form at least two layers of oxide layer, coloring treatment can be carried out during once oxidation wherein,
Oxidation processes can also be carried out in each oxidizing process, and then form required appearance color.Pass through oxygen two or more times
Change processing not only to the protecting effect of rear exterior surface more preferably, and at least two layers formed twice or more after this oxidation and oil
The adhesion of enamelled coating is more preferable.
In step 105, carry out spray painting at least once to the rear exterior surface after monochromatic oxidation processes to handle, outside bonnet
Surface forms at least one layer of skin of paint.At least one layer of skin of paint is formed in oxide layer.After at least one layer of skin of paint is located at
The outermost layer of exterior surface, its surface is smooth, and fingerprint not easy to stick, exterior surface cleaning is smooth after can keeping.
In certain embodiments, once spray painting processing can be carried out in oxide layer, forms one layer of skin of paint, can also be
The processing of spray painting two or more times is carried out in oxide layer, forms two layers or more than two layers of skin of paint.It should be noted that work as oxygen
When change layer only has one layer, once spray painting can be directly carried out in oxide layer and handled, formed one layer of skin of paint, can also aoxidize
The processing of spray painting two or more times is carried out on layer, forms two layers or more than two layers of skin of paint.
In certain embodiments, after the rear exterior surface after monochromatic oxidation processes carries out the processing of spray painting at least once,
Rear exterior surface can be toasted at least once, high-temperature baking can be used, the paint of rear exterior surface will be sprayed on
Drying forms skin of paint.For example baking temperature is 80 degree, baking time is rear exterior surface to be toasted in 1 hour.Need
It is bright, once baking processing can be carried out after the processing of spray painting each time.Illustrated below by taking processing of painting twice as an example,
Figure 14 is referred to, Figure 14 is the schematic flow sheet for the spray painting processing that the embodiment of the present application provides.The technical process of spray painting processing
Including:
In step 1051, first time spray painting processing is carried out to the rear exterior surface after monochromatic oxidation processes.At oxidation
Rear exterior surface after reason carries out first time spray painting, sprays celluloid paint.
In step 1052, the rear exterior surface after handling first time spray painting carries out first time baking processing, in bonnet
Outer surface forms the first skin of paint.Spray painting processing for the first time and baking processing can increase oxide layer and first time spray paint
Adhesion.
In step 1053, the rear exterior surface after handling first time baking carries out second of spray painting processing.First
Rear exterior surface after secondary baking processing carries out second of spray painting processing, sprays celluloid paint.
In step 1054, the rear exterior surface after handling second of spray painting carries out second of baking processing, outside bonnet
Surface forms the second skin of paint, and the second skin of paint is formed on the first skin of paint.
In certain embodiments, first skin of paint and the second skin of paint are that celluloid paint is formed.Need what is illustrated
Be have in the first skin of paint and the second skin of paint one layer for clean oil enamelled coating it is also possible.
It should be noted that can also be painted three times processing and baking processing three times, will not be repeated here.Wherein,
Thickness relationship between each skin of paint can refer to above content, will not be repeated here.
In certain embodiments, rear exterior surface that can be after the oxidising treat-ment carries out physical vapor deposition processing, with
Exterior surface forms binder course afterwards, in other words with reference to film, is specifically formed in oxide layer.The binder course can increase oxidation
Adhesion between layer and skin of paint.
In summary, the bonnet preparation method that the embodiment of the present application provides, can sequentially form bumps in rear exterior surface
Structure, at least one layer of oxide layer, one layer or two layers or multilayer skin of paint, concaveconvex structure and oxide layer can increase and skin of paint
Adhesion, skin of paint forms the outermost layer in rear exterior surface, its highlight surface, penetrating so that its surface is smooth, is not easy
Viscous fingerprint, exterior surface is clean and tidy after can keeping.
It will be understood by those skilled in the art that the structure of the electronic equipment 1 shown in Fig. 1 is not formed to electronic equipment 1
Restriction.Electronic equipment 1 can be included than illustrating more or less parts, either combine some parts or different portions
Part is arranged.Electronic equipment 1 can also include memory, bluetooth module etc., will not be repeated here.
Method for producing shell, housing and the electronic equipment provided above the embodiment of the present application is described in detail, this
Apply specific case in text to be set forth the principle and embodiment of the application, the explanation of above example is only intended to
Help understands the application.Meanwhile for those skilled in the art, according to the thought of the application, in embodiment and answer
With there will be changes in scope, in summary, this specification content should not be construed as the limitation to the application.
Claims (17)
1. a kind of method for producing shell, the housing is applied in electronic equipment, it is characterised in that the method for producing shell bag
Include:
One housing is provided;
The outer surface of the housing is processed by shot blasting;
Blasting treatment is carried out to the housing outer surface after the polishing;
Monochromatic oxidation processes are carried out to the housing outer surface after the blasting treatment;
Spray painting at least once is carried out to the housing outer surface after the monochromatic oxidation processes to handle, and is formed in the housing outer surface
At least one layer of skin of paint.
2. method for producing shell according to claim 1, it is characterised in that the shell to after the monochromatic oxidation processes
External surface carries out the step of spray painting processing at least once, specifically includes:
Once spray painting is carried out to the housing outer surface after the monochromatic oxidation processes to handle, and one layer is formed in the housing outer surface
Skin of paint.
3. method for producing shell according to claim 2, it is characterised in that the shell to after the monochromatic oxidation processes
After external surface carries out the step of once spray painting processing, the method for producing shell also includes:
Housing outer surface after handling the once spray painting carries out once baking and handled, and one layer is formed in the housing outer surface
Skin of paint.
4. method for producing shell according to claim 1, it is characterised in that the shell to after the monochromatic oxidation processes
External surface carries out the step of spray painting processing at least once, specifically includes:
The processing of spray painting twice is carried out to the housing outer surface after the monochromatic oxidation processes, is formed two layers in the housing outer surface
Skin of paint.
5. method for producing shell according to claim 4, it is characterised in that the shell to after the monochromatic oxidation processes
External surface is carried out the step of spray painting processing twice, including:
First time spray painting processing is carried out to the housing outer surface after the monochromatic oxidation processes;
Housing outer surface after handling the first time spray painting carries out first time baking processing, and first is formed in housing outer surface
Skin of paint;
Housing outer surface after handling the first time baking carries out second of spray painting processing;
Housing outer surface after handling second of spray painting carries out second of baking processing, and second is formed in housing outer surface
Skin of paint, second skin of paint are formed on first skin of paint.
6. method for producing shell according to claim 5, it is characterised in that the thickness of second skin of paint is more than described
The thickness of first skin of paint.
7. method for producing shell according to claim 5, it is characterised in that the shell to after the monochromatic oxidation processes
External surface carries out the step of spray painting processing for the first time, specifically includes:
To the housing outer surface spraying layer of transparent paint after the monochromatic oxidation processes.
8. method for producing shell according to claim 5, it is characterised in that after the processing to the first time baking
Housing outer surface carries out the step of second of spray painting processing, specifically includes:
Housing outer surface spraying layer of transparent paint after handling the first time baking.
9. according to the method for producing shell described in any one of claim 1 to 8, it is characterised in that described to the outer of the housing
Before the step of surface is processed by shot blasting, the method for producing shell also includes:
Grinding process is carried out to the outer surface of the housing;
The step of outer surface to the housing is processed by shot blasting specifically includes:
Housing outer surface after the grinding process is processed by shot blasting.
10. according to the method for producing shell described in any one of claim 1 to 8, it is characterised in that after the blasting treatment
Housing outer surface carries out the step of monochromatic oxidation processes, specifically includes:
Oxidation processes are carried out to the housing outer surface after blasting treatment;
Coloring treatment is carried out to the housing outer surface after oxidation processes.
11. a kind of housing, applied in electronic equipment, it is characterised in that the housing is used as any in claim 1 to 11
The item method for producing shell is formed.
12. a kind of housing, applied in electronic equipment, it is characterised in that the housing includes the inner surface that is oppositely arranged and outer
Surface, the housing include concaveconvex structure, oxide layer and the skin of paint formed on the outer surface, and the oxide layer is formed
On the concaveconvex structure, the skin of paint is formed in the oxide layer.
13. housing according to claim 12, it is characterised in that the skin of paint includes the first skin of paint and the second paint
Layer, first skin of paint are formed in the oxide layer, and second skin of paint is formed on first skin of paint.
14. housing according to claim 13, it is characterised in that first skin of paint and the second skin of paint at least one
The transparent setting of layer.
15. housing according to claim 13, it is characterised in that the thickness of second skin of paint is more than the described first oil
The thickness of enamelled coating.
16. housing according to claim 12, it is characterised in that the transparent setting of skin of paint.
17. a kind of electronic equipment, it is characterised in that including housing, the housing is such as any one of claim 11 to 16 institute
The housing stated.
Priority Applications (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201710916720.6A CN107740164A (en) | 2017-09-29 | 2017-09-29 | Method for producing shell, housing and electronic equipment |
PCT/CN2018/098107 WO2019062321A1 (en) | 2017-09-29 | 2018-08-01 | Housing manufacturing method, housing and electronic device |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201710916720.6A CN107740164A (en) | 2017-09-29 | 2017-09-29 | Method for producing shell, housing and electronic equipment |
Publications (1)
Publication Number | Publication Date |
---|---|
CN107740164A true CN107740164A (en) | 2018-02-27 |
Family
ID=61236501
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201710916720.6A Pending CN107740164A (en) | 2017-09-29 | 2017-09-29 | Method for producing shell, housing and electronic equipment |
Country Status (2)
Country | Link |
---|---|
CN (1) | CN107740164A (en) |
WO (1) | WO2019062321A1 (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN109015215A (en) * | 2018-09-06 | 2018-12-18 | 航嘉电器(合肥)有限公司 | A kind of processing method of housing of TV set pattern |
WO2019062322A1 (en) * | 2017-09-29 | 2019-04-04 | Oppo广东移动通信有限公司 | Housing manufacturing method, housing and electronic device |
WO2019062321A1 (en) * | 2017-09-29 | 2019-04-04 | Oppo广东移动通信有限公司 | Housing manufacturing method, housing and electronic device |
Citations (14)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101498021A (en) * | 2009-01-15 | 2009-08-05 | 浙江名琦机电制造有限公司 | Surface treating method for tap |
CN101665969A (en) * | 2008-09-03 | 2010-03-10 | 深圳富泰宏精密工业有限公司 | Method for processing anode of aluminum or aluminum alloy surface |
CN103297565A (en) * | 2012-02-24 | 2013-09-11 | 比亚迪股份有限公司 | Mobile phone shell and preparation method thereof |
CN105154953A (en) * | 2015-09-25 | 2015-12-16 | 广东欧珀移动通信有限公司 | Method for processing surface of metal battery cover of mobile phone |
CN105177669A (en) * | 2015-09-29 | 2015-12-23 | 广东欧珀移动通信有限公司 | Surface treatment method for aluminum alloy shell |
CN105220161A (en) * | 2015-11-19 | 2016-01-06 | 东莞金稞电子科技有限公司 | Stainless process of surface treatment |
CN105297105A (en) * | 2015-11-17 | 2016-02-03 | 惠州市泽宏科技有限公司 | Ceramic anodizing process for frosted glaze of aluminum alloy |
CN105350050A (en) * | 2015-11-19 | 2016-02-24 | 东莞金稞电子科技有限公司 | Surface treatment technology for plastic product |
CN105543928A (en) * | 2016-01-26 | 2016-05-04 | 广东欧珀移动通信有限公司 | Metal or alloy shell and manufacturing method thereof |
CN105543933A (en) * | 2015-12-17 | 2016-05-04 | 广东欧珀移动通信有限公司 | 3D effect surface treatment process |
CN105970269A (en) * | 2016-05-23 | 2016-09-28 | 沈阳富创精密设备有限公司 | Sand blasting oxalic acid anode process |
CN106222664A (en) * | 2016-08-16 | 2016-12-14 | 广东欧珀移动通信有限公司 | The surface treatment method of a kind of Al alloy parts, Al-alloy casing and mobile terminal |
CN106637342A (en) * | 2016-09-30 | 2017-05-10 | 乐视控股(北京)有限公司 | Treatment method for aluminum alloy materials |
CN107159541A (en) * | 2017-04-26 | 2017-09-15 | 句容市江电电器机械有限公司 | A kind of surface of workpiece processing method |
Family Cites Families (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
KR100575299B1 (en) * | 2003-07-01 | 2006-04-28 | 광성전자(주) | method for making outer decoration product with anodized and tilted glossy faces and the product made by the same |
US20160153109A1 (en) * | 2014-11-28 | 2016-06-02 | Htc Corporation | Casing of electronic device and manufacturing method thereof |
CN105578822B (en) * | 2016-02-01 | 2019-02-22 | Oppo广东移动通信有限公司 | Electronic product casing and preparation method thereof |
CN105792578B (en) * | 2016-04-30 | 2019-07-26 | 维沃移动通信有限公司 | The method of surface finish and electronic equipment of shell |
CN106498469A (en) * | 2016-09-30 | 2017-03-15 | 北京小米移动软件有限公司 | The manufacture method of metal-back, metal-back and terminal |
CN107708355B (en) * | 2017-09-29 | 2020-04-10 | Oppo广东移动通信有限公司 | Shell manufacturing method, shell and electronic equipment |
CN107740164A (en) * | 2017-09-29 | 2018-02-27 | 广东欧珀移动通信有限公司 | Method for producing shell, housing and electronic equipment |
-
2017
- 2017-09-29 CN CN201710916720.6A patent/CN107740164A/en active Pending
-
2018
- 2018-08-01 WO PCT/CN2018/098107 patent/WO2019062321A1/en active Application Filing
Patent Citations (14)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101665969A (en) * | 2008-09-03 | 2010-03-10 | 深圳富泰宏精密工业有限公司 | Method for processing anode of aluminum or aluminum alloy surface |
CN101498021A (en) * | 2009-01-15 | 2009-08-05 | 浙江名琦机电制造有限公司 | Surface treating method for tap |
CN103297565A (en) * | 2012-02-24 | 2013-09-11 | 比亚迪股份有限公司 | Mobile phone shell and preparation method thereof |
CN105154953A (en) * | 2015-09-25 | 2015-12-16 | 广东欧珀移动通信有限公司 | Method for processing surface of metal battery cover of mobile phone |
CN105177669A (en) * | 2015-09-29 | 2015-12-23 | 广东欧珀移动通信有限公司 | Surface treatment method for aluminum alloy shell |
CN105297105A (en) * | 2015-11-17 | 2016-02-03 | 惠州市泽宏科技有限公司 | Ceramic anodizing process for frosted glaze of aluminum alloy |
CN105220161A (en) * | 2015-11-19 | 2016-01-06 | 东莞金稞电子科技有限公司 | Stainless process of surface treatment |
CN105350050A (en) * | 2015-11-19 | 2016-02-24 | 东莞金稞电子科技有限公司 | Surface treatment technology for plastic product |
CN105543933A (en) * | 2015-12-17 | 2016-05-04 | 广东欧珀移动通信有限公司 | 3D effect surface treatment process |
CN105543928A (en) * | 2016-01-26 | 2016-05-04 | 广东欧珀移动通信有限公司 | Metal or alloy shell and manufacturing method thereof |
CN105970269A (en) * | 2016-05-23 | 2016-09-28 | 沈阳富创精密设备有限公司 | Sand blasting oxalic acid anode process |
CN106222664A (en) * | 2016-08-16 | 2016-12-14 | 广东欧珀移动通信有限公司 | The surface treatment method of a kind of Al alloy parts, Al-alloy casing and mobile terminal |
CN106637342A (en) * | 2016-09-30 | 2017-05-10 | 乐视控股(北京)有限公司 | Treatment method for aluminum alloy materials |
CN107159541A (en) * | 2017-04-26 | 2017-09-15 | 句容市江电电器机械有限公司 | A kind of surface of workpiece processing method |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2019062322A1 (en) * | 2017-09-29 | 2019-04-04 | Oppo广东移动通信有限公司 | Housing manufacturing method, housing and electronic device |
WO2019062321A1 (en) * | 2017-09-29 | 2019-04-04 | Oppo广东移动通信有限公司 | Housing manufacturing method, housing and electronic device |
CN109015215A (en) * | 2018-09-06 | 2018-12-18 | 航嘉电器(合肥)有限公司 | A kind of processing method of housing of TV set pattern |
Also Published As
Publication number | Publication date |
---|---|
WO2019062321A1 (en) | 2019-04-04 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN107911964A (en) | Method for producing shell, housing and electronic equipment | |
CN107683047A (en) | Method for producing shell, casing substrate, housing and electronic equipment | |
CN107864581A (en) | Method for producing shell, housing and electronic equipment | |
CN107645866A (en) | Method for producing shell, housing and electronic equipment | |
CN107740164A (en) | Method for producing shell, housing and electronic equipment | |
CN107716253A (en) | Method for producing shell, housing and electronic equipment | |
CN107708355A (en) | Method for producing shell, housing and electronic equipment | |
CN107708352A (en) | Method for producing shell, housing and electronic equipment | |
CN107734884A (en) | Method for producing shell, housing and electronic equipment | |
CN107734885A (en) | Method for producing shell, housing and electronic equipment | |
CN107744932A (en) | Method for producing shell, housing and electronic equipment | |
CN107708356A (en) | Method for producing shell, housing and electronic equipment | |
CN107670925A (en) | Method for producing shell, housing and electronic equipment | |
CN107683044A (en) | Method for producing shell, housing and electronic equipment | |
CN107708363A (en) | Method for producing shell, housing and electronic equipment | |
CN107896447A (en) | Method for producing shell, housing and electronic equipment | |
CN107683037A (en) | Method for producing shell, housing and electronic equipment | |
CN107734892A (en) | Method for producing shell, housing and electronic equipment | |
CN107890977A (en) | Method for producing shell, housing and electronic equipment | |
CN107734891A (en) | Method for producing shell, housing and electronic equipment | |
CN107716251A (en) | Method for producing shell, housing and electronic equipment | |
CN107889391A (en) | Method for producing shell, housing and electronic equipment | |
CN107708351A (en) | Method for producing shell, housing and electronic equipment | |
CN107899920A (en) | Method for producing shell, housing and electronic equipment | |
CN107708364A (en) | Method for producing shell, housing and electronic equipment |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PB01 | Publication | ||
PB01 | Publication | ||
SE01 | Entry into force of request for substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20180227 |